Search NASA⌕ Search

SEARCH · Search NASA

Results for “solidification cracking susceptibility”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Numerical Study of Solidification Crack Susceptibility in Novel Refractory Alloy Systems

Calculation of Phase Diagrams (CALPHAD) -based solidification computa­tions, such as Scheil or equilibrium computations, have been utilized to propose crack solidification susceptibility indices (CSSIs) of cracking. These CSSIs have been proposed in order to predict the cracking susceptibility of an alloy in the solidification range, as a function of its solidification frac­tion and as dependent upon its wt.% elemental composition through the CALPHAD computation & via comparative methods between one composition & the next. Recently Kou at al. have proposed a novel CSSI where the gradient of the e.x. Scheil solidification curve is obtained in the critical solidification cracking region of greater than 0.95 fraction of solid. Therefore, a direct Temperature dependent metric is now available for the prediction, and presumably the control, of solidification cracking. In this TM, the researchers apply this Kou gradient method to refractory alloys for the first time & discuss justification for the approach via Spearman rank correlation with Varestraint cracking test data as well as by comparisons with Thermocalc based vulnerability time CSSI calculations. A Python Pycalphad module example of the approach is provided & can be utilized as an open-source resource that utilizes also open-source available thermodynamical databases, making the CSSI quantitative aspect of ICME more available and freely available to practitioners.

ICME integrated computational materials engineerin↗

Open-source Numerical Modeling of Solidification Cracking Susceptibility: Application to Refractory Alloy Systems

Introduction. Alloys such as aluminum, nickel-base, and austenitic stainless steels are susceptible to solidification cracking during welding and 3D printing. Compositional optimization is one method used to effectively mitigate solidification cracking of those alloy systems. With the surge in hypersonic and in-space propulsion activities, refractory metals (Nb, Mo, Ta, W, and Re) and their alloy derivatives are increasing in importance due to their extreme high melting point and retention of high-temperature strength; however, their chemistry was most typically optimized to promote ductility during mechanical operations such as drawing and forming. Welding of such alloys has been a challenge due to a number of issues including solidification cracking, atmospheric contamination (O, C, and N), as well as a shift in ductile-to-brittle transition to higher temperature following grain growth induced by welding. Compositional optimization of refractory alloys for solidification cracking resistance in particular is desirable as their usage increases with the advent of advanced manufacturing methods such as 3D printing. This work evaluates the effect of compositional variation in refractory metal systems on the solidification cracking susceptibility with the goals of optimizing existing alloys and joining process techniques, and formulating new alloys with increased solidification cracking resistance. Experimental Procedures. A python code was developed in a Jupyter notebook environment (Michael and Sowards, 2023) to facilitate the calculation of crack susceptibility index proposed by Kou (2015). Composition is entered as a single point, or as a 1-D or 2-D array. The notebook calls pycalphad (Otis and Liu, 2017 and Bocklund et al, 2020) to calculate the evolution of fraction solid as a function of temperature (under either Scheil or equilibrium assumptions) and then evaluates steepness of the fraction solid curve near the terminal stage of solidification to predict solidification cracking resistance. Open source thermodynamic databases available at online repositories are used (van de Walle). The process is setup in an automated fashion to generate plots that show variation in solidification cracking susceptibility according to composition on 1-D line plots or 2-D contour plots. The Jupyter notebook and crack susceptibility algorithm was also integrated with a widely used commercial CALPHAD code for validation and alloy exploration. Results and Discussion. The crack susceptibility model was first validated against a series of refractory alloy compositions evaluated in past work which utilized a specialized Varestraint test built inside a vacuum chamber environment (Lessman and Gold, 1971). The alloys tested in the Varestraint apparatus included T-111 (Ta-8W-2Hf), ASTAR-811C (Ta-8W-1Re-0.7Hf-0.025C), FS-85 (Nb-27Ta-10W-1Zr), T-222 (Ta-9.6W-2.4Hf-0.01C), Ta-10W, B-66 (Nb-5Mo-5V-1Zr), and SCb-291 (Nb-10W-10Ta). The initial test of the model showed a strong correlation with empirical Varestraint data, i.e., a Spearman rank correlation between model predictions and hot cracking measurements was observed to be greater than 0.8. Following the validation, a set of refractory metal binary mixtures was investigated to evaluate sensitivity of Nb, Mo, W, and Ta to C, N, and O content. A series of plots were produced that suggest ppmw ranges of C, N, and O where solidification cracking increases significantly and reaches a maximum. Also comparative ranking of each primary refractory metal to each interstitial was produced. For example C produces greater cracking response in Mo whereas O produces greater cracking response in Ta and Nb. Such compositional values have utility in setting limits on pickup of these interstitial elements during welding and printing rather than using a one-size-fits-all approach. Furthermore, the results have use in determining additive powder recycling requirements, which is especially pertinent for refractory metal powders due to their high cost compared to conventional alloys. Another application created thousands of hypothetical alloys within the nominal specified composition range of two widely used refractory alloys C103 (Nb-10Hf-1Ti) and TZM (Mo-0.5Ti-0.1Zr). The cracking index was calculated for the alloys and results were fed into machine learning regression techniques including Multiple Linear Regression, Ridge Regression, and Lasso Regression to determine relative potency each alloying element had on computed solidification cracking index. A series of linear equations were produced that relate composition of C103 and TZM to solidification cracking index. The crack susceptibility of C103 for example is described by an equation of the form: cracking index ~ O + 0.667*C + 0.635*N + 0.00037*Ta – 0.0008*Hf (in wt.%) From that equation, it is clear that O has strong propensity to induce solidification cracking. Interestingly, Hf is shown to reduce calculated cracking response. Finally, realizing the potential of this method to discover new refractory alloy formulations across the period table that have low solidification cracking sensitivity, the code was applied to new untested alloy systems including W-Zr-C, W-Ta-C, and others. Conclusions. In summary, an open source numerical method has been developed using Python code to calculate Kou’s crack susceptibility index. The method was applied to refractory metals which are inherently difficult to study from a weldability testing standpoint since inert shielding gas is not sufficient and welding is typically done in vacuum, especially in light of findings presented here where oxygen has profound influence on solidification cracking. This work revealed the effect of compositional variations on a series of refractory metals and showed the framework defined here will be useful in 1) the development of new alloys that have improved weldability and 3D printability, 2) placing compositional limits on existing alloys, and 3) ensuring adequate controls of manufacturing processes such as 3D printing where powder reuse is critical. Keywords. pycalphad; Python; refractory metals; solidification cracking. References. B. Bocklund et. al. (2020) http://doi.org/10.5281/zenodo.3630657. S. Kou. (2015) https://doi.org/10.1016/j.actamat.2015.01.034. G.G. Lessmann and R.E. Gold. Welding Journal, issue 1, pp. 1-s – 8-s (1971). F.N. Michael and J.W. Sowards. NASA/TM-20230002218 (2023). R. Otis and Z.-K. Liu. (2017) http://doi.org/10.5334/jors.140. A. Van de Wallle et. al. (2018) https://doi.org/10.1016/j.calphad.2018.04.003.

pycalphad↗

Determination of Location-Specific Solidification Cracking Susceptibility for a Mixed Dissimilar Alloy Processed by Wire-Arc Additive Manufacturing

Solidification cracking is a major obstacle when joining dissimilar alloys using additive manufacturing. In this work, location-specific solidification cracking susceptibility has been investigated using an integrated computational materials engineering (ICME) approach for a graded alloy formed by mixing P91 steel and Inconel 740H superalloy. An alloy mixture of 26 wt.% P91 and 74 wt.% Inconel 740H, with high configurational and total entropy, was fabricated using wire arc additive manufacturing. Microstructure characterization revealed intergranular solidification cracks in the FCC matrix, which increased in length along with the enrichment of Nb (~27 to 56 wt.%) and Cu (~87 wt.%) in the middle and top regions. DICTRA simulations to model location-specific solidification cracking susceptibility showed that the top region with the highest cooling rate (270 K/s) has the highest solidification cracking susceptibility in comparison with the middle and bottom regions. This is in good agreement with the experimentally observed varying crack length. From Scheil simulations, it was deduced that enrichment of Nb and Cu affected the solidification range as high as ~77%, in comparison with the matrix composition. The overall solidification cracking susceptibility and freezing range was highest for the 26 wt.% P91 alloy amongst the mixed compositions between P91 steel and 740H superalloy, proving that solidification characteristics play a major role in alloy design for additive manufacturing.

20 FOSSIL-FUELED POWER PLANTS↗

An Open-Source Numerical Model for Mitigating Refractory Alloy Hot Cracking Susceptibility

Refractory alloys are susceptible to solidification cracking during welding and 3D printing. Composition control is an effective method of controlling solidification cracking. This work evaluates the effect of compositional variation in refractory metal systems on a computed solidification cracking susceptibility. A numerical model has been developed using Python code and open-source CALPHAD software to calculate Kou’s crack susceptibility index. The model is validated against past weldability studies performed on several refractory alloy systems. The approach is extended towards the development of new alloys with improved 3D printability and weldability and is shown to have utility in defining compositional limits for existing alloys and feedstocks. Furthermore, the model will aid in determining process controls for powder reuse and recycling.

pycalphad↗

A high strength Al-2Ni-0.5Zr conductor alloy fabricated via laser powder bed fusion

There is a current need for new aluminum alloy design strategies to target applications requiring high strength and conductivity with reductions in mass. A new lightweight Al-2Ni-0.5Zr (wt. %) conductor alloy was fabricated using laser powder bed fusion. A design of experiments probed the alloy's solidification cracking susceptibility. It was observed that solidification cracking was generally reduced with fast scan speeds, above 1500 mm/s, and smaller hatch spacings. The different cooling rates throughout the melt pool produced a heterogeneous distribution of cellular and equiaxed Al 3 Ni precipitates in the as-printed alloy. Additionally, the rapid solidification characteristic of laser powder bed fusion created a super-saturated Zr solid solution. An aging heat treatment at 375 °C for 24 h imparted strengthening through the precipitation of L1 2 -Al 3 Zr nanoprecipitates, which counteracted the softening caused by the fragmentation and coarsening of Al 3 Ni precipitates. The yield strength increased from 138 MPa in the as-printed condition to 168 MPa after aging, while the ductility remained constant at ∼21%. The aging treatment simultaneously increased the electrical conductivity from 40.8% IACS (International Annealed Copper Standard) to 53.5% IACS. Modeling of the strengthening mechanisms and electrical conductivity contributions rationalized the simultaneous increase in strength and conductivity upon aging. Furthermore, the strengthening efficacy of the Al 3 Ni and L1 2 -Al 3 Zr precipitates, combined with the low Ni and Zr solubility in the FCC Al matrix, facilitated both high strength and electrical conductivity. Overall, the combination of strength and electrical conductivity positions this alloy as a suitable choice for additively manufactured lightweight conductors.

Additive manufacturing↗

The Influence of Nominal Composition on the Microstructure, Tensile Properties, and Weldability of Cast Monel Alloys

Cast Monel alloys are used in many industrial applications that require a combination of good mechanical properties and excellent resistance to corrosion. Despite relative widespread use, there has been limited prior research investigating the fundamental composition–structure–property relationships. Here in this work, microstructural characterization, thermal analysis, electron probe microanalysis, tensile testing, and Varestraint testing were used to assess the effects of variations in nominal composition on the solidification path, microstructure, mechanical properties, and solidification cracking susceptibility of cast Monel alloys. It was found that Si segregation caused the formation of silicides at the end of solidification in grades containing at least 3 wt pct Si. While increases to Si content led to significant improvements in strengthening due to the precipitation of β 1 -Ni 3 Si, the silicide eutectics acted as crack nucleation sites during tensile loading which severely reduced ductility. The solidification cracking susceptibility of low-Si Monel alloys was found to be relatively low. However, increases to Si concentration and the onset of associated eutectic reactions increased the solidification temperature range and drastically reduced cracking resistance. Increases in the Cu and Mn concentrations were found to reduce the solubility limit of Si in austenite which promoted additional eutectic formation and exacerbated the reductions in ductility and/or weldability.

36 MATERIALS SCIENCE↗

Design of crack-free laser additive manufactured Inconel 939 alloy driven by computational thermodynamics method

Abstract This paper examined the effect of Si addition on the cracking resistance of Inconel 939 alloy after laser additive manufacturing (AM) process. With the help of CALculation of PHAse Diagrams (CALPHAD) software Thermo-Calc, the amounts of specific elements (C, B, and Zr) in liquid phase during solidification, cracking susceptibility coefficients (CSC) and cracking criterion based on $$\left| {{\text{d}}T/{\text{d}}f_{{\text{s}}}^{1/2} } \right|$$ d T / d f s 1 / 2 values ( T : solidification temperature, f s : mass fraction of solid during solidification) were evaluated as the indicators for composition optimization. It was found that CSC together with $$\left| {{\text{d}}T/{\text{d}}f_{{\text{s}}}^{1/2} } \right|$$ d T / d f s 1 / 2 values provided a better prediction for cracking resistance. Graphical abstract

Zeng, Congyuan (ORCID:0000000214764277)↗

LPBF Processability of NiTiHf Alloys: Systematic Modeling and Single-Track Studies

Research into the processability of NiTiHf high-temperature shape memory alloys (HTSMAs) via laser powder bed fusion (LPBF) is limited; nevertheless, these alloys show promise for applications in extreme environments. This study aims to address this limitation by investigating the printability of four NiTiHf alloys with varying Hf content (1, 2, 15, and 20 at. %) to assess their suitability for LPBF applications. Solidification cracking is one of the main limiting factors in LPBF processes, which occurs during the final stage of solidification. To investigate the effect of alloy composition on printability, this study focuses on this defect via a combination of computational modeling and experimental validation. To this end, solidification cracking susceptibility is calculated as Kou’s index and Scheil–Gulliver model, implemented in Thermo-Calc/2022a software. An innovative powder-free experimental method through laser remelting was conducted on bare NiTiHf ingots to validate the parameter impacts of the LPBF process. The result is the processability window with no cracking likelihood under diverse LPBF conditions, including laser power and scan speed. This comprehensive investigation enhances our understanding of the processability challenges and opportunities for NiTiHf HTSMAs in advanced engineering applications.

36 MATERIALS SCIENCE↗

Al-Cu-Zn-Mg Alloy for Additive Manufacturing by Electron Beam Deposition

The application of fusion-based additive manufacturing (AM) to aircraft structural components is limited by the lack of high-strength aluminum alloys optimized for AM processing. High strength aluminum alloys (such as 7050-T7451) are difficult to process by AM because of their solidification cracking susceptibility and loss of volatile alloying elements such as Zn and Mg. The performance of a proprietary Al-Cu-Zn-Mg alloy wire feedstock was evaluated for AM utilizing electron beam deposition. Deposit microstructure, composition, occurrence of porosity and cracking, and post-heat treatment tensile and fracture toughness were correlated with deposition parameters. Post-heat treatment strength, ductility, and fracture toughness were lower than typical values for wrought 7050-T7451, related to significant losses of Zn and Mg and to porosity. Recommendations are offered for modifications to wire feedstock composition and adjustments to deposition conditions and heat treatment to enable AM of electron beam deposited material that has strength comparable to 7050-T7451 wrought products.

Al-Cu-Zn-Mg alloy, electron beam deposition, mecha↗

Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High $\gamma ^{\prime }$ CoNi-Base Superalloy

Here, the cracking behavior of a high γ' volume fraction CoNi-base superalloy fabricated via laser powder bed fusion (LPBF) is studied in relation to the content of carbon and boron. Severe cracking occurred with the increase in boron content from 0.08 to 0.16 at. pct (0.015 to 0.029 wt pct), while compositions with 0.1 to 0.36 at. pct C (0.02 to 0.076 wt pct) and 0.08 at. pct B exhibited minimal cracking. Assessment of cracks in the high-boron composition shows a variation in crack density with printing parameters, and alignment of the cracks with the build direction. Scanning electron microscopy (SEM) of the crack surfaces shows evidence of a solidification cracking mode. Differential thermal analysis (DTA) reveals a decreased incipient melting temperature for the high-boron composition, and atom probe tomography (APT) is used to measure the enrichment at grain boundaries, revealing distinct boron segregation. Scheil-Gulliver solidification simulations for the different C and B levels are consistent with the incipient melting behavior observed with DTA. Evaluation of the solidification cracking susceptibility from the simulations allow for comparison of the CoNi alloy behavior to Ni-base superalloys studied for LPBF fabrication and displays how such metrics may aid in the design of new precipitation-strengthened superalloys for additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Interim Report on FY22 ORNL A709 Welding Research and Testing of Production Welds in Support of Developing ASME A709 Code Case Data Package

As part of the Alloy 709 ASME Code Case development effort under the Advanced Reactor Technologies (ART) Program, this work covers the development of the technical basis for weld fabrication and weld qualification of Alloy 709. This report summarizes the Alloy 709 welding research conducted at Oak Ridge National Laboratory (ORNL) in FY 2022. Two new production welds were fabricated on two commercial heats of Alloy 709 of different phosphorus (P) levels using Alloy 709 filler metal with P content less than 20 wppm with gas tungsten arc welding (GTAW). Both production welds successfully passed ASME Section IX weld qualification tests, and this concludes the Alloy 709 welding procedure development to scale up to 2-in thick plates. In FY 2022, we also demonstrated the success in welding of high P commercial Alloy 709 plates with weld wires having higher P content at 30 wppm. A test weld fabricated with the 30 wppm weld wire on the first commercial heat (140 wppm P) passed all weld qualification tests without issues. Additionally, experiment setup and testing procedure of the circular patch weldability test has been developed, for evaluating the P effect in weld wire on solidification cracking susceptibility of Alloy 709 weld, with the preliminary results summarized in this report. Research on further relaxing the P level restriction beyond 30 wppm are planned in FY 2023. The preliminary cross-weld creep tests results continue to show little or no creep strength reduction relative to the base metal.

36 MATERIALS SCIENCE↗

Solidification cracking of refractory alloys: a computational and machine learning study to investigate composition-dependence for improved weldability and additive manufacturability

Large-batch numerical, CALculation of PHAse Diagrams (CALPHAD)-based solidification cracking calculations are performed and then analyzed with machine learning methods to generate models that relate chemistry of refractory alloys to cracking susceptibility. Kou’s solidification cracking index is used to study the refractory alloys including O, N, C binary mixtures with Mo, Ta, Nb, and W, the molybdenum-based TZM, Niobium-based C103, and Tantalum-based T111 and Ta-10 W, as well as hypothetical refractory ternary alloys. Findings strongly validate Kou’s Crack Susceptibility Index (CSI) against Varestraint test data for Nb- and Ta-based alloys, establishing CSI thresholds where refractory alloys with CSI < 15,000 K are likely weldable, CSI > 15,000 K are prone to cracking, and CSI > 25,000 K are likely unweldable (or unprintable). Furthermore, interstitial elements C, N, and O significantly increase crack susceptibility, with some existing material specifications coinciding with peak cracking susceptibility concentrations. Finally, machine learning-derived elemental potency factors enable rapid prediction of CSI from alloy chemistry for C103, TZM, Ta-10 W, and T-111 alloys. These results provide practical guidance for feedstock selection, powder reuse limits, and alloy specification amendments for welding and additive manufacturing applications.

36 MATERIALS SCIENCE↗

Welding of Crack Sensitive Aluminum Alloys for Liquid Rocket Propulsion Applications

In this welding test campaign, electron beam welding (EBW) and manual gas tungsten arc welding (GTAW) processes were utilized to join an additively manufactured aluminum alloy nozzle to a wrought aluminum flange. Both aluminum alloys were 6061, which in their conventional form are susceptible to solidification cracking issues. The AM nozzle utilized a novel high-performance modified version of 6061 which exhibits crack resistant properties during the AM process and during welding. When manually conducting GTAWs a filler wire with the same modified version of 6061 was utilized to weld different combinations of 6061 coupons (either modified or unmodified). Due to the grain refinement technology in the modified 6061, either as filler material or base material, there was complete elimination of weld solidification cracking. During EBW development a combination of wrought 6061 with a modified and additively manufactured 6061 was investigated. The EBWs developed exhibited no crack like defects. Each weld development program utilized non-destructive evaluation, metallography, and mechanical testing to determine the final weld acceptance. Mechanical testing involved hardness evaluation and tension testing on welded coupons. Both welding techniques were successfully developed and exhibited adequate properties for the final test articles and met all requirements of the development campaign. These welds were ultimately developed to be utilized on a set of all-aluminum liquid rocket nozzles to demonstrate additively manufactured aluminum alloys for propulsion applications. These aluminum nozzles were tested at NASA Marshall Space Flight Center’s hot fire test facility and subsequently underwent a test campaign involving a variety of chamber pressures and liquid propellant combinations. Following the hot fire test campaign each weldment was investigated for post operation performance and any defects that may have evolved during testing.

Welding↗

Hot Cracking Behavior and Beam-Induced Grain Refinement in Electron Beam Freeform Fabricated Al 7075

Electron beam freeform fabrication (EBF 3 ) is a high deposition rate, wire-based directed energy deposition (DED) additive manufacturing (AM) process used to print metallic parts in a vacuum environment. While high specific strength 7xxx-series Al alloys are of interest in the aerospace and automotive industries, these alloys suffer from hot cracking issues during fusion welding and AM. In this work, linear deposits of Al 7075 were fabricated with EBF 3 to study the effects of baseplate thickness, preheat temperature, and beam focus on hot cracking behavior. Solidification cracks were observed in the first deposition layer, and by the third layer coalesced into large “macrocracks” running vertically through the build height. Fine, intergranular liquation “microcracks” appeared between macrocracks below the root of the final deposit layer fusion zone. Increasing the substrate preheat temperature from 165°C to 320°C deepened the partially melted zone and resulted in a more than twofold increase in the liquation microcrack density. Analysis of Scheil solidification diagrams revealed that fugitive losses of Zn and Mg during deposition increased the susceptibility to solidification cracking and promoted substrate liquation cracking. Focused electron beam (EB) conditions combined with a high aspect ratio elliptical raster pattern resulted in bands of refined, equiaxed grains. The refined microstructure suppressed solidification macrocracking and caused a nearly fivefold reduction in liquation crack density, demonstrating that beam-induced grain refinement may be a promising low-cost method for reducing hot cracking during AM.

aluminum↗

Additive manufacturing of an ultrastrong, deformable Al alloy with nanoscale intermetallics

Abstract Light-weight, high-strength, aluminum (Al) alloys have widespread industrial applications. However, most commercially available high-strength Al alloys, like AA 7075, are not suitable for additive manufacturing due to their high susceptibility to solidification cracking. In this work, a custom Al alloy Al 92 Ti 2 Fe 2 Co 2 Ni 2 is fabricated by selective laser melting. Heterogeneous nanoscale medium-entropy intermetallic lamella form in the as-printed Al alloy. Macroscale compression tests reveal a combination of high strength, over 700 MPa, and prominent plastic deformability. Micropillar compression tests display significant back stress in all regions, and certain regions have flow stresses exceeding 900 MPa. Post-deformation analyses reveal that, in addition to abundant dislocation activities in Al matrix, complex dislocation structures and stacking faults form in monoclinic Al 9 Co 2 type brittle intermetallics. This study shows that proper introduction of heterogeneous microstructures and nanoscale medium entropy intermetallics offer an alternative solution to the design of ultrastrong, deformable Al alloys via additive manufacturing.

Science & Technology - Other Topics↗

Metallic Powder Core Tubular Wire (PCTW) Development for Additive Manufacturing

NASA Langley Research Center (LaRC) in Hampton, VA, and the Center for Welding, Joining, and Coating Research (CWJCR) in the Department of Metallurgical and Materials Engineering at the Colorado School of Mines (CSM) in Golden, CO, have collaborated for nearly fifteen years to develop metallic powder core tubular wire (PCTW) feedstock for additive manufacturing (AM) using electron beam deposition. The motivation for this development was to offset dealloying observed during deposition of titanium and aluminum alloy solid wire feedstock in the LaRC electron beam freeform fabrication (EBF3) system and to explore novel alloy compositions by tailoring the powder fill. EBF3 is a fusion-based AM process that is performed under vacuum and is consequently prone to vaporization loss of low vapor pressure alloying elements. Research spanning four graduate student research projects succeeded in developing the basic methodology to fabricate PCTW, the mass balance equations used to define the powder fill, microstructure control through particulate inoculation, and the feasibility of producing metal matrix composite materials. Metallic PCTW is comprised of a thin foil sheath wrapped around a powder blend. Fabrication of PCTW at CSM was accomplished using a tubular wire mill system to first bend a flat strip into a u-shaped cross section, deposit a powder fill, create a lap joint to seal the wire, and draw to final diameter. Powder management systems were developed to ensure uniform mixing of powder constituents and identify feed rates for optimum fill ratios. Processing parameters were successfully developed for titanium and aluminum alloy sheaths to account for material work hardening during drawing. Mass balance equations were developed to account for compositional contributions of the sheath and powder fill. PCTW composition can be adjusted through selection of the sheath or powder materials. PCTWs were successfully developed to offset Al loss in deposits of Ti-6-4 and Mg loss in Al 6061, resulting in deposits that were within the composition limits for each material. Ti-6-4 deposits were fabricated using PCTW comprised of commercially pure (CP) titanium sheath and a fill of pre-alloyed Ti-6-4 powder with additions of elemental Al and V powders. Additions of both elements were required to account for the CP Ti from the sheath, and Al was further enhanced to offset documented losses in EBF3 deposits. For Al 6061 deposits, composition was modulated through the choice of sheath material. The PCTW was made using an Al 5052 sheath to supplement Mg content and a fill composition of pre-alloyed 6061 powder with additions of Si and Cu.The slower solidification rate of the EBF3 process compared with laser powder bed fusion processes can lead to coarse-grained microstructures and mechanical property anisotropy. EBF3deposits of Ti-6-4 exhibited large epitaxially grown β grains, which result in degraded mechanical properties in the deposition direction. Microstructure refinement was achieved through a combination of electron beam modulation and the use of a PCTW designed for Ti-6-4 deposits and modified by the addition of powder made from Fe and B. Resulting deposits exhibited reductions in β grain size, α phase colony intercept length and lath width, and an increased volume fraction of β phase. The mechanism of microstructure refinement was related to precipitation of boride particles. Hardness testing confirmed that mechanical property anisotropy was reduced and an overall increase in hardness was achieved.Metal matrix composite (MMC) materials offer strength and stiffness benefits over unreinforced materials. Two methods were investigated using PCTW technology for producing Al 6061 basedMMC materials; the direct addition of SiC reinforcing particles and the in-situ generation of reinforcements through reaction synthesis of precursor powders. Al 6061 based MMCs reinforced with SiC exhibited particle clustering and formation of aluminum carbides during deposition. The application of a Ni coating to the SiC particles prior to incorporation into the powder fill eliminated aluminum carbide formation and aided particle distribution during deposition. Modulation of beam focus and power further reduced aluminum carbide formation and aided particle distribution. In reaction synthesis, precursor additions undergo an exothermic reaction during deposition to form new ceramic products, generally of finer scale than the initial precursor components. The product phases provide reinforcement in the MMC and act as nucleation sites during solidification, resulting in grain refinement, improved mechanical properties, and reduced susceptibility to solidification cracking. Higher tensile strength and stiffness were demonstrated in Al 6061 based MMCs with 2 vol% reinforcement. These combined research efforts demonstrate the potential of PCTW technology for customizing of alloy composition and achieving microstructure control. A manufacturing process for titanium- and aluminum-based PCTWs was developed based on iterative design, theoretical calculations, and empirical data. PCTW technology successfully mitigated Al loss from Ti-6-4 and Mg loss in Al 6061, resulted in grain refinement in Ti-6-4, and demonstrated fabrication of Al based MMCs

Marcia S Domack↗

A transport-based framework for solidification cracking in Ni-based superalloys processed by laser powder bed fusion

Solidification cracking remains a persistent barrier to laser powder bed fusion (LPBF) processing of solid-solution-strengthened (SSS) Ni-based superalloys and is commonly attributed to carbide formation, liquation-type failure, or elemental segregation. In this work, the cracking behavior of three SSS Ni-based superalloys—Inconel 625 (625), Inconel 617 (617), and Haynes 230 (230)—is examined under comparable LPBF conditions to evaluate the origins of their cracking susceptibility. Carbides were present in both 625 and 230, yet cracking behavior differed significantly. MC-type carbides in 625 remain discrete and preserve liquid connectivity, whereas Cr-rich M23C6 carbides in 230 form at cellular triple junctions that bottleneck the interdendritic liquid network, influencing cracking through liquid connectivity rather than as an independent cause. Alloy 617 exhibited anomalous segregation without resolvable secondary phases yet cracked mildly, indicating that extensive carbide formation is not a prerequisite for cracking. To rationalize these observations, a transport-limited framework is proposed in which cracking occurs when terminal-liquid feeding cannot accommodate solidification-induced strain; among the mechanisms evaluated, this framework is most consistent with the physical constraints imposed by LPBF solidification. Transport-based crack-susceptibility indexes incorporating permeability, viscosity, and solidification kinetics distinguish the alloy hierarchy; permeability ratios Krat increased from approximately 7 (625) to 11.5 (617) and 14.5 (230), with corresponding increases in the μ-weighted mushy zone risk index (CSIMZRM). These results are consistent with transport-limited liquid feeding as a rate-limiting contributor to solidification cracking in LPBF-processed SSS Ni-based superalloys, providing a physically grounded basis for alloy and process design.

Hyer, Holden [ORNL] (ORCID:0000000343915561)↗

Assessment of critical flaw sizes and crack driving forces during additive manufacturing of metallic materials

Additive manufacturing (AM) of complex engineering components is often plagued by a high susceptibility to cracking, particularly in high-strength metallic materials. While alloy design efforts have made progress in mitigating solidification defects, there remains a need for mechanistic guidelines to predict susceptibility to solid-state cracking. To address this gap, driving forces for the growth of melt pool cracks are calculated across a wide range of alloys using an efficient computational framework. Calculations are coupled with rapid single track laser experiments to elucidate trends in cracking from laser melting. The analyses conducted here highlight the important role of material properties in susceptibility to cracking, notably fracture toughness and elastic modulus. An important finding is that residual stresses that are limited in magnitude to the yield stress of the material are likely insufficient to drive cracking during cooling. Furthermore, the implications of these results are discussed in the context of alloy design for AM and residual stress accumulation during AM.

36 MATERIALS SCIENCE↗