At least 19 records

Rapid solidification and dynamic compaction of Ni-base superalloy powders

A Ni-base superalloy containing 13Al-9Mo-2Ta (in at. percent) has been characterized in both the rapidly solidified condition and after dynamic compaction. Dynamically compacted specimens were examined in the as-compacted condition and observations related to current theories of interparticle bonding. In addition, the recrystallization behavior of the compacted material at relatively low temperature (about 0.5-0.75 Tm) was investigated.

Field, R. D.↗

The effects of Cr, Al, Ti, Mo, W, Ta, and Cb on the cyclic oxidation behavior of cast Ni-base superalloys at 1100 and 1150 C

Fifty Ni-base superalloys with concentrations of Cr, Al, Ti, Mo, W, Ta, and Cb systematically varied between two nonzero levels, were tested for cyclic oxidation resistance at 1100 and 1150 C. Oxidation resistance was interpreted in terms of the rate of specific weight change and the types of oxides formed. It is found that the resistance of the alloys to cyclic oxidation is largely determined by Al content, with a sharp increase in the oxidation resistance observed in the Al concentration range 5-8 at. pct. The effects of the other elements studied were small compared with that of aluminum. Best oxidation resistance characteristics were predicted for high Al (13 at. pct), low Cr (10 at. pct), low Ti (2 at. pct), low Cb (1 at. pct), and high Mo, W, and Ta (3 at. pct each). The effects of the refractory metals, however, are somewhat ambiguous and should be investigated further. Higher boron contents, which were unintentionally varied, were clearly detrimental even for the most resistant compositions.

Barrett, C. A.↗

Rapid solidification characteristics in melt spinning a Ni-base superalloy

The solidification kinetics involved in the process of melt spinning a Ni-base superalloy have been characterized. Through a correlation of ribbon thickness to melt puddle residence time, it was found that the solidification front velocity, V, is typically about 100 mm/sec at the ribbon surface not in contact with the spinning wheel. The rate of solidification varies within the ribbon, increasing with decreasing distance, S, from the wheel-contact surface as V = 3.65/s. Ribbon microstructure and texture characteristics are discussed in light of this kinetics result. The thickness-vs-time correlation was further analyzed to yield information about thermal history during ribbon formation. These thermal results are generally consistent with those deduced from dendrite arm spacing measurements.

Huang, S. C.↗

Estimate of conjugate gamma and gamma prime compositions in Ni-base superalloys

Approaches for estimating the composition of the matrix phase of alloys from the melt composition are reviewed. The first method is based on assigning essentially fixed stoichiometry to precipitating phases and is typified by PHACOMP. The second method uses analytical geometry to interpret phase diagrams and is applicable to a two-phase region of a six-component Ni-base system. The geometric method is also applicable to commercial Ni-base superalloys.

Dreshfield, R. L.↗

Estimation of conjugate gamma and gamma-prime compositions in Ni-base superalloys

To control the formation of unwanted phases, superalloy metallurgists have developed methods of estimating the composition of the matrix phase of alloys. That composition is then used to estimate the alloy's propensity toward sigma and other unwanted phase formations upon prolonged exposure to elevated temperatures in service. This paper reviews two approaches for estimating phase composition from the melt composition. One method is based on assigning essentially fixed stoichiometry to precipitating phases and is typified by 'PHACOMP'. The second method uses analytical geometry to interpret phase diagrams and is shown to be applicable to a two-phase region of a six-component Ni-base system. The geometric method is also shown to be applicable to commercial Ni-base superalloys.

Dreshfield, R. L.↗

The effects of Cr, Co, Al, Mo and Ta on the cyclic oxidation behavior of a prototype cast Ni-base superalloy based on a 2(5) composite statistically designed experiment

A series of cast Ni-base superalloys were systematically varied at selected levels of Co, Cr, Mo, Ta, and Al. The elemental levels varied were Mo, 0 to 4 percent; Cr, 6 to 18 percent; Co, 0 to 20 percent, Ta, 0 to 8 percent; and Al, 3.25 to 6.25 percent. The cyclic oxidation resistance was determined from specific weight change data as a function of time for 1 hr cycles in static air at 1100 C. The significant terms in decreasing order of their importance were Al, Ta, Cr2, Al-Cr, Cr-Co, Co2, Al-Mo, Cr-Mo, Al-Al, and Mo-Ta. The Al term alone accounted for close to 82 percent of the explained variability. The estimating equation showed that the Al level was the most important and should be at its 6.25 wt % maximum value. The Mo and Ta levels should also be at their maximum 4 and 8 wt % respectively. The cobalt composition should be as low as possible, i.e., 0 wt%. The Cr level optimum varies depending on the other 4 levels. The X-ray diffaction results indicate the most protective scales are alumina/aluminate spinel stabilizized with a tri-rutile oxide high in Ta and Mo.

Barrett, C. A.↗

The effect of Cr, Co, Al, Mo and Ta on a series of cast Ni-base superalloys on the stability of an aluminide coating during cyclic oxidation in Mach 0.3 burner rig

The influence of varying the content of Co, Cr, Mo, Ta, and Al in a series of cast Ni-based gamma/gamma'superalloys on the behavior of aluminide coatings was studied in burner rig cyclic oxidation tests at 1100 C. The alloys had nominally fixed levels of Ti, W, Cb, Zr, C, and B. The alloy compositions were based on a full 2(sup 5)-fractional statistical design supplemented by 10 star point alloys and a center point alloy. This full central composite design of 43 alloys plus two additional alloys with extreme Al levels allowed a complete second degree estimating equation to be derived from the 5-compositional variables. The weight change/time data for the coated samples fitted well to the paralinear oxidation model and enabled a modified oxidation attack parameter, K'(sub a) to be derived to rank the alloys and log K' (sub a ) to be used as the dependent variable in the estimating equation to determine the oxidation resistance of the coating as a function of the underlying alloy content. The most protective aluminide coatings are associated with the highest possible base ally contents of CR and Al and at a 4 percent Ta level. The Mo and Co effects interact but at fixed levels of 0, 5, or 10% Co. A 4% Mo level is optimum.

Zaplatynsky, I.↗

The effect of variations of cobalt content on the cyclic oxidation resistance of selected Ni-base superalloys

Cobalt levels were systematically varied in the Ni-base turbine alloys U-700 (cast), U-700m(PM/HIP), Waspaloy, Mar-M-247, In-738, Nimonic-115, U-720, and SX-R-150. The cobalt levels ranged from 0 wt % to the nominal commercial content in each alloy. The alloys were tested in cyclic oxidation in static air at 1000, 1100 and 1150 C for 500, 200 and 100 hr respectively. An oxidation attack parameter, Ka derived from the specific weight change versus time data was used to evaluate the oxidation behavior of the alloys along with X-ray diffraction analysis of the surface oxides. The alloys tend to form either Cr2O3/chromite spinel or Al2O3/aluminate spinel depending on the CR/Al ratio in the alloys. Alloys with a ratio of 3.5 or higher tend to favor the Cr oxides while those under 3.0 form mostly Al oxides. In general the Al2O3/aluminate spinel forming alloys have the better oxidation resistance. Increased cobalt content lowers the scaling resistance of the higher Cr alloys while a 5.0 wt % Co content is optimum for the Al controlling alloys. The refractory metals, particularly Ta, appear beneficial to both types of oxides perhaps due to the formation of the omni-present trirutile Ni(Ta,Cb,Mo,W)2O6. Both scales break down as increasing amounts of NiO is formed.

Barrett, C. A.↗

Reduction of chromium in Ni-base superalloys through element substitution and rapid solidification processing

The reduction in the use of Cr in Ni base superalloys by the combined approaches of both elemental substitution and rapid solidification processing is studied. The elements Si, Zr, Y and Hf were chosen as potential partial substitutes for Cr in Waspaloy and IN 713LC sine their separate addition to other alloys has previously resulted in enhanced oxidation resistance. The roles of Cr and these replacement elements in determining the microstructure and properties are evaluated. The elements Si, Zr, and Y and Hf are used as partial replacements for Cr in the base superalloys and these resultant alloys are processed using rapid solidification techniques. The mechanical properties and oxidation resistance of the processed materials are evaluated. The microstructure is characterized using state of the art techniques (e.g. analytical transmission electron microscopy), and the mechanism by which these structures are produced is determined.

Fraser, H. D.↗

The influence of hold times on LCF and FCG behavior in a P/M Ni-base superalloy

The relative importance of creep and environmental interactions in high temperature fatigue behavior has been investigated for as-HIP Rene 95. Strain-controlled low cycle fatigue and load-controlled fatigue crack growth tests were performed at elevated temperatures in argon, followed by fractographic analyses of the fracture surfaces by scanning electron microscopy. Fatigue lives were drastically reduced and crack growth rates increased one hundred fold as a result of superposition of hold times on continuous cycling. A change in fracture mode with hold time also was noted. Chromium oxide was detected on the fracture surface by Auger electron spectroscopy. The drastic changes in fatigue resistance due to hold times were attributed primarily to environmental interactions with fatigue processes.

Choe, S. J.↗

Synergistic erosion/corrosion of superalloys in PFB coal combustor effluent

Two Ni-based superalloys were exposed to the high velocity effluent of a pressurized fluidized bed coal combustor. Targets were 15 cm diameter rotors operating at 40,000 rpm and small flat plate specimens. Above an erosion rate threshold, the targets were eroded to bare metal. The presence of accelerated oxidation at lower erosion rates suggests erosion/corrosion synergism. Various mechanisms which may contribute to the observed oxide growth enhancement include erosive removal of protective oxide layers, oxide and subsurface cracking, and chemical interaction with sulfur in the gas and deposits through damaged surface layers.

Benford, S. M.↗

Synergistic erosion/corrosion of superalloys in PFB coal combustor effluent

Two Ni-based superalloys were exposed to the high velocity effluent of a pressurized fluidized bed coal combustor (PFBC). Targets were 15-cm diameter rotors operating at 40,000 rpm and small flat plate specimens. Above an erosion rate threshold (approximately 10 microns/hr), the targets were eroded to bare metal. The presence of accelerated oxidation at lower erosion rates suggests erosion/corrosion synergism. Various mechanisms which may contribute to the observed oxide growth enhancement include erosive removal of protective oxide layers, oxide and subsurface cracking, and chemical interaction with sulfur in the gas and deposits through damaged surface layers.

Benford, S. M.↗

Superalloy microstructural variations induced by gravity level during directional solidification

The Ni-base superalloy MAR-M246 (Hf) was directionally solidified during low gravity maneuvers aboard a NASA KC-135 aircraft. Gravity force variations during this process yielded a concomitant variation in microstructure and microsegregation. Secondary dendrite arm spacings are noted to be larger in the low-g portion; this, in turn, decreases the extent of interdendritic segregation. The amount of Hf in both the carbides and interdendritic eutectic increases as the gravity force diminishes. Fewer carbides are present in the low-g regions.

Johnston, M. H.↗

Diffusion welding of MA 6000 and a conventional nickel-base superalloy

A feasibility study of diffusion welding the oxide dispersion strengthened (ODS) alloy MA 6000 to itself and to conventional Ni-base superalloy Udimet 700 was conducted. Butt joints between MA 6000 pieces and lap joints between Udimet 700 and the ODS alloy were produced by hot pressing for 1.25 hr at temperatures ranging from 1000 to 1200 C (1832-2192 F) in vacuum. Following pressing, all weldments were heat treated and machined into mechanical property test specimens. While three different combinations of recrystallized and unrecrystallized MA 6000 butt joints were produced, the unrecrystallized to unrecrystallized joint was most successful as determined by mechanical properties and microstructural examination. Failure to weld the recrystallized material probably related to a lack of adequate deformation at the weld interface. While recrystallized MA 6000 could be diffusion welded to Udimet 700 in places, complete welding over the entire lap joint was not achieved, again due to the lack of sufficient deformation at the faying surfaces. Several methods are proposed to promote the intimate contact necessary for diffusion welding MA 6000 to itself and to superalloys.

Moore, T. J.↗

Creep-fatigue behavior of NiCoCrAlY coated PWA 1480

This study of high-temperature fatigue and creep-fatigue behavior is part of a program to identify the basic features of the effects of temperature, creep, fatigue, and environment on the behavior of a single crystal superalloy, a bulk coating alloy, and a coated alloy system. A system was selected which has had considerable production experience: the Ni-base superalloy, PWA 1480, and the NiCoCrAlY coating, PWA 276. Isothermal behavior was studied first. A series of fatigue and creep fatigue tests of the types commonly designated as pp, cp, pc and cc were conducted. These tests were conducted at various constant total strain ranges. The creep-fatigue cycles employed constant stress dwells at the maximum and/or minimum load. Test results are given.

Miner, R. V.↗

Long-term high-velocity oxidation and hot corrosion testing of several NiCrAl and FeCrAl base oxide dispersion strengthened alloys

Several oxide dispersion strengthened (ODS) alloys have been tested for cyclic, long-term, high gas-velocity resistance to oxidation at 1100 C and hot corrosion at 900 C. Both nominally Ni-16Cr-4Al and Fe-20Cr-4.5Al ODS alloys were subjected up to about 2500 cycles, where each cycle consisted of 1 hr in a hot, Mach 0.3 combusted gas stream followed by a 3-min quench in an ambient temperature, Mach 0.3 air blast. For comparison to existing technology, a coated superalloy was simultaneously tested. The ODS iron alloy exhibited clearly superior behavior, surviving 3800 oxidation and 2300 hot corrosion cycles essentially unscathed. While the ODS nickel alloys exhibited adequate oxidation resistance, the long-term hot corrosion resistance could be marginal, since the best life for such alloys under these conditions was only about 1100 cycles. However, the hot corrosion resistance of the ODS Ni-base alloys is excellent in comparison to that of traditional superalloys.

Lowell, C. E.↗