Delineating the Impact of Transition‐Metal Crossover on Solid‐Electrolyte Interphase Formation with Ion Mass Spectrometry

Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.

Chemistry↗

Unraveling interphase-driven failure pathways in LiMn0.6Fe0.4PO4/graphite pouch cells

LiMnxFe1−xPO4 (LMFP) is a promising high-voltage, thermally stable, and earth-abundant cathode material, yet its practical application is limited by interphase instability and Mn dissolution. In this work, we systematically evaluate LiMn0.6Fe0.4PO4/graphite pouch cells using three electrolyte formulations including control carbonate electrolyte, control + 2 wt% vinylene carbonate (VC), and control + 2 wt% VC + 1 wt% 1,3,2-dioxathiolane 2,2-dioxide (DTD), to establish how electrolyte composition governs interphase chemistry and long-term degradation. Electrochemical testing shows that both additives are preferentially reduced prior to ethylene carbonate (EC) during cell formation, generating robust cathode-electrolyte interphase (CEI) and solid-electrolyte interphase (SEI) layers that suppress gas evolution and raise the first-cycle coulombic efficiency to 89.3%. Additionally, the dual-additive electrolyte delivers the most stable performance, retaining over 85% capacity after 600 cycles while minimizing impedance growth under long-term cycling at C/3 and 40 °C. Soft X-ray absorption spectroscopy confirms that VC + DTD effectively suppresses electrolyte oxidation at the cathode surface, and micro-X-ray fluorescence shows substantially reduced Mn dissolution and deposition on the graphite anode. Density functional theory simulations further provided insights into the structural and energetic influences of alkoxide species on the cathode surface, proposing a Mn2+ extraction mechanism. The combined experimental and computational findings establish a mechanistic link between electrolyte composition and interphase evolution, highlighting the effectiveness of electrolyte engineering for extending the operational lifetime of LMFP-based lithium-ion batteries.

Chak, Chanmonirath Michael↗

Mechanistic Understanding of Interphase-driven Aging in Silicon Anodes

Conventional solid electrolyte interphases (SEIs) strongly adhere to micro-silicon (µ-Si) and crack under volume changes, causing poor cycling performance. Nano-silicon improves cycling performance but remains costly with limited calendar life. Here potentiostatic ageing tests demonstrate that both calendar and cycle ageing are governed by SEI cracking and dissolution with different relative contributions. When the system is not dominated by SEI dissolution, the relative calendar life of Si anodes could correlates positively with their cycle life. LiF-rich SEI that enables long cycle life in µ-Si is therefore expected to enhance calendar life as well. Using this framework, we screened electrolytes, SEIs and electrodes and validated them with full-cell storage. LiF-rich SEI minimizes cracking and dissolution, enabling μ-Si to achieve excellent calendar life, whereas nano-silicon suffers from SEI dissolution and needs reduced electrolyte–electrode contact for better calendar life. This work clarifies calendar-ageing behaviour and accelerates electrolytes and SEI development for long-life Si anodes.

Johnson, Christopher S.↗

High-Voltage Sodium–Metal Batteries with Asymmetric Fluoroalkoxylated Organoborate Anion Chemistry

The high reactivity of sodium (Na) metal restricts its compatibility to ether-based electrolytes, while the poor oxidative stability of ethers precludes their coupling to high-voltage cathodes, fundamentally limiting the operating voltage and energy density of sodium–metal batteries (SMBs). We present here a coordination-asymmetry strategy to reconcile this thermodynamic mismatch by generating in situ an asymmetric fluoroalkoxylated organoborate anion, [FB(OCH(CF 3 ) 2 ) 3 ] − (BOF – ), via a Lewis acid–base adduct reaction in ether electrolyte. The asymmetric ligand architecture differentiates oxidative and fluorination pathways: oxidizable B–O moieties mediate controlled interfacial reconstruction, whereas the terminal B–F units supply fluorine for chemical passivation. This self-adaptive chemistry yields nanoscale, conformal, compositionally graded interphases: a boron-oxide/boron-oxycarbide-rich cathode-electrolyte interphase (CEI) that mitigates ether oxidation and a bilayered inorganic–organic solid–electrolyte interphase (SEI) that regulates Na deposition. The nanostructured interphases enable highly reversible Na plating/stripping with an average Coulombic efficiency (CE) of 99.98% and sustain stable 4.3 V operation of anode-free SMBs in oxidation-prone ether electrolytes. Furthermore, this work establishes asymmetric boron coordination as a molecular-level design principle for creating chemically adaptive interphases that overcome the redox asymmetry in energy-dense electrochemical systems.

Anions↗

Interlayer Design for Halide Electrolytes in All‐Solid‐State Lithium Metal Batteries

Abstract All‐solid‐state lithium‐metal batteries (ASSLMBs) are promising for transportation electrification due to their superior safety and high energy density. Lithium halide electrolytes provide excellent processing flexibility, high ionic conductivity, and anodic stability (>4.1 V), making them highly compatible with high‐voltage cathodes, surpassing sulfide electrolytes (<2.1 V). Nevertheless, halide electrolytes suffer from low cathodic stability and form an electronically conductive interphase with lithium, resulting in a critical current density (CCD) of nearly zero. Herein, Li 3 YbCl 6 electrolytes are synthesized that are kinetically stable with lithium by forming an electronic insulating solid electrolyte interphase. Guided by critical overpotential criteria, a PI 3 interlayer is designed that transforms into Li 6 PI 3 upon contact with lithium, substantially reducing the interfacial resistance of Li 3 YbCl 6 against lithium to 34 Ω and achieving a high critical overpotential of 114 mV. By substituting Yb with Lu, Li 3 LuCl 6 electrolytes with Li 6 PI 3 interlayers reach a CCD of 1.0 mA cm −2 at a capacity of 1.0 mAh cm −2 , comparable to sulfide electrolytes but with higher oxidation stability. Additionally, Li 6 PI 3 enables stable cycling of Li//Li cells with Li 3 LuCl 6 electrolytes at 0.5 mA cm −2 for 400 cycles and maintains 86.5% capacity in Li//LiCoO 2 cells after 220 cycles at 30 °C, paving the way for high‐performance ASSLMBs.

Chemistry↗

Speciation of Transition Metal Dissolution in Electrolyte from Common Cathode Materials

Significant capacity loss has been observed across extended cycling of lithium-ion batteries cycled to high potential. One of the sources of capacity fade is transition metal dissolution from the cathode active material, ion migration through the electrolyte, and deposition on the solid-electrolyte interphase on the anode. While much research has been conducted on the oxidation state of the transition metal in the cathode active material or deposited on the anode, there have been limited investigations of the oxidation state of the transition metal ions dissolved in the electrolyte. Here, in this work, X-ray absorption spectroscopy has been performed on electrolytes extracted from cells built with four different cathode active materials (LiMn 2 O 4 (LMO), LiNi 0.5 Mn 1.5 O 4 (LNMO), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and (x Li 2 MnO 3 *(1-x) LiNi a Mn b Co c O 2 , with a+b+c=1) (LMRNMC)) that were cycled at either high or standard potentials to determine the oxidation state of Mn and Ni in solution. Inductively coupled plasma-mass spectrometry has been performed on the anodes from these cells to determine the concentration of deposited transition metal ions. While transition metal ions were found dissolved in all electrolytes, the oxidation state(s) of Mn and Ni were determined to be dependent on the cathode material and independent of cycling potential.

25 ENERGY STORAGE↗

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE↗

An Organic Carboxylate Host for Stable Sodium Metal Batteries

Sodium metal batteries (SMBs) hold great promise for the development of high-energy, sustainable energy storage solutions, but their practical deployment is hampered by unstable solid electrolyte interphases, uncontrollable sodium dendrite growth, and low Coulombic efficiency (CE) during repeated Na plating/stripping cycles. To address these challenges, we introduce an organic interlayer, containing perylenetetracarboxylic dianhydride sodium salt (Na4PT), on the surface of Cu current collector. This interlayer forms a sodiophilic organic interphase that lowers the nucleation barriers for sodium deposition and guides the formation of the interphase through polar carbonyl/carboxylate sites and a π-conjugated organic framework. A dendrite-free sodium metal anode is achieved using Na4PT coated Cu current collector. Under capacity-limited Na plating/stripping, Na||Na4PT@Cu half-cells deliver reversible capacities of 500 and 1,000 mAh g−1 at 0.1 and 1 A g−1 for 500 cycles with average CE above 99%. Post-cycling scanning electron microscopy and X-ray photoelectron spectroscopy measurements confirm that Na4PT@Cu promotes compact and uniform Na deposits and supports the formation of a stable interphase with reduced parasitic decomposition, directly correlating interfacial chemistry/morphology with high plating/stripping reversibility. These results highlight organic carboxylate coating as a practical interface engineering strategy for dendrite-free SMBs.

Chen, Chengxiang [University of Miami]↗

Tailored Solvent Treatment for Optimized Production of Upcycled Anodes from End-Of-Life Li-Ion Batteries

Recycling processes for lithium-ion batteries typically overlook graphite because of its lower market value relative to that of transition-metal-containing cathode materials. However, graphite recovered from cycled lithium-ion batteries holds additional engineered value associated with the solid-electrolyte interphase (SEI). The SEI contributes critical electronic passivation of the graphite surface but becomes highly resistive with extended cycling, yielding poor cell performance. In this work, we apply tailored solvent treatment to end-of-life (EOL) graphite anodes to selectively remove adverse SEI components while retaining beneficially passivating species. We evaluate a series of polar protic solvents to achieve targeted removal of SEI components and control selectivity through rational variation in solvent properties. The physiochemical properties of treatment solvents correlate with both the retained SEI composition and the corresponding electrochemical performance of solvent-treated “upcycled” graphite anodes. Within the initial set of solvents evaluated, top-performing candidates show capacity and Coulombic efficiency nearly equivalent to those of an analogous pristine anode, as well as promising electrochemical performance enhancement with regard to irreversible capacity-loss metrics. This study establishes critical design principles for an optimized anode upcycling method that enhances the value of recycled graphite by retaining and upgrading the SEI.

25 ENERGY STORAGE↗

Direct regeneration of degraded LiFePO4 cathodes via a separator-enabled prelithiation strategy

A persistent challenge in lithium-ion batteries is the loss of active lithium due to the solid electrolyte interphase (SEI) formation and associated side reactions. While prelithiation employing lithium replenishment separator (LRS) has been proven effective in compensating for lithium loss, previous studies have largely been accompanied by gas evolution or solid residue formation during the prelithiation process. To surmount this challenge, we present a LRS based on 4-fluoro-1,2-dihydroxybenzene lithium salt (LiDF), capable of mitigating lithium loss while producing decomposition products that integrate directly into the electrolyte as functional additives which can assist with the stability of the SEI, free from gas or solid formation, thus establishing a sustainable and environmentally benign strategy for lithium compensation. Incorporation of the LRS enables the pristine LiFePO4||graphite (Gr) full cell to achieve 10.8% higher capacity than the cell with a polypropylene separator (PPS) after 200 cycles at 0.5C. Remarkably, the degraded LiFePO4 (D-LFP)||Gr full cell with the LRS exhibits a 135.8% capacity improvement over the PPS-based cell after 500 cycles. These findings establish the LRS as a powerful approach for both boosting high-performance lithium-ion batteries and recovering the capacity of degraded batteries.

Tao, Fujun↗

Unravelling fast-charging degradation in NMC/Gr pouch cells: Lithium plating and SEI properties

As fast-charging technology expands across the electric vehicle and emerging energy-storage applications, understanding its impact on battery performance and longevity is critical. In this study, 1.8 Ah LiNi 0.6 Mn 0.2 Co 0.2 O 2 /graphite pouch cells were charged at various charging rates (0.5C, 2C, 4C, and 6C) to investigate the degradation mechanisms. Our results showed that well-designed NMC/Gr pouch cells could reach over 1000 cycles with a 2C charging rate, while only reaching around 500 cycles with 4C and 6C charging rates. Fast-charging effects on NMC and graphite electrodes were obtained through a series of post-mortem characterizations, including electrochemical impedance spectroscopy (EIS), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS). Although higher charging rates cause pulverization of NMC secondary particles, the dominant degradation mechanism driving the fading of fast-charging-related performance lies in the graphite anode, where lithium plating and LiF-rich solid electrolyte interphase (SEI) formation result in Li inventory loss and impedance growth. The postmortem results suggest that the formation of a LiF-rich SEI, which exacerbates anode impedance and some irreversible Li + ion loss, is likely driven by the substantial decomposition of PF 6 − during fast charging, an effect often overlooked in smaller laboratory-scale studies.

Luo, Mei [Argonne National Laboratory (ANL), Argon↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Self-Healing Lithium Dendrites through Spontaneous Passivating Layer Formation for Stable Solid-State Lithium–Metal Batteries

All-solid-state lithium–metal batteries have attracted significant attention, owing to their high energy density and superior safety. However, lithium–metal penetration through the solid electrolyte, leading to short-circuiting, remains a critical failure mode that demands comprehensive mitigation strategies. Most existing strategies are effective only prior to the initiation of lithium-dendrite formation and fail once dendrites begin to propagate through the electrolyte. In this study, we propose a self-healing mechanism in which the penetrated lithium reacts with a self-healing agent to form a passivating layer along the particle boundaries. Lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) was incorporated into a Li 6 PS 5 Cl solid electrolyte as the self-healing agent to suppress lithium-dendrite propagation even after dendrite formation initiated under high current densities. The self-healing induced by LiTFSI was verified through comprehensive experimental analyses and was further demonstrated in a full-cell configuration. Moreover, LiTFSI incorporation plays an important role in increasing the critical current density by reducing the overall electronic conductivity of the solid electrolyte and facilitating the formation of a robust LiF-containing solid-electrolyte interphase.

25 ENERGY STORAGE↗

Experimental considerations and applications for time-resolved impedance on silicon-anode battery systems

Dynamic electrochemical impedance spectroscopy (dEIS) utilizes a superimposed multi-sinusoidal waveform and enables temporally resolved investigations on various electrochemical processes; however, the signal-to-noise ratio must be maximized while retaining linearity and stationarity within the system. In the present work, we probe the impact of the waveform’s total amplitude as well as the waveform and phase profiles. The equal amplitude multi-sinusoidal waveform with 35 mV total amplitude (<1 mV per frequency) and random phase profile exhibits the lowest impedance noise. This input signal is sufficient in avoiding the high frequency signal attenuation from the potentiostat’s low-pass filter. Additionally, we demonstrate the optimized dEIS waveform’s utility in investigating surface passivation within thin-film and composite silicon (Si) anodes. Within a two-electrode Si-lithium metal coin cell, the charge transfer resistance (RCT) associated with alloying kinetics dominates the overall impedance. RCT increases with state of charge indicating a kinetic bottleneck at higher lithiation states. To explore this further, we utilize a three-electrode Si-LiNi0.8Mn0.1Co0.1O2 pouch cell to deconvolute the Si impedance contributions. The evolution of the solid electrolyte interphase (SEI) and charge transfer resistances correlate to specific Li–Si alloy phases. We attribute this to the influence of Si particle volume expansion on SEI instabilities and a kinetic bottleneck at higher lithiation states.

Lam, Steven [ORNL]↗

Electrode-omics reveals epochs in silicon anode evolution underpinning electrochemomechanical resilience

Here, we advance electrode-omics to identify evolutionary bursts by which ethereal locally superconcentrated electrolytes (LSCEs) mitigate silicon anode degradation through its epochs of electrochemical and chemical reactions. Anode composites form initially at high potential from ethereal solvent and anion [bis(fluorosulfonyl)imide (FSI − )] redox. A first evolutionary burst at lower potential enriches composites with lithium alkoxides (LiO–R) and lithium oxide (Li 2 O) and depletes sulfur oxides (SO x ) species. As the cells are cycled, a second evolutionary burst takes place, where previously extinct SO x species reemerge concurrently with a loss of LiO–R and Li 2 O. This identifies reactions rooted in “SuFEx” chemistry, where oxoanionic LiO–R and Li 2 O species, electrochemically generated in the solid-electrolyte interphase, chemically react with FSI − in the electrolyte to form emergent species. This sequence of evolutionary bursts produces a mechanically resilient composite that reduces silicon anode cracking over hundreds of cycles, leading to overpotential increase of only ~0.01 volts after 200 cycles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Reductively Stable Electrolyte Realizes Deep Cycling Behavior in Anode‐free Sodium Batteries

For anode‐free sodium batteries to achieve practical consideration, highly reversible chemistries require exceptional ≥99.95% coulombic efficiencies that maintain over prolonged cycling periods. To do so, consumption of this severely limited sodium inventory must be restricted while metal nucleation processes that comprise the in situ formed metal anode are improved. Herein, we describe a fluorine‐free carborane electrolyte that satisfies these criteria by emphasizing reductive stability and weakly coordinating anion behavior as design principles. We find this approach promotes the development of a thin, robust SEI chemistry rich in both organic speciation and boron. The electrolyte described herein exhibits ideal metal nucleation behavior on one‐micron thin carbonaceous current collector surfaces and achieves a metal deposition/stripping efficiency near parity for 400 cycles. This novel anode chemistry is introduced to anode‐free full cell configurations where 87% of the initial discharge capacity is retained after 1000 cycles at 2.0 C. In conclusion, post‐test characterization of deep‐cycled anode‐free cells reveals suppressed capacity fade in these systems is attributed to the chemical stability of the carborane anion.

anode-free↗

Ionic Interdiffusion at Cathode|Solid-Electrolyte Interface: A Machine Learning–Assisted Multiscale Investigation and Mitigation Strategies

Future lithium batteries are expected to use solid electrolytes to achieve higher energy density and fast charge capabilities. However, most solid electrolytes are thermodynamically unstable against layered oxide cathodes. In this study, the stability of LiCoO2 (LCO) cathode with Li10GeP2S12 (LGPS) solid electrolyte is investigated using ab initio molecular dynamics (AIMD) and machine learning molecular dynamics (MLMD). The propensity of ionic interdiffusion, formation of a passivating interphase layer, and corresponding decay in cell performance is addressed using a continuum model. Large-scale MLMD simulations confirm that the LCO|LGPS interface permits interdiffusion of cobalt (Co) and other ionic species, leading to the formation and growth of a resistive interphase and to dramatic capacity fade even in the first cycle. We examine the literature evidence that incorporating a thin layer of LiNb0.5Ta0.5O3 (LNTO) between LCO and LGPS prevents the interdiffusion of ions. Atomistic simulations suggest that substituting lithium (Li) in LNTO with Co is thermodynamically unfavorable, thereby inhibiting ionic interdiffusion. The stable Nb5+/Ta5+ states form a rigid metal-oxide framework, which consequently also prevents the substitution of niobium (Nb) or tantalum (Ta). However, continuum-level analysis suggests that the higher mechanical stiffness of LNTO can lead to interfacial delamination between the LCO and LNTO. This phenomenon reduces the effectiveness of the protective layer. This paper, therefore, highlights the need to develop novel interlayers that balance low ionic interdiffusion with low mechanical stiffness.

Ncube, Musawenkosi K.↗