At least 145 records · Page 8

Understanding Laser Powder Bed Fusion Surface Roughness

Abstract Surface roughness is a well-known consequence of additive manufacturing methods, particularly powder bed fusion processes. To properly design parts for additive manufacturing, a comprehensive understanding of the inherent roughness is necessary. While many researchers have measured different surface roughness resultant from a variety of parameters in the laser powder bed fusion process, few have succeeded in determining causal relationships due to the large number of variables at play. To assist the community in understanding the roughness in laser powder bed fusion processes, this study explored several studies from the literature to identify common trends and discrepancies amongst roughness data. Then, an experimental study was carried out to explore the influence of certain process parameters on surface roughness. Through these comparisons, certain local and global roughness trends have been identified and discussed, as well as a new framework for considering the effect of process parameters on surface roughness.

Engineering↗

Texture development in magnetostrictive Fe-Ga alloys processed by laser powder bed fusion

Iron-gallium (Fe-Ga, Galfenol) alloys are promising magnetostrictive materials for actuators, sensors, and energy harvesting, but their performance is highly sensitive to microstructure and texture. Additive manufacturing by laser powder bed fusion (LPBF) offers a pathway to engineer texture and integrate functional materials into complex geometries. Here, we fabricate Fe-Ga alloys (Fe 82.2 Ga 17.8 ) by LPBF of gas-atomized powders and systematically optimize laser power and scan speed to maximize density and control texture. Nearly full-density parts (up to 99.6 %) are achieved within a narrow processing window. Electron backscatter diffraction (EBSD) reveals a strong <100> fiber texture aligned with the build direction and columnar grains up to 1 mm long. Magnetostriction measurements show saturation magnetostriction of 190 ppm in the build direction. Correlating texture data with macroscopic magnetostriction, we estimate intrinsic magnetostriction constants (λ 100 = 228 ppm, λ 111 = 12 ppm), closely matching single crystal-derived values. These results demonstrate the critical interplay between processing, texture, and functional performance in additively manufactured Fe-Ga alloys and establish LPBF as a viable route for high-performance magnetostrictive materials.

Additive manufacturing↗

Mitigating keyhole pore formation by nanoparticles during laser powder bed fusion additive manufacturing

Keyhole pore formation is one of the most detrimental subsurface defects in the laser metal additive manufacturing process. However, effective ways to mitigate keyhole pore formation beyond tuning laser processing conditions during keyhole mode laser melting are still lacking. Here we report a novel approach to mitigate keyhole pore formation during laser powder bed fusion (LPBF) process by using stable nanoparticles. The critical keyhole depth for keyhole pore generation (i.e., the largest keyhole depth without keyhole pore formation) during LPBF of Al6061 increases from 246 µm to 454 µm (85% increase) after adding TiC nanoparticles. In-depth x-ray imaging studies and thermo-fluid dynamics simulation enable us to identify that two mechanisms work together to mitigate keyhole pore generation: (1) adding nanoparticles prevents the keyhole from collapsing by increasing the liquid viscosity to impede the protrusion development; (2) adding nanoparticles slows down the keyhole pore movement by increasing the liquid viscosity, resulting in the recapturing of the pore by the keyhole. We further demonstrate that adding TiC nanoparticles can also eliminate the keyhole fluctuation induced keyhole pore during LPBF of Al6061. Our research provides a potential way to mitigate keyhole pore formation for defect lean metal additive manufacturing.

36 MATERIALS SCIENCE↗

Formation of functionally graded steel by laser powder bed fusion via in-situ carbon doping

Additive Manufacturing (AM) enables functional integration by combining multiple components into a single part to shorten assembly time, reduce weight, and improve performance. Laser Powder Bed Fusion (LPBF) is an important AM method due to excellent spatial resolution, surface finish, and material properties without the need for extensive post-processing. Functional integration could be enhanced by spatial tuning of properties, but LPBF cannot readily vary material composition. Here, this paper addresses a method to add spatial composition control by printing small quantities of dopants via liquid carrier prior to laser fusion. The impact of carbon black suspension added to select regions of a Stainless Steel 316 L powder bed on melt pool dimension, hardness, and porosity is reported. The distribution of the carbon between the doped and plain layers and the resulting spatial variation in hardness is measured. Optical microscopy and composition analysis show that the carbon dispersed uniformly within the layer of deposition and diffused as little as 50 μm in the build direction. Keyhole conditions dramatically increase the inter-layer transport of the dopant. The added carbon increased hardness by >50 %. Porosity increased in doped regions but remained below 1.5 % for the best processing parameters. These results demonstrate that the composition of LPBF parts could be controlled in 3-dimensions using a dopant that is soluble in the melt pool. Additional work will be required to evaluate different dopant materials and optimize processing conditions for full density, but microalloying with soluble dopants appears to be a plausible solution to enhance functional integration with LPBF.

36 MATERIALS SCIENCE↗

Laser powder bed fusion of Inconel 718 on 316 stainless steel

The joining of Inconel 718 and 316 stainless steel has notable industrial importance. However, traditional arc-welding has many issues. In particular, the formation of the detrimental Nb-rich Laves phase in the heat affected zone can promote crack initiation and propagation, which leads to poor mechanical properties. The small heat input and the rapid solidification of laser powder bed fusion (PBF) has the potential to suppress this problem. Despite the infancy of the multi-material PBF, it is of interest to investigate the relationship among the process parameter, the microstructure at the materials joining point, and the mechanical performance. In this study, we used high-speed x-ray imaging to in-situ monitor the printing of Inconel 718 tracks on a 316H SS substrate via laser powder bed fusion, followed by post-build characterization and testing with SEM, XRD and nanoindentation. We observed that a higher linear energy density resulted in a more diffused interface and a smaller compositional gradient, but as a trade-off, generated more keyhole pores and thermal cracks. Furthermore, we also showed that the built layer exhibited chemical inhomogeneity at two length scales: a tens-of-mu m-scale compositional vortex due to the melt flow, and a sub-mu m-scale Nb-rich dendritic structure due to the non-equilibrium solidification that led to the formation of the Laves phase. It was inferred that the chemical inhomogeneity may benefit the mechanical properties at the interface by providing more interlocking between the two materials and also by limiting the effect of the brittle Laves phase to potentially short range.

36 MATERIALS SCIENCE↗

A LASER POWDER BED FUSION ADDITIVE MANUFACTURING CHARACTERIZATION APPROACH AND DATASET HIGHLIGHTING IMPLICATIONS FOR CROSS-PLATFORM PERFORMANCE CONSISTENCY

Additive Manufacturing (AM) has remained a rapidly growing technology over the past decade, which affords many benefits. However, there is one main hinderance to widespread adoption: Products produced on one Laser Powder Bed Fusion (LPBF) AM system can vary in mechanical performance from those produced on another system. This is due to the fact that while LPBF AM system is producing a product’s shape, it is also producing the product’s material. Due to the complex and dynamic nature of LPBF, items fabricated on one system can be different in terms of dimensions, microstructure and quality compared to items fabricated on a different make or model system. This lack of cross-platform performance consistency makes widespread adoption challenging. This work was created to help understand the variation between different Laser Powder Bed Fusion (LPBF) Additive Manufacturing (AM) systems across different manufacturers, models, and users, and to provide insight into how to ensure product consistency regardless of system selection.

36 MATERIALS SCIENCE↗

Simultaneous optimization of hatching orientations and lattice density distribution for residual warpage reduction in laser powder bed fusion considering layerwise residual stress stacking

The reduction in the residual warpage generated via fabrication is an emerging issue in metals’ laser powder bed fusion additive manufacturing (AM). One solution from a design for additive manufacturing (DfAM) perspective is to arrange a hatching strategy that utilizes the asymmetry of the residual stress generated from a molten pool. Another approach is to arrange the geometry of the parts, such as forming an inner lattice structure to arrange the effective stiffness. In this study, the simultaneous optimization of the laser hatching orientation and lattice density distribution was conducted to minimize the residual warpage in lattice infill structures and confirm their synergetic effect. The mutual effect of each layer was highlighted when considering the mechanical background of the optimal results because an imbalance in the residual stress caused the warpage of the AM parts between the layers. The proposed methodology was validated via experimental verification using a quasi-2D plate, 3D bracket, and 3D connecting-rod design problems. The residual warpage in the quasi-2D study, measured as the edge’s vertical deformation, was reduced from 23.4% to 39.4% compared with the benchmark design. In the 3D studies, the warpage reductions ranged from 13.1% to 20.7%.

36 MATERIALS SCIENCE↗

Microstructure-Based Understanding of High-Temperature Deformation Behaviors in Laser Powder Bed Fusion (LPBF) 316H Stainless Steel

This report presents the results of high-temperature mechanical property testing and microstructural analysis of laser powder bed fusion (LPBF) 316H stainless steel (SS) conducted during Fiscal Year 2025 (FY25) under the U.S. Department of Energy, Office of Nuclear Energy’s Advanced Materials and Manufacturing Technologies (AMMT) program. The study builds upon prior work by expanding the mechanical property test matrix and advancing a microstructure-based mechanistic understanding of LPBF 316H SS performance, with a focus on the solution annealed (SA, 1100°C for 1 hour) materials. High-temperature tension, creep, fatigue, and creep-fatigue tests were performed. Thermal aging studies were conducted. Advanced characterization techniques, including scanning electron microscopy (SEM), scanning transmission electron microscopy (STEM), and high-energy synchrotron X-ray diffraction, were employed to investigate the microstructural evolution during thermal aging and mechanical testing. It was discovered that the as-built (AB) LPBF 316H SS exhibited precipitation kinetics during thermal aging that are 10–100 times faster than its wrought counterpart due to the presence of high densities of preferred nucleation sites, while the precipitation kinetics in SA LPBF 316H was under investigation. The accelerated precipitation of embrittling phases such as sigma phase in LPBF 316H SS compared to its wrought counterpart led to significant impacts on creep ductility. The influence of laser printing parameters and build orientations on fatigue and creep-fatigue performance was observed. In assessing the creep-fatigue performance, it was discovered that the SA LPBF 316H samples failed in less than 200 cycles under 595°C, 0.5% (strain amplitude) with a 60-minute hold time. This work establishes a mechanistic framework for predicting the long-term behavior of LPBF 316H SS, supporting its rapid qualification under the ASME BPVC. The findings contribute to the broader goal of enabling the deployment of advanced materials in next-generation nuclear energy systems. An outlook for FY26 work, including continued aging studies, mechanical testing, and microstructural characterization, is provided.

36 MATERIALS SCIENCE↗

Plasticity and fracture behavior of Inconel 625 manufactured by laser powder bed fusion: Comparison between as-built and stress relieved conditions

In this work, the influence of stress relief on the plasticity and fracture behavior of Inconel 625 fabricated through laser powder bed fusion additive manufacturing (AM) was investigated. The as-built versus stress relieved microstructures were compared, showing similar grain structures but the presence of ~10 vol % δ phase in the stress relieved condition, and no δ phase in the as-built condition. Mechanical tests under plane strain tension were performed on the stress relieved samples, and an anisotropic plasticity model was calibrated and validated using finite element simulations. Uniaxial and notched tension tests were performed on both as-built and stress relieved samples to probe the effect of stress relief on stress state- and direction-dependent fracture behavior. It was found that on average, the fracture strain of the stress relieved samples along the build direction was 30% higher than that along the perpendicular build direction in the stress state range studied, and the stress relief heat treatment resulted in a 45% decrease in fracture strain. The fracture strain in stress relieved samples was more strongly dependent on stress state than in as-built samples.

36 MATERIALS SCIENCE↗

Simulated Microstructures for Laser Powder Bed Fusion Additive Manufacturing Using Myna, AdditiveFOAM, and ExaCA

This dataset provides sample datasets containing voxelized, three-dimensional representations of simulated grain structures and crystallographic orientations that can result from laser powder bed fusion additive manufacturing. The six microstructure files each contain approximately 1 cubic millimeter of material (1 mm x 1 mm cross-section over 26 simulated layers of deposition). Some of the microstructures have columnar grains that extend across nearly the entire simulation domain, while others have more equiaxed or truncated columnar grains. The process conditions to generate these microstructures were from the Peregrine v2023-10 dataset (10.13139/ORNLNCCS/2008021). The codes used are publicly available and released under open-source licenses. Myna (https://github.com/ORNL-MDF/Myna) was used for configuration of the cases from the Peregrine v2023-10 HDF5 dataset and to run the simulation workflow. AdditiveFOAM (https://github.com/ORNL/AdditiveFOAM) was used to simulate the melt pool and generate solidification conditions. And ExaCA (https://github.com/LLNL/ExaCA ) was used to simulate the three-dimensional microstructures.

36 MATERIALS SCIENCE↗

An assessment of spall failure modes in laser powder bed fusion fabricated stainless steel 316L with low-volume intentional porosity

Here, this paper reports on spall failure and damage modes in Laser Powder Bed Fusion fabricated Stainless Steel 316L (SS316L) with intentional levels of low-volume (1–5 vol. %) porosity and pore sizes of 200, 350, and 500 μm. The fabricated specimens were subjected to uniaxial-strain plate-impact loading at ~4.5 GPa, to initiate incipient spall failure. Analysis of velocimetry profiles measured using multi-probe photon-Doppler velocimetry coupled with post-mortem analysis of soft-recovered samples reveals local suppression of spall failure (termed as spall-dominated) as a function of porosity, as the failure mechanism transitions from spall-centered tensile stress dominated to a pore-centered microstructure-dominated damage mode involving void/crack nucleation and growth at pre-existing pores. The critical porosity level where the suppression of spall failure is first observed, as well as the spall location, is dependent on both the volume fraction and the size of the initially fabricated pores. In samples of 500 μm pore size, the suppression of spall failure is observed with as little as 1 vol. % porosity, while samples with smaller pores (200 μm) still experience spall-centered tensile stress dominated failure with higher levels (5 vol. %) of porosity. In the case of pore-centered microstructure-dominated failure, spall damage can occur but the spall plane is shifted toward the rear free surface, or more generally in areas further away from the region with pores. Highly heterogeneous deformation twinning, shear banding, grain rotation, and cracking are observed in the vicinity of pre-existing pores and expected spall failure sites.

36 MATERIALS SCIENCE↗

The role of cellular structure, non-equilibrium eutectic phases and precipitates on quasi-static strengthening mechanisms of as-built AlSi10Mg parts 3D printed via laser powder bed fusion

The quasi-static loading strengthening mechanism in the as-built state of an AlSi10Mg alloy 3D-printed via Laser Powder Bed Fusion (LPBF) was thoroughly identified and quantified using state-of-the-art electron microscopy and synchrotron X-ray diffraction techniques. The yield strength was comprehensively modelled through an in-depth characterization and quantification of the microstructural features as well as their effective volumes for strengthening. In particular, the non-equilibrium eutectic network was characterized with a two-fold structure: cell boundary particles as well as intracellular lamellar/fibrous networks, each consisting of discrete phases exhibiting a thru-thickness compositional gradient, a semi-coherent interface with the matrix and an abundance of crystal defects such as nano-sized sub-grains, microstrains and stacking faults. Further, these altogether made the eutectic phase the most potent contributor to the yield strength accounting for ~30–40% of the estimated value (i.e., cell boundary and eutectic network strengthening combined). Precipitates strengthening was identified as the second most potent mechanism via a shearing process only. Moreover, the presented methodology was able to capture the effect of LPBF processing variables on the individual strengthening contributions, e.g., the effect of a lower laser scanning speed on increasing the cell size as well as the mean precipitate size, which are shown to exhibit opposing impacts on strengthening.

36 MATERIALS SCIENCE↗

Characterization and Rationalization of Microstructural Evolution in GRCop-84 Processed by Laser-Powder Bed Fusion (L-PBF)

In this study, prismatic geometries of GRCop-84 [Cu-8Cr-4Nb (at. pct)] were built with laser-powder bed fusion (L-PBF) process. The samples were sectioned parallel or perpendicular to the build direction and characterized in the as-built and after post-processing with a hot-isostatically pressing (HIP) treatment. The microstructure and phase evolutions were evaluated with optical microscopy, scanning electron microscopy (SEM), electron backscattered diffraction (EBSD), and high-temperature X-ray diffraction (HTXRD) up to 1223 K. The samples in the as-built conditions exhibited predominantly columnar epitaxial and misoriented Cu-FCC grains. The microstructure evolutions are discussed based on locations within the overall build geometry, the dynamics of small melt pool shape and sectioning effects. The above grain structure did not change significantly during post-process HIP treatment. The stability of this FCC grain structure is attributed to the formation of primary stable Cr 2 Nb (Laves phase) during L-PBF, even before the emergence of FCC grains from liquid. The stability of Cr 2 Nb in both as-built and HIPed samples were evaluated using high-temperature X-ray diffraction measurements and compared with that of gas-atomized powder. The significance of these results is discussed with reference to aerospace applications.

36 MATERIALS SCIENCE↗

Characterization of Properties of Laser Powder Bed Fusion 3D-Printed Inconel 718 for Centrifugal Turbomachinery Applications

Here, this paper presents the results of a comprehensive effort to characterize the properties of Inconel 718 produced by a form of laser powder bed fusion (LPBF) additive manufacturing (AM) or 3D-printing, subsequently subjected to hot isostatic pressing (HIP) and heat treatment according to standards F3055-14a and AMS 5663, respectively. Material property data, while broadly available for traditional Inconel 718 presentations (e.g. forgings or castings), is currently lacking for the 3D-printed material. It is expected that while limited in size, the experimental data sets presented provide sufficient information to glean the capability of LPBF Inconel 718. These include: 1) Chemical composition, electron backscatter diffraction (EBSD), and x-ray energy dispersive spectroscopy (XEDS) characterization of 3D-printed material structure; 2) Tensile properties — 0.2% yield stress, ultimate stress, modulus of elasticity, and elongation to failure — based on 108 samples, as functions of temperature and sample print orientation; 3) Creep rupture data including the Larson-Miller parameter, based on 21 samples; and 4) High cycle fatigue data based on 21 samples as a function of temperature. Results are compared to available standards and/or data for forged, cast, and other AM Inconel 718. A key observation of this study, based on the EBSD results, is that while the material appears to approach full recrystallization following heat treatment, there is a detectable fraction of the material that does not fully recrystallize, resulting in a material with mechanical properties (e.g. yield stress, creep rupture) measurably lower than those of forgings, but higher than those of castings.

30 DIRECT ENERGY CONVERSION↗

Data-driven prediction of geometry- and toolpath sequence-dependent intra-layer process conditions variations in laser powder bed fusion

Geometrical features and toolpath sequence are two important factors that cause process condition variations, such as variations in the meltpool temperature or meltpool size, that might lead to undesired material properties in the laser powder bed fusion (LPBF) process. Due to the high dynamics and complex physics of the LPBF process, it is difficult to predict variations in process conditions with simulations alone. Advances in measurement technology and computational technologies open up new possibilities for smart manufacturing. In this paper, a data-driven method to predict intra-layer variations in the processing conditions that source from the toolpath sequence and part geometry is presented. The approach is demonstrated using two-color on-axis pyrometer measurements. Three demonstration cases are presented in which it is demonstrated (1) how the trained predictive model can be used as a filter to ease the interpretation of process variations and discover patterns related to toolpath and part geometry, and (2) how to generate predictions that can be used for feedforward control, i.e., for adjusting laser power or scanning speed along the toolpath using a meltpool temperature prediction model generated based on on-axis measurements. Results show that the developed prediction model is able to meaningfully predict process variations resulted from toolpath sequence and geometry. Predictions are aligned with the results from the related work of others and for the case of 180° laser path turnarounds in our high-speed X-ray imaging experiments. In conclusion, the potential issues related to the current maturity status of the process and measuring equipment that could in practice affect the performance of the proposed solutions are also discussed.

42 ENGINEERING↗

Leveraging Solute Segregation in Laser Powder Bed Fusion to Achieve Superior Strength and Ductility Via Single-Step Heat Treatment in Ti-Free Grade 300 Maraging Steel

Maraging steels are Fe-Ni precipitation-strengthened steels that can be heat treated for achieving high strength with an accompanying loss in ductility, a trend common to most metals. Here, we show that the segregation of Ni during laser powder bed fusion, commonly considered a nuisance that is dealt with via solutionizing heat treatments, can be leveraged via direct aging to achieve higher strength and ductility simultaneously, compared to a solutionized and aged condition. The high dislocation density in combination with solute segregation in the as-fabricated material promotes the precipitation of Mo-rich intermetallic phases that are responsible for the high strength, and the Ni segregated regions facilitate austenite reversion during direct aging. The reverted austenite enhances the elongation via transformation-induced plasticity. While overcoming the strength–ductility conundrum, direct aging can significantly reduce the energy and emissions associated with multistep heat treatments, especially in the global tool and die industry, while laser powder bed fusion (LPBF) can enable tools with integrated cooling channels for increased downstream production efficiency.

36 MATERIALS SCIENCE↗

A Co-Registered In-Situ and Ex-Situ Tensile Properties Dataset from a Laser Powder Bed Fusion Additive Manufacturing Process (Peregrine v2023-11)

This release contains a co-registered in-situ and ex-situ Peregrine dataset from five Concept Laser M2 Laser Powder Bed Fusion (L-PBF) stainless steel 316L builds containing 6,299 SS-J3 individually tracked tensile coupons. These data were collected at the Manufacturing Demonstration Facility (MDF) located at Oak Ridge National Laboratory (ORNL). The dataset includes layer-wise visible-light in-situ imaging data, the laser scan paths and parameters, in-situ temporal sensor data, room-temperature static tensile test results, and the target part geometries. Additionally, anomaly detections produced by a modified Dynamic Segmentation Convolutional Neural Network (DSCNN) are provided.

36 MATERIALS SCIENCE↗

A Co-Registered In-Situ and Ex-Situ Dataset from a Laser Powder Bed Fusion Additive Manufacturing Process (Peregrine v2023-10)

This release contains a co-registered in-situ and ex-situ Peregrine dataset from a single Concept Laser M2 Laser Powder Bed Fusion (L-PBF) stainless steel 316L build. These data were collected at the Manufacturing Demonstration Facility (MDF) located at Oak Ridge National Laboratory (ORNL). The dataset includes layer-wise visible-light in-situ imaging data, the laser scan paths and parameters, in-situ temporal sensor data, X-Ray Computed Tomography (X-CT) scans, pycnometry and tensile test results, etched micrographs from selected locations, and the target part geometries. Additionally, anomaly detections produced by a modified Dynamic Segmentation Convolutional Neural Network (DSCNN) are provided.

36 MATERIALS SCIENCE↗