Reaction of sulfur dioxide with modified 440C, studied by Auger electron spectroscopy and depth profiling
Auger electron spectroscopy and sputtering were used to study the interaction of SO2 with modified 440C, which is a nominally 77-wt%-Fe, 14-wt%-Cr, and 4-wt%-Mo bearing steel with C, S, Si, Ni, V, P, and Mn making up the balance. The sample was polycrystalline. Three temperatures were used: room temperature, 500 C, and 600 C. The reaction time was varied from 30 minutes to 2 hours. A surface cleaned of oxides was the starting point for each reaction. For reactions at 500 C, the major constituents Cr, O, Fe, and S were present in the surface film. At 600 C, the principal constituents of the film were Cr, O, and S with no Fe present. Therefore, a transition in film composition occurred between 500 and 600 C. Oxides were the primary constituents of the films at both temperatures. Room-temperature reactions indicated that SO2 adsorbed dissociatively, with approximately equal quantities of S and O on the surface. For the same reaction time (1 hr) and pressure, a strong temperature dependence of film thickness was observed. The film formed at 600 C was approximately seven times thicker than that formed at 500 C.