Surveillance Test Articles Development
Overview of previous work at ANL: • Initial designs tested with A617 driver • 3 families of specimens: - Large: demonstrate failure during test - Small: demonstrate realistic-sized samples - Reference: to validate the strain-gauge thermal strain correction • Thermal cycling between 500 and 650, over a period of about 200 minutes • Demonstrated basic surveillance approach • Large specimens failed in gauge section • The bimetallic welds appeared intact at the end of testing (316H-A617) • Gradual decrease in strain range over time • Strain gauge reliability was an issue: at least one gauge failed • Failure mode (buckling) was not what we had expected