Search NASA⌕ Search

SEARCH · Search NASA

Results for “solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,459 records · Page 81

Microstructural evaluation of thin-wall sections of 316L stainless steel produced by laser powder-bed fusion processing

Laser powder bed fusion (LBPF) is a method of additive manufacturing (AM) that offers a means to fabricate complex components with features which rely upon the mechanical integrity of thin-wall (less than 0.4 mm thick) structures. The microstructure of a 316L AM thin wall is investigated as metallographically prepared from a cylindrical shell. Optimization is pursued through mechanical polishing and chemical etching to minimize the effects of surface roughness. Microanalysis measurements of the sectioned component reveal the sample has high microstructural fidelity, uniform composition and phase content across grain as well as powder layer boundaries within the thin wall. The results are attributed to a uniform thermal gradient at the part scale during rapid solidification.

36 MATERIALS SCIENCE↗

Additive Manufactured Composite Phase-Change Material for Thermal Energy Storage Applications

Phase-change materials play a critical role in industrial energy storage applications to drive efficiency improvements, thermal energy management, and carbon emissions reductions. Recently, it has been shown that rapid solidification of alloys with metastable immiscibility in the liquid phase has the potential to form unique microstructures in which a low-melting phase is uniformly distributed in a high-melting matrix. This feature can be exploited using additive manufacturing to produce components with complex geometries containing such unique phase-change microstructures. Phase-field simulations utilizing high-performance computing were used to provide a detailed description of the evolution of the active phase during service in terms of their morphology and composition in different polycrystalline matrix grain morphologies that are typically produced during additive manufacturing. Phase field simulations were performed using, MEUMAPPS-SL (Microstructure Evolution Using Massively Parallel Phase-field Simulations – Solid Liquid) code that was developed in-house by the Oak Ridge National Laboratory. The simulations utilized the capabilities of the Kestrel supercomputer at the National Renewable Energy Laboratory. The simulation results were compared with experimental results generated at Siemens Energy, Inc. The results indicate that the kinetics of liquid spreading along grain boundaries is largely determined by the mobility of the triple line along the intersection of the grain boundary liquid and the grain boundary plane.

25 ENERGY STORAGE↗

Laser Powder Directed Energy Deposition of Steels for Nuclear Applications

This comprehensive investigation examines the structure–property relationships in two nuclear alloy systems—Alloy 709 (A709) austenitic stainless steel and Grade 92 (G-92) ferritic/martensitic (F/M) steel—manufactured via directed energy deposition (DED) for sodium-cooled fast reactor applications. This study establishes the fundamental mechanisms for controlling microstructures for optimizing the mechanical performance of additively manufactured nuclear materials through systematic heat treatment optimization and multiscale characterization. As-deposited A709 steel develops a complex multiscale strengthening architecture consisting of a fine cellular solidification structure with diameter of 2-3 µm within10–50 µm grains, elevated dislocation densities from rapid thermal cycling, and grain boundary precipitates that activate concurrent Hall–Petch, dislocation, and precipitation hardening mechanisms to achieve exceptional properties [yield strength (YS): 603 MPa, ultimate tensile strength (UTS): 844 MPa, Vickers hardness: 220 HV] that achieve a 44% superior strength compared to that of the wrought material. Heat treatments produce different results. Solution annealing (SA) dissolves the cellular structure and reduces the hardness to 190 HV. Precipitation treatment (PT) keeps the cellular structure but adds carbides, allowing the hardness to reach 205 HV. The best approach combines both treatments (SA+PT) and creates uniform precipitate distributions with M 23 C 6 carbides at the grain boundaries and MX carbonitrides in the matrix, achieving a hardness of 195 HV. However, directional differences persist, with a 12%–15% strength variation between orientations due to the inherited layered microstructural architecture that survives aggressive heat treatment. While tensile testing at 550°C demonstrates 40%–50% thermal softening with dynamic strain aging, DED A709 steel still maintains a 71% higher YS than that of the wrought material. Ion irradiation studies (100–400 dpa) of DED A709 steel reveal progressive radiation damage with increasing void density and radiation-induced segregation causing nickel enrichment and chromium depletion, which will ultimately compromise mechanical properties. As-deposited G-92 exhibits exceptional strength (UTS: 1650–1700 MPa, 430 HV) through a complex microstructure containing both ferrite and martensite phases, a high geometrically necessary dislocation (GND) density (17.04×10 14 /m 2 ), and fine carbides. Heat treatments create distinct changes. Normalizing produces fresh martensite with the highest hardness (460 HV) and an increased GND density (20.23×10 14 /m 2 ). Tempering develops dual precipitation systems and reduces the hardness to 290 HV. The optimal approach uses sequential normalizing plus tempering, achieving balanced properties with the lowest hardness (250 HV) and a reduced GND density (11.01×10 14 /m 2 ). A processing-dependent anisotropy is observed: horizontal specimens achieve superior ductile behavior, while vertical specimens exhibit brittle failure. A tempering heat treatment successfully mitigates this anisotropic behavior by transforming the hard martensitic as-deposited structure into tempered martensite enabling both horizontal and vertical specimens to exhibit similar stress–strain characteristics with visible necking behavior. Remarkably, testing at 550°C reveals a reversal in the anisotropy, where as-deposited specimens achieve near isotropy with superior thermal stability (a 15%–20% strength reduction), while tempered specimens develop an orientation dependence with a 25%–30% strength reduction. Both alloy systems demonstrate that DED processing creates specimens with a superior strength through refined microstructural features, though with distinct strengthening mechanisms—austenitic through cellular structures and precipitates versus F/M through phase transformations and precipitates. Heat treatment optimization requires alloy-specific approaches, with A709 benefiting from controlled precipitation while G-92 requires careful phase transformation control. The results show that DED manufacturing can produce nuclear materials with exceptional performance, but directional effects and temperature-dependent behavior must be carefully considered for reactor component design and qualification.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Degradation science: Integrating modeling and experiments to predict localized corrosion processes (Annual Progress Report)

Additively manufactured (AM) eutectic high-entropy alloys (EHEAs), such as nano-lamellar AlCoCrFeNi 2.1 , have excellent strength, ductility, and wear resistance even at elevated temperatures, but their corrosion behavior in aggressive acids at different length scales remain poorly understood. This work investigates the corrosion behavior of laser powder bed–fused (L-PBF) AlCoCrFeNi 2.1 as a function of annealing temperatures, probing degradation mechanisms from nanoscopic to macroscopic length scales. The alloy is dual phase consisting of a ductile FCC L1 2 phase and a high-strength BCC B2 phase. Rapid solidification during L-PBF produces a far-from-equilibrium nano-lamellar structure with nearly homogeneous elemental distribution, which tends to evolve upon annealing toward Cr/Co/Fe-enriched FCC and Al/Ni-enriched B2. Three conditions were studied: as-printed, 600 °C/5 h, and 1000 °C/1 h, over which B2 lamellae coarsen, lamellar spacing increases, and elemental segregation becomes more prominent. Microstructure and chemistry were characterized by scanning electron microscopy (SEM) and energy-dispersive spectroscopy (EDS), while in-situ electrochemical atomic force microscopy (EC-AFM) was used to link early (<5 h) local dissolution to microstructure after exposure in sulfuric acid. EC-AFM highlights preferential dissolution of the BCC/B2 phase where the surrounding matrix is Cr-depleted and directly quantifies the dissolution rates within individual phases, tracks the transition from early nano-scale attack to partial repassivation, to correlate height differences with current and impedance responses. To monitor longer-term behavior (up to 96 h), ex-situ AFM, SEM, and confocal imaging were combined with conventional bulk electrochemical tests, bridging nanoscale observations to micro/meso-scale damage morphologies. At the meso-scale, the deepest dissolution channels align with the build-direction lamellae and melt-pool boundaries, indicating that printing directionality guides the propagation of these localized corrosion sites. Annealing modifies corrosion by restructuring BCC/FCC phase fractions, lamellar spacing, and Cr/Al segregation, thereby changing the cathode/anode ratio and passive film stability. The results clarify how as-printed and annealed nano-lamellar architectures differ in their susceptibility to selective dissolution; how elemental segregation competes with residual stresses along the build direction. With these insights, future work will use CALPHAD-guided alloy modification to stabilize higher Cr contents in the B2 phase while retaining a dominant FCC+B2/BCC microstructure, with the goal of designing mechanically robust, corrosion-resistant EHEAs for safety-critical applications to leverage the LLNL’s broader national and global security mission.

36 MATERIALS SCIENCE↗

Molten Salt Corrosion Tests of Additively Manufactured Stainless Steel 316H

Molten salt reactors (MSRs) have drawn considerable interest due to their favorable safety features, high thermal efficiency, and compatibility with different fuel cycles. Yet, the success of MSRs hinges critically on the performance of structural materials to be used in these aggressive molten salt environments, where corrosion and material compatibility remain primary challenges to long-term reliability. Additively manufactured (AM) nuclear structural materials prompt the use of novel geometries and compositions to enhance material performance and reduce costs of constructing MSRs. The rapid solidification conditions inherent to AM processing impart distinctive microstructural features, including cellular sub-structures, dislocation densities, residual stress, and oxide inclusions, which can influence material performance in MSR components. While the mechanical properties of AM stainless steels have been widely studied, their corrosion behavior, particularly in molten salt environments, has received far less attention. Addressing these needs, the Advanced Materials and Manufacturing Technologies (AMMT) program provides a framework for systematically evaluating how unique microstructures produced by AM processes influence the performance of these materials in these demanding environments and for developing reproducible testing workflows that can support future code qualification efforts and standards development. Bridging this knowledge gap is essential for assessing the viability of AM alloys in MSRs and informing qualification strategies. A further challenge is the absence of standardized protocols for molten salt corrosion testing. Accordingly, this report provides an account of the corrosion evaluation of AM 316H stainless steel in NaCl 2 -MgCl 2 molten salt at 550 °C, with exposure times of 100 and 500 hours. It documents the experimental procedures implemented under the AMMT program, including salt preparation, exposure protocols, and post-test characterization methods, to establish reproducibility and transparency. Importantly, the study examines AM 316H samples in the as-fabricated condition, directly reflecting the surface state most relevant to engineering applications, and compares their behavior to machine-cut surfaces. Overall, preliminary evaluations have noted that surface conditions (e.g. morphology, contamination, etc.) have a noticeable impact on the corrosion resiliency. The impact of the corrosion is difficult to detect at 100h, unless, in the case of AM 316H, the specimen surface is decontaminated. After 500 h, as-fabricated surfaces of AM and wrought 316H display evidence of general versus preferential corrosion attack, respectively. Both AM and wrought 316H machine-cut surfaces exhibit a continuous Cr depletion zone, evident of general corrosion. While the estimated extent of corrosion appears within the same order of magnitude regardless of the surface condition, it is apparent that more predictable behavior is observed on machine-cut surfaces. Nonetheless, further investigation is necessary to fully elucidate the corrosion mechanism under these conditions.

36 - MATERIALS SCIENCE↗

Microstructural evaluation of thin-wall sections of 316L stainless steel produced by laser powder-bed fusion processing

The synthesis of thin wall sections that are only 0.4 mm thick is achieved with LPBF AM. Sample preparation is optimized using metallographic polishing to produce samples with only 0.3 um rms roughness for scanning electron microanalysis with EBSD and EDS. A fully austenitic 316L phase is found without evidence of secondary phases. Unlike some AM products that can readily evidence composition segregation due to solute rejection as attributable to temperature gradients within the solidification

Jankowski, Alan F. [Sandia National Laboratories (↗

Influence of Powder Characteristics and Processing Methods on Creep Performance of Powder Metallurgy Hot Isostatic Pressed SS316

The U.S. nuclear energy expansion goals are driving the demand for manufacturing routes that can rapidly produce large, complex, near net shape components. Powder metallurgy hot isostatic pressing (PM HIP) is an advanced manufacturing technique that can be economically scaled-up, while alleviating the supply chain challenges that forging and casting face in terms of cost and lead time constraints. This makes PM-HIP a viable technology to aid and accelerate large-scale part manufacturing for nuclear applications. However, large-scale qualification and deployment of this technology require a thorough understanding of the influence of powder feedstock quality, powder handling history, hot isostatic pressing (HIP) parameters, and subsequent heat treatment on microstructural evolution and elevated temperature mechanical performance. The present work focusses on 316 austenitic stainless steel (SS316) which is most commonly used in high temperature environments for nuclear applications Results from this study show that PM HIPed SS316 meets ASME tensile requirements at room temperature and at elevated temperature. However, creep performance of PM-HIPed SS316 remains inferior to its wrought counterpart, demonstrating that tensile performance alone is not a reliable metric for long duration high temperature integrity. Further, this report delineates powder derived microstructural features that govern creep damage, with key evidences pointing to “microstructural inheritance” from gas atomized powder feedstocks. Commercial SS316 powders of varying chemical compositions and recycling histories were studies, and the results showed large differences in elemental segregation, oxide surface layers and secondary phase distributions. Multi-scale characterization revealed segregation of chromium, molybdenum, manganese and silicon at the boundaries and the precipitation of manganese-, silicon-, and molybdenum-oxides. During HIP consolidation, these surface oxides transform into decorated prior particle boundaries (PPBs) and grain boundary inclusions that persist through conventional post-HIP solution annealing treatment. The retained oxides in post-HIP microstructures were found to influence grain growth, precipitation behavior, and ultimately creep cavitation and fracture. Such post-HIP heat treatments are therefore limited by a complex trade-off between grain growth, and oxide coarsening which aggravate creep damage by acting as nucleation sites for cavities. The objective of this work is to establish an integrated processing–structure–property framework for PM-HIP 316 stainless steel by investigating the influence of powder feedstock characteristics in pre- and post-HIP processing as well as to understand the significance of post-HIP heat treatment on microstructural evolution and creep properties. The results from this report emphasize the significance of powder feedstock integrity in improving creep performance of PM-HIPed SS316, by highlight the effect of rapid solidification, elemental segregation, oxide formation and powder recycling on microstructural defect inheritance following HIP consolidation. Rather than considering HIP processing, solution annealing, and mechanical performance independently, this report treats powder production, HIP consolidation, post-HIP thermal processing, and creep deformation as interconnected stages within a continuous metallurgical process. The resulting framework will provide a scientific basis for developing feedstock engineering strategies capable of improving long-term reliability of PM-HIP stainless steels and accelerating their qualification for advanced nuclear applications.

Ajjarapu, Pavan [Oak Ridge National Laboratory (OR↗

SECONDARY WASTE MANAGEMENT STRATEGY FOR EARLY LOW ACTIVITY WASTE TREATMENT

This study evaluates parameters relevant to River Protection Project secondary waste streams generated during Early Low Activity Waste operations and recommends a strategy for secondary waste management that considers groundwater impact, cost, and programmatic risk. The recommended strategy for managing River Protection Project secondary waste is focused on improvements in the Effiuent Treatment Facility. Baseline plans to build a Solidification Treatment Unit adjacent to Effluent Treatment Facility should be enhanced to improve solid waste performance and mitigate corrosion of tanks and piping supporting the Effiuent Treatment Facility evaporator. This approach provides a life-cycle benefit to solid waste performance and reduction of groundwater contaminants.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

RESULTS FOR THE THIRD QUARTER 2007 TANK 50H WAC SLURRY SAMPLE: CHEMICAL AND RADIONUCLIDE CONTAMINANT RESULTS

The Saltstone Facility is designed and permitted to immobilize and dispose of low-level radioactive and hazardous liquid waste (salt solution) remaining from the processing of radioactive material at the Savannah River Site. Low activity wastewater streams from the Effluent Treatment Project (ETP), H-Canyon, and the high level waste (HLW) storage tanks, are stored as a mixture in Tank 50H until it can be pumped to the Saltstone Facility for treatment and disposal. Specific waste acceptance criteria (WAC) must be met for the transfer of low-level aqueous waste from Tank 50H to the Saltstone Facility. Low level waste which meets the WAC can be transferred, stored and treated in the Saltstone Production Facility (SPF) for subsequent disposal as saltstone in the Saltstone Disposal Facility (SDF). Waste Solidification Engineering (WSE) has requested through a Technical Task Request (TTR) that the Savannah River National Laboratory (SRNL) measure the concentrations of chemical and radionuclide contaminants listed in the currently approved Saltstone Waste Acceptance Criteria (WAC). A Task Technical and Quality Assurance Plan and Analytical Study Plan has been written for this request. WAC determinations are needed on a quarterly basis for chemical contaminants and every first and third quarter for radioactive contaminants. This memorandum presents the results for the chemical and radionuclide contaminants in the third quarter, from the samples taken from Tank 50 in September, 2007.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

AMMONIA CONCENTRATION IN SALTSTONE HEADSPACE SUMMARY REPORT

The Saltstone Facility Documented Safety Analysis (DSA) is under revision to accommodate changes in the Composite Lower Flammability Limit (CLFL) from the introduction of Isopar into Tank 50. Saltstone samples were prepared with an 'MCU' type salt solution spiked with ammonia. The ammonia released from the saltstone was captured and analyzed. The ammonia concentration found in the headspace of samples maintained at 95 C and 1 atm was, to 95% confidence, less than or equal to 3.9 mg/L. Tank 50 is fed by several influent streams. The salt solution from Tank 50 is pumped to the salt feed tank (SFT) in the Saltstone Production Facility (SPF). The premix materials cement, slag and fly ash are blended together prior to transfer to the grout mixer. The premix is fed to the grout mixer in the SPF and the salt solution is incorporated into the premix in the grout mixer, yielding saltstone slurry. The saltstone slurry drops into a hopper and then is pumped to the vault. The Saltstone Facility Documented Safety Analysis (DSA) is under revision to accommodate changes in the Composite Lower Flammability Limit (CLFL) from the introduction of Isopar{reg_sign} L into Tank 50. Waste Solidification-Engineering requested that the Savannah River National Laboratory (SRNL) perform testing to characterize the release of ammonia in curing saltstone at 95 C. The test temperature represents the maximum allowable temperature in the Saltstone Disposal Facility (SDF). Ammonia may be present in the salt solution and premix materials, or may be produced by chemical reactions when the premix and salt solution are combined. A final report (SRNS-STI-2008-00120, Rev. 0) will be issued that will cover in more depth the information presented in this report.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Thermodynamic prediction of glass formation tendency, cluster-in-jellium model for metallic glasses, ab initio tight-binding calculations, and new density functional theory development for systems with strong electron correlation

Solidification of liquid is a very rich and complicated field, although there is always a famous homogeneous nucleation theory in a standard physics or materials science text book. Depending on the material and processing condition, liquid may solidify to single crystalline, polycrystalline with different texture, quasi-crystalline, amorphous solid or glass (Glass is a kind of amorphous solid in general, which has short-range and medium-range order). Traditional oxide glass may easily be formed since the covalent directional bonded network is apt to be disturbed. In other words, the energy landcape of the oxide glass is so complicated that system need extremely long time to explore the whole configuration space. On the other hand, metallic liquid usually crystalize upon cooling because of the metallic bonding nature. However, Klement et.al., (1960) reported that Au-Si liquid underwent an amorphous or “glassy” phase transformation with rapid quenching. In recent two decades, bulk metallic glasses have also been found in several multicomponent alloys[Inoue et al., (2002)]. Both thermodynamic factors (e.g., free energy of various competitive phase, interfacial free energy, free energy of local clusters, etc.) and kinetic factors (e.g., long range mass transport, local atomic position rearrangement, etc.) play important roles in the metallic glass formation process. Metallic glass is fundamentally different from nanocrystalline alloys. Metallic glasses have to undergo a nucleation process upon heating in order to crystallize. Thus the short-range and medium-range order of metallic glasses have to be completely different from crystal. Hence a method to calculate the energetics of different local clusters in the undercooled liquid or glasses become important to set up a statistic model to describe metalllic glass formation. Scattering techniques like x-ray and neutron have widely been used to study the structues of metallic glasses. Meanwhile, computer simulation also plays an important role, as it may directly track the movement of every atom. Simulation time is a major limit for molecular dynamics, not only because of “slow” computer speed, but also because of the accumulation error in the numerical treatment of the motion equations. There is also a great concern about the reliability of the emperical potentials if using classical molecular dynamics. Ab initio methods based on density functional theory(DFT) do not have this problem, however, it suffers from small simulation cells and is more demanding computationally. When crystal phase is involved, size effect of the simulation cell is more pronounced since long-range elastic energy would be established. Simulation methods which are more efficient in computation but yet have similar reliability as the ab initio methods, like tight-binding method, are highly desirable. While the complexity of metallic glasses comes from the atomistic level, there is also a large field which deals with the complexity from electronic level. The only “ab initio” method applicable to solid state systems is density functional theory with local density approximation( LDA) or generalized gradient approximation(GGA) for the exchange-correlation energy. It is very successful for simple sp element, where it reaches an high accuracy for determining the surface reconstruction. However, there is a large class of materials with strong electron correlation, where DFT based on LDA or GGA fails in a fundamental way. An “ab initio” method which can generally apply to correlated materials, as LDA for simple sp element, is still to be developed. The thesis is prepared to address some of the above problems.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

RESULTS FOR THE MAY 19, 2010 INADVERTENT TRANSFER TO THE SALTSTONE DISPOSAL FACILITY SLURRY: SAMPLE ANALYTICAL RESULTS

This report details the chemical analysis results for the characterization of the May 19, 2010 inadvertent transfer from the Saltstone Production Facility (SPF) to the Saltstone Disposal Facility (SDF). On May 19, 2010, the Saltstone Processing Facility (SPF) inadvertently transferred approximately 1800 gallons of untreated low-level salt solution from the salt feed tank (SFT) to Cell F of Vault 4. The transfer was identified and during safe configuration shutdown, approximately 70 gallons of SFT material was left in the Saltstone hopper. After the shutdown, the material in the hopper was undisturbed, while the SFT has received approximately 1400 gallons of drain water from the Vault 4 bleed system. The drain water path from Vault 4 to the SFT does not include the hopper (Figure 1); therefore it was determined that the material remaining in the hopper was the most representative sample of the salt solution transferred to the vault. To complete item No.5 of Reference 1, Savannah River National Laboratory (SRNL) was asked to analyze the liquid sample retrieved from the hopper for pH, and metals identified by the Resource Conservation and Recovery Act (RCRA). SRNL prepared a report to complete item No.5 and determine the hazardous nature of the transfer. Waste Solidification Engineering then instructed SRNL to provide a more detailed analysis of the slurried sample to assist in the determination of the portion of Tank 50 waste in the hopper sample.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Real-time phase evolution of Selective Laser Melted (SLM) Inconel 718 with temperature through synchrotron X-rays

Selective laser melting (SLM) is an additive manufacturing process that uses laser scanning to achieve melting and solidification of a metal powder bed. This process, when applied to develop high temperature material systems, holds great promise for more efficient manufacturing of turbine components that withstand extreme temperatures, heat fluxes, and high mechanical stresses associated with engine environments. These extreme operational conditions demand stringent tolerances and an understanding of the material evolution under thermal loading. This work presents a real-time approach to elucidating the evolution of precipitate phases in SLM Inconel 718 (IN718) under high temperatures using high-energy synchrotron x-ray diffraction. Four representative samples (taken along variable build height) were studied in room temperature conditions. Two samples were studied as-processed (samples 1 and 4) and two samples after different thermal treatments (samples 2 and 3). The as-processed samples were found to contain greater amounts of weakening phase, δ. Precipitation hardening of Sample 2 reduced the detectable volume of δ, while also promoting growth of γ00 in the γ matrix. Inversely, solution treatment of Sample 3 produced an overall decrease in precipitate phases. High-temperature, in-situ synchrotron scans during ramp-up, hold, and cool down of two different thermal cycles show the development of precipitate phases. Sample 1 was held at 870°C and subsequently ramped up to 1100°C, during which the high temperature instability of strengthening precipitate, γ00, was seen. γ00 dissolution occurred after 15 minutes at 870°C and was followed by an increase of δ-phase. Sample 4 was held at 800°C and exhibited growth of γ00 after 20 minutes at this temperature. These experiments use in-situ observations to understand the intrinsic thermal effect of the SLM process and the use of heat treatment to manipulate the phase composition of SLM IN718.

Sarley, Brooke A.↗

Toward Process-Based Quality through a Fundamental Understanding of Weld Microstructural Evolution

Here, in this overview paper, the possibility of qualifying welded components by integrating software and hardware tools that are capable of describing physical processes that occur during welding is explored. The existing and emerging tools to define geometrical boundary conditions, process parameters, heat and mass transfer, solidification, solid-state transformation, plastic deformation, distortion, residual stress, and performance of welded components are reviewed. Existing challenges relevant to the fundamental understanding of complex alloying, processing environment, and transients in energy deposition are discussed with reference to microstructure evolution. Finally, approaches to address these challenges were articulated with published case studies relevant to welding and additive manufacturing.

36 MATERIALS SCIENCE↗

Large-Scale Reactive Extrusion Deposition of Sparse Infill Structures with Solid Perimeters

Large-scale additive manufacturing of reactive polymer systems offers significant improvements over thermoplastics through improved mechanical properties, faster deposition rates, and deposition at ambient temperatures. At ambient temperatures, the resin exists as a viscoelastic liquid which require additional additives for improved rigidity and bead stability. These filler-reinforced resins, or yield stress fluids, are soft solid-like materials able to withstand compressive forces from successive layer deposition until curing leads to bead solidification. When bead deposition is unsupported by previous layers, as is the case when bridging a gap, the creep due to gravitational loading can lead to bead instabilities which result in excessive sagging or bead breakage. These bead instabilities are material dependent and susceptible to changes in filler composition and temperature rises due to exothermic reactions. This work implements a design solution for bridging sparse infill patterns in additively manufactured parts which are essential in the reduction of weight. A series of span tests over a range of distances, as multiples of nozzle diameter, were conducted to determine the critical distance where a bead would break. Additional layer depositions determined the number of layers needed to recover from sagging effects. This recovery was essential in the transition of sparse infill to solid infill printing, where solid infill is milled for a smooth surface finish. Without the capability of sparse-solid transition, additively manufactured parts would require further surface treatments such as spray coating, adding to cost and increasing production time. A standard domed-mold geometry is presented to show the success of this printing process.

Hershey, Christopher↗

Processing of Alnico Magnets by Additive Manufacturing

Permanent magnets without rare earth (RE) elements, such as alnico, will improve supply stability and potentially decrease permanent magnet cost, especially for traction drive motors and other increased temperature applications. Commercial alnico magnets with the highest energy product are produced by directional solidification (DS) to achieve a < 001 > columnar grain orientation followed by significant final machining, adding to the high cost. Additive manufacturing (AM) is an effective method to process near net-shape parts with minimal final machining of complex geometries. AM also, has potential for texture/grain orientation control and compositionally graded structures. This report describes fabrication of alnico magnets by AM using both laser engineered net shaping (LENS)/directed energy deposition (DED) and electron beam melting powder bed fusion (EBM/PBF). High pressure gas atomized (HPGA) pre-alloyed alnico powders, with high purity and sphericity, were built into cylindrical and rectangular samples, followed by magnetic annealing (MA) and a full heat treatment (FHT). The magnetic properties of these AM processed specimens were different from their cast and sintered counterparts of the same composition and show a great sensitivity to heat treatment. The AM process parameters used in this developmental study did not yet result in any preferred texture within the alnico AM builds. These findings demonstrate feasibility for near net-shape processing of alnico permanent magnets for use in next generation traction drive motors and other applications requiring increased operating temperatures and/or complex engineered part geometries, especially with further AM process development for texture control.

36 MATERIALS SCIENCE↗

Nanocrystalline Materials: Synthesis, Characterization, Properties, and Applications

Nanostructuring is a commonly employed method of obtaining superior mechanical properties in metals and alloys. Compared to conventional polycrystalline counterparts, nanostructuring can provide remarkable improvements in yield strength, toughness, fatigue life, corrosion resistance, and hardness, which is attributed to the nano grain size. In this review paper, the current state-of-the-art of synthesis methods of nanocrystalline (NC) materials such as rapid solidification, chemical precipitation, chemical vapor deposition, and mechanical alloying, including high-energy ball milling (HEBM) and cryomilling was elucidated. More specifically, the effect of various process parameters on mechanical properties and microstructural features were explained for a broad range of engineering materials. This study also explains the mechanism of grain strengthening using the Hall-Petch relation and illustrates the effects of post-processing on the grain size and subsequently their properties. This review also reports the applications, challenges, and future scope for the NC materials.

36 MATERIALS SCIENCE↗

Effect of Cooling Rate on Nano-Eutectic Formation in Laser Surface Remelted and Rare Earth Modified Hypereutectic Al-20Si Alloys

Laser Surface Remelting (LSR) was applied to arc-melted Al-20Si-0.2Sr, Al-20Si-0.2Ce, and Al-20Si hypereutectic alloys to refine microstructures. Experiments revealed that microstructures in the melt pool varied from fully eutectic to a mixture of Al dendrites and inter-dendritic eutectic. We calculated cooling rates using the Eagar-Tsai model and correlated cooling rates with characteristic microstructures, revealing that a cooling rate on the order of 104 K/s could lead to maximized fully eutectic microstructure morphology. Due to rapid solidification, the Si composition in the LSR eutectic was measured at 18.2 wt.%, higher than the equilibrium eutectic composition of 12.6 wt.%Si. Compared to Al-20Si, Ce addition had no significant effect on the volume fraction of the fully eutectic structure but refined Si fibers to approximately 30 nm in diameter. Sr addition did not further refine the diameter of eutectic Si fibers compared to Al-20Si but increased the volume fraction of the fully eutectic microstructure morphology. The refinement ratio (φ) of the Si fiber diameter from the bottom of the melt pool to the surface for the three alloys was similar, at around 28%. The established correlation between the cooling rate and the size and morphology of the microstructure within the melt pool will enable tailoring of the microstructure in laser-processed as well as deposited alloys for high strength and plasticity.

36 MATERIALS SCIENCE↗