At least 19 records

Reaction Between Thin Gold Wires and Pb-Sn-In Solder (37.5%, 37.5%, 25%), Part A: The Radial Reaction Inside The Solder Mounds, Its Linear Reaction Model, Statistical Variation of Reaction Rate, and Induced Structural Changes In The Solder Mounds.

Thermodynamics favors the reaction between indium and gold, since the heat of formation of AuIn{sub 2} is 6 kcal/mole, substantially larger than the heat of formation of any other possible reaction product. Thermodynamic equilibrium between gold and the elements in the solder mound is reached only when ALL gold is converted to AuIn{sub 2}. There are two aspects to this conversion: (A) the reaction WITHIN the solder mound (called here 'radial reaction') and (B) the reaction OUTSIDE the solder mound (called here 'axial reaction') and the transition from (A) to (B). The reaction between thin gold detonator wires and the In/Pb/Sn solder mound in older detonators has been looked at repeatedly. There are, in addition, two studies which look at the reaction between indium and gold in planar geometry. All data are shown in tables I to V. It is the objective of this section dealing with aspect (A), to combine all of these results into a reaction model and to use this reaction model to reliably and conservatively predict the gold-solder reaction rate of soldered gold bridge-wires as a function of storage temperature and time.

36 MATERIALS SCIENCE↗

Reaction Between Thin Gold Wires and Pb-Sn-In Solder (37.5%, 37.5%, 25%), Part B. The Axial Reaction Of Gold Wires Soldered To PbSnIn Solder Mounds, Its effect On Electrical Resistance And Physical Structure.

Here we describe the gold-indium reaction along gold wires soldered at both ends. It begins with the combined radial/axial reaction in the vicinity of the solder mound as seen in metallurgical sections along the axis of the wire. We show that this combined radial/axial reaction has no effect on the resistance of the system, even though it shortens the length of the gold wire while converting it to gold indide. After this radial/axial reaction is complete, a purely axial reaction begins. For thin gold wires (i.e. 38.1 {micro}m diameter) the onset of that reaction is strongly correlated with the time at which the linear reaction model predicts the complete consumption of the gold wire inside the solder mounds. This purely axial reaction converts the whole wire rapidly to gold indide, and leads to substantial resistance changes and complete distortion of the wire between the solder mounds. The reaction product is AuIn{sub 2} everywhere, but both Sn and Pb also are identified everywhere on the surface by Electron Dispersive Spectroscopy.

36 MATERIALS SCIENCE↗

Reaction Between Thin Gold Wires and Pb-Sn-In Solder (37.5%, 37.5%, 25%), Part B. The "Axial Reaction" of Gold Wires Solder To PbSnIn Solder Mounds, Its Effect on Electrical Resistance and Physical Structure

Here we describe the gold-indium reaction along gold wires soldered at both ends. It begins with the combined radial/axial reaction in the vicinity of the solder mound as seen in metallurgical sections along the axis of the wire. We show that this combined radial/axial reaction has no effect on the resistance of the system, even though it shortens the length of the gold wire while converting it to gold indide. After this radial/axial reaction is complete, a purely axial reaction begins. For thin gold wires (i.e. 38.1μm diameter) the onset of that reaction is strongly correlated with the time at which the linear reaction model predicts the complete consumption of the gold wire inside the solder mounds. This purely axial reaction converts at elevated temperatures the whole wire rapidly to gold indide, and leads to substantial resistance changes and complete distortion of the wire between the solder mounds. The reaction product is AuIn 2 everywhere, but both Sn and Pb also are identified everywhere on the surface by Electron Dispersive Spectroscopy.

36 MATERIALS SCIENCE↗

Solderability of AZ31B Magnesium Alloy Coated by Copper and Strength of the Solder Joints

Magnesium alloys are promising as light materials, while their high chemical reactivity makes them difficult to be soldered. In this study, the AZ31B alloy was pretreated by zincification and coated by an electrodeposited Cu layer, and then soldered with Sn-58Bi solder in air furnace. The microstructure and properties of the AZ31B/Cu(Zn)/SnBi solder joints were characterized to evaluate the solderability of the Cu-coated Mg alloy and the influence of soldering on the Cu coating. It was found that the Cu coating is dense, and little defect exists along the Cu(Zn)/AZ31B interface. The soldering process has little negative effect on the bonding between the Cu coating and the AZ31B substrate, and the AZ31B/Cu(Zn)/SnBi solder joints of high metallurgical quality were obtained. Tensile fracture of the solder joint occurs mainly in the solder, with no peeling of the Cu coating. Under shear loading, cracks initiate inside the SnBi solder and the final fracture of the joint occurs around the Cu{sub 6}Sn{sub 5}/solder interface or along the Cu(Zn)/AZ31B interface. The tensile and shear strength of the AZ31B/Cu(Zn)/SnBi solder joints are close to that of the SnBi/Cu solder joints. It is demonstrated that the Cu-coated Mg alloy shows superior solderability and can be soldered by the Sn-based low-melting solder in air.

36 MATERIALS SCIENCE↗

Evaluating MetGlasTM Solderability with Tin-Silver-Copper and Tin-Silver-Bismuth Solder Alloys

The solderability of MetGlas TM (subsidiary of Hitachi Metals, America Ltd) 2826 MB, a rapidly solidified metallic foil, was evaluated by the meniscus height/wetting force method for tin-silver-copper (SnAgCu) and tin-silver-bismuth (SnAgBi) solders to understand the effects of the extreme non-equilibrium condition of the MetglasTM surface on solderability performance. Of the variables studied here (solder temperature, heat treatment, and solder composition), solder composition had the largest impact on contact angle. Flux and foil composition remained constant throughout; but, these factors would also be predicted to significantly affect solderability. A greater understanding of the manner whereby non-equilibrium cooling affects solderability of these foils will broaden the application of soldering technology of structures fabricated by rapid cooling process (i.e. additively manufactured coatings and parts). Developing a robust database for Pb-free solderability behavior is also necessary, as industry transitions from tin-lead (SnPb) to lead free (Pb-free) solders.

36 MATERIALS SCIENCE↗

Effect of the Soldering Atmosphere on the Wettability Between Sn4.0Ag0.5Cu (in wt.%) Lead-Free Solder Paste and Various Substrates

The “degree of wetting,” which is related to the contact angle (θ) between the molten solder and the substrate, is a useful parameter on the solderability process control. The contact angle, however, is strongly dependent on the type of substrate surface finish and used atmosphere (inert or non-inert). Furthermore, the surface tension, being an important parameter on the solderability process and performance, can also be achieved if the contact angle is known. In this study, the SAC405 [Sn4.0Ag0.5Cu (in wt.%)] solder paste contact angle was measured, by the “sessile drop” method, as a function of the temperature, surface pad finish and used atmosphere. The results are discussed, and the contact angles obtained for the different conditions are compared and discussed. Then, the surface tension (experimental) was obtained from the measured contact angle and compared with the obtained by using computation models (theoretical). The experiments performed in high vacuum conditions, i.e., low oxygen content, over a temperature range, allowed the evaluation and understanding of the surface oxides layers role on the solder wettability. The present study shows that in the soldering process, even in an inert atmosphere, usually used in industry, occurs the formation of superficial oxides, over the liquid solder and/or at the pad surfaces, that strongly affects the solder paste wettability, specially with Sn and OSP (organic solderability preservative) finishing. Differences in contact angle of ≥ 10° were determined between the two types of used atmospheres. The experimental surface tension and theoretical surface tension obtained, for the NiAu substrate type, present good correlation. The lower contact angle values were obtained for the NiAu and OSP finish types, independently of the atmosphere type.

36 MATERIALS SCIENCE↗

Solder Reflow Failures in Electronic Components During Manual Soldering

This viewgraph presentation reviews the solder reflow failures in electronic components that occur during manual soldering. It discusses the specifics of manual-soldering-induced failures in plastic devices with internal solder joints. The failure analysis turned up that molten solder had squeezed up to the die surface along the die molding compound interface, and the dice were not protected with glassivation allowing solder to short gate and source to the drain contact. The failure analysis concluded that the parts failed due to overheating during manual soldering.

Teverovsky, Alexander↗

Understanding the reliability of solder joints used in advanced structural and electronics applications: Part 1 - Filler metal properties and the soldering process

Soldering technology has made tremendous strides in the past half-century. Whether structural or electronic, all solder joints must provide a level of reliability that is required by the application. This Part 1 report examines the effects of filler metal properties and soldering process on joint reliability. Solder alloy composition must have the appropriate melting and mechanical properties that suit the product's assembly process(es) and use environment. The filler metal must also optimize solderability (wetting-and-spreading) to realize the proper joint geometry. Here, the soldering process also affects joint reliability. The choice of flux and thermal profile support the solderability performance of the molten filler metal to successfully fill the gap and complete the fillet.

36 MATERIALS SCIENCE↗

Methods of fabricating vacuum housings with hermetic solder seals using capillary solder wicks

Hermetically sealed electronic devices and methods for fabricating the hermetically sealed electronic devices are provided. The devices include a solder sealed vacuum housing. The solder seal is formed using a solder wick having an external solder reservoir. When the reservoir is filled with molten solder, the solder is drawn via capillary action into a precisely defined narrow gap between two components of the housing where it forms an airtight and vacuum-tight seal.

Frisch, Henry J.↗

Microstructural characterization and mechanical property of active soldering anodized 6061 Al alloy using Sn-3.5Ag-xTi active solders

Active solders Sn-3.5Ag-xTi varied from x = 0 to 6 wt.% Ti addition were prepared by vacuum arc re-melting and the resultant phase formation and variation of microstructure with titanium concentration were analyzed using X-ray diffraction, optical microscopy and scanning electron microscopy. The Sn-3.5Ag-xTi active solders are used as metallic filler to join with anodized 6061 Al alloy for potential applications of providing a higher heat conduction path. Their joints and mechanical properties were characterized and evaluated in terms of titanium content. The mechanical property of joints was measured by shear testing. The joint strength was very dependent on the titanium content. Solder with a 0.5 wt.% Ti addition can successfully wet and bond to the anodized aluminum oxide layers of Al alloy and posses a shear strength of 16.28 {+-} 0.64 MPa. The maximum bonding strength reached 22.24 {+-} 0.70 MPa at a 3 wt.% Ti addition. Interfacial reaction phase and chemical composition were identified by a transmission electron microscope with energy dispersive spectrometer. Results showed that the Ti element reacts with anodized aluminum oxide to form Al{sub 3}Ti-rich and Al{sub 3}Ti phases at the joint interfaces. - Highlights: Black-Right-Pointing-Pointer Active solder joining of anodized Al alloy needs 0.5 wt.% Ti addition for Sn-3.5Ag. Black-Right-Pointing-Pointer The maximum bonding strength occurs at 3 wt.% Ti addition. Black-Right-Pointing-Pointer The Ti reacts with anodized Al oxide to form Al{sub 3}Ti-rich and Al{sub 3}Ti at joint interface.

36 MATERIALS SCIENCE↗

Soldering tool heats workpieces and applies solder in one operation

Fountain-pen type soldering iron heats workpieces and applies solder to joints in densely packed electronics assemblies. The basic soldering tool is used with different-sized orifice tips, eliminating the need for an assortment of conventional soldering guns.

Gudkese, V. W.↗

Rapid Solidification of Sn-Cu-Al Alloys for High-Reliability, Lead-Free Solder: Part II. Intermetallic Coarsening Behavior of Rapidly Solidified Solders After Multiple Reflows

Controlling the size, dispersion, and stability of intermetallic compounds in lead-free solder alloys is vital to creating reliable solder joints regardless of how many times the solder joints are melted and resolidified (reflowed) during circuit board assembly. In this article, the coarsening behavior of Cu x Al y and Cu 6 Sn 5 in two Sn-Cu-Al alloys, a Sn-2.59Cu-0.43Al at. pct alloy produced via drip atomization and a Sn-5.39Cu-1.69Al at. pct alloy produced via melt spinning at a 5-m/s wheel speed, was characterized after multiple (1-5) reflow cycles via differential scanning calorimetry between the temperatures of 293 K and 523 K (20 °C and 250 °C). Little-to-no coarsening of the Cu x Al y particles was observed for either composition; however, clustering of Cu x Al y particles was observed. For Cu 6 Sn 5 particle growth, a bimodal size distribution was observed for the drip atomized alloy, with large, faceted growth of Cu 6 Sn 5 observed, while in the melt spun alloy, Cu 6 Sn 5 particles displayed no significant increase in the average particle size, with irregularly shaped, nonfaceted Cu 6 Sn 5 particles observed after reflow, which is consistent with shapes observed in the as-solidified alloys. The link between original alloy composition, reflow undercooling, and subsequent intermetallic coarsening behavior was discussed by using calculated solidification paths. As a result, the reflowed microstructures suggested that the heteroepitaxial relationship previously observed between the Cu x Al y and the Cu 6 Sn 5 was maintained for both alloys.

36 MATERIALS SCIENCE↗

Analysis of Axial Growth of Gold Indide by Indium Diffusing away from Solder Mounds and Creating the Gold to Gold-Indide Interface Angle Inside the Solder Mound

The interfacial angle between gold and gold-indide in gold wires at the edge of PbSnIn (37.5,37.5,25.) solder mounds has been deduced by measuring the reduction in gold-wire length caused by “axial” gold-indide growth along the surface of gold wires outside the solder mounds and comparing that growth to the known “radial” gold-indide growth inside the solder mound. That interfacial angle has been found to be, on average, thirty degrees independent of temperature for samples aged between ninety and sixty degrees for 3.9 months, but shows large scatter, from a minimum of fifteen degrees for fast axial gold-indide growth, to a maximum of ninety degrees for fast gold-indide growth.

36 MATERIALS SCIENCE↗

Method and device for a high temperature vacuum-safe solder stop utilizing laser processing of solderable surfaces for an electronic module assembly

A process for manufacturing an electronic component having attaches includes providing a first component having a first attach, forming trenches on a portion of the first attach with a laser to form a solder stop, and providing a second component comprising a second attach. The process further includes providing solder between the first attach and the second attach to form a connection between the first component and the second component, where the trenches contain the solder to a usable area. A device produced by the process is disclosed as well.

Stabach, Jennifer↗

Method and device for a high temperature vacuum-safe solder resist utilizing laser ablation of solderable surfaces for an electronic module assembly

A process for manufacturing an electronic component having attaches includes providing a first component having a first attach, forming trenches on a portion of the first attach with a laser to form a solder stop, and providing a second component comprising a second attach. The process further includes providing solder between the first attach and the second attach to form a connection between the first component and the second component, where the trenches contain the solder to a usable area. A device produced by the process is disclosed as well.

Stabach, Jennifer↗