Cold Spray NDE for Porosity and Other Process Anomalies

This paper describes a technology review of non-destructive examination (NDE) methods that can be applied to cold spray coatings. Cold spray is a process for depositing metal powder at high velocity so that it bonds to the substrate metal without significant heating that would be likely to cause additional residual tensile stresses. Coatings in the range from millimeters to centimeters are possible at relatively high deposition rates. Cold spray coatings that may be used for hydroelectric components that are subject to erosion, corrosion, wear, and cavitation damage are of interest. The topic of cold spray NDE is treated generally however and may be considered applicable to virtually any cold spray application except where there are constraints of the hydroelectric component application that bear special consideration. Hydroelectric turbine components are primarily made from low carbon and austenitic stainless steels. They are typically very large components that are partially assembled on-site. Transport of these components within the hydroelectric facility and away from the hydroelectric facility is challenging due to the component’s size and weight, high cost of disassembly, and the confined space of the dam. One method for prolonging component life is application of cold spray and thermal powder metal coatings to the components most susceptible to erosion, corrosion, cracking, and mechanical wear. Process controls and visual inspections have historically been applied to cold spray application; however, quantitative NDE could detect anomalies not readily apparent from such a visual examination. Optical profilometry, Eddy current, ultrasound, and hardness tests are shown for one set of good, fair, and poor Nickle-Chrome (NiCr) on 304 stainless steel (304SS) cold spray samples to demonstrate inspection possibilities. The primary indicator of cold spray quality is the cold spray porosity that is most directly measured with witness-sample destructive examinations (DE) – mostly photo-micrographs. These DE generated porosity values are correlated with optical profilometry, eddy current, ultrasound, and hardness test NDE methods to infer the porosity and other Information of interest. These parameters of interest primarily include: • Porosity primarily caused by improper process conditions (temperature, gas velocity, spray standoff, spray angle, powder size, condition, surface cleanliness, surface oxide, etc.). • Presence/absence of the cold spray coating including possible over-sprayed voids • Coating thickness Optical profilometry measurements of surface roughness trended with porosity plus if compared with a reference measurement or reference drawing would provide information on the coating thickness. Ultrasound could provide similar surface profile information plus attenuation measurements trended with porosity. The ultrasound measurements however may be limited to geometries where the substrate back-wall is normal to the cold spray surface and not too thick. Eddy current showed a strong correlation with porosity. Eddy currents can also be sensitive to cracks and do not need fluid coupling to make measurements. Eddy currents however are not sensitive to coating thicknesses in most cases. Vickers hardness measurements also tracked well with porosity. These types of hardness measurements however are also not sensitive to coating thickness. An NDE program may include multiple measurements. Acknowledgement: This work is sponsored by Bonneville Power Administration (BPA) under their technology innovation project program. Such support does not constitute BPA endorsement of views expressed in this work.

Glass, Samuel W.↗

Optimization of thermal barrier coating performance and durability over a drive cycle

A methodology to thermo-mechanically optimize a piston thermal barrier coating over a full drive cycle was established. The optimization objective was to minimize the heat transfer to the engine wall while maintaining structural integrity of the coating. Over 800 candidate materials were investigated and the optimization required more than one million non-road transient drive cycle calculations; real materials were investigated to ensure a realizable result and the existence of thermal and mechanical properties. High computational efficiency was achieved using a recently developed analytical heat transfer technique for multilayer engine walls. An uncoupled approach was utilized for the optimization, wherein the gas temperature and heat transfer coefficient profiles from a fully coupled and calibrated baseline model over the 20-min drive cycle were employed. The coating/piston interface temperature was constrained to be below the maximum piston service temperature limit. The durability was assessed using a recently developed analytical coating delamination framework for engine in-cylinder coatings based on the energy release rate when a crack forms. Results are presented for a mechanically unconstrained optimization and for cases constrained to three fixed levels of drive-cycle maximum energy release rate, and also constrained by the individual material’s toughness. The best-performing coating materials identified were verified using the fully coupled system-level model, which compared well to the uncoupled predictions. A study on the effect of adding a sealing layer to some high-performing, but porous, coatings showed a reduction in fuel consumption benefit and an increased exhaust temperature over the cycle, but the system still outperformed the uncoated case. The results of the study elucidate the importance of including engine performance and mechanical failure considerations in thermal barrier coating design.

Engineering↗

Dynamic oxidation of (Mn,Co) 3 O 4 -Coated interconnects for solid oxide electrolysis cells

Solid oxide electrolysis cell stacks are expected to experience dynamic conditions when using renewable electricity derived from wind or solar power. To address this scenario, (Mn,Co) 3 O 4 (MCO)-coated Crofer 22 APU interconnect coupons are subjected to thermal cycling, and intermittent current density, with gas compositions relevant to high-temperature electrolysis (elevated steam:hydrogen ratio and oxygen content). Defects are also intentionally introduced in the MCO coating, to assess whether the difference in oxidation properties of the adjacent coated and uncoated (defective) surfaces causes sufficient stress to damage the protective oxide scale. Specimens with defects are subjected to oxidation for 1000 h at 800 °C, or thermal cycling. Before thermal cycling, some specimens are pre-oxidized to create a thick oxide scale to mimic the scale thickness expected after ~30 kh operation. In all cases, the coating and oxide scale remain well adhered with no cracking observed. Area-specific resistance (ASR) is monitored in both single-atmosphere and dual-atmosphere conditions, and the ASR is stable and is not impacted by dynamic cycling of the current density. Finally, this work provides confidence that the MCO coated interconnect will function as needed in dynamic operation conditions, even with coating defects.

08 HYDROGEN↗

A Novel Low-Temperature Fiffusion Aluminide Coating for Ultrasupercritical Coal-Fried Boiler Applications

An ultrasupercritical (USC) boiler with higher steam temperature and pressure is expected to increase the efficiency of the coal-fired power plant and also decrease emissions of air pollutants. Ferritic/martensitic alloys have been developed with good creep strength for the key components in coal-fired USC plants. However, they typically suffer excessive steam-side oxidation, which contributes to one of main degradation mechanisms along with the fire-side corrosion in coal-fired boilers. As the steam temperature further increases in USC boilers, oxidation of the tube internals becomes an increasing concern, and protective coatings such as aluminide-based diffusion coatings need to be considered. However, conventional aluminizing processes via pack cementation or chemical vapor deposition are typically carried out at elevated temperatures (1000-1150 C). Thermochemical treatment of ferritic/martensitic alloys at such high temperatures could severely degrade their mechanical properties, particularly the alloy's creep resistance. The research focus of this project was to develop an aluminide coating with good oxidation resistance at temperatures {le} 700 C so that the coating processing would not detrimentally alter the creep performance of the ferritic/martensitic alloys. Nevertheless, when the aluminizing temperature is lowered, brittle Al-rich intermetallic phases, such as Fe{sub 2}Al{sub 5} and FeAl{sub 3}, tend to form in the coating, which may reduce the resistance to fatigue cracking. Al-containing binary masteralloys were selected based on thermodynamic calculations to reduce the Al activity in the pack cementation process and thus to prevent the formation of brittle Al-rich intermetallic phases. Thermodynamic computations were carried out using commercial software HSC 5.0 for a series of packs containing various Cr-Al binary masteralloys. The calculation results indicate that the equilibrium partial pressures of Al halides at 700 C were a function of Al content in the Cr-Al alloys. Cr-25Al and Cr-15Al were chosen as the masteralloys in the pack cementation process. In contrast to pure Al masteralloy which led to the formation of Fe{sub 2}Al{sub 5} coatings at 650 C, a coating consisting of a thin Fe{sub 2}Al{sub 5} outer layer and an FeAl inner layer was formed at 700 C with the Cr-25Al masteralloy. By switching to the Cr-15Al masteralloy, thin FeAl coatings ({approx}12 {micro}m) containing < 50 at.% Al were achieved at 700 C. The effect of the amount of masteralloys on coating growth was also studied by employing packs containing 2NH{sub 4}Cl-x(Cr-15Al)-(98-x)Al{sub 2}O{sub 3}, where x = 10, 20, 30, 40, 50, 60, and 70 wt.%. It was noticed that when the Cr-15Al masteralloy was increased from 10 to 40 wt.% in the pack, both coating thickness and surface Al content increased, suggesting that gas phase kinetics played an important role in Al deposition. However, with further increase of the masteralloy, solid state diffusion became the rate-limiting factor. The long-term oxidation performance of the aluminide coatings synthesized at 700 C with Cr-25Al and Cr-15Al masteralloys was evaluated in the water vapor environment at 650-700 C. The low-temperature pack coatings demonstrated excellent oxidation resistance at 650 C in humid air after {approx}1.2 yr testing. Longer lifetimes can be expected for these thin coatings due to minimal interdiffusion at this testing temperature. Exposure at 700 C was conducted to accelerate coating failure via increased interdiffusion of Al with the substrate alloy. The coatings also exhibited good oxidation protection up to 6,000-8,000 h at 700 C, with longer testing needed for coating failure to occur. Furthermore, the oxidation results indicate that in addition to the Al reservoir (as determined by the Al content and coating thickness), the initial coating surface quality had a significant impact on the oxidation behavior. In addition, the effect of various pack aluminide coatings on the creep resistance of coated T91 was investigated. Three representative types of coatings with different thicknesses, Al concentrations and phase constituents were included in the creep test. The creep experiments were performed at 650 C in air at uniaxial stress levels of 100-120 MPa. The thick aluminide coating made at 1050 C showed a considerable reduction ({approx} 42%) in the creep rupture life of the coated alloy, due to the decrease of the load-bearing section. In contrast, the low-temperature thin coatings developed in this project did not significantly reduce the creep resistance of the coated T91 alloy, particularly the thin FeAl coating synthesized at 700 C using the Cr-15Al masteralloy.

36 MATERIALS SCIENCE↗

Caltalyst Layer Crack Detector, or CLCD ("clicked") [SWR-20-60]

The Caltalyst Layer Crack Detector, or CLCD ("clicked") is a program that takes in optical micrographs of catalyst coatings for PEM fuel cells or electrolyzers and calculates the percent area that consist of cracks. It does so using a custom algorithm that searches for dark features larger than the background graininess of the catalyst layer.

Pfeilsticker, Jason↗

Heat treatment effects on mechanical properties of atmospheric plasma sprayed Fe{sub x}B coatings on Al substrate

In this work, we draw attention to determination of heat-treatment effects on mechanical properties of atmospheric plasma sprayed (APS) Fe{sub x}B coatings on aluminum substrates by micro-indentation technique. With this regard, iron boride powders of Fe-18.8B-0.2C-0.5Si-0.8Al (wt.%) were deposited onto Al substrates by APS in order to improve the mechanical properties of Al surface. As-sprayed coatings are composed of mainly Fe{sub x}B and iron matrix supersaturated with boron owing to the rapid solidification of molten droplets flattened on a substrate. It was observed that APS coatings exhibited characteristic wavy layered structure having porosity, inclusions, and semi-melted particles. The postfurnace treatment of APS coatings was carried out at temperatures ranged from 450 to 550°C in an argon atmosphere. The post-treatment applied for APS deposits led to increase in hardness of 40% without showing cracks. Furthermore, micro-mechanical properties of Fe{sub x}B coatings were examined by Shimadzu Dynamic Ultra-Microhardness Tester for estimating Young’s modulus and hardness due to load—unload sensing analysis by applying different loads such as 160, 320, and 640 mN to determine load and indentation depth dependency of APS Fe{sub x}B on Al substrate for each samples, in details.

36 MATERIALS SCIENCE↗

Review Article: Stress in thin films and coatings: Current status, challenges, and prospects

The issue of stress in thin films and functional coatings is a persistent problem in materials science and technology that has congregated many efforts, both from experimental and fundamental points of view, to get a better understanding on how to deal with, how to tailor, and how to manage stress in many areas of applications. With the miniaturization of device components, the quest for increasingly complex film architectures and multiphase systems and the continuous demands for enhanced performance, there is a need toward the reliable assessment of stress on a submicron scale from spatially resolved techniques. Also, the stress evolution during film and coating synthesis using physical vapor deposition (PVD), chemical vapor deposition, plasma enhanced chemical vapor deposition (PECVD), and related processes is the result of many interrelated factors and competing stress sources so that the task to provide a unified picture and a comprehensive model from the vast amount of stress data remains very challenging. This article summarizes the recent advances, challenges, and prospects of both fundamental and applied aspects of stress in thin films and engineering coatings and systems, based on recent achievements presented during the 2016 Stress Workshop entitled “Stress Evolution in Thin Films and Coatings: from Fundamental Understanding to Control.” Evaluation methods, implying wafer curvature, x-ray diffraction, or focused ion beam removal techniques, are reviewed. Selected examples of stress evolution in elemental and alloyed systems, graded layers, and multilayer-stacks as well as amorphous films deposited using a variety of PVD and PECVD techniques are highlighted. Based on mechanisms uncovered by in situ and real-time diagnostics, a kinetic model is outlined that is capable of reproducing the dependence of intrinsic (growth) stress on the grain size, growth rate, and deposited energy. The problems and solutions related to stress in the context of optical coatings, inorganic coatings on plastic substrates, and tribological coatings for aerospace applications are critically examined. This review also suggests strategies to mitigate excessive stress levels from novel coating synthesis perspectives to microstructural design approaches, including the ability to empower crack-based fabrication processes, pathways leading to stress relaxation and compensation, as well as management of the film and coating growth conditions with respect to energetic ion bombardment. Future opportunities and challenges for stress engineering and stress modeling are considered and outlined.

36 MATERIALS SCIENCE↗

Corrosion and Fatigue Behavior of High-Strength Steel Treated with a Zn-Alloy Thermo-diffusion Coating

High and low cycle fatigue tests were conducted on high-strength steel using four-point bending. The materials tested were ASTM A723 steel in the as-machined condition, grit-blasted condition, MIL-DTL-16232 heavy manganese phosphate-coated condition, and ASTM A1059 Zn-alloy thermo-diffusion coated (Zn-TDC). The ASTM A723 steel base material exhibits a yield strength of ~1000 MPa. The effects of the surface treatments versus uncoated steel were examined. The fatigue life of the Zn-TDC specimens was generally reduced on as-coated specimens versus uncoated or phosphate-coated specimens. Several mechanisms are examined including the role of compressive residual stress relief with the Zn-TDC process as well as fatigue crack initiation from the hardened Zn-Fe alloy surface layer produced in the gas-metal reaction. Additionally, the effects of corrosion pitting on the fatigue life of coated specimens are explored as the Zn-TDC specimens exhibit significantly improved corrosion resistance over phosphate-coated and oiled specimens.

36 MATERIALS SCIENCE↗

Parametric Optimization of Erosive Wear Response of TiAlN-Coated Aluminium Alloy Using Taguchi Method

In this research work, high-velocity oxy-fuel thermal spraying is used to develop TiAlN coatings on AA1050 and AA5083 aluminium alloy substrates. Slurry wear behavior of coatings is evaluated using jet-type test rig. Surface studies were carried out to investigate the potential erosion mechanism. The influence of key parameters identified using the Taguchi analysis is also corroborated with a wear model. The potential mechanism identified by wear model is in excellent convergence with that observed experimentally. Mixed ploughing and cutting, formation of platelets, abrasion grooves and cracks are witnessed as primary mechanisms causing loss of coating. Results indicate that impact velocity is recognized as a highly contributing parameter with contribution ratio of 79.24 and 83.75% followed by impingement angle with contribution ratio of 15.81 and 11.58% for AA1050 and AA5083, respectively. The important sequences of the control parameters are recognized to be impact velocity > impingement angle > erodent feed rate > erodent size for AA1050 and impact velocity > impingement angle > erodent size > erodent feed rate for AA5083. The best possible combination of control parameters for AA1050 and AA5083 to achieve minimal wear rate with respect to impact velocity, erodent size, impingement angle and erodent feed rate is 30 m/s, 225 µm, 30°, 160 g/min and 25 m/s, 150 µm, 30°, 160 g/min, respectively.

36 MATERIALS SCIENCE↗

Self-generated concentration and modulus gradient coating design to protect Si nano-wire electrodes during lithiation

Surface coatings as artificial solid electrolyte interphases have been actively pursued as an effective way to improve the cycle efficiency of nanostructured Si electrodes for high energy density lithium ion batteries, where the mechanical stability of the surface coatings on Si is as critical as Si itself. However, the chemical composition and mechanical property change of coating materials during the lithiation and delithiation process imposed a grand challenge to design coating/Si nanostructure as an integrated electrode system. In our work, we first developed reactive force field (ReaxFF) parameters for Li–Si–Al–O materials to simulate the lithiation process of Si-core/Al 2 O 3 -shell and Si-core/SiO 2 -shell nanostructures. With reactive dynamics simulations, we were able to simultaneously track and correlate the lithiation rate, compositional change, mechanical property evolution, stress distributions, and fracture. A new mechanics model based on these varying properties was developed to determine how to stabilize the coating with a critical size ratio. Furthermore, we discovered that the self-accelerating Li diffusion in Al 2 O 3 coating forms a well-defined Li concentration gradient, leading to an elastic modulus gradient, which effectively avoids local stress concentration and mitigates crack propagation. Finally, based on these results, we propose a modulus gradient coating, softer outside, harder inside, as the most efficient coating to protect the Si electrode surface and improve its current efficiency.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The effect of bond coating surface modification on the performance of atmospheric plasma spray thermal barrier coatings

Asperities in atmospheric plasma sprayed (APS) CoNiCrAlY bond coatings were observed to rapidly form spinel-type oxides growing into the APS yttria-stabilized zirconia (YSZ) top coating during isothermal exposures. To minimize these transient oxides, bond coatings were either lightly or heavily modified to remove asperities, prior to top coating deposition. After a 100 h isothermal exposure at 1100 °C in dry air, modified regions formed a thin, Al-rich thermally grown oxide (TGO) scale while unmodified regions formed Cr- and Ni-rich transient oxide. However, in 1-h furnace cycle testing (FCT) at 1100 °C, the modified bond coatings showed a reduced average lifetime compared to the specimens with unmodified bond coatings. The benefit of asperities may be to geometrically inhibit crack propagation, but the volume of transient oxide formed may also densify the adjacent YSZ and further inhibit cracking.

36 MATERIALS SCIENCE↗

Crack Growth Rate at Oxygen Electrode/Electrolyte Interface in Solid Oxide Electrolysis Cells Predicted by Experiment Coupled Multiphysics Modeling

Solid oxide electrolysis cell (SOEC) is a very efficient hydrogen production technology, but the cell degradation is a serious limiting factor for its long-term implementation. Oxygen electrode (OE) delamination is reported to be the critical degradation mechanism. In this study, we present a methodology to understand the delamination failure of the OE due to chemical stress in a better perspective. Several OE configurations were tested: baseline strontium-doped lanthanum cobalt iron oxide (LSCF) single layer design and tantalum-doped strontium cobalt oxide (SCT) - LSCF bilayer designs with different SCT loadings. An electro-chemo-mechanical model is developed to associate the electrochemical behavior of the cell with solid mechanics for calculating crack growth of the cell during long term test. The bilayer configuration with SCT 20 wt% has better performance as it survived in the long-term life test with the least crack length. This study implies that an additional nano-coating of SCT over the OE have improved the species transport and oxygen evolution with reduced chemical stress. As the operating current density decreases, it takes longer time for the cell to reach the delamination with the same critical crack length of 6.5 μ m (∼93% of the electrode/electrolyte interface length). Finally, it was concluded that chemical stress plays a significant role in interface delamination failure, however it may not be the only source of stresses at the interface.

08 HYDROGEN↗

Numerical modeling of the SNS H{sup −} ion source

Ion source rf antennas that produce H- ions can fail when plasma heating causes ablation of the insulating coating due to small structural defects such as cracks. Reducing antenna failures that reduce the operating capabilities of the Spallation Neutron Source (SNS) accelerator is one of the top priorities of the SNS H- Source Program at ORNL. Numerical modeling of ion sources can provide techniques for optimizing design in order to reduce antenna failures. There are a number of difficulties in developing accurate models of rf inductive plasmas. First, a large range of spatial and temporal scales must be resolved in order to accurately capture the physics of plasma motion, including the Debye length, rf frequencies on the order of tens of MHz, simulation time scales of many hundreds of rf periods, large device sizes on tens of cm, and ion motions that are thousands of times slower than electrons. This results in large simulation domains with many computational cells for solving plasma and electromagnetic equations, short time steps, and long-duration simulations. In order to reduce the computational requirements, one can develop implicit models for both fields and particle motions (e.g. divergence-preserving ADI methods), various electrostatic models, or magnetohydrodynamic models. We have performed simulations using all three of these methods and have found that fluid models have the greatest potential for giving accurate solutions while still being fast enough to perform long timescale simulations in a reasonable amount of time. We have implemented a number of fluid models with electromagnetics using the simulation tool USim and applied them to modeling the SNS H- ion source. We found that a reduced, single-fluid MHD model with an imposed magnetic field due to the rf antenna current and the confining multi-cusp field generated increased bulk plasma velocities of > 200 m/s in the region of the antenna where ablation is often observed in the SNS source. We report here on comparisons of simulated plasma parameters and code performance using more accurate physical models, such as two-temperature extended MHD models, for both a related benchmark system describing a inductively coupled plasma reactor, and for the SNS ion source. We also present results from scaling studies for mesh generation and solvers in the USim simulation code.

07 ISOTOPE AND RADIATION SOURCES↗

Development of a Radial Deconsolidation Method

A series of experiments have been initiated to determine the retention or mobility of fission products* in AGR fuel compacts [Petti, et al. 2010]. This information is needed to refine fission product transport models. The AGR-3/4 irradiation test involved half-inch-long compacts that each contained twenty designed-to-fail (DTF) particles, with 20-μm thick carbon-coated kernels whose coatings were deliberately fabricated such that they would crack under irradiation, providing a known source of post-irradiation isotopes. The DTF particles in these compacts were axially distributed along the compact centerline so that the diffusion of fission products released from the DTF kernels would be radially symmetric [Hunn, et al. 2012; Hunn et al. 2011; Kercher, et al. 2011; Hunn, et al. 2007]. Compacts containing DTF particles were irradiated at Idaho National Laboratory (INL) at the Advanced Test Reactor (ATR) [Collin, 2015]. Analysis of the diffusion of these various post-irradiation isotopes through the compact requires a method to radially deconsolidate the compacts so that nested-annular volumes may be analyzed for post-irradiation isotope inventory in the compact matrix, TRISO outer pyrolytic carbon (OPyC), and DTF kernels. An effective radial deconsolidation method and apparatus appropriate to this application has been developed and parametrically characterized.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Engineering Precisely Controlled Negative and Zero Thermal Expansion Behaviors in Metal-Organic Frameworks

Positive thermal expansion can cause significant stress or even catastrophic device failure in applications where materials are placed in confined environments. At material interfaces such as coatings, thermal expansion effects can also lead to cracking and peeling behavior. The ability to impart controlled thermal expansion properties in an array of designs via additive manufacturing technologies would mitigate such problems and bring significant value to various materials science and engineering challenges. Negative thermal expansion materials are of interest for composite material applications whereby they can compensate for the behavior of a positive thermal expansion matrix. This Truman Fellowship LDRD research project presents complimentary experimental and molecular modeling results towards the fundamental understanding and development of metal-organic framework (MOF) materials with controlled thermal expansion properties. Design strategies for imparting precisely tailored negative, zero, and positive thermal expansion regimes in MOFs are studied and the implications of these design strategies for the use of MOFs as an emergent negative thermal expansion material class are examined. Challenges towards exploiting this nanoscale behavior at length scales relevant to composite material systems are introduced. ACKNOWLEDGEMENTS I will be forever grateful to the Truman Fellowship Selection Committee for providing me with the opportunity to pursue this research project. The unique opportunity to carry out this exciting scientific research with all of the resources and support that Sandia has to offer has been a truly rewarding experience. I would like to especially thank Yolanda Moreno for her endless assistance throughout my time as a Truman Fellow. It is hard to imagine a more supportive and stimulating scientific environment to carry out this research. I would also like to thank all of my colleagues and the individuals that have collaborated with me throughout this Fellowship, both internal and external to Sandia. Many of you appear as co-authors on the publications resulting from this LDRD, including especially fruitful collaborations with researchers at the Georgia Institute of Technology and the University of Amsterdam. I cannot express enough my gratitude for the significant role that you all played in shaping my educational experience and the success during my time at Sandia as a Truman Fellow.

36 MATERIALS SCIENCE↗

The influence of electrode crack dimensions on the durability of polymer electrolyte membrane fuel cells

Electrode cracks in polymer electrolyte membrane fuel cells (PEMFCs) are correlated with early onset failures. Here, in this work we investigate the influence of cracked gas diffusion electrodes (GDEs) on the durability of the membrane electrode assembly (MEA) using a combined chemical-mechanical accelerated stress test (AST). Electrode crack dimensions were systematically tuned using ink formulations and material selection strategies. A parameter to describe the crack width areal density (Φ CW ) was used to quantify the degree of discontinuity in the electrode surfaces. Open circuit voltage (OCV) transient analyses were used to benchmark and characterize the failure mechanisms in the MEAs as a function of the Φ CW . While smaller electrode-level cracks, on the order of microns, yielded a 28 % decrease in operating lifetime, larger cracks that propagated from a discontinuous, microporous layer (MPL) coating, decreased the operating lifetime by 56 %. This work emphasizes the need for material processing strategies that consider defect tolerances to limit membrane failures in PEMFCs.

08 HYDROGEN↗

Electrodeposited Mo x S y O z /Ni Tribological Coatings

Deposition of molybdenum disulfide (MoS 2 ) coatings using physical vapor deposition (PVD) and mechanical burnishing has been widely assessed for solid lubricants in space applications but still suffers from line-of-sight constraints on complex geometries. Here, we highlight one of the first demonstrations of electrodeposited Mo x S y O z and Mo x S y O z /Ni thin-film coatings from aqueous solutions of ammonium tetrathiomolybdate for solid lubricant applications and their remarkable ability to provide low coefficients of friction and high wear resistance. Characterization of the coating morphology shows amorphous microstructures with a high oxygen content and cracking upon drying. Even so, electrodeposited Mo x S y O z can achieve low steady-state coefficients of friction (μ ∼ 0.05–0.06) and wear rates (2.6 × 10 –7 mm 3 /(N m)) approaching those of physical vapor deposited coatings (2.3 × 10 –7 mm 3 /(N m)). Additionally, we show that adding dopants such as nickel increased the wear rate (7.5 × 10 –7 mm 3 /(N m)) and initial coefficient of friction (μ i = 0.23) due to compositional modifications such as dramatic sub-stoichiometry (S/Mo ∼ 1) and expression of a NiO x surface layer, although doping did reduce the degree of cracking upon drying.

Babuska, Tomas F.↗

Cyclic nanoindentation studies on CrN thin films prepared by RF sputtering on Zr-based metallic glass

Cyclic nanoindentation tests were carried out to study the influence of the chromium nitride thin films on the mechanical properties of Zr-based metallic glass. Chromium nitride thin coatings have been deposited on Zr{sub 50}Cu{sub 40}Al{sub 10} metallic glass substrate by RF sputtering. The deposition process was done at room temperature under nitrogen reactive gas using a metallic chromium target. The CrN films have a thickness of 300 nm. Several cyclic nanoindentation measurements were conducted on CrN films and Zr{sub 50}Cu{sub 40}Al{sub 10} metallic glass substrate samples at various loading rate values. We have found that the coated metallic glass sample shows high mechanical properties such as hardness and reduced elastic modulus. Cyclic nanoindentation results show a hardening behaviour for these CrN coatings. Moreover, the CrN coated on Zr-based metallic glass was found to have a high value of resistance to crack propagation, as being analysed through the SEM pictures of the residual Vickers indentation impressions.

36 MATERIALS SCIENCE↗