Search NASA⌕ Search

SEARCH · Search NASA

Results for “advanced coating”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Testbed for Lunar Extreme Environment Wear Tolerant Applications

The abrasive dust from lunar regolith poses significant long-term durability and performance challenges to materials, vehicles, mechanisms and structures that will be used for the next generation of lunar exploration. The development of advanced materials, coatings and device technologies that can withstand these abrasive particles and extreme environmental conditions is critical. However, the lack of standardized and accessible methods for evaluating such materials and devices in a facsimile of the harsh lunar environment hinders progress in dust-tolerant technologies. To address this challenge, NASA Langley Research Center is creating an extreme environment testbed. This reconfigurable testbed will allow rapid, repeatable wear testing of material and candidate mechanisms under vacuum conditions, facilitating the development of critical materials technologies for lunar exploration. Preliminary results from exposing an actuating mechanism similar to a pin joint to lunar regolith simulant under high vacuum are reported.

lunar dust↗

Testbed for Lunar Extreme Environment Wear Tolerant Applications

The abrasive dust from lunar regolith poses significant long-term durability and performance challenges to materials, vehicles, mechanisms and structures that will be used for the next generation of lunar exploration. The development of advanced materials, coatings and device technologies that can withstand these abrasive particles and extreme environmental conditions is critical. However, the lack of standardized and accessible methods for evaluating such materials and devices in a facsimile of the harsh lunar environment hinders progress in dust-tolerant technologies. To address this challenge, NASA Langley Research Center is creating an extreme environment testbed. This reconfigurable testbed will allow rapid, repeatable wear testing of material and candidate mechanisms under vacuum conditions, facilitating the development of critical materials technologies for lunar exploration. Preliminary results from exposing an actuating mechanism similar to a pin joint to lunar regolith simulant under high vacuum are reported.

lunar dust↗

Oxidation Study of an Ultra High Temperature Ceramic Coatings Based on HfSiCN

High temperature fiber-reinforced ceramic matrix composites (CMCs) are important for aerospace applications because of their low density, high strength, and significantly higher-temperature capabilities compared to conventional metallic systems. The use of the SiCf/SiC and Cf/SiC CMCs allows the design of lighter-weight, more fuel efficient aircraft engines and also more advanced spacecraft airframe thermal protection systems. However, CMCs have to be protected with advanced environmental barrier coatings when they are incorporated into components for the harsh environments such as in aircraft engine or spacecraft applications. In this study, high temperature oxidation kinetics of an advanced HfSiCN coating on Cf/SiC CMC substrates were investigated at 1300 C, 1400 C, and 1500 C by using thermogravimetric analysis (TGA). The coating oxidation reaction parabolic rate constant and activation energy were estimated from the experimental results. The oxidation reaction studies showed that the coatings formed the most stable, predominant HfSiO4-HfO2 scales at 1400 C. A peroxidation test at 1400 C then followed by subsequent oxidation tests at various temperatures also showed more adherent scales and slower scale growth because of reduced the initial transient oxidation stage and increased HfSiO4-HfO2 content in the scales formed on the HfSiCN coatings.

Environmental Barrier Coatings↗

Oxidation Study of an Ultra High Temperature Ceramic Coatings Based on HfSiCN

High temperature fiber-reinforced ceramic matrix composites (CMCs) are important for aerospace applications because of their low density, high strength, and significantly higher-temperature capabilities compared to conventional metallic systems. The use of the SiCf/SiC and Cf/SiC CMCs allows the design of lighter-weight, more fuel efficient aircraft engines and also more advanced spacecraft airframe thermal protection systems. However, CMCs have to be protected with advanced environmental barrier coatings when they are incorporated into components for the harsh environments such as in aircraft engine or spacecraft applications. In this study, high temperature oxidation kinetics of an advanced HfSiCN coating on Cf/SiC CMC substrates were investigated at 1300 C, 1400 C, and 1500 C by using thermogravimetric analysis (TGA). The coating oxidation reaction parabolic rate constant and activation energy were estimated from the experimental results. The oxidation reaction studies showed that the coatings formed the most stable, predominant HfSiO4-HfO2 scales at 1400 C. A peroxidation test at 1400 C then followed by subsequent oxidation tests at various temperatures also showed more adherent scales and slower scale growth because of reduced the initial transient oxidation stage and increased HfSiO4-HfO2 content in the scales formed on the HfSiCN coatings.

Ultra High Temperature Ceramics (UHTC)↗

Exposure of Highly Reflective Far-Ultraviolet Coatings to LEO Environment for TRL Advancement for the Habitable Worlds Observatory

Over the past several years, our team at the NASA Goddard Space Flight Center (GSFC), in collaboration with the Jet Propulsion Laboratory (JPL) and the Naval Research Laboratory (NRL), have developed several new protected Al coating technologies with improved Far-Ultraviolet (FUV) reflectance performance and more robust environmental stability. These include Al protected with lithium-based fluoride (LiF) coatings such as hot deposited LiF (eLiF), XeF 2 -passivated LiF coatings (XeLiF), Li 3 AlF 6 overcoats, AlF 3 (plasma passivated), and XeF 2 passivated MgF 2 coatings (XeMgF 2 ). However, despite these developments, relatively little experimental information exists regarding the long-term stability of these coatings after simultaneous exposure to the Low Earth Orbit (LEO) environment. To evaluate their environmental durability and advance their Technology Readiness Level (TRL), representative samples of these coating technologies, Al+XeLiF, Al+eLiF, Al+Li 3 AlF 6 , Al+AlF 3 , Al+XeMgF 2 , and bare Al as reference samples, were flown onboard the International Space Station (ISS) as part of the Materials International Space Station Experiment 20 (MISSE-20). The MISSE platform is operated by Aegis Aerospace for relatively long-duration (e.g. 6 months) external exposure experiments in a space environment. The coatings were deposited on ULE and Zerodur substrates, and witness samples deposited on the same coatings runs, but on glass slides were left on Earth as control. A subset of the flight samples were fitted with MgF 2 windows to reduce direct exposure to atomic oxygen (AO) and charged particles, and still let through UV and other types of radiation on these samples. After approximately 6 months of exposure in the forward-facing (RAM) direction, the samples were returned to Earth and characterized by performing FUV/NUV/VIS/NIR reflectance measurements to quantify degradation, spectroscopic ellipsometry to evaluate coating thickness and optical constants, atomic force microscopy (AFM) to quantify surface roughness evolution during the flight in the ISS. The MgF 2 protective windows were also analyzed through FUV transmission measurements. Comparison with the witness samples left on the ground and with the flown bare Al samples (with just the naturally occurring Al 2 O 3 layer) provided a quantitative assessment of coating thickness variations, optical performance degradation, and morphological changes induced by prolonged exposure to the LEO environment.

Far Ultraviolet (FUV)↗

Oxidation Study of an Ultra High Temperature Ceramic Coatings Based on HfSICN

High temperature fiber-reinforced ceramic matrix composites (CMCs) are important for aerospace applications because of their low density, high strength, and significantly higher-temperature capabilities compared to conventional metallic systems. The use of the SiC(sub f)/SiC and C(sub f)/SiC CMCs allows the design of lighter-weight, more fuel efficient aircraft engines and also more advanced spacecraft airframe thermal protection systems. However, CMCs have to be protected with advanced environmental barrier coatings when they are incorporated into components for the harsh environments such as in aircraft engine or spacecraft applications. In this study, high temperature oxidation kinetics of an advanced HfSiCN coating on C(sub f)/SiC CMC substrates were investigated at 1300 C, 1400 C, and 1500 C by using thermogravimetric analysis (TGA). The coating oxidation reaction parabolic rate constant and activation energy were estimated from the experimental results. The oxidation reaction studies showed that the coatings formed the most stable, predominant HfSiO4-HfO2 scales at 1400 C. A peroxidation test at 1400 C then followed by subsequent oxidation tests at various temperatures also showed more adherent scales and slower scale growth because of reduced the initial transient oxidation stage and increased HfSiO4-HfO2 content in the scales formed on the HfSiCN coatings.

environmental barrier coatings (EBCs)↗

Delamination Mechanisms of Thermal and Environmental Barrier Coatings on SiC/SiC Ceramic Matrix Composites

Advanced ceramic thermal harrier coatings will play an increasingly important role In future gas turbine engines because of their ability to effectively protect the engine components and further raise engine temperatures. However, the coating durability issue remains a major concern with the ever-increasing temperature requirements. In this paper, thermal cyclic response and delamination failure modes of a ZrO2-8wt%Y2O3 and mullite/BSAS thermaVenvironmenta1 barrier coating system on SiC/SiC ceramic matrix composites were investigated using a laser high-heat-flux technique. The coating degradation and delamination processes were monitored in real time by measuring coating apparent conductivity changes during the cyclic tests under realistic engine temperature and stress gradients, utilizing the fact that delamination cracking causes an apparent decrease in the measured thermal conductivity. The ceramic coating crack initiation and propagation driving forces under the cyclic thermal loads, in conjunction with the mechanical testing results, will be discussed.

Zhu, Dongming↗

Delamination Mechanisms of Thermal and Environmental Barrier Coatings on SiC/SiC Ceramic Matrix Composites

Advanced ceramic thermal barrier coatings will play an increasingly important role in future gas turbine engines because of their ability to effectively protect the engine components and further raise engine temperatures. However, the coating durability issue remains a major concern with the ever-increasing temperature requirements. In this paper, thermal cyclic response and delamination failure modes of a ZrO2-8wt%Y2O3 and mullite/BSAS thermal/environmental barrier coating system on SiC/SiC ceramic matrix composites were investigated using a laser high-heat-flux technique. The coating degradation and delamination processes were monitored in real time by measuring coating apparent conductivity changes during the cyclic tests under realistic engine temperature and stress gradients, utilizing the fact that delamination cracking causes an apparent decrease in the measured thermal conductivity. The ceramic coating crack initiation and propagation driving forces under the cyclic thermal loads, in conjunction with the mechanical testing results, will be discussed.

Zhu, Dongming↗

Performance Evaluation and Modeling of Erosion Resistant Turbine Engine Thermal Barrier Coatings

The erosion resistant turbine thermal barrier coating system is critical to the rotorcraft engine performance and durability. The objective of this work was to determine erosion resistance of advanced thermal barrier coating systems under simulated engine erosion and thermal gradient environments, thus validating a new thermal barrier coating turbine blade technology for future rotorcraft applications. A high velocity burner rig based erosion test approach was established and a new series of rare earth oxide- and TiO2/Ta2O5- alloyed, ZrO2-based low conductivity thermal barrier coatings were designed and processed. The low conductivity thermal barrier coating systems demonstrated significant improvements in the erosion resistance. A comprehensive model based on accumulated strain damage low cycle fatigue is formulated for blade erosion life prediction. The work is currently aiming at the simulated engine erosion testing of advanced thermal barrier coated turbine blades to establish and validate the coating life prediction models.

Miller, Robert A.↗

Application and Development of Atomic Layer Deposition Techniques to Improve Thermo-Optical Coatings for Spacecraft Thermal Control and Advanced Optical Instruments

A key technology development driver in environmental control systems and next generation optics are discussed utilizing thin film development borrowed from the semiconductor industry. The optical and physical properties of spacecraft radiator coatings are dictated by orbital environmental conditions. For example, coatings must adequately dissipate charge buildup when orbital conditions, such as polar, geostationary or gravity neutral, result in surface charging. Current dissipation techniques include depositing a layer of ITO (indium tin oxide) on the radiator surface in a high temperature process. The application of these enhanced coatings must be such that the properties in question are tailored to mission-specific requirements. The multi-billion-dollar semiconductor industry has adopted Atomic Layer Deposition (ALD) for self-assembly and atomic-scale placement. ALD is a cost-effective nanoadditive-manufacturing technique that allows for the conformal coating of substrates with atomic control in a benign temperature and pressure environment. By using ALD, modification of these coatings can be accomplished during coating application preprocessing. The preprocessing is rendered directly on the coating dry pigment before binding. Through the introduction of paired precursor gases, thin films can be deposited on a myriad of substrates ranging from glass, polymers, aerogels, metals, powders, and other high aspect-ratio micro- and nano- structures. By providing atomic-level control, where single layers of atoms can be deposited, the fabrication of metal transparent films, precise nano-laminates, and coatings of nano-channels and pores is achievable. A method has been demonstrated for the ALD of In2O3 and films on a variety of substrates from Si(100) wafers, glass slides, and on Z93P pigments resulting in a direct spaceflight application. Results will be presented that verify the chemical composition of ALD pigments and charge dissipation properties when the pigment goes through its binding and coating process and we present early results of ALD for carbon nanotube formation and encapsulation.

Dwivedi, Vivek H.↗

Environmental Barrier Coating Fracture, Fatigue and High-Heat-Flux Durability Modeling and Stochastic Progressive Damage Simulation

Advanced environmental barrier coatings will play an increasingly important role in future gas turbine engines because of their ability to protect emerging light-weight SiC/SiC ceramic matrix composite (CMC) engine components, further raising engine operating temperatures and performance. Because the environmental barrier coating systems are critical to the performance, reliability and durability of these hot-section ceramic engine components, a prime-reliant coating system along with established life design methodology are required for the hot-section ceramic component insertion into engine service. In this paper, we have first summarized some observations of high temperature, high-heat-flux environmental degradation and failure mechanisms of environmental barrier coating systems in laboratory simulated engine environment tests. In particular, the coating surface cracking morphologies and associated subsequent delamination mechanisms under the engine level high-heat-flux, combustion steam, and mechanical creep and fatigue loading conditions will be discussed. The EBC compostion and archtechture improvements based on advanced high heat flux environmental testing, and the modeling advances based on the integrated Finite Element Analysis Micromechanics Analysis Code/Ceramics Analysis and Reliability Evaluation of Structures (FEAMAC/CARES) program will also be highlighted. The stochastic progressive damage simulation successfully predicts mud flat damage pattern in EBCs on coated 3-D specimens, and a 2-D model of through-the-thickness cross-section. A 2-parameter Weibull distribution was assumed in characterizing the coating layer stochastic strength response and the formation of damage was therefore modeled. The damage initiation and coalescence into progressively smaller mudflat crack cells was demonstrated. A coating life prediction framework may be realized by examining the surface crack initiation and delamination propagation in conjunction with environmental degradation under high-heat-flux and environment load test conditions.

Mechanical creep and fatigue loading condition↗

Creep, Fatigue and Fracture Behavior of Environmental Barrier Coating and SiC-SiC Ceramic Matrix Composite Systems: The Role of Environment Effects

Advanced environmental barrier coating (EBC) systems for low emission SiCSiC CMC combustors and turbine airfoils have been developed to meet next generation engine emission and performance goals. This presentation will highlight the developments of NASAs current EBC system technologies for SiC-SiC ceramic matrix composite combustors and turbine airfoils, their performance evaluation and modeling progress towards improving the engine SiCSiC component temperature capability and long-term durability. Our emphasis has also been placed on the fundamental aspects of the EBC-CMC creep and fatigue behaviors, and their interactions with turbine engine oxidizing and moisture environments. The EBC-CMC environmental degradation and failure modes, under various simulated engine testing environments, in particular involving high heat flux, high pressure, high velocity combustion conditions, will be discussed aiming at quantifying the protective coating functions, performance and durability, and in conjunction with damage mechanics and fracture mechanics approaches.

Environmental Barrier Coatings↗

Environmental Barrier Coating Development for SiC/SiC Ceramic Matrix Composites: Recent Advances and Future Directions

This presentation briefly reviews the SiC/SiC major environmental and environment-fatigue degradations encountered in simulated turbine combustion environments, and thus NASA environmental barrier coating system evolution for protecting the SiC/SiC Ceramic Matrix Composites for meeting the engine performance requirements. The presentation will review several generations of NASA EBC materials systems, EBC-CMC component system technologies for SiC/SiC ceramic matrix composite combustors and turbine airfoils, highlighting the temperature capability and durability improvements in simulated engine high heat flux, high pressure, high velocity, and with mechanical creep and fatigue loading conditions. This paper will also focus on the performance requirements and design considerations of environmental barrier coatings for next generation turbine engine applications. The current development emphasis is placed on advanced NASA candidate environmental barrier coating systems for SiC/SiC CMCs, their performance benefits and design limitations in long-term operation and combustion environments. The efforts have been also directed to developing prime-reliant, self-healing 2700F EBC bond coat; and high stability, lower thermal conductivity, and durable EBC top coats. Major technical barriers in developing environmental barrier coating systems, the coating integrations with next generation CMCs having the improved environmental stability, erosion-impact resistance, and long-term fatigue-environment system durability performance will be described. The research and development opportunities for turbine engine environmental barrier coating systems by utilizing improved compositions, state-of-the-art processing methods, and simulated environment testing and durability modeling will be briefly discussed.

Environmental Barrier Coatings↗

Design and Performance Optimizations of Advanced Erosion-Resistant Low Conductivity Thermal Barrier Coatings for Rotorcraft Engines

Thermal barrier coatings will be more aggressively designed to protect gas turbine engine hot-section components in order to meet future rotorcraft engine higher fuel efficiency and lower emission goals. For thermal barrier coatings designed for rotorcraft turbine airfoil applications, further improved erosion and impact resistance are crucial for engine performance and durability, because the rotorcraft are often operated in the most severe sand erosive environments. Advanced low thermal conductivity and erosion-resistant thermal barrier coatings are being developed, with the current emphasis being placed on thermal barrier coating toughness improvements using multicomponent alloying and processing optimization approaches. The performance of the advanced thermal barrier coatings has been evaluated in a high temperature erosion burner rig and a laser heat-flux rig to simulate engine erosion and thermal gradient environments. The results have shown that the coating composition and architecture optimizations can effectively improve the erosion and impact resistance of the coating systems, while maintaining low thermal conductivity and cyclic oxidation durability

Zhu, Dongming↗

Advances in Detector-Integrated Filter Coatings for the Far Ultraviolet

We report on the continued development of multilayer optical coatings on back-illuminated silicon imaging sensors in order to enhance the functionality of such systems at ultraviolet wavelengths. This includes the development metal-dielectric filter structures to enable solar-blind operation, and graded thickness coatings to tune the spatial response of a detector system to the dispersion of a spectrometer. Such systems can maintain the high internal quantum efficiency afforded by the delta-doping process utilized at NASA JPL, while also providing long-wavelength rejection or a spatially optimized efficiency (or both). We present the characterization of CCD and CMOS image sensors incorporating these processes, and describe the atomic layer deposition coating processes. Such detectors are currently being developed for ground-based high energy physics applications as well as NASA orbital astrophysics instruments operating at wavelengths shorter than 200 nm.

Nikzad, Shouleh↗

Thermal control/oxidation resistant coatings for titanium-based alloys

Extensive research and development efforts have been expended toward development of thermal control and environmental protection coatings for NASP and generic hypersonic vehicle applications. The objective of the coatings development activities summarized here was to develop light-weight coatings for protecting advanced titanium alloys from oxidation in hypersonic vehicle applications. A number of new coating concepts have been evaluated. Coated samples were exposed to static oxidation tests at temperatures up to 1000 C using a thermogravimetric apparatus. Samples were also exposed to simulated hypersonic flight conditions for up to 10 hr to determine their thermal and chemical stability and catalytic efficiency. The emittance of samples was determined before and after exposure to simulated hypersonic flight conditions.

Clark, Ronald K.↗

Materials Overview

The Materials and Structures for High Performance project has made excellent progress in the development of advanced high-temperature materials and computational materials science tools to enable high-performance, hgh-efficiency, and environmentally compatible propulsion systems. Ceramic matrix composite (CMC) systems with 2700 O F temperature capability are initially being developed for low NO, combustor liners and turbine vanes. The feasibility of pushing CMC technologies to 3000 O F through revolutionary concepts is also being pursued. Achieving fuel savings of 8 to 15 percent requires higher turbine inlet temperatures as well as reductions in engine weight. An advanced disk alloy has been evaluated for application in future engines. Advanced thermal barrier coatings (TBC s) will enable 3200 O F turbine rotor inlet temperature capability. Advanced alloy development and the development of computational tools for the design of these future alloys will further enable attainment of these goals. Innovative lightweight materials, and structural and nozzle aerodynamic concepts are also being developed to reduce the weight of engine static structures to contribute toward overall fuel savings. Rig tests will demonstrate long-term durability of CMC linersand vanes and advanced turbine airfoil alloy systems, as well as fabricability of components with the highest payoff potential using the lightweight materials and structures concepts being developed.

Draper, Robert↗

Materials and structural aspects of advanced gas-turbine helicopter engines

Advances in materials, coatings, turbine cooling technology, structural and design concepts, and component-life prediction of helicopter gas-turbine-engine components are presented. Stationary parts including the inlet particle separator, the front frame, rotor tip seals, vanes and combustors and rotating components - compressor blades, disks, and turbine blades - are discussed. Advanced composite materials are considered for the front frame and compressor blades, prealloyed powder superalloys will increase strength and reduce costs of disks, the oxide dispersion strengthened alloys will have 100C higher use temperature in combustors and vanes than conventional superalloys, ceramics will provide the highest use temperature of 1400C for stator vanes and 1370C for turbine blades, and directionally solidified eutectics will afford up to 50C temperature advantage at turbine blade operating conditions. Coatings for surface protection at higher surface temperatures and design trends in turbine cooling technology are discussed. New analytical methods of life prediction such as strain gage partitioning for high temperature prediction, fatigue life, computerized prediction of oxidation resistance, and advanced techniques for estimating coating life are described.

Freche, J. C.↗