At least 19 records

Decoupling the capacity fade contributions in polymer electrolyte-based high-voltage solid-state batteries

Polymer electrolyte (PE)-based solid-state batteries (PE-SSBs) made with high-voltage cathodes are known to suffer from severe capacity fade, stemming primarily from the poor oxidative stability of most PEs under high-voltage cycling conditions. PEs also suffer from greater ion-transport limitations compared to liquid or solid electrolytes. However, often, these limitations are collectively stated to be responsible for the observed capacity fade, and it is challenging to decouple the contributions of different factors. Herein, a tunable cell fabrication platform was developed to systematically investigate and decouple the two primary capacity fade drivers (cell impedance growth and kinetic limitations), while keeping the other cell parameters constant. Three PE types with distinct transport characteristics were compared. By utilizing a voltage profile analysis method, the contribution of the cell's internal impedance growth was quantitatively decoupled from the kinetic limitations stemming from the high concentration gradient in the polymer catholyte and slow charge transfer reactions. We demonstrate that the high interfacial impedance did not necessarily correlate with the high capacity fade rate. Kinetic limitations that are not reflected by impedance measurements can play a dominant role in causing cumulative capacity decay.

Ock, Ji-young [Oak Ridge National Laboratory (ORNL↗

Non-fluorinated electrolyte for high-voltage anode-free sodium metal battery

Abundant sodium (Na) batteries are a sustainable alternative to resource-constrained lithium-ion batteries, offering huge cost advantages. However, developing high-voltage anode-free sodium metal batteries (SMBs) to narrow the energy density gap with lithium-ion batteries is hindered by a critical challenge: existing electrolytes cannot simultaneously achieve ultra-high Na coulombic efficiency and anodic stability. Here, in this study, we present a rationally designed non-fluorinated electrolyte (1.0 M NaPF 6 in 1,2-diethoxyethane/1,2-di-tert-butoxyethane) to address this key limitation, achieving Na coulombic efficiency of >99.95% and anodic stability of >4.8 V. For coin cells (2.0 mAh cm −2 , N/P = 1.7), our electrolyte design enables 4.0 V Na | |Na 3 V 2 (PO 4 ) 3 (NVP) at 5 C and 4.3 V Na | |NaNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) at 0.3 C for 5,000 and 500 cycles with a capacity retention >80%. Remarkably, the 50 mAh anode-free pouch cells 4.0 V Al | |NVP and 4.3 V Al | |NMC622 also achieve 500 and 300 cycles (retention >75%) with a specific energy of >360 Wh kg (electrode) −1 . This work focuses on electrolyte optimization and conceptual advances, whereas critical aspects such as safety, large-scale manufacturability and practical feasibility of SMBs require further investigation. The electrolyte design using non-fluorinated solvents enhances the anodic stability without sacrificing Na efficiency, laying groundwork for advancing low-cost, high-energy SMBs and supporting the transition to sustainable battery technologies.

25 ENERGY STORAGE↗

Solvent–Diluent Engineering of Normal-Concentration Organosulfur Electrolytes for High-Voltage Lithium-Ion Batteries

Enabling high‑voltage batteries depends critically on rational electrolyte design. Conventional carbonate electrolytes with LiPF 6 suffer from insufficient oxidative stability, motivating the use of lithium bis(fluorosulfonyl)imide (LiFSI) for its superior high‑temperature and high‑voltage performance. However, LiFSI is relatively costly, and its electrolytes often require high concentrations to suppress aluminum current collector corrosion in cathode architectures and to adequately passivate electrode interfaces. Here, a low‑concentration LiFSI electrolyte is realized by combining a high‑voltage organosulfur solvent, ethyl methyl sulfone (EMS), with a non‑solvating fluorinated diluent, fluorobenzene (FB). Extended cycling of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) full cells to 4.5 V reveals substantial long‑term performance advantages over conventional carbonate electrolytes. Comparison with a popular cyclic sulfone, tetramethylene sulfone (TMS), shows that ring‑containing structures such as TMS strongly influence passivation behavior, ultimately limiting performance and narrowing the viable operating window. Overall, EMS is identified as a uniquely stable solvent for LiFSI‑based electrolytes operating at moderately high voltages.

Dato, Michael A. [Argonne National Laboratory (ANL↗

Lattice-Oxygen-Driven Selective Oxidation Strategy for Stable Argyrodite Solid-State Lithium Metal Batteries

All-solid-state lithium metal batteries (ASSLMBs) with Li6PS5Cl argyrodite electrolytes and high-voltage LiNi0.8Mn0.1Co0.1O2 (NMC811) cathodes offer high energy density but suffer from rapid capacity fading due to the layered-to-rock-salt transition of NMC811 and structural degradation of Li6PS5Cl from parasitic interfacial reactions. Here, we demonstrate a catholyte engineering strategy using a Li2S scavenging additive to suppress interfacial reactivity and preserve the structural and electrochemical stability of both NMC811 and Li6PS5Cl. Incorporating 0.10 wt.% Li2S enables exceptional cycling stability, achieving 76% capacity retention after 550 cycles at C/10 and 88% retention after 800 cycles at C/3 at 60 degrees C, compared with rapid failure in pristine cells. Spectroscopic, electrochemical, and morphological analyses confirm that Li2S maintains electrode integrity by sustaining particle contact and suppressing phase decomposition. This work elucidates interfacial degradation pathways in NMC811/argyrodite systems and introduces a low-cost, scalable strategy to stabilize nickel-rich oxide cathodes in ASSLMBs, advancing their practical viability.

25 ENERGY STORAGE↗

High-Voltage Sodium–Metal Batteries with Asymmetric Fluoroalkoxylated Organoborate Anion Chemistry

The high reactivity of sodium (Na) metal restricts its compatibility to ether-based electrolytes, while the poor oxidative stability of ethers precludes their coupling to high-voltage cathodes, fundamentally limiting the operating voltage and energy density of sodium–metal batteries (SMBs). We present here a coordination-asymmetry strategy to reconcile this thermodynamic mismatch by generating in situ an asymmetric fluoroalkoxylated organoborate anion, [FB(OCH(CF 3 ) 2 ) 3 ] − (BOF – ), via a Lewis acid–base adduct reaction in ether electrolyte. The asymmetric ligand architecture differentiates oxidative and fluorination pathways: oxidizable B–O moieties mediate controlled interfacial reconstruction, whereas the terminal B–F units supply fluorine for chemical passivation. This self-adaptive chemistry yields nanoscale, conformal, compositionally graded interphases: a boron-oxide/boron-oxycarbide-rich cathode-electrolyte interphase (CEI) that mitigates ether oxidation and a bilayered inorganic–organic solid–electrolyte interphase (SEI) that regulates Na deposition. The nanostructured interphases enable highly reversible Na plating/stripping with an average Coulombic efficiency (CE) of 99.98% and sustain stable 4.3 V operation of anode-free SMBs in oxidation-prone ether electrolytes. Furthermore, this work establishes asymmetric boron coordination as a molecular-level design principle for creating chemically adaptive interphases that overcome the redox asymmetry in energy-dense electrochemical systems.

Anions↗

Molecular Tuning of Ether Cosolvent Chemistry for High-Voltage Sodium-Ion Batteries

Ethers as electrolyte cosolvents in sodium-ion batteries (SIBs) provide favorable Na + solvation and interfacial properties, but their low oxidative stability limits their use in high-voltage SIBs. Herein, we address this limitation via molecular tuning of ether cosolvents for high-voltage (4.2 V) hard carbon || NaNi 0.33 Fe 0.33 Mn 0.33 O 2 full cells. Tetrahydropyran (THP) is functionalized with a nitrile group to form tetrahydropyran-4-carbonitrile (THPCN). To delineate the effect of nitrile functionalization and benchmark ether against a conventional carbonate, THP, THPCN, and diethyl carbonate (DEC) are evaluated as cosolvents with ethylene carbonate. Nitrile functionalization lowers the HOMO energy of the ether, extends the electrolyte stability window, and alters Na⁺ solvation. Spectroscopic techniques and molecular dynamics simulations reveal that THPCN exhibits predominantly aggregate-dominated solvation (95.1 %) with weakened Na + -solvent interactions, producing the most anion-rich environment relative to DEC and THP cosolvents. THPCN-modified solvation promotes the formation of highly conductive, fluorine-enriched interphases that suppress parasitic reactions. Pouch full cells with THPCN sustained ~ 600 cycles at 4.2 V, outperforming THP and DEC. Operando gas analysis reveals that THPCN reduces CO 2 generation by 45% and H 2 generation by 30% relative to THP. Furthermore, the findings demonstrate nitrile functionalization as a molecular design strategy to stabilize ethers and enable high-voltage SIBs.

25 ENERGY STORAGE↗

Novel Organosulfur-Based Electrolytes for Safe Operation of High Voltage Li-ion Batteries over a Wide Operating Temperature

This project addresses the failure of conventional electrolytes and enables high-voltage operation of lithium-ion batteries (LIBs) by developing a novel organosulfur-based electrolyte system. To achieve this goal, we first designed and synthesized new organosulfur solvents that functionalized with strong electron-withdrawing groups such as fluoroalkyl and cyano substituents. Through regio-specific molecular engineering, supported by theoretical calculations, we lowered the highest occupied molecular orbital (HOMO) energy levels of these molecules to increase their anodic stability for high-voltage operation. We then optimized the formulation of the organosulfur-based electrolyte with additives, co-solvents and salts tailored to the newly synthesized solvent molecules. In parallel, we utilized advanced spectroscopic techniques—including in situ FTIR, EIS, and DEMS—to thoroughly elucidate the mechanisms of interaction between the electrolyte and electrode materials. Finally, we evaluated 2 Ah pouch cells under both normal and extreme conditions. Pouch cells with the newly developed electrolyte system demonstrated >90% capacity retention after 500 cycles under 4.5 V operating voltage, >80% capacity retention after 1000 cycles in coin cell level. In addition, the cells exhibited high safety and reliable operation capability over a wide temperature range from −30 °C to +45 °C.

25 ENERGY STORAGE↗

Improving Ionic Conformality Across Polymer Electrolyte|Electrode Interfaces

Maintaining uniform ionic transport at electrode|electrolyte interfaces, i.e., ionic conformality, remains challenging in polymer electrolyte (PE)-based solid-state batteries. Morphological conformality does not necessarily imply ionic conformality. In PEs, which typically consist of a mechanically supporting component and distinct ionically conductive components, the rearrangement or depletion of mobile ion-conductive domains at interfaces can disrupt ionic transport pathways. Such localized ionic depletion contributes to interfacial instability and capacity degradation in high-voltage lithium-metal batteries. Herein, an electrolyte design approach aimed at minimizing interfacial heterogeneities is demonstrated through compositional adjustments, characterized by spatially resolved structural and chemical X-ray techniques and NMR diffusometry to elucidate ion transport dynamics. This approach improves ionic conformality at electrode interfaces, enhancing cycling stability in Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) coin and pouch cells cycled at high voltages. These results contribute to understanding interfacial behaviors in multiphase PEs and inform strategies for improving stability across solid-state battery interfaces.

36 MATERIALS SCIENCE↗

Networks of electrochemical oxidation of common lithium-ion Battery solvents revealed by NMR spectroscopy

Raising the upper cutoff voltage of lithium-ion batteries (LIBs) to increase energy density often exceeds the electrolyte’s anodic stability limit, accelerating degradation and creating a major durability tradeoff. Designing electrolytes that can sustain long-term high-voltage cycling requires a clearer understanding of the fundamental mechanisms occurring when commercial carbonate solvents oxidize. Here, to this end, simplified single-salt, single-solvent formulations of LiClO 4 and LiPF 6 in dimethyl carbonate (DMC), ethylene carbonate (EC), or ethyl methyl carbonate (EMC) were anodically electrolyzed on inert electrodes and monitored for extended periods of time using 1 H, 13 C, 19 F, and 35 Cl nuclear magnetic resonance (NMR) spectroscopy. The controlled environment of the experiments, coupled to the unique sensitivity of NMR, unveiled novel metastable intermediates and the formation of branching networks of products with temporal evolution. Oxidation of the pristine solvent primarily proceeds through a radical pathway that also produces highly reactive protons but faces competition from a second pathway involving a radical carbocation intermediate. In all cases, the intermediates follow a variety of downstream pathways that can intersect with each other. The concomitant network of reactions represents a significant increase in complexity compared to common descriptions in the literature, yet, critically, it helps explain the wide range of products typically identified in electrolyte oxidation in complete cells. The results highlight the need for refocusing fundamental research on anodic stability to analysis of the hierarchy of reaction networks to better inform efforts to mitigate the detrimental effects on battery performance, including prevention and harvesting of proton and radical products.

Electrolytes↗

Solvated Ionic Liquid-based Electrolytes: Experimental Characterization, Atomistic Modeling and Applications in Energy Storage

This study aimed on understanding the molecular structure and transport mechanisms of high-concentration lithium electrolytes, with a particular focus on solvate ionic liquids (SILs) based on glyme solvents, for use in next-generation, high-voltage energy storage systems. The hypothesis is that the composition of the solvents in these electrolytes can be designed and adjusted to control cation solvation, enabling charge transport via an ion-hopping mechanism. This mechanism resembles Grotthuss conduction of protons in water and is independent of electrolyte viscosity. The experimental studies employed linear and nonlinear infrared spectroscopy (FTIR and 2D IR), electrochemical measurements, and vibrational probes.

25 ENERGY STORAGE↗

Advanced LiFSI-LiPF6 Electrolyte for Wide-Temperature and Thermally Stable Lithium-Ion Batteries

A new optimized LiFSI–LiPF6 dual-salt controlled-solvation electrolyte (E-DS) is demonstrated to enable practical graphite||LiNi0.8Mn0.1Co0.1O2 cells (˜4.0 mAh cm?²) to achieve exceptional performance and safety under extreme conditions. By optimizing anion coordination with the smaller, more dissociating FSI? anion, the E-DS forms ultrathin, dense, and inorganic-rich electrode/electrolyte interphases that dramatically suppress solvent decomposition, transition-metal dissolution, and surface reconstruction compared to the conventional LiPF6/carbonate electrolyte. Consequently, E-DS cells deliver >78% capacity retention after 300 cycles at 60 °C, retain fast discharging capacity at 30 °C, and operate effectively at -20 °C. Most strikingly, fully charged full cells with E-DS, even under overcharging to 4.8 V, show a lower heat evolution in stable formulations — transforming a traditionally unstable high-voltage/high-temperature configuration into an intrinsically safe state. This work establishes a new benchmark for carbonate-containing electrolytes, simultaneously achieving high energy density, fast-discharging capability, wide-temperature operation (-20 to 60 °C), and outstanding thermal safety in nickel-rich lithium-ion batteries.

electrode/electrolyte interphase↗

Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC Cathodes

Degradation of LiNi x Mn y Co 1-x-y O 2 (NMC)-based lithium-ion batteries depends strongly on cut-off voltage ranges. In addition to the high upper cut-off voltage, a high depth of discharge (i.e., lower cut-off voltage) significantly worsens cathode impedance growth and capacity fade during long-term cycling. However, there is currently no consensus on the mechanism behind the negative role of a deep discharge. Here, this phenomenon was investigated in graphite||NMC cells with single-crystal cathodes (LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC622) or LiNi 0.76 Co 0.14 Mn 0.10 O 2 (NMC76)) using targeted aging protocols (constant high-voltage holds vs. charge–discharge cycling), while monitoring transition-metal (TM) dissolution, cathode-electrolyte interface (CEI) impedance, and NMC surface composition. We demonstrate a correlation between discharge-driven CEI impedance growth and increased TM dissolution. Furthermore, this degradation pathway is more pronounced in lower-Ni NMC622 than in higher-Ni (NMC76) under comparable delithiation states at charge, with both compositions undergoing the H2→H3 phase transition. X-ray photoelectron spectroscopy (XPS) reveals NMC composition-dependent evolution of surface lattice oxygen and restructured surface layer composition between charged and discharged states. These findings add mechanistic depth to the role of discharge as an active driver of interfacial degradation and provide new insights into its composition dependence.

25 ENERGY STORAGE↗

Manganese‐Based Spinel Cathodes: A Promising Frontier for Solid‐State Lithium‐Ion Batteries

Recently, all-solid-state lithium-ion batteries (ASSLIBs), which exhibit improved safety and enhanced energy density compared to conventional commercialized lithium-ion batteries (LIBs), thereby have garnered extensive research interest. Among the promising cathode candidates, Mn-based spinel cathodes LiMn 2 O 4 (LMO) and LiNi 0.5 Mn 1.5 O 4 (LNMO), with the unique characteristics of low cost, structural stability, and 3D Li-ion diffusion channels, have demonstrated excellent performance in LIBs and presented great potential in ASSLIBs applications. However, several challenges, including structural degradations, poor interfacial contact, large interfacial resistance, and Mn-dissolution/diffusion during the electrochemical cycling, hinder their practical applications and commercialization in the ASSLIBs. Particularly, the high-voltage LNMO cathodes suffer from the challenge of electrochemical incompatibility with most of the solid-state electrolytes (SSEs). Herein, the spinel structure, the electrochemical behavior, and the structural degradation of the LMO/LNMO are explored. The characteristics and recent progress of the mitigating strategies to the challenges of various SSEs, including polymer-, oxide-, composite-, sulfide-, halide-, and LiPON-based SSEs, are introduced when paired with LMO/LNMO. Finally, the directions for future research to advance Mn-based spinel cathodes and fulfill the requirements of the next-generation ASSLIBs are also discussed.

Dou, Yu [Concordia University, Montreal, QC (Canad↗

Coupling Redox Compensation and Interfacial Stabilization in Low-Ni O3-Type Sodium Layered Oxide Cathodes

Low-Ni O3-type sodium layered oxides are attractive cathodes for cost-robust sodium-ion batteries, yet high-voltage cycling is often limited by Fe-driven degradation, including cation migration/dissolution, irreversible slab gliding with large strain, particle cracking, and accelerated interfacial parasitic reactions. Here, in this study, we introduce a redox-interface codesign strategy using stoichiometric, charge-balanced Cu 2+ /Ti 4+ cosubstitution while preserving full Na stoichiometry, transitioning from NaNi 1/4 Fe 1/2 Mn 1/4 O 2 to NaNi 1/4 Fe 1/5 Mn 1/4 Cu 3/20 Ti 3/20 O 2 . With the cosubstitution, Cu and Ti suppress Fe migration and dissolution and facilitate sustained Fe oxidation at high voltage. Meanwhile, Cu is also shown to be redox-active, providing reversible cationic charge compensation that mitigates the capacity penalty typically associated with reducing Fe participation. Operando diffraction and spectroscopy collectively indicate a more reversible high-voltage structural evolution with suppressed Fe-related irreversibility. Particularly, spontaneous Ti enrichment at surface/grain-boundary regions stabilizes the cathode−electrolyte interface and promotes a more NaF-rich interphase signature. This work establishes a generalizable route to reconcile stability and capacity in low-Ni, Fe-containing O3 sodium layered oxide cathodes via compositionally encoded bulk-interfacial coupling.

25 ENERGY STORAGE↗

Unraveling interphase-driven failure pathways in LiMn0.6Fe0.4PO4/graphite pouch cells

LiMnxFe1−xPO4 (LMFP) is a promising high-voltage, thermally stable, and earth-abundant cathode material, yet its practical application is limited by interphase instability and Mn dissolution. In this work, we systematically evaluate LiMn0.6Fe0.4PO4/graphite pouch cells using three electrolyte formulations including control carbonate electrolyte, control + 2 wt% vinylene carbonate (VC), and control + 2 wt% VC + 1 wt% 1,3,2-dioxathiolane 2,2-dioxide (DTD), to establish how electrolyte composition governs interphase chemistry and long-term degradation. Electrochemical testing shows that both additives are preferentially reduced prior to ethylene carbonate (EC) during cell formation, generating robust cathode-electrolyte interphase (CEI) and solid-electrolyte interphase (SEI) layers that suppress gas evolution and raise the first-cycle coulombic efficiency to 89.3%. Additionally, the dual-additive electrolyte delivers the most stable performance, retaining over 85% capacity after 600 cycles while minimizing impedance growth under long-term cycling at C/3 and 40 °C. Soft X-ray absorption spectroscopy confirms that VC + DTD effectively suppresses electrolyte oxidation at the cathode surface, and micro-X-ray fluorescence shows substantially reduced Mn dissolution and deposition on the graphite anode. Density functional theory simulations further provided insights into the structural and energetic influences of alkoxide species on the cathode surface, proposing a Mn2+ extraction mechanism. The combined experimental and computational findings establish a mechanistic link between electrolyte composition and interphase evolution, highlighting the effectiveness of electrolyte engineering for extending the operational lifetime of LMFP-based lithium-ion batteries.

Chak, Chanmonirath Michael↗

Amorphous ZrCl 4 -Based Superionic Conductor as a Cost-Effective Solid Electrolyte for Batteries

Developing highly conductive and cost-effective solid electrolytes is essential for the commercialization of all-solid-state batteries (ASSBs). Zr-based halide electrolytes hold great promise due to their low estimated cost and high oxidation stability. However, the ionic conductivities of most of them are not high enough to enable moderate- and high-rate cycling of ASSBs. Here, fast ion transport is achieved in a group of cost-effective ZrCl 4 -based electrolytes via a design strategy to create highly disordered amorphous structures. Amorphous Li 0.8 ZrCl 4 (SO 4 ) 0.4 , with a low estimated cost of $21 kg –1 , achieves an ionic conductivity of 1.86 mS cm –1 at 25 °C. It also shows a high oxidation limit of 4.5 V vs Li/Li + and good compatibility with high-voltage cathodes, as demonstrated by the stable cycling of ASSBs (73.7% capacity retention after 1000 cycles at 1 C). Synchrotron X-ray diffraction, pair distribution function analysis, and electrochemical impedance spectroscopy reveal that the outstanding conductivity of these amorphous electrolytes is closely related to their short-range and medium-range ordering, revealing new insights for designing high-performance, cost-effective solid electrolytes.

Zhang, Guangxing [Georgia Institute of Technology,↗

Stabilizing Cathode–Electrolyte Interphase of Nickel-Rich Single-Crystal Cathodes for Lithium-Ion Batteries

Nickel-rich single-crystal (SC) layered oxides are promising cathode candidates for next-generation lithium-ion batteries (LIBs) owing to their high energy density and structural robustness against intergranular cracking. However, their intrinsic surface reactivity with liquid electrolytes accelerates parasitic reactions at the cathode–electrolyte interphase (CEI), leading to transition-metal dissolution, gas generation, and impedance buildup. In this work, we synthesized SC-Li x Ni 0.9 Mn 0.05 Co 0.05 O 2 (NMC9055, 1 ≤ x ≤ 1.2) using a eutectic-assisted method and investigated interface stabilization strategies. A nickel-deficient Li x Ni 0.6 Mn 0.2 Co 0.2 O 2 (NMC622, 1 ≤ x ≤ 1.2) coating was applied via evaporation-based deposition to suppress CEI degradation pathways. Structural and compositional analyses confirmed uniform shell formation and preserved particle integrity. Half-cell electrochemical testing against lithium metal revealed ∼10% higher capacity retention and improved reversibility compared with pristine SC NMC9055, particularly under high-voltage operation. In conclusion, these results highlight the critical role of controlled surface chemistry in mitigating CEI instability in nickel-rich SC cathodes, offering a pathway toward enabling durable high-energy LIBs.

Coating processes↗

Unveiling the High‐Voltage Reactivity and Gas Evolution With Aluminum‐Based Chloride and Oxychloride Catholytes in Solid‐State Sodium Batteries

All-solid-state sodium batteries (ASSBs) employing halide solid electrolytes (SEs) offer a cost-effective and energy-dense alternative to conventional liquid electrolyte systems. However, their high voltage (>4 V vs. Na/Na + ) performance remains limited by interfacial instability between the cathode active material (CAM) and the SE. We present here the electrochemical and interfacial behaviors of crystalline NaAlCl 4 and amorphous sodium–aluminum–oxychloride (NACO) SEs when combined with NaNi 0.5 Mn 0.5 O 2 cathode. While oxygen incorporation in NACO enhances ionic conductivity by nearly three orders of magnitude relative to NaAlCl 4 , it does not improve high-voltage cycling stability. Cells employing NACO exhibit accelerated capacity fade, increased cell impedance growth, and intrinsic oxygen evolution above 4.5 V vs. Na 3 Sn, as revealed by operando electrochemical mass spectrometry. In contrast, the NaAlCl 4 -based cells show no detectable gas release, underscoring their superior high-voltage stability and safety. Time-of-flight secondary-ion mass spectrometry confirms the formation of Al─O and Ni/Mn─Cl species, respectively, in the SE and CAM, indicating redox-driven anion exchange that contributes to kinetic hindrance of high-voltage phase transitions. The findings establish that while oxygen incorporation enhances ionic transport, it can compromise interfacial stability, suggesting pure chloride SEs may offer a more robust and intrinsically safer pathway for developing high-energy ASSBs.

25 ENERGY STORAGE↗