Search NASA⌕ Search

SEARCH · Search NASA

Results for “superalloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Understanding the deformation mechanisms in Ni-based superalloys with using crystal plasticity finite element method

Nl-based superalloy is considered as a good candidate due to its excellent resistance to elevated temperature deformation for long term period application. Understanding the deformation and failure mechanisms of Ni-Based superalloys is very helpful for providing design guidelines for processing Ni-based superalloys. Experimental characterization indicates that the deformation mechanisms of Ni based superalloy is strongly microstructure dependent. Besides, damage transform from the void nucleation to the macro cracks by voids growth leading to the failure of the Ni-based superalloys are also showing strong microstructure sensitivity. Therefore, this work focuses on the prediction and comprehension of the deformation and void growth behavior in Ni based superalloy at different working conditions via crystal plasticity finite element modeling and simulation. Physically based crystal plasticity frameworks were developed for newly Ni- based superalloy Haynes 282. It was found that dislocation shearing through the precipitates were acting as the main contributor to the strength of Haynes 282 at room temperature and 815°C. Our analysis of the creeping behavior of Haynes 282 exhibited that resistance of general climb replaced by the resistance induced by the deposited climb dislocation density. In addition, in the study of void growth behavior, our simulation results demonstrated that as the main loading axis perpendicular to the grain boundary (GB), voids grow more slowly on tilt GBs in bicrystals than those in single and bicrystals with twist GBs. And tilt GBs would promote the void grow into irregular shape.

36 MATERIALS SCIENCE↗

Advancing Development and Application of Superalloys

This JOM topic is sponsored by the High Temperature Alloys Committee of TMS and addresses advances in the development and application of superalloys. Each year, the High Temperature Alloys Committee organizes symposia at the TMS and Materials Science and Technology annual meetings. In 2020, two symposia were organized for the TMS annual meeting on February 23–27 in San Diego, CA: Materials Design Approaches & Experiences V, co-sponsored by the Integrated Computational Materials Engineering Committee and Advancing Current and State-of-the-Art Applications of Ni- and Co-base Superalloys, co-sponsored by the Corrosion and Environmental Effects Committee. Later this year, the 14th International Symposium on Superalloys will be held on September 13-17 in Seven Springs, PA. The conference, held every 4 years, convenes members of the superalloy community to discuss recent challenges and discoveries affecting future performance and use of superalloys. The TMS High Temperature Alloys Committee meets at both the TMS Annual Meeting & Exhibition and the annual Materials Science and Technology conference. The meetings are open to anyone interested in high-temperature alloys. This special topic on Advancing Development and Application of Superalloys includes a range of sub-topics including mechanical performance, corrosion resistance, processing and advanced manufacturing techniques, which were submitted by research groups from industry, national laboratories and universities.

36 MATERIALS SCIENCE↗

Utilizing a Dynamic Segmentation Convolutional Neural Network for Microstructure Analysis of Additively Manufactured Superalloy 718

Additive manufacturing (AM) is revolutionizing almost all industries through the production of intricate geometries previously prohibited by cost or machinability. Ni-based superalloys form a primary alloy class for high temperature applications in the petrochemical, aerospace, and nuclear industries because of their intrinsic resistance to creep and the ability to heat treat the superalloy for high strength. Despite these attractive properties, the extreme work hardening of Ni-based superalloys makes traditional manufacturing of complex shapes difficult and thus, these alloys are an attractive target for AM. Superalloy 718 was chosen as an example superalloy because of the wide variety of precipitates that can form within its composition space from the repetitive heating and cooling cycles of the AM process. The precipitates and other microstructure features, such as grain boundaries and dislocations, will dictate the mechanical properties and thus, there is an extensive challenge to characterize the size, number density, composition, and volume fraction of each microstructural feature from AM fabrication using analytical electron microscopy. This work focused on the application of a pixel-wise classification machine learning (ML) model called a dynamic segmentation convolutional neural network (DSCNN) to identify the microstructural features of an as-fabricated additively manufactured superalloy 718.

Taller, Stephen↗

Additive manufacturing of nickel-based superalloys: A state-of-the-art review on process-structure-defect-property relationship

Fusion-based additive manufacturing (AM) has significantly grown to fabricate Nickel-based superalloys with design freedom across multiple length scales. Several phenomena such as feedstock/energy source/melt pool interactions, solidification and phase transformations occur during fusion-based AM processes of Nickel-based superalloys, which determine the ultimate microstructure and mechanical performance of the built parts. In this review, here we elaborate a comprehensive discussion on AM Nickel-based superalloys and influential factors including feedstock characteristics (powder morphology, chemistry, contamination, flowability, recycling) and AM processing (parameters, and powder spreading/wall/balling/spattering effects) on their microstructure (micro-segregation, phases formations and grain structures), defect generation (sub-surface/internal defects, microcracks, surface roughness, and residual stress). Furthermore, the mechanical properties of AM Nickel-based superalloys such as tensile, creep and fatigue at room/elevated temperatures are analyzed in accordance with the initial, and post processing effects. Additionally, the commonly utilized modeling approaches in literature to predict the microstructure and mechanical behavior of these alloys are highlighted. Finally, the current challenges and mitigation approaches for future research are identified considering the gaps in the AM Nickel-based superalloys.

36 MATERIALS SCIENCE↗

Using post-processing heat treatments to elucidate precipitate strengthening of additively manufactured superalloy 718

The poor machinability and extensive work hardening of Ni-based superalloys makes additive manufacturing an attractive option for producing geometrically complex components with distinct microstructures. Although previous studies show recovery of high strength at room temperature, very few studies demonstrate successful properties at elevated temperatures required for industrial applications. Here, the objectives of this study are to present a post-build heat treatment for high strength across a wide temperature range, determine the strength contribution of nanoscale precipitating phases to the overall mechanical properties of superalloy 718, and from these, provide a comprehensive microstructure-property relationship for wrought and AM 718 to guide efforts to simulate the properties of AM components. Laser powder bed fusion–produced superalloy 718 was characterized at multiple length scales using scanning electron microscopy and transmission electron microscopy in the as-built condition and with multiple heat treatments designed to form combinations of γ', γ", and δ precipitates. Uniaxial tensile tests performed from room temperature to 600 °C on subsize specimens determined the yield strength, elastic modulus, ultimate tensile strength, fracture stress, and uniform elongation. Precipitates in this work proved to be weak barriers to dislocation motion through a dispersed barrier model, but they provided strength to the alloy through their consistent high density. The relative contribution to the yield strength from γ" remained consistent between 48% and 57% of the total strength up to 600 °C, the primary influence on the high temperature strength of superalloy 718. The strength factors for γ" and δ precipitates were found to trend inversely with tensile test temperature and may be attributable to the differences in precipitate coherency. A post-build heat treatment is recommended to maintain high strength at elevated temperatures. A quantitative microstructure-property relationship, dependent on precipitate size, density, and morphology, was derived and can estimate the yield strength across a wide temperature range applicable to the operational regimes for superalloy 718.

36 MATERIALS SCIENCE↗

Microstructure Evolution of a Multimodal Gamma-Prime Ni-Based Superalloy Characterized by In Situ Diffraction

The relationship between the evolution of microstructure, deformation micromechanisms and mechanical properties is difficult to establish in multimodal size distribution $_γ$$'$ superalloys, as the microstructure evolves with both temperature and time, and multiple strengthening mechanisms across each size distribution contribute to mechanical performance. In situ X-ray scattering can offer unparalleled insight regarding microstructure evolution at the temperatures and stresses of importance to gas-turbine applications; however, in situ X-ray diffraction has not been applied to the study of multimodal $_γ$$'$ distribution superalloys. Herein, lattice parameter evolution of secondary and tertiary $_γ$$'$ precipitates in a representative superalloy, Nimonic 115, is determined between 750 °C and 950 °C and correlated to room-temperature SEM and microhardness values. A large positive lattice parameter misfit of secondary $_γ$$'$ induces precipitate splitting, and the tertiary $_γ$$'$ goes into dissolution at ~ 800 °C, but with little apparent change in hardness values. The volume fraction of $_γ$$'$ decreases above 900 °C and precipitate-matrix coherency is lost, and there is a corresponding decrease in microhardness values. Importantly, the diffraction analysis demonstrates the capability to determine critical microstructural parameters of both precipitate size distributions in situ, representing an additional tool for determining microstructure-mechanical property relationships of multimodal superalloys.

36 MATERIALS SCIENCE↗

Molecular Dynamics Study of Creep Deformation in Nickel-based Superalloy

The present study employs molecular dynamics simulations of Ni-based superalloy to investigate the creep behavior under uniaxial compression test. Dislocation dynamics is analyzed for the nickel-based single crystal superalloy with the presence of void and with varying the distribution of gamma-prime phase The results show that multiple-void systems are more prone to yield than single-void systems and single-void systems are more prone to yield than the system withoutvoid. From the simulations, it has been determined that the creep mechanism in Ni/Ni3Al is subject to change on the applied stress depending on the distribution of gamma-prime phases change. Dislocation behavior is also observed in addition to the time evolution of dislocation nucleation and growth to quantify the propensity and mechanism of creep in nickel-based single crystal superalloy. The studies confirmed that dislocation length prior to plastic deformation decreased as the number of voids increased. In addition, the deformation behavior for finegrained nickel-based polycrystalline superalloy upon grain size variation is also investigated. Our findings show that both the movement mechanisms of the grains and grain boundaries and the relationship between grain size and yield strength are highly affected by the grain size of the materials. All the databases have then been classified to accurately predict the target class vi machine learning using the data mining tool WEKA.

creep, nickel-based superalloy, molecular dynamics↗

Tensile Deformation of DED Graded IN718-René41 Superalloy at 650°C by in-situ Neutron Diffraction and Digital Image Correlation

A compositionally graded material comprised IN718 (718, γ'/γ" strengthened superalloy) and René41 (R41, a medium γ' strengthened superalloy) was fabricated using laser blown-powder directed energy deposition (DED/LB-M). Hot gas path components that require high and low temperature capabilities at different locations may benefit from such graded superalloy, potentially eliminating the use of welded or mechanically joined components and reducing cost. In the present work, microstructure and 650°C tensile behavior of 718-R41 graded superalloy in as-built and heat-treated states are investigated by Digital Image Correlation (DIC), in-situ neutron diffraction, coupled with conventional characterization techniques. The applied heat treatment generates static recrystallization and equiaxed grains in 718 rich compositions, while R41 rich compositions remain partially or un-recrystallized. Yield strengths of 718 and R41 sections in heat-treated state are comparable to wrought forms but the graded compositions show weakness. From neutron experiment, diffraction elastic constants and single crystal elastic constants are calculated, which show small difference between the as-built and heat-treated states and between the γ and γ' phases. Grain-level load transfer from the (220) grains to (200) grains is found to be composition dependent, and qualitatively agrees with DIC measured macroscopic yield strength. Within the (200) grains, the γ/γ' phases deform elastically until the γ phase yields and afterwards the γ' phase takes load from γ phase.

digital image correlation↗

Methods for preparing superalloy articles and related articles

A method for preparing an improved article including a nickel-based superalloy is presented. The method includes heat-treating a workpiece including a nickel-based superalloy at a temperature above the gamma-prime solvus temperature of the nickel-based superalloy and cooling the heat-treated workpiece with a cooling rate less than 50 degrees Fahrenheit/minute from the temperature above the gamma-prime solvus temperature of the nickel-based superalloy so as to obtain a cooled workpiece. The cooled workpiece includes a coprecipitate of a gamma-prime phase and a gamma-double-prime phase, wherein the gamma-prime phase of the coprecipitate has an average particle size less than 250 nanometers. An article having a minimum dimension greater than 6 inches is also presented. The article includes a material having a coprecipitate of a gamma-prime phase and a gamma-double-prime phase, wherein the gamma-prime phase of the coprecipitate has an average particle size less than 250 nanometers.

36 MATERIALS SCIENCE↗

Direct measurements of slip irreversibility in a nickel-based superalloy using high resolution digital image correlation

Fatigue crack nucleation in crystalline materials typically develops due to highly localized cyclic slip. During a fatigue cycle, reverse slip differs locally from slip in the forward direction particularly in precipitate-containing materials such as superalloys. In this paper we report the first direct measurements of irreversibility at the scale of individual slip bands by high-resolution digital image correlation (DIC) in a polycrystalline nickel-based superalloy. Quantitative measurements of the slip irreversibility are challenging for regions of material that have a size that captures the microstructure and its variability. High spatial resolution at the nanometer scale during experimental measurements is needed to observe slip localization during deformation. Moreover, large fields are also needed to obtain the material response over statistically representative populations of microstructural configurations. Recently, high resolution scanning electron microscope (SEM) digital image correlation (DIC) has been extended for quantitative analysis of discontinuities induced by slip events using the Heaviside-DIC method. Therefore, this novel method provides quantitative measurements of slip localization at the specimen surface. In this paper, the Heaviside-DIC method is used to measure slip irreversibility and plastic strain accumulation in a nickel-based superalloy. The method detects bands with high levels of irreversibility early in cycling that ultimately form fatigue cracks upon further cycling. The local microstructural configurations that induce large amounts of plasticity and slip irreversibility are correlated to crack nucleation locations.

36 MATERIALS SCIENCE↗

Evolution of carbide precipitates in Haynes® 282 superalloy processed by wire arc additive manufacturing

Precipitation hardening regulated with heat treatments is a critical technique for tuning the mechanical properties of Ni-based superalloys fabricated with additive manufacturing, where mechanical deformation is no longer viable for microstructural refinement. As one of the key precipitates, carbides prevail in the additively manufactured alloys, whose precipitation kinetics remain largely vague. This work studies the influence of heat treatments on the evolution of MC- and M 23 C 6 -type carbides within a Haynes® 282 superalloy prepared by wire arc additive manufacturing (WAAM). SEM-EDS analysis was performed to identify the evolution pathways of the carbides, and TEM and XRD characterizations were carried out to track the crystallographic features. The MC-type carbides are originally present in the as-printed alloy, which distribute uniformly across the whole material and remain largely unchanged in size during the heat treatments. By contrast, the incipiently non-existent M 23 C 6 -type carbides precipitate during an aging treatment at 1010 °C, which majorly extend along the grain boundaries as kinetically feasible sites. Further experimental and computational analysis confirms the enhancing effect of the M 23 C 6 -type carbides on the Vickers hardness. For the first time, this work revealed the evolution pathways of carbides within a Haynes® 282 superalloy prepared by WAAM, providing critical information for tunning the microstructure and mechanical properties. Finally, the carbide evolution kinetics established in this work can be potentially extended to other alloys prepared with WAAM, providing critical information to prevent mechanical failures associated with carbide coarsening.

36 MATERIALS SCIENCE↗

Custom-designed heat treatment simultaneously resolves multiple challenges facing 3D-printed single-crystal superalloys

Single-crystal Ni-based superalloys are currently the material of choice for turbine blade applications, especially with the emerging additive manufacturing (AM) that facilitates the manufacture/repair of these single crystals. This promising AM route, however, comes with a dilemma: in the fusion and heat affected zones after e-beam or laser induced melting, one needs a solutionizing annealing to relieve the residual stresses and homogenize the chemical/microstructure. The super-solvus solutionizing temperature is usually adopted from the protocol for the cast superalloys, which almost always causes recrystallization and stray grain growth, resulting in a polycrystalline microstructure and degrading the high-temperature mechanical performance. Here, in this paper, we demonstrate a custom-designed post-printing heat treatment to replace the conventional super-solvus one. The recovery and relatively low temperature diminish the driving force for recrystallization and the movement of stray grain boundaries, without suffocating the chemical/microstructural homogenization thanks to the narrow dendrite width and short element segregation distance. The optimal duration of the heat treatment is proposed to achieve atomic-diffusion mediated chemical homogenization while limiting γ'-particle coarsening in the interdendritic regions. Our strategy makes it practically feasible to resolve several bottleneck problems with one processing/treatment, removing a seemingly formidable obstacle to effective additive manufacturing of superalloy single crystal products.

36 MATERIALS SCIENCE↗

The Application of Differential Scanning Calorimetry to Investigate Precipitation Behavior in Nickel-Base Superalloys Under Continuous Cooling and Heating Conditions

In this study, a suite of experimental tools and fast-acting, numerical-simulation techniques was used to quantify the precipitation behavior of three nickel-base superalloys: IN-100, LSHR, and 718. Experimental methods comprised differential scanning calorimetry (DSC) to establish the specific heat as a function of temperature and selected direct-resistance heating trials (using a Gleeble ® machine) to obtain samples for microstructural analysis. For the DSC experiments, each alloy was cooled at a prescribed constant rate (between 5 and 20 K/min) after an initial soak/equilibration in the high-temperature, single-phase (supersolvus) temperature regime. On-heating DSC trials beginning at ambient temperature were also performed on alloy 718 in three different starting conditions: super- δ -solvus solution treated and water quenched (denoted as ST), solution treated and aged (STA), and solution treated and overaged (STOA). DSC results, revealing the thermal signatures associated with the kinetics of precipitation of γ ' (IN-100, LSHR) or γ ' and γ " (718), were interpreted using a previously-developed fast-acting routine that treats concurrent nucleation, growth, coarsening, and dissolution. For these simulations, special attention was paid to various thermo-kinetic input parameters including equilibrium solvus-approach curves, bulk free energies of transformation, matrix-precipitate interface energies, and effective diffusivities. For the γ - γ ' superalloys (IN-100 and LSHR), estimates of precipitate volume fraction as a function of temperature from the specific-heat data revealed semi-quantitative agreement with simulation predictions. For the γ - γ '- γ " superalloy (718), simulation predictions of precipitate volume fractions were converted to specific heat as a function of temperature and showed semi-quantitative agreement with the direct measurements.

36 MATERIALS SCIENCE↗

Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High $\gamma ^{\prime }$ CoNi-Base Superalloy

Here, the cracking behavior of a high γ' volume fraction CoNi-base superalloy fabricated via laser powder bed fusion (LPBF) is studied in relation to the content of carbon and boron. Severe cracking occurred with the increase in boron content from 0.08 to 0.16 at. pct (0.015 to 0.029 wt pct), while compositions with 0.1 to 0.36 at. pct C (0.02 to 0.076 wt pct) and 0.08 at. pct B exhibited minimal cracking. Assessment of cracks in the high-boron composition shows a variation in crack density with printing parameters, and alignment of the cracks with the build direction. Scanning electron microscopy (SEM) of the crack surfaces shows evidence of a solidification cracking mode. Differential thermal analysis (DTA) reveals a decreased incipient melting temperature for the high-boron composition, and atom probe tomography (APT) is used to measure the enrichment at grain boundaries, revealing distinct boron segregation. Scheil-Gulliver solidification simulations for the different C and B levels are consistent with the incipient melting behavior observed with DTA. Evaluation of the solidification cracking susceptibility from the simulations allow for comparison of the CoNi alloy behavior to Ni-base superalloys studied for LPBF fabrication and displays how such metrics may aid in the design of new precipitation-strengthened superalloys for additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Creep Deformation and Damage Mechanisms in an Advanced High-Temperature Additively Manufactured Nickel-Base Superalloy

Abstract This research investigates the processing–structure–properties–performance relationship in a novel nickel-base superalloy, ABD ® -900AM, designed for extreme environments. Specifically tailored for additive manufacturing (AM), ABD ® -900AM maintains mechanical integrity at high temperatures and is comparable to other nickel-based superalloys with a 30–40% gamma-prime volume fraction. A comprehensive study was conducted using laser-beam powder bed fusion and electron-beam powder bed fusion methods. Factors such as heat treatment, porosity, build orientation, and hot isostatic pressing were evaluated to understand their effects on microstructure and mechanical performance. Microstructural characterization revealed significant differences in grain size and orientation across build processes and heat treatments. High-temperature mechanical testing indicated that grain size, heat treatment, and orientation significantly influence creep behavior. A super-solvus heat treatment led to recrystallization and grain growth, significantly improving creep properties compared to a near-solvus heat treatment. Various creep mechanisms were identified across different conditions, and creep rupture models were developed for each build process. Post-test microstructural analysis showed grain boundary damage, with differences in creep cavitation morphology under varying stress conditions. It was shown that MC carbides grow at the expense of gamma-prime near grain boundaries, leading to precipitate-free zones in specimens tested at higher temperatures. This study fills a significant gap in fundamental research by offering a deeper insight into the high-temperature mechanical behavior of additively manufactured nickel-base superalloys. It also explores critical research questions regarding the role of carbides and the significance of heat treatment. The insights gained enhance confidence in the industry adoption of ABD ® -900AM and similar alloys for high-temperature applications, bridging the knowledge gap and supporting the development of reliable AM processes for extreme environments.

Bridges, Alex (ORCID:000000030338759X)↗

A transport-based framework for solidification cracking in Ni-based superalloys processed by laser powder bed fusion

Solidification cracking remains a persistent barrier to laser powder bed fusion (LPBF) processing of solid-solution-strengthened (SSS) Ni-based superalloys and is commonly attributed to carbide formation, liquation-type failure, or elemental segregation. In this work, the cracking behavior of three SSS Ni-based superalloys—Inconel 625 (625), Inconel 617 (617), and Haynes 230 (230)—is examined under comparable LPBF conditions to evaluate the origins of their cracking susceptibility. Carbides were present in both 625 and 230, yet cracking behavior differed significantly. MC-type carbides in 625 remain discrete and preserve liquid connectivity, whereas Cr-rich M23C6 carbides in 230 form at cellular triple junctions that bottleneck the interdendritic liquid network, influencing cracking through liquid connectivity rather than as an independent cause. Alloy 617 exhibited anomalous segregation without resolvable secondary phases yet cracked mildly, indicating that extensive carbide formation is not a prerequisite for cracking. To rationalize these observations, a transport-limited framework is proposed in which cracking occurs when terminal-liquid feeding cannot accommodate solidification-induced strain; among the mechanisms evaluated, this framework is most consistent with the physical constraints imposed by LPBF solidification. Transport-based crack-susceptibility indexes incorporating permeability, viscosity, and solidification kinetics distinguish the alloy hierarchy; permeability ratios Krat increased from approximately 7 (625) to 11.5 (617) and 14.5 (230), with corresponding increases in the μ-weighted mushy zone risk index (CSIMZRM). These results are consistent with transport-limited liquid feeding as a rate-limiting contributor to solidification cracking in LPBF-processed SSS Ni-based superalloys, providing a physically grounded basis for alloy and process design.

Hyer, Holden [ORNL] (ORCID:0000000343915561)↗