Toward Optimizing Electrospun Nanofiber Fuel Cell Catalyst Layers: Microstructure and Pt Accessibility

This work investigates how local ionomer/platinum (Pt) interactions and ionomer distribution in electrospun Pt/Vulcan nanofiber electrodes impact ionomer coverage, proton accessibility, and oxygen reduction reaction (ORR) performance in proton-exchange membrane fuel cells. Insights from various in situ electrochemical diagnostics were utilized in conjunction with ex situ microscopic characterization to understand how the electrode microstructure—both at the aggregate level and near the ionomer/platinum interface—is affected by electrospinning in comparison to ultrasonic spraying. The effect of the carrier polymer poly(acrylic acid) (PAA) concentration from 5–20 wt % (with respect to total ink solids) on the resulting nanofiber morphology is discussed. Electron microscopy observations and CO displacement measurements indicated that Pt/Vulcan nanofibers prepared with a higher PAA concentration (15 wt %) were conformally coated with a film of ionomer on the exterior of the fiber, which resulted in an overall lower ionomer coverage on both Pt and carbon throughout the fiber diameter. In contrast, 10 wt % PAA leads to a uniform intrafiber distribution of the ionomer within the fibers, increasing the overall ionomer coverage and proton accessibility under both wet and dry conditions. These differences in the local ionomer coverage on Pt between 10 and 15 wt % PAA were also attributed to differences in the adsorption/interaction affinities between PAA and the ionomer onto the catalyst surface in the ink using zeta potential measurements. Additional fuel cell electrochemical tests on the electrospun electrodes show improvements in ORR kinetics and high-current-density H 2 /air performance compared to the ultrasonically sprayed electrodes.

25 ENERGY STORAGE↗

Coupled continuum and network model framework to study catalyst layers of polymer electrolyte fuel cells

The nanostructured thin film (NSTF) catalyst layers which have demonstrated high power densities, mass activities, and exceptional metal and support stability can have limited operational robustness due to their thin thickness and the hydrophilicity of the metal-coated nano whiskers. The dispersed nanostructured thin film (dNSTF) catalyst layers have been developed by dispersing the NSTF Pt whiskers with ionomer and carbon support to increase the thickness and hydrophobicity. Continuum and network models (NM) are coupled through boundary conditions to study the polymer electrolyte fuel cell with a dNSTF cathode catalyst layer. The coupled model combines the computational efficiency of the continuum model with the pore-scale information in the dNSTF cathode catalyst layer of the NM. It captures the special morphology of the partially ionomer/water covered cylindrical whiskers, as well as water percolation through the pore structures and their impact on the cell performance. Here we observe optimal ionomer coverage on whiskers to be 0.5, ionomer to carbon ratio to be 0.9 and higher whisker to carbon ratios to be desired.

08 HYDROGEN↗

Tailoring electrode microstructure via ink content to enable improved rated power performance for platinum cobalt/high surface area carbon based polymer electrolyte fuel cells

Improvements in polymer electrolyte fuel cell (PEFC) electrode performance have primarily focused on catalyst and ionomer developments, marginalizing the importance of catalyst ink formulation. In this study, the effect of ink formulation is examined across a series of cathodes comprised of PtCo supported on high surface area carbon (PtCo/ HSC ) and Nafion ionomer using an array of in situ electrochemical and ex situ characterization techniques. In contrast to prior work on Pt/Vu systems, ink water content had little effect on the electrochemically determined ionomer coverage for the PtCo/HSC electrocatalyst examined here. Characterization using nano-scale resolution X-ray computed tomography (nano-CT) demonstrated that water-rich ink formulations lead to a reduction in aggregate size (ionomer + PtCo/HSC), improving local O 2 transport. This understanding, combined with the use of a commercially-available electrocatalyst was used to produced state-of-the-art membrane electrode assemblies with Pt loadings of 0.03/0.08 mg Pt /cm 2 on the anode and cathode respectively, having; i) > 1 A/mg Pt (0.9 V iR-free , 150 kPa, 80 °C, 100% RH, H 2 /O 2 ), ii) 320 mA/cm 2 at 0.8 V, 150 kPa, 80 ° C, 100% RH, H 2 /Air), and iii) > 1 W/cm 2 elec at rated power (0.67 V, 250 kPa, 94 °C, 65% RH, H 2 /Air) or < 0.11 g Pt /kW rated .

25 ENERGY STORAGE↗

Unraveling the core of fuel cell performance: engineering the ionomer/catalyst interface

The biggest obstacle to the widespread implementation of polymer electrolyte membrane fuel cells (PEMFCs) is their cost, primarily due to the use of platinum catalysts. The high intrinsic catalyst activity exhibited on a rotating disk electrode (RDE) is rarely realized in a membrane electrode assembly (MEA), which is a long-standing challenge for PEMFCs and a cause of low catalyst utilization. To translate the high RDE performance of a catalyst into a MEA, the design of an ideal ionomer/catalyst interface is proposed: a thin, conformal ionomer film covers the maximum surface of a Pt nanoparticle and thus simultaneously maximizes catalyst utilization, (i.e., high mass activity and electrochemically active surface area) and O 2 diffusion rate (i.e., high current density performance) without compromising proton conduction. Building such an interface is a long-standing challenge due to the lack of interaction between the ionomer and catalyst particles, resulting in large ionomer agglomerates and inhomogeneous ionomer coverage over the catalyst nanoparticle, with consequent poor fuel cell performance. In this work, this ionomer/catalyst interface has been engineered, utilizing the electrostatic attraction between positively charged catalyst and negatively charged ionomer particles in a catalyst ink and preserved in a solid catalyst layer. As a result, this interface leads to previously unachieved proton exchange membrane fuel cell performance in terms of both catalyst utilization (75% vs. 45%) and peak/rated power density (i.e., 1.430/0.930 W cm -2 , H 2 /air, cathode Pt loading: 0.1 mgPt cm -2 ) for pure Pt catalysts, even better than those of Pt alloy catalysts. This work demonstrates the formation of an interface in the liquid phase (using ultra-small-angle X-ray scattering in combination with cryo-TEM, isothermal–titration–calorimetry) and the preservation of the interface in the solid catalyst layer (using TEM) and estimates the effective coverage and thickness of the ionomer film (using limiting current density, RDE and fuel cell performance).

25 ENERGY STORAGE↗

Impact of Platinum Primary Particle Loading on Fuel Cell Performance: Insights from Catalyst/Ionomer Ink Interactions

A variety of electrochemical energy conversion technologies, including fuel cells, rely on solution-processing techniques (via inks) to form their catalyst layers (CLs). The CLs are heterogeneous structures, often with uneven ion-conducting polymer (ionomer) coverage and underutilized catalysts. Various platinum-supported-on-carbon colloidal catalyst particles are used, but little is known about how or why changing the primary particle loading (PPL, or the weight fraction of platinum of the carbon-platinum catalyst particles) impacts performance. Here, by investigating the CL gas-transport resistance and zeta-potentials of the corresponding inks as a function of PPL, a direct correlation between the CL high current density performance and ink zeta-potential is observed. This correlation stems from likely changes in ionomer distributions and catalyst-particle agglomeration as a function of PPL, as revealed by pH, zeta-potential, and impedance measurements. These findings are critical to unraveling the ionomer distribution heterogeneity in ink-based CLs and enabling enhanced Pt utilization and improved device performance for fuel cells and related electrochemical devices.

30 DIRECT ENERGY CONVERSION↗

Single Cobalt Sites Dispersed in Hierarchically Porous Nanofiber Networks for Durable and High-Power PGM-Free Cathodes in Fuel Cells

Increasing catalytic activity and durability of atomically dispersed metal–nitrogen–carbon (M–N–C) catalysts for the oxygen reduction reaction (ORR) cathode in proton-exchange-membrane fuel cells remains a grand challenge. In this study, a high-power and durable Co–N–C nanofiber catalyst synthesized through electrospinning cobalt-doped zeolitic imidazolate frameworks into selected polyacrylonitrile and poly(vinylpyrrolidone) polymers is reported. The distinct porous fibrous morphology and hierarchical structures play a vital role in boosting electrode performance by exposing more accessible active sites, providing facile electron conductivity, and facilitating the mass transport of reactant. The enhanced intrinsic activity is attributed to the extra graphitic N dopants surrounding the CoN 4 moieties. The highly graphitized carbon matrix in the catalyst is beneficial for enhancing the carbon corrosion resistance, thereby promoting catalyst stability. The unique nanoscale X-ray computed tomography verifies the well-distributed ionomer coverage throughout the fibrous carbon network in the catalyst. The membrane electrode assembly achieves a power density of 0.40 W cm –2 in a practical H 2 /air cell (1.0 bar) and demonstrates significantly enhanced durability under accelerated stability tests. The combination of the intrinsic activity and stability of single Co sites, along with unique catalyst architecture, provide new insight into designing efficient PGM-free electrodes with improved performance and durability.

25 ENERGY STORAGE↗

Anolyte Enhances Catalyst Utilization and Ion Transport Inside a CO 2 Electrolyzer Cathode

Electrochemical CO 2 reduction is a promising technology to capture and convert CO 2 to valuable chemicals. High Faradaic efficiencies of CO 2 reduction products are achieved with zero-gap alkaline CO 2 electrolyzers with a supporting electrolyte at the anode (anolyte). Herein, we investigate the effect of anolyte on the electrode properties such as catalyst utilization, ionic accessibility etc. of a CO 2 reduction cathode using electrochemical techniques and cell configurations that avoid the complexities related to co-electrolysis. Using 1M KOH as the anolyte and a Cu gas-diffusion-electrode with low Nafion content as the model CO 2 reduction electrode, we find that electrode capacitance (proxy for electrochemically active surface area) and ionic conductivity inside the cathode increase approximately 4 and 447 times, respectively, in presence of KOH. Liquid anolyte wets the electrode’s pore structure more efficiently than capillary condensation of feed water vapor. The ionomer coverage is very low, and its distribution inside the electrode is highly fragmented. Surface ion conduction mechanisms inside the electrode are orders of magnitude lower than the bulk ion conduction in presence of anolyte. This study shows that when an anolyte (e.g., KOH) is used, catalyst utilization and ionic accessibility inside the electrode increase significantly.

30 DIRECT ENERGY CONVERSION↗

A novel approach to identify the ionomer phase in PEMFC by EELS

Proton exchange membrane fuel cells are one of the most promising technologies of energy conversion for both automotive and stationary applications, due to their ultimate cleanness and high efficiency. A critical factor, which strongly affects the fuel cell performance, is the ionomer distribution and coverage over the carbon support, since the catalysts, which are typically Pt and/or Pt-alloy nanoparticles, must be located at the carbon support/ionomer interface to catalyze the sluggish oxygen reduction reaction. However, the characterization and identification of the ionomer film, in terms of ionomer distribution and coverage over the carbon surface, is a long standing challenge. This is because the ionomer film may suffer from beam damage during the characterization, either from x-rays, neutrons or an electron beam, which causes morphological changes. In this regard, we report here a novel approach to identify and differentiate the ionomer, using the carbon signal produced by STEMEELS. Using this approach, not only the ionomer distribution, but also the carbon support distribution, can be probed at high spatial resolutions. In addition, this new approach allows us to identify ionomer-rich and carbon-support rich regions, which are quite challenging to determine using other methods.

08 HYDROGEN↗

Elucidating the Role of Ionomer in the Performance of Platinum Group Metal-free Catalyst Layer via in situ Electrochemical Diagnostics

The ionomer content in platinum group metal (PGM)-free polymer electrolyte fuel cell (PEFC) cathode catalyst layer (CCL) plays an important role in the electrode gas transport properties, proton conductivity, and hence, membrane electrode assembly (MEA) performance. In this work, the ionomer content in the CCL is varied, influencing electrode microstructure by altering porosity, tortuosity, as well as ionomer distribution and coverage of the catalyst particles. A novel technique consisting of a H 2 pump, combined with a Pt black sensor layer, is used to measure the bulk mass transport resistance of a series of PGM-free CCL prepared with different ionomer contents. The values for bulk electrode mass transport resistance are contrasted with electrode proton transport resistance in the cathode catalyst layer, establishing a clearly defined trade-off between two key performance limiting phenomena and identifying a need for novel PGM-free electrode fabrication strategies.

25 ENERGY STORAGE↗

Anions in Corrosion: Influence of Polymer Electrolytes on the Interfacial Ion Transfer Kinetics of Cu at Au(111) Surfaces

The corrosion kinetics of metals in the presence of polymer electrolytes—which are often used in devices for the electrochemical production of hydrogen, hydrocarbons, and alcohols—is convoluted by transport and ill-defined reactive interfaces which mask the fundamental reaction kinetics. Underpotential-deposited monolayers of Cu at Au(111) surfaces provide a structurally welldefined active site for interfacial ion transfer, with a fixed number of sites available for adsorption. Here, we investigate the adsorption behavior of Cu at Au(111) surfaces across a series of sulfate and sulfonate electrolytes, to understand how anion structure influences the kinetics of elementary interfacial ion-transfer reactions. The influence of anion structure is most significant at high adsorbate coverage, with similar adsorption isotherms and kinetics observed for all three molecular sulfates and sulfonates. In contrast, a suspended perfluorosulfonic acid ionomer reduced both the equilibrium coverage of Cu as well as the standard exchange rate at Au(111) at low coverages of Cu. These results suggest that electrocatalyst corrosion is inhibited for metal nanoparticles supported at polymer electrolytes due to changes in adsorbate coverage as well as suppressed kinetics for interfacial ion transfer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding Platinum Ionomer Interface Properties of Polymer Electrolyte Fuel Cells

A well-designed cathode catalyst layer with optimal ionomer distribution is critical to minimizing amount of Platinum (Pt) content in polymer electrolyte fuel cells (PEFCs). The impact of Pt loading, ionomer content and carbon support types on the catalyst/ionomer interface were also investigated at dry and wet conditions. Higher Pt loadings resulted in higher double layer capacity (C dl ) and similar electrochemical surface area (ECSA) due to well dispersed ionic phase material. Higher ionomer content resulted in higher ionic conductivity but also showed similar SO 3 − group coverage. High surface area (HSA) carbon support had larger ECSA and C dl at both dry and wet conditions, as less agglomerated Pt was well dispersed in the meso-pores of the support. Lower SO 3 − group coverages were observed for HSA carbon than for Vulcan carbon due to Pt particles being buried within the porous HSA carbon support. The effect of cell conditioning and voltage recovery on the PEFC cathode catalyst layer was shown to have minimal impact on SO 3 − group coverage despite a decrease in C dl and ECSA due to the size increase of Pt particles. At dry condition, a significant increases in SO 3 − group coverage were observed for all MEAs due to higher adsorptivity of ionomer in dry conditions.

25 ENERGY STORAGE↗

Physically Based Modeling of PEMFC Cathode Catalyst Layers: Effective Microstructure and Ionomer Structure–Property Relationship Impacts

Abstract This work presents a pseudo-two-dimensional proton exchange membrane fuel cell (PEMFC) model incorporating Nafion ionomer structure–property relationships in the cathode catalyst layer (CL) to capture and explain losses at low Pt loading. Structural data from neutron reflectometry and thin film Nafion conductivity measurements predict variations in the oxygen diffusion coefficient and ionic conductivity with changing CL ionomer thickness and Pt loading. By including these structure–property relationships, predicted polarization curves agree closely with previously published experimental data from cells with Pt loadings between 0.025 and 0.2 mg/cm2. Results demonstrate that structure–property relationships based on physically measurable ionomer and CL properties provide a feasible interpretation of PEMFC CL phenomena for a range of Pt loadings and help explain previously unaccounted-for losses at low Pt. Results also show that simulations must account for surface species coverage variations in order to properly capture the kinetic losses. Finally, results suggest that an increase in ionomer thickness surrounding the C/Pt surfaces may lead to improved cell performance due to improved ionic conductivity.

Electrochemistry↗

Platinum Surface Oxide and Oxygen Reduction Reaction Kinetics during Transient Fuel Cell Operation

Pt surface oxide coverage (POC) and Oxygen Reduction Reaction (ORR) were measured under a range of operating conditions in a Proton Exchange Membrane Fuel Cell (PEMFC). Sensitivity analysis suggests that adsorption of sulfonate groups of the ionomer on the Pt surface plays an important role in POC and ORR kinetics. Although both Pt oxide growth and ORR activity decay follow a logarithm of time behavior, it is found that ORR kinetics are affected by at least two different types of Pt oxide. A semi-empirical ORR kinetic model is proposed taking into account the effect of ionomer and Pt oxide types. The model is capable of providing a quantitative prediction of POC and ORR activity over a range of potential, temperature, relative humidity, and time that is relevant to normal PEMFC operation.

Electrochemistry↗

Toward Optimizing Electrospun Nanofiber Fuel Cell Catalyst Layers: Polymer–Particle Interactions and Spinnability

We investigate the effect of the poly(acrylic acid) (PAA) carrier polymer concentration on the microstructure and rheological properties of catalyst inks for electrospun polymer–electrolyte membrane fuel-cell catalyst layers. Characterization of an ink microstructure using oscillatory shear rheology showed that the catalyst particles (platinum on carbon) are significantly agglomerated in the absence of PAA or an ionomer. Both the ionomer and PAA promoted the stability of the particles against agglomeration via electrosteric stabilization by adsorbing onto the particle surface. Increasing the PAA concentration increased the stability of the particles (or reduced the agglomerated structure) due to increasing PAA coverage onto the free surface area of the particles. However, beyond a certain increase in concentration, PAA was found to predominantly remain as an excess free polymer in the ink due to an insufficient free/available surface area on the particles for further PAA coverage. Extensional rheology measurements demonstrated that PAA enhances the extensional viscosities of the inks. Consequently, increasing the PAA concentration in the ink promoted the evolution of uniform nanofibers. However, beyond a certain concentration, a significant increase in the shear viscosities of the inks led to defective fiber morphologies because of the onset of flow instabilities. Electrochemical performance comparisons between catalyst layers with different PAA concentrations showed maximum performance at the PAA concentration that led to the least agglomerated structure of the catalyst, most uniform fiber morphologies, and low concentrations of free (non-adsorbing) PAA in the electrode. These results provide a rationale for optimization of electrospun catalyst nanofibers for both spinnability and electrochemical performance.

25 ENERGY STORAGE↗

The ionomer as an oxygen evolution reaction promoter: piperidinium’s impact on mechanistic pathways on NiO, IrO 2 , and Fe–NiO

The commercial viability of anion exchange membrane (AEM) electrolysis requires optimization of various stack components, with specific catalyst-ionomer combinations often yielding higher current densities, lowered Tafel slopes, and improved mass activity. In this joint theoretical-experimental study, theoretical calculations detail the impact of Versogen’s piperidinium functional group on the complex, kinetically limiting oxygen evolution reaction, finding that the functional group can act as a promoter of specific steps (O*/O 2 * formation; H 2 O/O 2 desorption with reaction enthalpies ranging between 0.2–0.6 eV at higher coverages of O x H y intermediates) on NiO and NiFeO x catalysts. In particular, Fe sites on the NiFeO x catalyst facilitate concerted mechanisms of O*/O 2 * formation and H 2 O desorption with a low enthalpy of 0.5 eV; O 2 desorption alone requires only 0.3 eV. In contrast, Versogen-IrO 2 results in stronger Ir–O bonds, where the enthalpies for bond breaking (Ir–OH 2 and Ir–O 2 ) are considerably higher (1.4 eV and 1.6 eV, respectively). Rotating disk electrode studies utilized commercially available NiO and IrO 2 and synthesized 7.5 wt % Fe in NiFeO x catalysts in combination with Versogen, a common AEM ionomer, and Nafion, an alternative binder. Electrochemical testing validated the impact of these mechanistic changes on ionomer-catalyst combinations, finding that Versogen particularly activates NiO and NiFeO x compared to IrO 2 . Following a 13.5 h hold at 1.8 V, mass activities and Tafel slopes improved to 34 ± 13 A g −1 and 79 ± 2 mV dec −1 (NiO) and 82 ± 4.9 A g −1 and 72 ± 2 mV dec −1 (NiFeO x ). In contrast, Versogen-IrO 2 only reached 17 ± 2.9 A g −1 and 81 ± 3 mV dec −1 . Optimization of the ionomer-catalyst can yield significant increases in performance from initial activity and after an electrochemical conditioning procedure: this enhancement to the mass activity resulted in a 200.9 ± 106.1% improvement for Versogen-NiFeO x and 1284.2 ± 260.5% for Versogen-NiO. In contrast, Nafion-NiFeO x and -NiO offered moderate improvements of 39.1 ± 30.5% and 120.9 ± 59.1%, respectively.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗