Microstructure and corrosion of CrFeMnV multi-principal element alloy

In this study, a multi-principal element alloy consisting of equiatomic concentrations of Cr, Fe, Mn, and V was produced by arc melting. The combination of X-ray diffraction, scanning electron microscopy and energy-dispersive X-ray spectroscopy indicated that the CrFeMnV MPEA was comprised of a BCC matrix with a dispersion of a secondary phase. Cyclic potentiodynamic polarization tests in 0.6M NaCl revealed high corrosion resistance – superior to that of stainless steel 304L, as evident from high breakdown and repassivation potentials. X-ray photoelectron spectroscopy and time-of-flight secondary ion mass spectrometry provided insight into the formed multi-layer surface film after constant immersion and potentiostatic conditioning.

36 MATERIALS SCIENCE↗

Superior wear resistance of diamond and DLC coatings

As the hardest known material, diamond and its coatings continue to generate significant attention for stringent applications involving extreme tribological conditions. Likewise, diamond-like carbon (DLC, especially the tetragonal amorphous carbon, ta-C) coatings have also maintained a high level interest for numerous industrial applications where efficiency, performance, and reliability are of great importance. Additionally, the strong covalent bonding or sp 3 -hybridizaiton in diamond and ta-C coatings assures high mechanical hardness, stiffness, chemical and thermal stability that make them well-suited for harsh tribological conditions involving high-speeds, loads, and temperatures. In particular, unique chemical and mechanical nature of diamond and ta-C surfaces plays an important role in their unusual friction and wear behaviors. As with all other tribomaterials, both diamond and ta-C coatings strongly interact with the chemical species in their surroundings during sliding and hence produce a chemically passive top surface layer which ultimately determines the extent of friction and wear. Thick micro-crystalline diamond films are most preferred for tooling applications, while thinner nano/ultranano-crysalline diamond films are well-suited for mechanical devices ranging from nano- (such as NEMS) to micro- (MEMS and AFM tips) as well as macro-scale devices including mechanical pump seals. The ta-C coatings have lately become indispensable for a variety of automotive applications and are used in very large volumes in tappets, piston pins, rings, and a variety of gears and bearings, especially in the Asian market. This paper is intended to provide a comprehensive overview of the recent developments in tribology of super-hard diamond and DLC (ta-C) films with a special emphasis on their friction and wear mechanisms that are key to their extraordinary tribological performance under harsh tribological conditions. Finally, based on the results of recent studies, the paper will also attempt to highlight what lies ahead for these films in tribology and other demanding industrial applications.

36 MATERIALS SCIENCE↗

Electrochemical stability and corrosion behavior of Ni-Cr alloy in molten LiCl-KCl salt

This study investigated the electrochemical properties and potential-dependent stability of Cr(II) and Ni(II) in a eutectic LiCl-KCl molten salt at 500 °C under an argon atmosphere using a three-electrode cell configuration with a glassy carbon working electrode, Ag/Ag + reference electrode, and graphite counter electrode. Cyclic voltammetry was employed to characterize the Cr(0)/Cr(II)/Cr(III) and Ni(0)/Ni(II) redox transitions, yielding diffusion coefficients of 0.50 (±0.01) × 10 −5 cm 2 s −1 for Cr(II) and 0.91 (±0.16) × 10 −5 cm 2 s −1 for Ni(II) at 500 °C. The redox stability domains of these species provided insight into the corrosion mechanisms of a Ni-Cr alloy (80–20 wt %) in LiCl-KCl salt. The measured open circuit potential of the alloy corresponded to the range of potentials where the Ni(0) and Cr(II) species are stable, indicating a preferential dissolution of Cr. Immersion testing of the alloy for 336 h confirmed significant Cr depletion (or Ni-enrichment) at the surface layer, corroborating Cr dealloying as the dominant corrosion reaction under open circuit conditions. Additionally, the application of a small anodic overpotential (0.11 V) resulted in selective Cr dissolution while a large anodic overpotential (0.25 V) resulted in co-dissolution of both Cr and Ni. Furthermore, these results demonstrate that the corrosion mechanisms of a Ni-Cr alloy in LiCl-KCl depend upon the applied potential, and thus the redox conditions of the molten salt should be carefully controlled in the design of a redox buffer to mitigate corrosion in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

On the dissolution of a borosilicate glass with the use of isotopic tracing – Insights into the mechanism for the long-term dissolution rate

An understanding of the mechanisms responsible for controlling the long-term corrosion rate of nuclear waste glass is paramount if reliable glass dissolution models are to be used to calculate the controlled release of radionuclides from nuclear waste glass under geologic disposal conditions. Additionally, understanding silicate glass dissolution is also important for natural glasses to understand the role from the dissolution of these glasses has on the composition of natural aquatic systems. Two general mechanisms appear to be responsible for the elemental release from glass to the surrounding biosphere - ion exchange (release principally of alkalis) and matrix dissolution (release of the structural components of the glass). Key unknowns related to these mechanisms are the impact of surface layers on the altered glass and how these layers participate in corrosion. To better understand the impact of these layers on glass corrosion, we made two glasses of the same elemental composition, but with selected elements enriched in specific isotopes, e.g. more 10 B than 11 B. We reacted these glasses for 1 y then the solutions from each were exchanged and the chemistry of the solutions and the solids were followed for another 2 y and in some cases 3 y. This allowed us to follow changes in the glasses with respect to these elements and how these elements were transported through the alteration layers with time and, for at least one element, into the glass. Results from these experiments demonstrate that the release behavior of different elements is strongly dependent on their structural role in the glass (e.g. network formers and modifiers), but, more importantly, the role of water transport and subsequent ion exchange has in the long-term dissolution of the glass studied here. In this article, we highlight the behavior of four elements: lithium, sodium, silicon, and boron. Lithium and sodium, network modifying elements, have similar chemistries. The behavior of Li could be tracked in more detail by following both 6 Li and 7 Li; Li penetrates through the gel layer in both directions without hinderance and into and released from the glass deeper than sodium. Silicon, a network forming element, reacts with the silica-rich alteration layer. Boron, a network forming element, does not accumulate in the gel or the pristine glass and has a very sharp elemental profile between the pristine glass and alteration layer. Boron, lithium, and sodium elemental profiles suggest that there is little if any transport control within the alteration layer. The correlation between the Li and Na profiles and that of a water species suggest that the limiting release is a steady state between the diffusion of a water species and matrix dissolution that results in a low release rate for alkali and this provides a steady driving force for the long-term dissolution of glass.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

High manganese redox variability and manganate predominance in temperate soil profiles as determined by X-ray absorption spectroscopy

Manganese speciation is a key to understanding the fate of contaminants, nutrients, and organic matter in soils. To date, quantification of Mn species in bulk soils has been performed mainly by sequential extraction methods and rarely supported by spectroscopic analysis. In order to obtain quantitative information on the Mn species inventory of soils, we investigated 46 soil horizons (<2-mm fraction, 45.1–2,280 mg/kg Mn) of nine typical Central European soils (Cambisols, Chernozems, Luvisols, Podzol, Stagnosol) by chemical Mn analyses and Mn K-edge X-ray absorption spectroscopy, and related speciation results to major soil properties. Amounts of Mn 2+ , Mn 3+ , and Mn 4+ and the average oxidation state of Mn were evaluated by linear combination fitting (LCF) of X-ray absorption near edge structure (XANES) spectra. Additionally, we used extended X-ray absorption fine structure (EXAFS) spectroscopy to identify and quantify major Mn species. For this, EXAFS spectra of 20 organic and mineral soil samples from five soils (Cambisols, Chernozem, Luvisol) were analyzed by LCF and shell fitting. XANES analyses revealed a high Mn redox variability in organic surface layers, with Mn 2+ being most abundant (≤100%, $\overline{x}$ = 54%), followed by Mn 3+ (≤80%, $\overline{x}$ = 32%) and Mn 4+ (≤55%, $\overline{x}$ = 14%). Mineral soil horizons contained significantly less Mn 2+ (≤56%, $\overline{x}$ = 23%), about equal quantities of Mn 3+ (≤68%, $\overline{x}$ = 31%), and were enriched in Mn 4+ (≤89%, $\overline{x}$ = 46%). EXAFS analyses implied the presence of six major Mn species groups: manganates, organically complexed Mn, Mn(III) oxyhydroxides, silicate-bound Mn, Mn oxides without tunnel- or layer structure, and physisorbed Mn. In litter horizons, Mn was mainly present in organic complexes (58–91%, $\overline{x}$ = 78%) and as physisorbed Mn (≤15%), but individual horizons also comprised manganates, Mn(III) oxyhydroxides, and silicate-bound Mn. Manganates, likely mixtures of phyllomanganates with hexagonal layer symmetry and tectomanganates, dominated in all mineral soil horizons (37–94%, $\overline{x}$ = 67%). Correlation analysis showed that manganates dissolve completely during dithionite-citrate and acid ammonium oxalate extractions, and suggested that Mn 4+ -rich manganates preferentially form under less acidic soil conditions, partly by oxidation of organically complexed Mn(II), and that they are enriched in the soil clay fraction. Mineral soil horizons also contained minor quantities of organically complexed Mn (≤39%, $\overline{x}$ = 11%), silicate-bound Mn (≤30%, $\overline{x}$ = 8%), Mn(III) oxyhydroxides (≤37%, $\overline{x}$ = 7%), Mn oxides without tunnel- or layer structure (≤18%, $\overline{x}$ = 5%), and physisorbed Mn (≤14%, $\overline{x}$ <1%). The detection of Mn(III) oxyhydroxides such as feitknechtite (β-MnOOH) or groutite (α-MnOOH) as well as the spinel hausmannite (Mn 3 O 4 ) in acidic soils is remarkable, since their formation is normally linked to neutral or alkaline pH conditions. Minor contributions of silicate-bound Mn indicate the release of Mn from primary minerals already at early stages of soil formation, and low concentrations of physisorbed Mn suggest that exchangeable Mn is rapidly converted into manganates in oxic soils. In conclusion, the predominance of manganates in mineral soils has far-reaching implications for the functioning of soils and biogeochemical element cycles, as these minerals play an important role in metal binding, plant nutrition, and redox-related processes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantifying spatial and vertical variations in soil C:N relationships in permafrost-affected landscapes

Permafrost regions are experiencing rapid changes that affect carbon (C) and nitrogen (N) cycles, with implications for vegetation dynamics and gas exchanges with the atmosphere. Soil C:N ratio is a key indicator of organic matter quality, yet spatial estimates of N stocks and C:N ratios lag behind those for C. We used quantile regression forests to compare direct and indirect digital soil mapping approaches for predicting soil C:N ratios at 0–30, 30–60, and 60–100 cm depths across a latitudinal transect in Alaska. The indirect approach – deriving C:N from separately predicted C and N stocks – outperformed direct mapping for the surface layer (0–30 cm), while direct mapping was marginally better at greater depths. However, prediction accuracy decreased with depth for both methods. Temperature and topography were the most important predictors. Both approaches overestimated low and underestimated high C:N ratios, with direct mapping showing greater bias. Our results underscore the challenges of modeling C:N ratios in heterogeneous, data-sparse permafrost soils, but also suggest that indirect mapping holds promise if supported by more extensive datasets.

54 ENVIRONMENTAL SCIENCES↗

Hydroxide melt induced corrosion of Ni at elevated temperatures under steam electrolysis conditions

Molten alkali electrolyte based high temperature water electrolysis (HTWE) process offers an efficient pathway to integrate renewable energy resources for large scale and economic hydrogen production. Long term and stable operation of these systems require an in-depth understanding of materials stability under anodic and cathodic exposure conditions of the cell and cell stacks. In the present study, we report our findings on the corrosion of Ni in the presence and absence of (LieNa) hydroxide melt at 600 °C under oxidizing and reducing conditions representative of HTWE. While the Ni electrode was found to remain thermodynamically stable in metallic form under cathodic (reducing) exposure conditions, the corrosion rate in molten hydroxide under oxidizing conditions was found to be nonparabolic in nature. A cyclic voltammetry study provides the breakdown of the passive metal-oxide surface layer at the anodic overpotential region between 0.45 V and 2 V in molten hydroxide under oxidizing conditions. As a result, a thermochemical process for accelerated corrosion based on the oxide scale fluxing in hydroxide melt has been developed.

08 HYDROGEN↗

Microstructural Characterization of Deformation Localization at Small Strains in a Neutron Irradiated 304 Stainless Steel

Deformation localization and structure evolution were investigated in an AISI 304 austenitic stainless steel deformed to 0.8% strain. Using SEM-EBSD, it was shown local plastic deformation may reach significant levels even when the bulk averaged strain level remains below 1%. Local misorientation values up to 24 were observed in these regions of high local plastic deformation. EBSD analysis of FIB lift-out specimens demonstrated that local misorientation level was highest near the free surface and diminished with increasing depth. (S)TEM observations on the same specimen indicated the local density of dislocation channels may vary up to an order of magnitude depending on local grain configuration, distance to the surface and/or local grain boundary structure. It was found that in the case of RT deformation, dislocation defect-free channels may contain twin or may be twin-free with twinning occurring inside channels. Formation of BCC-phase colonies (martensite) was observed in near-surface layer whereas no transformation in the volume of the specimen was detected at this strain level. Martensite formation was associated with channel-grain boundary intersection points where high local misorientation was observed using EBSD.

Deformation↗

Corrosion-induced microstructural developments in 316 stainless steel during exposure to molten Li 2 BeF 4 (FLiBe) salt

The microstructural evaluation and characterization of 316 stainless steel samples that were tested in molten Li 2 BeF 4 (FLiBe) salt were investigated in this study for evaluating its performance in high-temperature molten fluoride salts. Recently, 316 stainless steel and FLiBe salt are being actively considered as the main structural alloy and primary coolant of fluoride salt-cooled high-temperature reactor (FHR), a leading nuclear reactor concept for the next generation nuclear plants (NGNP). In support of the materials development for the FHR, high-temperature corrosion tests of 316 stainless steel in molten FLiBe salt at 700°C have been conducted in both bare graphite crucibles and 316 stainless steel-lined crucibles in an inert atmosphere for up to 3000 hours. The microstructure of the tested samples was comprehensively characterized using scanning electron microscopy (SEM) in conjunction with energy dispersive x-ray spectroscopy (EDS) and electron backscatter diffraction (EBSD), and scanning transmission electron microscopy (STEM) with EDS. In addition to the noticeable intergranular corrosion attack on surface, the corrosion in terms of the Cr depletion along high angle grain boundaries (15-180º) extended to 22µm in depth after 3000-hour exposure to molten FLiBe salt in graphite crucible. The coherent Σ3 grain boundary appeared high resistance to the Cr depletion. The substantial Cr depletion from the near-to-surface layer induced phase transformation from γ-martensite to α-ferrite phase (FeNi x ) during corrosion at 700ºC. Furthermore, the presence of graphite in the molten salt doubled the corrosion attack depth and led to the formation of round Mo2C, hexagonal Cr 7 C 3 and needle-like Al 4 C 3 phase within the alloy as deep as 50 µm after 3000-hour corrosion testing. Based on the microstructural analysis, the corrosion mechanisms of 316 stainless steel in molten FLiBe salt in different corrosion crucibles were illuminated through schematic diagrams. Additionally, a thermal diffusion controlled corrosion model was developed and validated by experimental data for predicting the long-term corrosion attack depth.

36 MATERIALS SCIENCE↗

Interaction of beryllium with 316H stainless steel in molten Li 2 BeF 4 (FLiBe)

The increased demand in renewable energy resources has led to a renewed interest in nuclear reactors including a new generation of molten salt reactors. One of the issues encountered in handling of molten chloride or fluoride salts is the inability of metals to form and retain a protective oxide surface layer, generally chromium oxide. The low chromium content, nickel-based alloy INOR-8, later marketed as Hastelloy N, was specifically developed to contain molten fluorides. This alloy had some deficiencies, but its composition resulted in it incurring far less chromium depletion by the molten fluoride salts than alloys like 316 stainless steel. For the next generation of molten salt reactors, an alloy with pressure vessel code approval and higher temperature capability than Hastelloy N is required. Consequently, several reactor designers have reportedly chosen to build the reactor containment vessel from 316H stainless steel. In order to minimize corrosion of the stainless steel by the molten fluoride salt (2LiF-BeF 2 ), it is proposed to add beryllium metal to the salt to react with impurities and provide a means to lower the oxidation potential thus making the salt less corrosive. Even so, there is a concern whether the beryllium would react with components of the stainless steel. To address this concern, static capsule tests were conducted in which selected amounts of beryllium were added to capsules containing 2LiF-BeF 2 (FLiBe) salt and 316H stainless steel and Hastelloy N samples. Following exposure, the samples were cleaned and examined using a variety of analysis techniques including, optical microscopy, SEM-EDS, XPS, LIBS, XRD and EPMA. Tensile samples were also exposed in capsules, and those were subjected to tensile testing. Notably, It was found that for the level of beryllium additions used in this study, intermetallic compounds were formed which could be detrimental to the long-term performance of the 316H stainless steel.

36 MATERIALS SCIENCE↗

FLiBe compatibility of fusion-relevant materials

There is current interest in a 2LiF-BeF2 (FLiBe) molten salt blanket for fusion applications, however, very little compatibility data are available for fusion relevant materials. Initial static capsule testing results for 500 h at 550°-750 °C are presented for V-4Cr-4Ti, Fe-8Cr-2W (alloy F82H) compared to type 316H stainless steel and monolithic SiC as a surrogate for SiC/SiC composites. In addition, sintered Be12Ti specimens with varying additions of Be (0–20%) and a Be2C specimen were exposed with F82H coupons at 650 °C in individual Mo capsules. The V-4Cr-4Ti and SiC specimens exposed at 650 °C had small mass changes. Steel specimens showed increasing mass losses with increasing exposure temperature. However, when Be12Ti-Be specimens were included in a capsule with an F82H coupon, increasing F82H mass gains were observed with increasing Be content due to the formation of a Fe-Be surface layer. No layer and no mass gain were observed for the F82H specimen tested with Be2C.

Pint, Bruce [Oak Ridge National Laboratory (ORNL) ↗

Diffusional lithium trapping as a failure mechanism of aluminum foil anodes in lithium-ion batteries

Aluminum foils are an appealing anode for lithium-ion batteries due to high capacity and low-cost, but their viability has been limited due to poor cyclability arising from pulverization and solid-electrolyte interphase growth. Here, we show that significant capacity degradation of aluminum foil anodes during electrochemical cycling also occurs due to diffusional lithium trapping. Scanning electron microscopy of cross-sectioned, cycled foils in the delithiated state reveals large regions of β-LiAl that are passivated by a surface layer of α-Al, which has poor Li + diffusivity. It is found that lithium diffusion occurs preferentially along the β-LiAl grain boundaries, so the grain structure after initial lithiation significantly affects the trapping behavior. Diffusional lithium trapping is exacerbated by both higher delithiation rates and higher areal capacity, presenting a challenge towards commercialization of aluminum foil anodes. We further demonstrate that diffusional trapping in aluminum foil anodes can be mitigated through alloy design, with the addition of 2–3 wt% Li yielding improved first cycle efficiency, and the addition of 1 wt% Si yielding improved cycle life. These results provide a mechanistic understanding of diffusional lithium trapping in aluminum foil anodes and highlight compositional design of alloys as a promising strategy to overcome it.

25 ENERGY STORAGE↗

Microstructure refinement and mechanical properties improvement by developing IAF on inclusions in Ti–Al complex deoxidized HSLA steel

The present study focused on microstructure refinement in Ti–Al complex deoxidized low alloy structural steel by developing IAF on inclusions. The goal was to establish more determined relation between Ti, Al in steel and the produced microstructures. In steel sample with Ti and Al contents of 0.0035% and 0.0004%, respectively, IAF was well developed by inclusions characterized by TiO{sub x}–MnO oxide cores enwrapped by (MnO–SiO{sub 2}–Al{sub 2}O{sub 3})–MnS or (MnO–SiO{sub 2})–MnS surface layers. With the rise of Ti and Al contents, IAF volume decreased greatly because of different inclusion chemistry, TiO{sub x} + MnS, TiO{sub x}–Al{sub 2}O{sub 3} or Al{sub 2}O{sub 3}, which inhibit the formation of IAF. Thermodynamic calculations were carried out for optimal Ti and Al contents in steel to target inclusions with proper chemistry for nucleating IAF. These laboratorial findings were successfully applied and reproducibly observed in pilot trials. It was indicated that low temperature impact toughness at 0 °C and − 20 °C of the produced medium plate was effectively improved despite lower Ti contents than common process, which was very meaningful in saving the cost of high Ti content steels. - Highlights: • IAF volume showed close relationship to Ti or Al contents. • To target IAF, there is no need to add too many titanium alloys. • Optimal Ti and Al were about 0.0020–0.0060% and 0.0005–0.0020%, respectively. • Impact toughness of steel plate at 0 °C and − 20 °C was successfully improved.

36 MATERIALS SCIENCE↗

Microstructure development and texture evolution of aluminum multi-port extrusion tube during the porthole die extrusion

Aluminum multi-port extrusion tube is processed by the porthole die extrusion and the internal tube walls are welded through the solid state metallurgical bonding. In order to observe the development of grains and their orientations under severe plastic deformation and solid state welding, the extrusion butt together with the die is quenched immediately after extrusion to preserve the grain structure in the processing. The forming histories of selected material points are obtained by analyzing the optical microscopy graph. The evolution of the microstructure along the forming path is characterized by electro backscattered diffraction. It is found that geometrical dynamic recrystallization happens in the process. Grains are elongated, scattered at the transition zone and shear intensive zone, and then pinched off when they are pushed out from the die orifice. The shear-type orientations are predominant at the surface layer on the longitudinal section of the tube web and have penetrated into the intermediate layer. The rolling-type orientations are formed at the central layer. Texture gradient through the thickness of the tube web is observed. And cube orientated grains are found at the seam weld region. - Highlights: •Microstructure of extrusion butt is preserved after the micro scale porthole die extrusion. •Grain morphology history along forming path is investigated. •Texture evolutions on three material flows are present. •Texture gradient exists on the longitudinal section of the internal wall of profile. •Rolling-type and cube textures are found at the solid state welding region.

36 MATERIALS SCIENCE↗

Magnetic properties of Fe implanted SrTiO{sub 3} perovskite crystal

Graphical abstract: - Highlights: • The results of investigations of magnetic properties of Fe implanted SrTiO{sub 3} are presented. • The measurements of the temperature dependence of the magnetization were performed. • Ferromagnetic hysteresis loops in Fe implanted SrTiO{sub 3} were observed at low temperatures. • Superparamagnetic behavior of the samples at high temperatures was revealed. • It was shown that the magnetization of the samples depends on the fluency of implantation. - Abstract: The results of investigations of magnetic properties of SrTiO{sub 3} perovskite crystal implanted with 40 keV Fe ions at the fluencies between 0.5 × 10{sup 17} and 1.5 × 10{sup 17} ion/cm{sup 2} are presented. It has been revealed that high-fluency implantation with Fe ions results in the formation of a granular metal particulate composite in the irradiated near-surface layer of SrTiO{sub 3} substrate, which exhibits remarkable ferromagnetic behavior. The measurements of the temperature dependence of the magnetic moment showed that the samples exhibit blocking temperature at about 350 K, above which a superparamagnetic behavior has been observed. Ferromagnetic ordering and magnetic hysteresis loops were observed in Fe implanted SrTiO{sub 3} at the temperatures lower than 350 K. It has been shown that the magnetization of the ferromagnetic state depends on the fluency of implantation.

36 MATERIALS SCIENCE↗

Preparation of morphology-controlled TiO{sub 2} nanocrystals for the excellent photocatalytic activity under simulated solar irradiation

Graphical abstract: Morphology-controlled TiO{sub 2} nanocrystals with excellent photocatalytic activity under simulated solar irradiation were successfully synthesized. - Highlights: • TiO{sub 2} nanocrystals (NCs) with different morphologies were synthesized. • The growth mechanism of morphology-controlled TiO{sub 2} NCs was proposed. • The core-shell structured TiO{sub 2} NCs (co-TiO{sub 2}) had a narrow band gap (2.67 eV). • The co-TiO{sub 2} NCs possessed excellent photocatalytic activity and recyclability. - Abstract: A simple synthetic approach based on solvothermal technique and hydrogenation was developed for preparation of TiO{sub 2} nanocrystals with different morphologies such as elongated rhombic, dog-bone, oval and core-shell structured oval. The effect of oleic acid (OA) and oleylamine (OM) as two capping surfactants on the growth of TiO{sub 2} nanocrystals was investigated. The physicochemical properties of the obtained samples were characterized by various techniques including TEM, XRD, UV–vis absorption, Raman, XPS, BET, PL and photocurrent measurement. In photodegradation of RhB under simulated solar irradiation, the oval-shaped TiO{sub 2} nanocrystals with core-shell structure (co-TiO{sub 2}) was superior to other TiO{sub 2} nanocrystals in catalytic activity. Moreover, the co-TiO{sub 2} nanocrystals exhibited well recyclability during multiple photocatalytic tests. These excellent properties of co-TiO{sub 2} were attributed to its special structure, including lattice-disordered surface layer and well-crystallized lattice core, and narrow band gap (2.67 eV).

36 MATERIALS SCIENCE↗

The subsurface structure of abraded Al–Zn–Mg–Cu alloy

Surface abrasion has been shown to introduce heavy shear stress and produce a few hundred nanometers thick altered surface layer (ASL) on Al alloys. Such ASLs exhibit microstructural changes at room temperature and different corrosion resistance than the underlying substrate. Here, we report how sample dimensions and temperature affect the deformed subsurface microstructure evolution on an abraded Al–Zn–Mg–Cu alloy using transmission electron microscopy (TEM) and atom probe tomography. The ASL microstructure evolves differently in the bulk sample than in the thin TEM specimen. In the freshly abraded ASL, the original η'/η precipitates and grain boundaries were deformed toward the abrasion direction. After 7-day natural aging of the freshly abraded bulk sample, well-defined subgrains formed locally in the ASL, and unusual Al 2 Cu (θ) and Mg x Zn y phases precipitated at the subgrain boundaries. However, during natural aging of this TEM specimen taken from the abraded and aged bulk samples, much faster changes occurred, including the continued formation of subgrains and θ particles in the entire ASL, and the diffusion of Zn atoms out of Mg x Zn y particles to form a Zn particle. On the other hand, no obvious microstructural changes occurred in the ASL during 3-month natural aging of the TEM specimen immediately taken from the freshly abraded sample. Finally, this work advances the understanding of how Al alloy microstructures respond during and following any shear deformation, and complex and unexpected effects of sample dimensions on the behavior.

36 MATERIALS SCIENCE↗

Separation Nanotechnology of Diethylenetriaminepentaacetic Acid Bonded Magnetic Nanoparticles for Spent Nuclear Fuel

A nanomagnetic separation method based on Diethylenetriaminepentaacetic acid (DTPA) conjugated with magnetic nanoparticles (MNPs) is studied for application in spent nuclear fuel separation. The high affinity of DTPA towards actinides aids in separation from the highly acidic medium of nuclear waste. The solubility and magnetization of particles at low pH is protected by encapsulating them in silica layer. Surface functionalization of silica coated particles with polyamines enhances the loading capacity of the chelators on MNPs. The particles were characterized before and after surface modification using transmission electron microscopy (TEM), helium ion microscopy (HIM), Fourier transform-infrared (FT-IR) spectrometry, and X-ray diffractometry. The coated and uncoated samples were studied using vibrating sample magnetometer (VSM) to understand the change in magnetic properties due to the influence of the surface functionalization. The hydrodynamic size and surface charge of the particles are investigated using Dynamic Light Scattering (DLS). The uptake behavior of Am(III), Pu(IV), U(VI), and Np(V) from 0.1M NaNO3 solution was investigated. The sorption result shows the strong affinity of DTPA towards Am(III) and Pu(IV) by extracting 97% and 80% of actinides, respectively. The high removal efficiency and fast uptake of actinides make the chelator conjugated MNPs an effective method for spent nuclear fuel separation.