Search NASA⌕ Search

SEARCH · Search NASA

Results for “LLZO solid-state electrolyte”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Mapping of fracture and ionic conductivity changes in ion implanted solid electrolytes: Insights from molecular dynamics

Ion implantation emerges as a promising technique to address the persistent challenge of lithium (Li) filament growth in solid-state electrolytes as it can induce compressive stresses inhibiting crack growth and deflect dendrites, de facto mitigating early electrolyte failure. In this study, we examine the potential paradox of ion implantation: while aiming to enhance electrolyte performance, the radiation damage associated with implantation might inadvertently compromise both the ionic conductivity and the intrinsic fracture toughness of the material, rendering the material unsuitable for battery applications. Specifically, we employed molecular dynamics simulations to examine the scope of the downsides of ion implantation, specifically: (i) reduced ionic conductivity (due to radiation-induced amorphization) and (ii) mechanical stability (due to radiation-induced embrittlement) in ion-implanted Li 7 La 3 Zr 2 O 12 (LLZO) solid-state electrolytes. We explore how radiation damage impacts LLZO’s crystalline structure, Li-ion diffusion, and fracture properties at various temperatures and radiation damage levels. The study aims to provide insights into the competing effects of ion implantation and suggest potential engineering strategies for developing more robust solid-state electrolytes with improved conductivity and dendrite resistance.

Conductivity↗

Digital light processing of porous LLZTO scaffolds for Li-garnet solid-state batteries

Li 7 La 3 Zr 2 O 12 (LLZO)-based solid-state electrolytes (SEs) are promising materials for next-generation solid-state batteries. In this work, digital light processing (DLP), an emerging additive manufacturing technology, is employed to produce porous Ta-doped LLZO (LLZTO) scaffolds. The self-standing scaffolds are 100 μm thick and have 40% porosity. The scaffolds demonstrate symmetric cell cycling stability exceeding 1,500 h at 0.1 mA/cm2 current density, with a capacity of 0.1 mAh/cm 2 (1 h for each half cycle). At higher current densities, reversible soft shorts frequently happen, while immediate hard shorts are prevented due to Li dendrite growth being hindered by the tortuous pore network. In addition to the cycling stability, the phase stability of LLZTO is investigated during the post-printing thermal process for printing resin removal. We discovered that the LLZTO partially decomposes into Li 2 Zr 2 O 7 and other impurity phases from 400°C to 800°C, but the pure LLZTO phase is restored upon the completion of resin removal beyond 800°C.

Li-metal anode↗

Investigation of MgO additives on microstructure and properties of thin LLZO electrolytes for all-solid-state batteries

To realize high-energy density lithium lanthanum zirconate (LLZO)-based solid-state batteries (SSB), LLZO electrolytes should be fabricated with low thickness and high mechanical strength. An effective strategy for strengthening ceramic materials is to use additives. Here, we employed MgO nanopowders and fibers as additives for the thin LLZO electrolyte in order to improve the mechanical strength. The microstructure, mechanical properties, and electrochemical properties are characterized to investigate the effects of adding MgO and sintering time. The MgO remains at grain boundaries after sintering, making the microstructure of LLZO fine and uniform. The mechanical strength of the MgO-added LLZO was enhanced by more than 60% while maintaining high ionic conductivity (1 × 10 -4 S cm -1 ) at room temperature. Li symmetric cells using the MgO fiber–LLZO and MgO powder–LLZO exhibit 2 and 3 times higher critical current density (CCD) than those of pure LLZO, and a solid-state full cell exhibits stable cycling performance. Further, these results demonstrate that the use of MgO nanopowder or fiber as an additive for thin LLZO is beneficial for high-current density cycling, by improving mechanical properties and microstructure.

25 ENERGY STORAGE↗

Rapid scalable plasma processing of thin-film Li–La–Zr–O solid-state electrolytes

Solid-state electrolytes, such as lithium lanthanum zirconium oxide (LLZO), show promise as technologies for next-generation high-energy-density batteries, but commercial development has been hindered by a lack of scalable processing methods. Current fabrication methods are costly or require long annealing steps to create dense films. We report an atmospheric pressure blown-arc nitrogen plasma jet process to rapidly form sub-micrometer-thick, dense amorphous LLZO (a-LLZO) films from sol-gel precursors. Films are processed in less than 2 min, an order of magnitude faster than what has previously been reported. We demonstrate 500-nm-thick a-LLZO films processed at 350°C with an ionic conductivity of 2 × 10 −6 S/cm at 30°C and 2 × 10 −3 S/cm at 100°C and a conductance of 19 S at 100°C, the highest conductance of any LLZO phase to date. Here, the films exhibit outstanding smooth surface morphology with low defectivity, advancing atmospheric plasma processing as a scalable processing method for solid-state electrolytes.

25 ENERGY STORAGE↗

Effect of Propagating Dopant Reactivity on Lattice Oxygen Loss in LLZO Solid Electrolyte Contacted with Lithium Metal

Lithium lanthanum zirconium oxide (LLZO) is widely known as the most stable solid electrolyte against lithium metal electrodes. This thermodynamic stability can be lost by the presence of dopants which are required to stabilize the cubic phase of LLZO and can be reduced by lithium metal. However, the role of oxygen in such reactions is taken for granted. In this work, the reduction of Nb-substituted LLZO (Nb-LLZO) is explored by Li metal and shows that interfacial reactions propagate and lead to the decomposition with substantial Nb 5+ reduction deep into the bulk electrolyte. Scanning Transmission Electron Microscopy with Energy Dispersive X-ray Spectroscopy and thermogravimetric analyses show much of the reduction is due to oxygen vacancies formed, leading to increased electronic conductivity mapped with conductive Atomic Force Microscopy. Density functional theory calculations indicate oxygen release is favored by increased excess lithiation of Nb-LLZO. Electrochemical impedance of polycrystalline Nb-LLZO shows the continuous evolution of ionically resistive interphases near the lithium metal interface with Nb-LLZO while single crystals show little reactivity at room temperature and self-limiting reduction at 60°C. This work underlines the role of grain boundaries in propagating destructive solid electrolyte reactions and highlights previously unseen mechanisms involving lattice oxygen in LLZO.

Li metal, solid-state electrolytes↗

Phase instability-coupled fracture behavior in garnet LLZO solid electrolytes: a machine learning-enabled atomistic study

Fracture in the garnet-type solid electrolyte Li 7 La 3 Zr 2 O 12 (LLZO) poses a critical threat to both the performance and safety of solid-state batteries. To unravel the coupled chemomechanical processes that govern fracture in LLZO under external loading, we carry out large-scale molecular-dynamics simulations with a validated machine-learning force field. Our results demonstrate that triaxial stresses at crack flanks trigger a localized cubic-to-tetragonal phase transformation, which is accompanied by Li-ion rearrangement. The emergent tetragonal domains feature lattice contraction normal to the fracture plane, imposing coherent misfit strains that provide an additional driving force for further crack propagation. Crucially, introducing Li deficiencies stabilizes the cubic phase, postponing the phase transition and thereby delaying fracture initiation. These findings highlight the role of intrinsic phase instability in dictating LLZO's fracture resistance and its critical connection to local Li concentration. This chemomechanical coupling points toward targeted strategies to enhance the mechanical robustness of garnet electrolytes, including tuning Li content, ensuring dopant homogeneity, and refining processing protocols.

Materials science↗

Ultrafast Sintering and Dopant Effects in Garnet LLZO Solid Electrolytes

High-throughput, low-cost manufacturing, and optimization of solid electrolytes are necessary for the adoption of solid-state batteries. In this work, garnet-type Li 7 La 3 Zr 2 O 12 (LLZO) with different aliovalent dopants, 𝑇𝑎$_{^·_{𝑍𝑟}}$, 𝐴𝑙$^{··}_{𝐿𝑖}$, and 𝐺𝑎$^{··}_{𝐿𝑖}$, have been ultrafast-sintered with different temperature ramping rates. The densification behavior, phases, their evolution, and surface chemistry of different LLZO have been investigated and linked to their electrochemical performances. It has been shown that LLZO with 𝑇𝑎$_{^·_{𝑍𝑟}}$ dopant demonstrates the highest garnet phase purity and overall best electrochemical performances, and ultrafast sintering further improves densification, ionic conductivity, and electrochemical stability. On the other hand, LLZO doped with 𝐴𝑙$^{··}_{𝐿𝑖}$ and 𝐺𝑎$^{··}_{𝐿𝑖}$ are reaching higher cubic phase purities and ionic conductivities via conventional sintering, indicating undesirable dopant migration and segregation during the ultrafast sintering process. In conclusion, these findings provide insights into the manufacturing of solid electrolyte materials.

36 MATERIALS SCIENCE↗

Grain boundary zirconia-modified garnet solid-state electrolyte

Here, we report a method for promoting electrochemical stability in garnet Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 solid-state electrolyte based on a composite two-phase oxide–oxide microstructure. Grain boundary precipitation of the controlled distribution of amorphous zirconium oxide microparticles is achieved through the addition of reactive tantalum carbide. During ambient-atmosphere sintering, the carbide decomposes through an in situ reaction, the ‘extra’ Ta substituting for Zr within the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 lattice. Density functional theory (DFT) calculations identify a thermodynamically favourable reaction path and show how substituting Ta 5+ at Zr 4+ sites affects the crystal structure as well as bulk ionic and electronic conductivities. Quantitative stereology highlights that zirconia also acts as a sintering aid, reducing compact porosity. Cryogenic focused-ion-beam scanning electron microscopy and fractography analysis of cycled solid-state electrolytes illustrates that near-universally observed intergranular Li-metal dendrite propagation is suppressed by the two-phase microstructure, favouring transgranular dendrites instead. Importantly, DFT demonstrates that compared with the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 surface, the zirconium oxide surface per se is less electronically conductive and does not trap excess electrons to reduce Li ions. This is a key reason for the substantial improvement in the electrochemical properties over the single-phase baseline.

36 MATERIALS SCIENCE↗

Radiation Damage Mechanisms in Oxide-Based Solid Electrolytes

Ion implantation is a promising approach to mitigate dendrite formation in metal anode solid-state batteries by modifying the chemical and mechanical properties of oxide-based electrolyte surfaces such as Li 7 La 3 Zr 2 O 12 (LLZO). Yet, the detailed atomistic mechanisms and potentially adverse side effects of ion implantation remain poorly understood. In this study, we used molecular dynamics simulations to elucidate the evolution of radiation-induced damage in LLZO. The results reveal that radiation damage is primarily driven by recoils from heavy ions in the lattice, producing antisite defect clusters whose density decreases as recoil energy increases, a counterintuitive finding that highlights complex cascade fragmentation. Radiation-induced disruption to the crystal sublattice connectivity, especially in the La–O network critical for Li-ion transport, leads to degradation in ionic pathways at low energies, while higher energy cascades can form new conduction pathways via enhanced Zr–O network connectivity. These findings provide a mechanistic foundation for optimizing ion implantation strategies that balance disruption of the lattice for surface modification for dendrite resistance with preservation of essential ionic conductivity.

Defects↗

Developing cathode infiltration processes for all-solid-state bilayer LLZO cells

To realize the bilayer architecture of lithium lanthanum zirconate (LLZO) for application in solid-state batteries (SSBs), the scaffold structure must be optimized, and effective cathode infiltration strategies must be established. In this study, we fabricate a modified bilayer LLZO using a sacrificial layer to enhance surface porosity, and systematically investigate various cathode infiltration techniques to fill the scaffold with oxide cathode active materials (CAM). Structural characterizations showed that the sacrificial layer significantly increased open surface porosity, enabling the surface of the scaffold to be filled with CAM. To further increase infiltration depth, applying vacuum or vibration was compared, with the full-depth infiltration achieved using a sonicator-based vibration. Full cells prepared using the modified bilayer LLZO and vibration-assisted technique demonstrated successful operation. This work demonstrates a practical and scalable approach for engineering bilayer LLZO structures and integrating oxide cathodes into porous scaffolds, offering a promising pathway toward high-performance solid-state batteries.

Bilayer↗

Heterogeneous doping via nanoscale coating impacts the mechanics of Li intrusion in brittle solid electrolytes

Lithium dendrite intrusion in solid-state batteries limits fast charging and causes short-circuiting, yet the underlying regulating mechanisms are not well-understood. Here, in this work, we discover that heterogeneous Ag + doping dramatically affects lithium intrusion into Li 6.6 La 3 Zr 1.6 Ta 0.4 O 12 (LLZO), a brittle solid electrolyte. Nanoscale Ag + doping is achieved by thermally annealing a 3-nm-thick metallic coating on LLZO, inducing Ag–Li ion exchange and Ag diffusion into grains and grain boundaries. Density functional theory calculations and experimental characterization show negligible impact on the electronic properties and surface wettability from Ag + incorporation. Mechanically, nanoindentation experiments show a fivefold increase in the mechanical force required to fracture the surface Ag + -doped LLZO, indicating substantial doping-induced surface toughening. Operando microprobe scanning electron microscopy experiments show that the Ag + -doped LLZO surface exhibits improved lithium plating at >250 mA cm −2 and an electroplating diameter that is expanded by over fourfold, even under an extreme indentation stress of 3 GPa. This demonstrates enhanced defect tolerance in LLZO, rather than electronic or adhesion effects. Our study reveals a chemo-mechanical mechanism via surface heterogeneous doping, complementing present bulk design rules to minimize mechanical failures in solid-state batteries.

36 MATERIALS SCIENCE↗

Improved interfacial li-ion transport in composite polymer electrolytes via surface modification of LLZO

Composite polymer electrolytes that incorporate ceramic fillers in a polymer matrix offer mechanical strength and flexibility as solid electrolytes for lithium metal batteries. However, fast Li + transport between polymer and Li + -conductive filler phases is not a simple achievement due to high barriers for Li + exchange across the interphase. This study demonstrates how modification of Li 7 La 3 Zr 2 O 12 (LLZO) nanofiller surfaces with silane chemistries influences Li + transport at local and global electrolyte scales. Anhydrous reactions covalently link amine-functionalized silanes [(3-aminopropyl)triethoxysilane (APTES)] to LLZO nanoparticles, which protects LLZO in air. APTES functionalization lowers the poly (ethylene oxide) (PEO)-LLZO interphase resistance to half that of unmodified LLZO and increases effective Li + transference number, while insulating Al 2 O 3 completely blocks ion exchange and lowers transference number and conductivity in PEO-lithium bis(trifluoromethanesulfonyl)imide (LiTFSI)-LLZO composites. Modeling an inner resistive interphase between LLZO and PEO surrounded by an outer conductive interphase explains non-linear conductivity trends. Solid-state 7 Li & 6 Li nuclear magnetic resonance shows Li + only exchanges between PEO-LiTFSI and some LLZO interphase, with no appreciable Li + transport through bulk LLZO. Surface functionalization is a promising path toward lowering the polymer-ceramic interphase resistance. This work demonstrates that local changes in Li + transport affect macroscopic performance, highlighting the intricate relationships between all interfaces in inherently heterogeneous composite polymer electrolytes.

25 ENERGY STORAGE↗

Methods for Quantitative Thermal Analysis of Lithium Solid-State and Beyond Battery Safety

The use of differential scanning calorimetry (DSC) to measure the thermal behavior of individual components and electrolyte/electrode combinations is common. However, here we focus on DSC tests on an anode, cathode, and electrolyte (ACE) component combination over a temperature range that includes many of the phase transitions and key reactions (i.e., to 500 °C) that contribute to thermal runaway. This method can help quantify the complex reaction network in a full cell, thereby informing potential safety issues. Here, we used DSC heat flow data from a solid-state Li 0.43 CoO 2 +C+PVDF | LLZO | Li metal ACE sample and its components to quantify key factors affecting results. We focused on three areas: (1) ACE sample preparation and assembly in DSC pans, (2) DSC measurement parameters, and (3) heat flow analysis. Key points include the choice of component ratios (e.g., commercially relevant N:P capacity ratio), the importance of conductive carbon and binder, type of pan used, DSC ramp rate, and integration method used when dealing with broad and overlapping exothermic peaks. This work deepens the scientific basis and best practices for obtaining heat flow data from ACE samples for early-stage evaluation of solid-state and beyond battery safety.

25 ENERGY STORAGE↗

Ion Size Effects on the Thermodynamic, Kinetic, and Mechanical Properties during Ion Exchange in Solid-State Electrolytes

Ion exchange offers a pathway to impose residual compressive stresses to mitigate the electro-chemo-mechanical cracking of solid-state electrolytes such as lithium lanthanum zirconium oxide. This study uses a coupled multiscale framework (integrating density functional theory (DFT), molecular dynamics (MD), and continuum modeling) to examine how exchange ion size influences stress, diffusion, fracture toughness, and electronic properties. Larger isovalent ions (Na + , Ag + , K + ) were exchanged with Li + , with DFT confirming their preference for octahedral 96h sites and a linear relationship between ion size and chemical free expansion coefficient. MD simulations reveal stress and concentration effects on exchange ion diffusivity at elevated temperatures, with Na + and Ag + maintaining favorable mobility while K + showing concentration-dependent clustering. Continuum modeling predicts the range of fracture strength improvements and the required ion exchange concentration profile. It was shown that a 5% surface exchange concentration can induce ∼0.6 GPa of surface compressive stress using Na + and ∼1.0 GPa of surface compressive stress using Ag + . On the other hand, larger ion exchange species may penalize Li + diffusivity by increasing the activation volume and activation energy. Interestingly, Na + has a negligible penalty on Li-ion diffusivity. The room temperature Li + ion diffusivity is reduced by ∼40% with Ag + ion exchange. Electronic band structure analysis shows no size-dependent change in the bandgap, though Ag + introduces localized defect states near the valence band maximum. This study highlights ion size as a key factor in optimizing LLZO properties, offering a framework to improve the solid-state battery performance.

Jagad, Harsh D. [Brown Univ., Providence, RI (Unit↗

Identifying Bounds of Inorganic Content in Solventless Processing of Hybrid Solid Electrolytes

Solid-state lithium batteries require safe, robust electrolytes to enable higher energy densities and improved safety over conventional cells. Hybrid polymer–ceramic electrolytes are a promising solution, combining the processability of polymers with the high ionic conductivity and mechanical strength of inorganic fillers. In this work, we demonstrate a solventless, UV-curing method to produce hybrid solid electrolytes using a poly(ethylene glycol) dimethyl ether (PEGDME)-based photocurable matrix incorporating Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 (LAGP) or Li 7 La 3 Zr 2 O 12 (LLZO) ceramic electrolyte. Inorganic filler loadings up to ∼55 wt.% could be successfully incorporated via this process which was the highest inorganic content at which the slurry remains processable and cured into a uniform film. The resulting UV-cured composite electrolytes remain flexible and exhibit room-temperature ionic conductivities on the order of 10 −4 S·cm −1 , along with notably improved lithium-ion transference numbers compared to conventional polymer electrolytes. Similar performance and processing limits were observed for both LAGP and LLZO, indicating that ceramic filler chemistry does not significantly affect the UV-curing process or the electrolyte's ion transport properties in this regime. Eliminating solvents from fabrication not only simplifies processing and mitigates environmental concerns but also enables higher solid contents that enhance mechanical strength and help suppress lithium dendrite formation. In conclusion, this scalable approach thus paves the way for manufacturing robust composite solid electrolytes for next-generation solid-state batteries (SSBs).

Batteries↗

Demonstration of the Reproducibility Challenges in the Sintering Behavior of Lithium‐Stuffed Garnets in Scaling up Synthesis

Lithium-stuffed garnets, such as Li 7 La 3 Zr 2 O 12 (LLZO), are promising candidates for next-generation solid-state batteries because of their high room-temperature ionic conductivity and chemical stability against lithium metal anodes, which are crucial for achieving higher energy density. However, realizing LLZO's potential in practical devices requires synthesis methods that can be scaled reliably to large batch sizes for manufacturing. Herein, we investigate the sintering reproducibility of LLZO synthesized at larger scales using ultrasonic spray pyrolysis, a cost-effective and scalable synthesis route. Two 100 g batches of Al-doped LLZO are prepared and their sintering behavior is examined in detail. Both Al-LLZO batches contain over 90 wt.% cubic-phase LLZO, and both batches exhibit room temperature conductivities greater than 1 × 10 −4 S cm −1 at a relative density above 0.8. However, variations in secondary phases and subtle differences in Al content lead to significant differences in densification and microstructure. These results demonstrate that LLZO's sintering behavior is highly sensitive to small changes in secondary phases and Al content, creating reproducibility challenges when moving from laboratory- to manufacturing-scale synthesis.

36 MATERIALS SCIENCE↗

Particle‐Size‐Dependent Lithium‐Ion Transport in PEO/LLZO Composite Electrolytes

Lithium-metal batteries with solid electrolytes can deliver higher energy density and improved safety than conventional Li-ion batteries. Among solid electrolyte candidates, polymer/ceramic composite electrolytes are attractive because they combine polymer flexibility with the high ionic conductivity of ceramics. However, whether ceramic fillers synergistically reduce polarization losses in the polymer matrix remains unclear. A central unknown is the critical polymer/ceramic interfacial resistance (Rint,crit), below which adding ceramics lowers electrolyte overpotential. Here, we present the first macroscale model framework to quantify R int,crit for composite electrolytes based on polyethylene oxide (PEO) and Ta-doped Li 7 La 3 Zr 2 O 12 (LLZO). A 1D model for DC-polarization of tri-layer cells (PEO-LiTFSI/LLZO/PEO-LiTFSI) shows that LLZO surface functionalization reduces the PEO/LLZO interfacial resistance, consistent with electrochemical impedance measurements. Extending to a 2D composite model, we show notably that Rint,crit scales linearly with LLZO particle diameter and shifts toward experimentally accessible values (e.g., 28.8 Ωcm 2 ) as particle size increases. At fixed ceramic volume fraction, larger LLZO particles reduce the number of interfacial crossings, driving more current through the ceramic phase and lowering concentration polarization. In contrast, R int,crit is largely independent of ceramic volume fraction. These results demonstrate that ceramic filler-size engineering can enable synergistic, energy-efficient transport in polymer/ceramic composite electrolytes.

25 ENERGY STORAGE↗

Electrochemical Oxidation in Garnet-Type Solid Electrolyte by Formation of Point Defects

All-solid-state batteries hold greater promise for improving safety and energy density over conventional battery technology employing organic liquid electrolytes. One of the required features of a Li + conducting solid electrolyte is electrochemical stability, attained thermodynamically or kinetically, within the targeted operating voltage and temperature ranges. Therefore, understanding of the oxidative or reductive degradation mechanism is important to allow the design of stable solid electrolyte materials. This work contributes to building an understanding of the oxidative degradation mechanism in lithium solid electrolytes at cell operating conditions. Here, we have focused on resolving the oxidative decomposition mechanism of Al-doped lithium garnet Li 6.28 Al 0.24 La 3 Zr 2 O 12 (LLZO) as a state-of-the-art inorganic ceramic electrolyte. By combining experimental and computational analyses, we show that oxidation of LLZO occurs by simultaneous loss of oxygen and lithium from the structure, resulting in substoichiometric LLZO, at a moderate temperature (80 °C) and a high electrode potential (4.3 V vs Li/Li + ). Based on X-ray absorption and diffraction analyses, we find that the zirconium coordination shells in LLZO contract while the crystal structure experiences positive chemical strain upon electrochemical oxidation. The results from ex situ structural characterization of both the local structure and crystal symmetry are supported by a substoichiometric LLZO with lithium and oxygen vacancies, modeled by density functional theory (DFT) calculations. These chemical and structural changes in LLZO suppress effective lithium-ion conductivity by an order of magnitude. Formation of lithium and oxygen vacancies in LLZO upon electrochemical oxidation is different from prior thermodynamic predictions of phase decomposition of LLZO. The difference here is that the experiments were conducted at near-room temperature, which can hinder the kinetics of phase separation, and thus, the resultant LLZO solid electrolyte is still single-phase but substoichiometric in Li and O. In conclusion, these findings contribute an important degradation mechanism of the electrolyte, relevant for practical operational conditions of solid-state batteries.

36 MATERIALS SCIENCE↗