Effect of substrate orientation and anisotropic strength on corrosion pits

The complexities of pitting corrosion and its associated pit morphologies are critical for predicting and preventing pit-related failure in materials. With the advances in computational tools, modeling of pitting corrosion has lately gained momentum. We recently developed a phase field model for 3-D pit morphology, and in the current work, the model is utilized to gain insight into the role of substrate orientation and anisotropic strength on crystallographic pits. The influence of these parameters on pit morphology and corrosion metrics such as pit volume, current, pit area, current density, and pit depth are studied. The crystallographic pit morphology changes with substrate orientation but not significantly with anisotropic strength. Finally, the anisotropic strength strongly influences the corrosion metrics whereas most corrosion metrics remain unaffected by substrate orientation.

36 MATERIALS SCIENCE↗

Pitting Corrosion in 316L Stainless Steel Fabricated by Laser Powder Bed Fusion Additive Manufacturing: A Review and Perspective

Abstract 316L stainless steel (316L SS) is a flagship material for structural applications in corrosive environments, having been extensively studied for decades for its favorable balance between mechanical and corrosion properties. More recently, 316L SS has also proven to have excellent printability when parts are produced with additive manufacturing techniques, notably laser powder bed fusion (LPBF). Because of the harsh thermo-mechanical cycles experienced during rapid solidification and cooling, LPBF processing tends to generate unique microstructures. Strong heterogeneities can be found inside grains, including trapped elements, nano-inclusions, and a high density of dislocations that form the so-called cellular structure. Interestingly, LPBF 316L SS not only exhibits better mechanical properties than its conventionally processed counterpart, but it also usually offers much higher resistance to pitting in chloride solutions. Unfortunately, the complexity of the LPBF microstructures, in addition to process-induced defects, such as porosity and surface roughness, have slowed progress toward linking specific microstructural features to corrosion susceptibility and complicated the development of calibrated simulations of pitting phenomena. The first part of this article is dedicated to an in-depth review of the microstructures found in LPBF 316L SS and their potential effects on the corrosion properties, with an emphasis on pitting resistance. The second part offers a perspective of some relevant modeling techniques available to simulate the corrosion of LPBF 316L SS, including current challenges that should be overcome.

Voisin, T. (ORCID:0000000287462659)↗

The effect of tempering temperature on pitting corrosion resistance of 420 stainless steels

The AISI Type 420 stainless steels are commonly used to steam generators, mixer blades, etc. These stainless steels are most prone to pitting in dissolved Cl{sup −} containing environments. In this paper, the effect of tempering temperature on pitting corrosion resistance of AISI Type 420 stainless steels was studied. The AISI Type 420 stainless steels specimens were heat treated at the temperature of 1050°C for 1 hour to reach austenite stabilization and then quench in the oil. After that, the specimens were tempered at the temperature of 150, 250, 350 and 450°C for 30 minutes and then air cooled to the room temperature. The electrochemical potentiodynamic polarization test was conducted at 3.5% sodium chloride solution to evaluate corrosion rate and pitting corrosion behaviour. The Scanning Electron Microscope (SEM), Energy Dispersive X-Ray Spectroscopy (EDS) were used to evaluate the pitting corrosion product. The result have shown that highest pitting potential was found in the sample tempered at 250°C and corrosion pits were found to initiate preferentially around chromium carbides.

36 MATERIALS SCIENCE↗

Automated Image Segmentation and Processing Pipeline Applied to X–Ray Computed Tomography Studies of Pitting Corrosion in Aluminum Wires

Understanding pitting corrosion is critical, yet its kinetics and morphology remain challenging to study from X-ray computed tomography (XCT) due to manual segmentation barriers. To address this, an automated pipeline leveraging deep learning for efficient large-scale XCT analysis is developed, revealing new corrosion insights. The pipeline enables pit segmentation, 3D reconstruction, statistical characterization, and a topological transformation for visualization. Here, the pipeline is applied to 87 648 XCT images capturing commercial purity aluminum (1100 Al) wire exposed to sodium chloride (NaCl) salt particles over a period of 122 h. The pipeline achieves complete feature extraction and statistical quantification across the entire XCT dataset, leveraging distributed computing environment for high efficiency. Global growth kinetics such as high-level stepwise sigmoidal volume loss patterns and granular individual pit developments are both captured for 36 detected pits. By combining automation, computer vision, and extensive XCT datasets, this research accelerates precise corrosion assessment to enable materials science discoveries at scale.

36 MATERIALS SCIENCE↗

Dependence of Crystallographic Orientation on Pitting Corrosion Behavior of Ni-Fe-Cr Alloy 028

The influence of crystallographic orientation on the pitting corrosion behavior of Ni-Fe-Cr alloy 028 was studied using a combination of X-ray diffraction (XRD), electron backscatter diffraction (EBSD), potentiodynamic polarization technique, and atomic force microscopy (AFM). The results show that there is anisotropy of pitting corrosion that strongly depends on crystallographic orientation of the surface plane. The distribution of pit density in a standard stereographic triangle indicates that the crystallographic planes close to {100} are more prone to pitting corrosion compared to planes {110} and {111}. The surface energy calculation of (001) and (111) shows that the plane with a high atomic packing density has a low surface energy with concomitant strong resistance to pitting corrosion. A correlation function between crystallographic orientation and pitting corrosion susceptibility suggests a method that not only predicts the pitting resistance of known textured materials, but also could help to improve corrosion resistance by controlling material texture.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Critical role of slags in pitting corrosion of additively manufactured stainless steel in simulated seawater

Abstract Pitting corrosion in seawater is one of the most difficult forms of corrosion to identify and control. A workhorse material for marine applications, 316L stainless steel (316L SS) is known to balance resistance to pitting with good mechanical properties. The advent of additive manufacturing (AM), particularly laser powder bed fusion (LPBF), has prompted numerous microstructural and mechanical investigations of LPBF 316L SS; however, the origins of pitting corrosion on as-built surfaces is unknown, despite their utmost importance for certification of LPBF 316L SS prior to fielding. Here, we show that Mn-rich silicate slags are responsible for pitting of the as-built LPBF material in sodium chloride due to their introduction of deleterious defects such as cracks or surface oxide heterogeneities. In addition, we explain how slags are formed in the liquid metal and deposited at the as-built surfaces using high-fidelity melt pool simulations. Our work uncovers how LPBF changes surface oxides due to rapid solidification and high-temperature oxidation, leading to fundamentally different pitting corrosion mechanisms.

36 MATERIALS SCIENCE↗

Effect of annealing temperature on the pitting corrosion resistance of super duplex stainless steel UNS S32750

The pitting corrosion resistance of commercial super duplex stainless steels SAF2507 (UNS S32750) annealed at seven different temperatures ranging from 1030 deg. C to 1200 deg. C for 2 h has been investigated by means of potentiostatic critical pitting temperature. The microstructural evolution and pit morphologies of the specimens were studied through optical/scanning electron microscope. Increasing annealing temperature from 1030 deg. C to 1080 deg. C elevates the critical pitting temperature, whereas continuing to increase the annealing temperature to 1200 deg. C decreases the critical pitting temperature. The specimens annealed at 1080 deg. C for 2 h exhibit the best pitting corrosion resistance with the highest critical pitting temperature. The pit morphologies show that the pit initiation sites transfer from austenite phase to ferrite phase as the annealing temperature increases. The aforementioned results can be explained by the variation of pitting resistance equivalent number of ferrite and austenite phase as the annealing temperature changes.

36 MATERIALS SCIENCE↗

Influence of Realistic, Cyclic Atmospheric Cycles on the Pitting Corrosion of Austenitic Stainless Steels

Pitting corrosion was evaluated on stainless steels 304H, 304, and 316L the surfaces of which had ASTM seawater printed on them as a function of surface roughness after exposure to an exemplar realistic atmospheric diurnal cycle for up to one year. Methods to evaluate pitting damage included optical imaging, scanning electron microscopy imaging, profilometry analysis, and polarization scans. The developed cyclic exposure environment did not significantly influence pitting morphology nor depth in comparison to prior static exposure environments. Cross-hatching was observed in a majority of pits for all material compositions with the roughest surface finish (#4 finish) and in all surface finishes for the 304H composition. Evidence is provided that cross-hatched pit morphologies are caused by slip bands produced during the grinding process for the #4 finish or by material processing. Additionally, micro-cracking was observed in pits formed on samples with the #4 surface finish and was greatly reduced or absent for pits formed on samples with smooth surface finishes. This suggests that both a low RH leading to an MgCl 2 -dominated environment and a rough surface containing significant residual stress are necessary for micro-cracking. Finally, the use of various characterization techniques and cross sectioning was employed to both qualitatively and quantitatively assess pitting damage across all SS compositions and surface finishes.

36 MATERIALS SCIENCE↗

Phase Field Modeling of Crystallographic Corrosion Pits

The modeling of corrosion to understand and predict corrosion behavior is a topical issue. Here, a 3D phase field model is developed to simulate the pit morphology, primarily focusing on crystallographic pits. A crystallographic function is employed to incorporate different corrosion rates for different crystallographic planes. The model is benchmarked and validated against an analytical solution for a simple case. 3D crystallographic pits in a single crystal are simulated and the effect of substrate orientation on the pit morphology is studied. The crystallographic pit morphology changes significantly with the substrate orientation and these morphologies have a symmetry consistent with the substrate orientation. This first 3D phase field model of crystallographic pits will help in predicting the intricate shapes of pits, thereby, pushing the frontiers of pitting corrosion modeling.

36 MATERIALS SCIENCE↗

Direct observation of pitting corrosion evolutions on carbon steel surfaces at the nano-to-micro- scales

The Cl¯-induced corrosion of metals and alloys is of relevance to a wide range of engineered materials, structures, and systems. Because of the challenges in studying pitting corrosion in a quantitative and statistically significant manner, its kinetics remain poorly understood. Herein, by direct, nano- to micro-scale observations using vertical scanning interferometry (VSI), we examine the temporal evolution of pitting corrosion on AISI 1045 carbon steel over large surface areas in Cl¯-free, and Cl¯-enriched solutions. Special focus is paid to examine the nucleation and growth of pits, and the associated formation of roughened regions on steel surfaces. By statistical analysis of hundreds of individual pits, three stages of pitting corrosion, namely, induction, propagation, and saturation, are quantitatively distinguished. By quantifying the kinetics of these processes, we contextualize our current understanding of electrochemical corrosion within a framework that considers spatial dynamics and morphology evolutions. In the presence of Cl¯ ions, corrosion is highly accelerated due to multiple autocatalytic factors including destabilization of protective surface oxide films and preservation of aggressive microenvironments within the pits, both of which promote continued pit nucleation and growth. Furthermore these findings offer new insights into predicting and modeling steel corrosion processes in mid-pH aqueous environments

36 MATERIALS SCIENCE↗

Influence of Heat Input and Cold Wire Feeding Rate on Pitting Corrosion Resistance of Submerged Arc Welding Duplex Stainless Steel Welds

Welding thermal cycles may severely impair duplex stainless steel (DSS) performance, especially local pitting resistance and toughness. The restricted welding energy between 0.5 and 2.5 kJ mm{sup −1} represents a limiting factor for productivity increase in DSS welding, and the addition of cold wire is an interesting alternative to increase the welding deposition rate without adding extra heat. The aim of this work is to evaluate the influence of the cold wire feeding rate (CW) and heat input (HI) on pitting corrosion behavior of DSS UNS S32304 bead-on-plate welds obtained by submerged arc welding (SAW). Cyclic potentiodynamic polarization was carried out in transverse weld sections using 1 mol L{sup −1} NaCl solution at room temperature. Most pitting corrosion spots were located on the heat-affected zone (HAZ), and the pitting potentials were lower than the base metal due to higher ferrite fractions and the presence of chromium nitrides. Considering the same CW, the HI increasing reduced E{sub pit} for 1.6, 1.9, 2.2 kJ mm{sup −1}, but increased E{sub pit} for 2.7 kJ mm{sup −1}, due to a balance between the HAZ width and the austenite fraction.

36 MATERIALS SCIENCE↗

The effect of inhibitor sodium nitrate on pitting corrosion of dissimilar material weldment joint of stainless steel AISI 304 and mild steel SS 400

This study experimentally evaluated the effect of Sodium Nitrate inhibitor (NaNO{sub 3}) of 0.1%, 0.3%, and 0.5% on NaCl 3.5% toward pitting corrosion of dissimilar metal welding joint between stainless steel AISI 304 and mild steel SS 400. Electrochemical corrosion was tested using potentiodynamic polarization. Further the Scanning Electron Microscope (SEM) conducted to analyze the specimen. Chemical composition analysis used Energy Dispersive X-ray Spectrometry (EDS). The highest efficiency of sodium nitrate for ER 308 attained 63.8% and 64.89%for ER 309L. The specimen surface which observed through SEM showed decrease of pitting corrosion respectively with the addition of sodium nitrate content as inhibitor.

36 MATERIALS SCIENCE↗

Atomic-scale decoration for improving the pitting corrosion resistance of austenitic stainless steels

Stainless steels are susceptible to the localized pitting corrosion that leads to a huge loss to our society. Studies in the past decades confirmed that the pitting events generally originate from the local dissolution in MnS inclusions which are more or less ubiquitous in stainless steels. Although a recent study indicated that endogenous MnCr 2 O 4 nano-octahedra within the MnS medium give rise to local nano-galvanic cells which are responsible for the preferential dissolution of MnS, effective solutions of restraining the cells from viewpoint of electrochemistry are being tantalizingly searched. Here we report such a galvanic corrosion can be greatly resisted via bathing the steels in Cu 2+ -containing solutions. This chemical bath generates Cu 2–δ S layers on the surfaces of MnS inclusions, invalidating the nano-galvanic cells. Our study provides a low-cost approach via an atomic scale decoration to improve the pitting corrosion resistance of stainless steels in a volume-treated manner.

36 MATERIALS SCIENCE↗

Effects of Inclusions in HSLA Carbon Steel on Pitting Corrosion in CaCl2

Susceptibility of high strength low alloy steel to localized corrosion was studied in 6.7 M CaCl{sub 2} for oil and natural gas drilling applications. Results of the immersion and electrochemical experiments showed that the steel is susceptible to pitting corrosion. Optical microscopy investigations of the polished samples revealed that 10% of the surface area was occupied by defects in the form of pits. The energy dispersive X-ray (EDX) and wavelength dispersive X-ray (WDX) chemical analyses revealed higher concentrations of Mn and S compared to the metal matrix in defected areas. These areas served as the sites for development of corrosion pits during both immersion and electrochemical experiments. The fatigue results of the corroded samples indicate that if the pit was the most significant defect, the fatigue crack initiated and propagated at this site.

03 NATURAL GAS↗

Pitting Corrosion of 10Ni8CrMoV High-Strength Steel Induced by a Potential Perturbation

Pitting corrosion of high-strength steel 10Ni8CrMoV under square wave polarization (SWP) in simulated deep-sea environment is investigated and the possible mechanism is proposed. The results show that potential perturbation generates periodic intensification effect on both anodic and cathodic processes by frequently breaking the electrode equilibrium state. The intensity of periodic intensification effect essentially depends on the concentration gradient of Fe{sup 2+} cations at the steel/solution interface which acts as the forced electrochemical oscillator. The concentration gradient and the resulting concentration polarization effect increase periodically with the increase in SWP potential range. The morphology observation of the pitting and electric charge calculation indicate that the periodic intensification effect can promote the initiation and growth of pits by enhancing the anodic dissolution even under cathodic protection, but it is ineffective below the hydrogen evolution potential. The decrease in either upper or lower potential can mitigate anodic dissolution. Through the statistical analysis of pitting size, it is found that the wide potential range tends to activate the metastable pitting formed under hydrostatic pressure, forming densely distributed pitting. Meanwhile, it is more favorable to the formation of fully grown pits with high size dispersion degree when the proportion of electric charge in the anodic process is higher.

36 MATERIALS SCIENCE↗

Phase-field model of pitting corrosion kinetics in metallic materials

This study presents a thermodynamically consistent phase field model for the quantitative prediction of the pitting corrosion kinetics in metallic materials. An order parameter is introduced to represent the metal’s physical state at each point in the entire domain. The free energy of the metal-electrolyte system is defined in terms of its metal ion concentration and the order parameter. The mass transport in the electrolyte and the electrochemical reactions in the electrolyte/metal interface are taken into consideration in the model to simulate metal corrosion in a corrosive environment. The governing equations for mass transport and the order parameter are solved in such a manner that the system’s free energy is reduced as a result of diffusion and migration processes, and the distribution of electrostatic potential is governed by Poisson’s equation. A calibration study is performed to couple the kinetic interface parameter with the corrosion current density, which results in a direct relationship between overpotential and the kinetic interface parameter. A comparative study is performed to validate the phase field model against the experimental results. Several case studies are also examined to understand the corrosion behavior of closely located pits, stressed material, ceramic particles-reinforced steel, and crystallographic orientation dependence.

36 MATERIALS SCIENCE↗

Influence of surface modifications on pitting corrosion behavior of nickel-base alloy 718. Part 1: Effect of machine hammer peening

The effect of surface modifications induced by machine hammer peening on pitting corrosion behavior of nickel-base alloy 718 in a 3.5 wt.% NaCl solution is investigated. Severe work hardening and high compressive residual stress are generated with surface smoothing and microstructure evolution in terms of formation of nano-grains and nano-twins in the near surface region after machine hammer peening. Electrochemical tests results show that machine hammer peening has a beneficial influence on the corrosion resistance, indicated by a significant increase of the critical pitting potential (+134 mV) accompanied with lower corrosion current density and higher polarization resistance.

36 MATERIALS SCIENCE↗

A space-time adaptive finite element method with exponential time integrator for the phase field model of pitting corrosion

In this paper we propose a space-time adaptive finite element method for the phase field model of pitting corrosion, which is a parabolic partial differential equation system consisting of a phase variable and a concentration variable. A major challenge in solving this phase field model is that the problem is very stiff, which makes the time step size extremely small for standard temporal discretizations. Another difficulty is that a high spatial resolution is required to capture the steep gradients within the diffused interface, which results in very large number of degrees of freedom for uniform meshes. To overcome the stiffness of this model, we combine the Rosenbrock–Euler exponential integrator with Crank–Nicolson scheme for the temporal discretization. Moreover, by exploiting the fact that the speed of the corroding interface decreases with time, we derive an adaptive time stepping formula. For the spatial approximation, we propose a simple and efficient strategy to generate adaptive meshes that reduces the computational cost significantly. Thus, the proposed method utilizes local adaptivity and mesh refinement for efficient simulation of the corrosive dissolution over long times in heterogeneous media with complex microstructures. We also present an extensive set of numerical experiments in both two and three dimensional spaces to demonstrate efficiency and robustness of the proposed method.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗