Compatibility of several iron-base, cobalt- base, and nickel-base alloys with refluxing potassium at 1800 deg F
Corrosion resistance tests for compatibility of several iron, cobalt, and nickel based alloys with refluxing potassium
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Corrosion resistance tests for compatibility of several iron, cobalt, and nickel based alloys with refluxing potassium
Nickel and nickel- base alloys are amenable to joining with many of the familiar joining processes. Some new joining processes also have been used successfully. In general, conventional joining procedures are used with only slight required modifications, depending on the particular alloy to be welded. However, some special precautions must be taken. Harmful materials must be removed from the joint or surrounding areas or they may damage the weld and the nearby heated parent metal. Some high-strength age hardenable alloys are prone to cracking in or near joint areas, unless the material is in the proper condition of heat treatment prior to joining operations. Foreign material and flux residues left from joining operations can cause trouble in subsequent service if not removed. Procedures for joining these alloys have been developed that eliminate or minimize the usual difficulties that have been experienced. When proper procedures are employed, joining of nickel and nickel- base alloys can be performed satisfactorily.
Nickel-base superalloy has a strength of 20,000 psi at 2,200 degrees F, approximately double the strength of the strongest available cast nickel-base alloys. It is not subject to the formation of embrittling phases upon long time exposure at intermediate temperatures.
Iron base and nickel base alloys susceptibilities to internal hydrogen and hydrogen environment embrittlements, studying crack initiation inside and at metal surface
A nickel base superalloy for use at temperatures of 2000 F (1095 C) to 2200 F (1205 C) was developed for use as stator vane material in advanced gas turbine engines. The alloy has a nominal composition in weight percent of 16 tungsten, 7 aluminum, 1 molybdenum, 2 columbium, 0.3 zirconium, 0.2 carbon and the balance nickel.
Nickel-based superalloys designed for use in gas turbine engines blades are difficult and expensive to properly machine without undue surface damage, due in part to their superior mechanical properties at high temperatures. Numerically controlled electrical discharge machining (EDM) has progressed to commonly be used as a machining process for initial sectioning, detailed roughing, and even some finishing operations. The objective of this study was to examine the effect of EDM on resulting surface conditions of superalloy 718 after slicing using typical rough, semi-finish, and finish condition sets with a typical wire EDM machine. Surface roughness, residual stress, and microstructures were compared for these conditions. The varied EDM conditions influenced surface roughness as intended. The residual stresses and surface roughness directly corresponding to the EDM steps were determined. While roughness decreased when progressing from rough to finish EDM conditions, tensile residual stresses unexpectedly increased. Brief assessments after EDM of two higher performance powder metallurgy disk superalloys ME209 and LSHR indicated this inverse relationship of roughness versus tensile residual stress was also present for these superalloys, where tensile residual stresses were significantly enhanced.
The joining of four types of nickel-base materials is described: (1) high-nickel, nonheat-treatable alloys, (2) solid-solution-hardening nickel-base alloys, (3) precipitation-hardening nickel-base alloys, and (4) dispersion-hardening nickel-base alloys. The high-nickel and solid-solution-hardening alloys are widely used in chemical containers and piping. These materials have excellent resistance to corrosion and oxidation, and retain useful strength at elevated temperatures. The precipitation-hardening alloys have good properties at elevated temperature. They are important in many aerospace applications. Dispersion-hardening nickel also is used for elevated-temperature service.
A nickel-based superalloy that resists embrittlement by hydrogen more strongly than does nickel alloy 718 has been developed. Nickel alloy 718 is the most widely used superalloy. It has excellent strength and resistance to corrosion as well as acceptably high ductility, and is recognized as the best alloy for many high-temperature applications. However, nickel alloy 718 is susceptible to embrittlement by hydrogen and to delayed failure and reduced tensile properties in gaseous hydrogen. The greater resistance of the present nickel-based superalloy to adverse effects of hydrogen makes this alloy a superior alternative to nickel alloy 718 for applications that involve production, transfer, and storage of hydrogen, thereby potentially contributing to the commercial viability of hydrogen as a clean-burning fuel. The table shows the composition of the present improved nickel-based superalloy in comparison with that of nickel alloy 718. This composition was chosen to obtain high resistance to embrittlement by hydrogen while maintaining high strength and exceptional resistance to oxidation and corrosion. The most novel property of this alloy is that it resists embrittlement by hydrogen while retaining tensile strength greater than 175 kpsi (greater than 1.2 GPa). This alloy exhibits a tensile elongation of more than 20 percent in hydrogen at a pressure of 5 kpsi (approximately equal to 34 MPa) without loss of ductility. This amount of elongation corresponds to 50 percent more ductility than that exhibited by nickel alloy 718 under the same test conditions.
Nickel- (Ni-) base superalloy single crystals represent the state-of-the-art for turbine engine airfoil applications because they offer the best balance of properties under the high operating temperatures required for efficient engine operation. Current trends in alloy design take advantage of improved creep rupture strength with the addition of higher levels of refractory elements. In particular, the addition of significantly higher levels of rhenium in third-generation superalloys is key for both microstructural stability and creep rupture strength. Although refractories provide strength benefits, alloys tend to be unstable when their refractory content is high because of topologically close-packed (TCP) phases. The formation of these phases in sufficient amount is detrimental to the performance of these alloys because of their brittle nature and because they deplete the Nirich matrix of potent solid-solution strengthening elements.
Properties of nickel-base alloys which do not require vacuum melting techniques and which provide high strength properties at elevated temperatures
Exposure of nickel-base alloys to overtemperature indicates that their creep resistance is sensitive to particle size and spacing in their microstructure
Four cast nickel-base superalloys were oxidized at 1000 and 1100 C for times up to 100 hr in static air and a Mach 1 gas stream. The oxidation resistance was judged by weight change, metal thickness loss, depletion-zone formation, and oxide formation and morphology. The alloys which formed mostly nickel aluminate (NiAl2O4) and aluminum oxide (Al2O3) (B-1900, VIA, and to a lesser extent 713C) were more oxidation resistant. Poorer oxidation resistance was associated with the appearance of chromium sesquioxide (Cr2O3) and chromite spinel (738X). Refractory metal content had little effect on oxidation resistance. Refractory metals appeared in the scale as tapiolite (NiM2O6, where M represents the refractory metal). Thermal cycling in static air appeared to supply sufficient data for the evaluation of oxidation resistance, especially for alloys which form oxides of low volatility. For alloys of higher chromium levels with high propensities toward forming a chromium-bearing scale of higher volatility, testing under conditions of high gas velocity is necessary to assess fully the behavior of the alloy.
Nickel was substituted for Co to produce 0, 5, and the standard 10% versions of MAR-M247, a cast nickel-base superalloy. The microstructures of the alloys were examined in as-cast, heat treated, aged, and stress-rupture tested conditions using a variety of metallographic techniques and differential thermal analysis. As cobalt concentration was reduced from 10 to 0 wt %, the gamma-prime weight fraction decreased from 59 to 41%; W and Ti concentrations in the gamma-prime phase increased from 5 to 8 and 2 to 3 at.%, respectively; the mean gamma-prime particle size increased from 0.6 to 0.8 micron; Cr and Al concentrations in the gamma matrix decreased from 17 to 13 and 15 to 12 at.%, respectively; and the weight fraction of carbides increased by approximately 1%.
Single crystal nickel-base superalloys used as turbine engine blades can have much higher creep and fatigue resistance than many polycrystalline superalloys due to the absence of weak grain boundaries as well as the ability to orient the blades in the primary loading direction on to the low elastic modulus [001] orientation, which significantly lowers the stresses imposed on the blades. However, grain defects can occur in these crystals, impairing these advantages. In the present study, fatigue tests of a single crystal superalloy uncovered unexpected defective grains in the test specimens, which initiated premature fatigue failures. The characteristics of these defective grains and the associated failures were evaluated and related to the observed fatigue lives.
Single crystal nickel-base superalloys used as turbine engine airfoils can have much higher creep and thermal fatigue resistance required for blades and vanes than polycrystalline superalloys due to the absence of weak grain boundaries, as well as the low elastic modulus in the [001] single crystal growth direction (Refs. 1 and 2). This has allowed an increase in the turbine rim inlet temperatures for improved performance and efficiency. However, these advantages in performance require constraints on acceptable levels of single crystal defects, such as macroscopic grain boundaries at low angles to the primary grain (i.e., low angle boundaries or LAB), higher angle boundaries, small new grains nucleated at the blade surface (a.k.a. freckles), larger new grains, and also the single crystal blades’ orientation, typically degrees off of the [001] direction and the orientation of a transverse [010] direction with respect to blade geometry. Therefore, single crystal turbine airfoils, which are frequently used with as-cast surfaces, are grain etched and inspected before and after heat treatments to ensure these aspects conform to acceptability limits.
The thermoelectric properties alloys of the nickel-base, iron-base, and cobalt-base groups containing from 1% to 25% 106 chromium were compared and correlated with the following material characteristics: atomic percent of the principle alloy constituent; ratio of concentration of two constituents; alloy physical property (electrical resistivity); alloy phase structure (percent precipitate or percent hardener content); alloy electronic structure (electron concentration). For solid-solution-type alloys the most consistent correlation was obtained with electron concentration, for precipitation-hardenable alloys of the nickel-base superalloy group, the thermoelectric potential correlated with hardener content in the alloy structure. For solid-solution-type alloys, no problems were found with thermoelectric stability to 1000; for precipitation-hardenable alloys, thermoelectric stability was dependent on phase stability. The effects of the compositional range of alloy constituents on temperature measurement uncertainty are discussed.
A directionally solidified multivariant eutectic gamma + beta nickel-base superalloy casting having improved high temperature strength and oxidation resistance properties is provided. This comprises a two phase eutectic structure containing, on a weight percent basis, 5.0-15.0 tungsten, 8.5-14.5 aluminum, 0.0-35.0 cobalt and the balance being nickel. Embedded within the gamma phase nickel-base matrix are aligned eutectic beta phase (primarily (NiCo)Al reinforcing lamellae.
The final results of an oxidation-reduction rig evaluation of aluminide coatings are presented, as applied to 1N-100 and B1900 nickel-base and X-10 and WI-52 cobalt-base alloys. Burner rigs were used which operated on JP-5 fuel and air, producing a gas velocity of 0.85 (2000 to 2500 ft/sec) at the specimen's leading edge. One-hour heating cycles were used with three minutes of air blast cooling. Results of testing at temperatures ranging from T sub max of 1850 to 2050 F indicate that coated B1900 has the longest oxidation life at all temperatures, followed by IN-100X-40WI-52, based on a weight change criterion. Coatings on nickel-base alloys provided more than twice the life of coating on cobalt-base alloys at comparable temperatures. The coatings with higher aluminum content and comparable thickness had longer lives. Silicon appeared to be a beneficial additive in the nickel-base alloy coatings for long term, low temperature life, but not for short term, high temperature performance. Chromium was identified in all coatings. Extrapolating the life results obtained to 1600 F, all the selected coatings on the four alloys would be protective for at least 10,000 hours.