Search NASA⌕ Search

SEARCH · Search NASA

Results for “VAPOR PHASE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,585 records · Page 88

Oxygen incorporation effects in annealed epitaxial La{sub (1-x)}Sr{sub x}MnO{sub 3} thin films

This paper presents our results regarding oxygen incorporation effects in epitaxial La{sub (1-x)}Sr{sub x}MnO{sub 3} thin films, deposited on SrTiO{sub 3} (001) single crystal substrates, by annealing in different gas mixtures of argon and oxygen. A particular emphasis is placed on the correlation of structural properties with the magnetic properties of the films, Curie temperature, and coercive field. In this sense, we demonstrate that the evolution of the diffuse part of the {omega}-scans performed on the films are due to oxygen excess in the film lattice, which creates cationic vacancies within the films. Also, we show that two regimes of oxygen incorporation in the films exist, one in which the films evolve toward a single phase and oxygen stoichiometry is recovered, and a second one dominated by oxygen over-doping effects. In order to support our study, XPS measurements were performed, from which we have evaluated the Mn{sup 3+}/Mn{sup 4+} ionic ratio.

36 MATERIALS SCIENCE↗

High-power single-mode laser diodes based on carbon-doped quantum-well InGaAs/AlGaAs heterostructures

Emission parameters of single-mode laser diodes based on InGaAs/GaAs/AlGaAs heterostructures doped with carbon and grown by using the metallorganic vapour phase epitaxy (MOVPE) technique are studied. The obtained results show that maintaining a certain doping profile ensuring optimisation of series resistance and internal optical losses during all fabrication stages of the active element of a diode laser, provides for enhancement of the laser efficiency. Based on laser heterostructures studied in this paper, highly efficient single-transverse-mode laser diodes emitting 300 mW at 980 nm have been manufactured. (lasers)

36 MATERIALS SCIENCE↗

Growth temperature control of the epitaxy, magnetism, and transport in SrTiO{sub 3}(001)/La{sub 0.5}Sr{sub 0.5}CoO{sub 3} thin films

The authors report a detailed study of the influence of deposition temperature on the microstructure, phase purity, nanoscale chemical homogeneity, stoichiometry, and magnetic and electronic properties of epitaxial La{sub 0.5}Sr{sub 0.5}CoO{sub 3} thin films grown on SrTiO{sub 3}(001) substrates via reactive dc magnetron sputtering. The results are interpreted in terms of the temperature-dependent interplay between crystallization, strain relaxation, and cation mobility (which improve with increasing deposition temperature), and oxygenation (which deteriorates at the highest deposition temperatures). In addition to the established approach to epitaxial sputter deposition based on high temperature deposition combined with subsequent ex situ annealing in O{sub 2}, our results also identify a narrow deposition temperature window {approx}600-625 deg. C, where single phase, highly crystalline, low surface roughness epitaxial films can be obtained with close to ideal stoichiometry without postdeposition annealing. Electronic and magnetic properties similar to bulk single crystals can be obtained in this region.

36 MATERIALS SCIENCE↗

Spectral characteristics of multimode semiconductor lasers with a high-order surface diffraction grating

We have studied the spectral characteristics of multimode semiconductor lasers with high-order surface diffraction gratings based on asymmetric separate-confinement heterostructures grown by metalorganic vapour phase epitaxy (λ = 1070 nm). Experimental data demonstrate that, in the temperature range ±50 °C, the laser emission spectrum is ∼5 Å in width and contains a fine structure of longitudinal and transverse modes. A high-order (m = 15) surface diffraction grating is shown to ensure a temperature stability of the lasing spectrum dλ/dT = 0.9 Å K{sup -1} in this temperature range. From analysis of the fine structure of the lasing spectrum, we have evaluated the mode spacing and, thus, experimentally determined the effective length of the Bragg diffraction grating, which was ∼400 μm in our samples. (lasers)

36 MATERIALS SCIENCE↗

Nonstoichiometry of ZnGeP{sub 2} crystals probed by static tensimetric method

Abstracts: The nonstoichiometry of ZnGeP{sub 2} has been determined based on the p-T dependences measured above ZnP{sub 2}-Ge samples in the temperature range of 980-1225 K by a high-sensitive and precise tensimetric static method with a quartz Bourdon gauge. Scanning of the compositional range 49-51 mol% ZnP{sub 2} in the closed system and construction of the p-T dependences were possible due to incongruent evaporation of ZnGeP{sub 2} and formation of volatile species Zn(g), P{sub 4}(g) and P{sub 2}(g). The maximum homogeneity range of the solid ZnGeP{sub 2} was determined between 50.03 and 49.61 mol% ZnP{sub 2} at a temperature of 1128 K, based on the inflection points on the p-T dependences, corresponding to transitions of the three-phase (solid-solid-vapor) equilibrium to a two-phase (solid-vapor) one and vice visa. The nonstoichiometry as the overall concentration of defects is considered to gain a better insight into the defect chemistry of ZnGeP{sub 2}. - Graphical abstract: The nonstoichiometry of ZnGeP{sub 2} on the T-x diagram of the ZnP{sub 2}-Ge system.

36 MATERIALS SCIENCE↗

Optically pumped semiconductor laser based on a type-II CdS/ZnSe heterostructure

An optically pumped semiconductor laser based on a type-II CdS/ZnSe nanoheterostructure containing 10 quantum wells (QWs) was studied. The structure was grown by metal-organic vapour phase epitaxy on a GaAs substrate. The lifetime of electron-hole pairs at a low pump level was measured by luminescence decay to be ∼0 ns. The peak power of the microcavity semiconductor laser at room temperature and longitudinal pumping by a repetitively pulsed N{sub 2} laser was 7.2 W at a wavelength of 514 nm. The relatively low laser slope efficiency (0.35 %) is explained by amplified spontaneous emission propagating along the structure. The peak power and efficiency of the laser in the case of transverse pumping increase to 70 W and 3.5 %, respectively. (lasers)

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

InGaN: Direct correlation of nanoscopic morphology features with optical and structural properties

A comprehensive study on the impact of growth modes on the structural and optical properties of thick InGaN layers suitable for photovoltaic application is presented. Samples grown by metalorganic vapour phase epitaxy with different growth rates and thicknesses have been analyzed. The application of slow growth rates result in smooth layers while higher growth rates induce a meandering surface morphology. Using low-temperature cathodoluminescence, a direct correlation of the morphology to local luminescent properties is obtained: the top of meandering structures reveals a spectrally red-shifted emission compared to the emission wavelength expected from the average indium content determined by X-ray diffraction. The origin of this shift is identified and explained by increased indium incorporation on top of the meander due to a spatially localized compositional pulling effect.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

AlGaAs/GaAs laser diode bars (λ = 808 nm) with improved thermal stability

Two series of AlGaAs/GaAs laser heterostructures have been grown by metal-organic vapour phase epitaxy, and 808-nm laser diode bars fabricated from the heterostructures have been investigated. The heterostructures differed in waveguide thickness and quantum well depth. It is shown that increasing the barrier height for charge carriers in the active region has an advantageous effect on the output parameters of the laser sources in the case of the heterostructures with a narrow symmetric waveguide: the slope of their power – current characteristics increased from 0.9 to 1.05 W A{sup -1}. Thus, the configuration with a narrow waveguide and deep quantum well is better suited for high-power laser diode bars under hindered heat removal conditions. (lasers)

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Epitaxial growth and magnetic properties of Fe{sub 3}O{sub 4} films on TiN buffered Si(001), Si(110), and Si(111) substrates

Epitaxial Fe{sub 3}O{sub 4} thin films were grown on TiN buffered Si(001), Si(110), and Si(111) substrates by dc reactive sputtering deposition. Both Fe{sub 3}O{sub 4} films and TiN buffer are fully epitaxial when grown at substrate temperatures above 150 deg. C, with textured single phase Fe{sub 3}O{sub 4} resulting from room temperature growth. The initial sputtered Fe{sub 3}O{sub 4} formed nuclei islands and then coalesced to epitaxial columnar grains with increasing film thickness. The magnetization decreases and the coercive field increases with decreasing film thickness. There is no in-plane magnetic anisotropy of epitaxial Fe{sub 3}O{sub 4}(001) on Si(001) but Fe{sub 3}O{sub 4} films grown on Si(110) and Si(111) substrates show uniaxial in-plane magnetic anisotropy.

36 MATERIALS SCIENCE↗

Dual-wavelength laser diodes based on epitaxially stacked heterostructures

AlGaAs/GaAs double laser heterostructures containing two different active regions have been grown by metalorganic vapour phase epitaxy in a single growth process, and their properties have been studied. A typical slope of their power - current curves is 2.3 W A{sup -1}, which is almost twice that for a laser diode (1.2 W A{sup -1}). We demonstrate lasing of the emitter regions of the dual-wavelength lasers in the range 800 - 815 nm, with a separation between the peaks of {approx}7 nm. The observed effect of pump current on the lasing wavelength of the active regions in the dual-wavelength and single lasers indicates that the emitter region farther away from the heat sink is more sensitive to pump current variations. (lasers)

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Comparative study of polar and semipolar (112⁻2) InGaN layers grown by metalorganic vapour phase epitaxy

InGaN layers were grown simultaneously on (112⁻2) GaN and (0001) GaN templates by metalorganic vapour phase epitaxy. At higher growth temperature (≥750°C), the indium content (<15%) of the (112⁻2) and (0001) InGaN layers was similar. However, for temperatures less than 750°C, the indium content of the (112⁻2) InGaN layers (15%–26%) were generally lower than those with (0001) orientation (15%–32%). The compositional deviation was attributed to the different strain relaxations between the (112⁻2) and (0001) InGaN layers. Room temperature photoluminescence measurements of the (112⁻2) InGaN layers showed an emission wavelength that shifts gradually from 380 nm to 580 nm with decreasing growth temperature (or increasing indium composition). The peak emission wavelength of the (112⁻2) InGaN layers with an indium content of more than 10% blue-shifted a constant value of ≈(50–60) nm when using higher excitation power densities. This blue-shift was attributed to band filling effects in the layers.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Relaxation and critical strain for maximum In incorporation in AlInGaN on GaN grown by metal organic vapour phase epitaxy

Quaternary AlInGaN layers were grown on conventional GaN buffer layers on sapphire by metal organic vapour phase epitaxy at different surface temperatures and different reactor pressures with constant precursor flow conditions. A wide range in compositions within 30-62% Al, 5-29% In, and 23-53% Ga was covered, which leads to different strain states from high tensile to high compressive. From high-resolution x-ray diffraction and Rutherford backscattering spectrometry, we determined the compositions, strain states, and crystal quality of the AlInGaN layers. Atomic force microscopy measurements were performed to characterize the surface morphology. A critical strain value for maximum In incorporation near the AlInGaN/GaN interface is presented. For compressively strained layers, In incorporation is limited at the interface as residual strain cannot exceed an empirical critical value of about 1.1%. Relaxation occurs at about 15 nm thickness accompanied by strong In pulling. Tensile strained layers can be grown pseudomorphically up to 70 nm at a strain state of 0.96%. A model for relaxation in compressively strained AlInGaN with virtual discrete sub-layers, which illustrates the gradually changing lattice constant during stress reduction is presented.

36 MATERIALS SCIENCE↗

Structure and strain relaxation effects of defects in In{sub x}Ga{sub 1–x}N epilayers

The formation of trench defects is observed in 160 nm-thick In{sub x}Ga{sub 1–x}N epilayers with x≤0.20, grown on GaN on (0001) sapphire substrates using metalorganic vapour phase epitaxy. The trench defect density increases with increasing indium content, and high resolution transmission electron microscopy shows an identical structure to those observed previously in InGaN quantum wells, comprising meandering stacking mismatch boundaries connected to an I₁-type basal plane stacking fault. These defects do not appear to relieve in-plane compressive strain. Other horizontal sub-interface defects are also observed within the GaN pseudosubstrate layer of these samples and are found to be pre-existing threading dislocations which form half-loops by bending into the basal plane, and not basal plane stacking faults, as previously reported by other groups. The origins of these defects are discussed and are likely to originate from a combination of the small in-plane misorientation of the sapphire substrate and the thermal mismatch strain between the GaN and InGaN layers grown at different temperatures.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Growth of non-polar (11-20) InGaN quantum dots by metal organic vapour phase epitaxy using a two temperature method

Non-polar (11-20) InGaN quantum dots (QDs) were grown by metal organic vapour phase epitaxy. An InGaN epilayer was grown and subjected to a temperature ramp in a nitrogen and ammonia environment before the growth of the GaN capping layer. Uncapped structures with and without the temperature ramp were grown for reference and imaged by atomic force microscopy. Micro-photoluminescence studies reveal the presence of resolution limited peaks with a linewidth of less than ∼500 μeV at 4.2 K. This linewidth is significantly narrower than that of non-polar InGaN quantum dots grown by alternate methods and may be indicative of reduced spectral diffusion. Time resolved photoluminescence studies reveal a mono-exponential exciton decay with a lifetime of 533 ps at 2.70 eV. The excitonic lifetime is more than an order of magnitude shorter than that for previously studied polar quantum dots and suggests the suppression of the internal electric field. Cathodoluminescence studies show the spatial distribution of the quantum dots and resolution limited spectral peaks at 18 K.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Ferromagnetic and paramagnetic magnetization of implanted GaN:Ho,Tb,Sm,Tm films

The SQUID magnetic measurements were performed on the GaN films prepared by metal-organic vapour phase epitaxy and implanted by Tb{sup 3+}, Tm{sup 3+}, Sm{sup 3+}, and Ho{sup 3+} ions. The sapphire substrate was checked by the electron paramagnetic resonance method which showed a content of Cr{sup 3+} and Fe{sup 3+} impurities. The samples 5 × 5 mm{sup 2} were positioned in the classical straws and within an estimated accuracy of 10{sup −6 }emu, no ferromagnetic moment was detected in the temperature region of 2–300 K. The paramagnetic magnetization was studied for parallel and perpendicular orientation. In the case of GaN:Tb sample, at T = 2 K, a pronounced anisotropy with the easy axis perpendicular to the film was observed which can be explained by the lowest quasi-doublet state of the non-Kramers Tb{sup 3+} ion. The Weiss temperature deduced from the susceptibility data using the Curie-Weiss (C-W) law was found to depend substantially on the magnetic field.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Epitaxial growth and piezoelectric characterization of the (1-x)BiScO{sub 3}-(x)PbTiO{sub 3} ultrathin film

We studied ferroelectric properties of morphotropic phase boundary (1-x)BiScO{sub 3}-(x)PbTiO{sub 3} (BSPT, x = 0.64) epitaxial thin films on SrTiO{sub 3} (001) and Nb:SrTiO{sub 3} (001). BSPT thin films with various thicknesses were deposited using off-axis radio frequency magnetron sputtering. By analyzing x-ray data of BSPT thin films with various thicknesses, we confirmed that films thinner than {approx}22 nm were in a strained state. Films thicker than {approx}22 nm were in a relaxed state because of the strain relaxation mechanism caused by misfit dislocation formation. Clear piezoresponses and polarization reversal phenomena can be observed in the ultrathin limit down to 8 nm through Piezo Force Microscope experiments. The piezoresponse data as a function of thickness correlates with the structural modification of thin films.

36 MATERIALS SCIENCE↗

Cloud Influence on ERA5 and AMPS Surface Downwelling Longwave Radiation Biases in West Antarctica

The surface downwelling longwave radiation component (LW?) is crucial for the determination of the surface energy budget and has significant implications for the resilience of ice surfaces in the polar regions. Accurate model evaluation of this radiation component requires knowledge about the phase, vertical distribution, and associated temperature of water in the atmosphere, all of which control the LW? signal measured at the surface. In this study, we examine the LW? model errors found in the Antarctic Mesoscale Prediction System (AMPS) operational forecast model and the ERA5 reanalysis model relative to observations from the AWARE campaign at McMurdo Station and the West Antarctic Ice Sheet (WAIS) Divide. The errors are calculated separately for observed clear sky conditions, ice cloud occurrences, and liquid-bearing cloud layer (LBCL) occurrences. The analysis results show a tendency (in both models at each site) to underestimate the LW? during clear sky conditions, high error variability (standard deviations > 20 W/m2) during any type of cloud occurrence, and negative LW? biases when LBCLs are observed (bias magnitudes > 15 W/m2 in tenuous LBCL cases; > 43 W/m2 in optically thick/opaque LBCLs instances). We suggest that a generally dry and liquid water-deficient atmosphere responsible for the identified LW? biases in both models is the result of excessive ice formation and growth, which could stem from model initial and lateral boundary conditions, microphysics scheme, aerosol representation, and/or limited vertical resolution.

Silber, Israel↗

Single- and dual-variant atomic ordering in GaAsP compositionally graded buffers on GaP and Si substrates

Here, we investigate the material properties of GaAsP graded buffers on both GaP and Si substrates in order to determine limitations to dislocation glide in GaAsP. Phase separation is not observed in these GaAsP buffers, but CuPt B atomic ordering is present, and has an impact on the Burgers vector distribution of gliding dislocations. Tellurium surfactant eliminates ordering in GaAsP, allowing control over the glide plane distribution while highlighting the importance of the growth surface and choice of dopant. The impact of single-variant CuPtB ordering of GaAsP buffers grown on GaP substrates is investigated by monitoring the threading dislocation density throughout the buffer in sequential steps. The dislocation density rises steadily throughout the graded buffer, implying that factors other than ordering-induced glide plane switches play a dominant role in the final dislocation density. We observe an increase in surface roughness throughout the buffer and speculate that a dislocation nucleation source on the surface has a low activation energy and may lead to increased threading dislocation density. On Si substrates, the GaAsP buffer displays dual-variant CuPt B ordering rather than single-variant ordering due to the surface step geometry. We discuss how dual-variant ordering leads to a variable glide force, and thus has a different impact on dislocation dynamics than single-variant ordering. Because the III-V on Si nucleation procedure determines the step geometry, it also influences the dislocation dynamics.

36 MATERIALS SCIENCE↗