Search NASA⌕ Search

SEARCH · Search NASA

Results for “superalloys”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Creep Deformation and Damage Mechanisms in an Advanced High-Temperature Additively Manufactured Nickel-Base Superalloy

Abstract This research investigates the processing–structure–properties–performance relationship in a novel nickel-base superalloy, ABD ® -900AM, designed for extreme environments. Specifically tailored for additive manufacturing (AM), ABD ® -900AM maintains mechanical integrity at high temperatures and is comparable to other nickel-based superalloys with a 30–40% gamma-prime volume fraction. A comprehensive study was conducted using laser-beam powder bed fusion and electron-beam powder bed fusion methods. Factors such as heat treatment, porosity, build orientation, and hot isostatic pressing were evaluated to understand their effects on microstructure and mechanical performance. Microstructural characterization revealed significant differences in grain size and orientation across build processes and heat treatments. High-temperature mechanical testing indicated that grain size, heat treatment, and orientation significantly influence creep behavior. A super-solvus heat treatment led to recrystallization and grain growth, significantly improving creep properties compared to a near-solvus heat treatment. Various creep mechanisms were identified across different conditions, and creep rupture models were developed for each build process. Post-test microstructural analysis showed grain boundary damage, with differences in creep cavitation morphology under varying stress conditions. It was shown that MC carbides grow at the expense of gamma-prime near grain boundaries, leading to precipitate-free zones in specimens tested at higher temperatures. This study fills a significant gap in fundamental research by offering a deeper insight into the high-temperature mechanical behavior of additively manufactured nickel-base superalloys. It also explores critical research questions regarding the role of carbides and the significance of heat treatment. The insights gained enhance confidence in the industry adoption of ABD ® -900AM and similar alloys for high-temperature applications, bridging the knowledge gap and supporting the development of reliable AM processes for extreme environments.

Bridges, Alex (ORCID:000000030338759X)↗

A transport-based framework for solidification cracking in Ni-based superalloys processed by laser powder bed fusion

Solidification cracking remains a persistent barrier to laser powder bed fusion (LPBF) processing of solid-solution-strengthened (SSS) Ni-based superalloys and is commonly attributed to carbide formation, liquation-type failure, or elemental segregation. In this work, the cracking behavior of three SSS Ni-based superalloys—Inconel 625 (625), Inconel 617 (617), and Haynes 230 (230)—is examined under comparable LPBF conditions to evaluate the origins of their cracking susceptibility. Carbides were present in both 625 and 230, yet cracking behavior differed significantly. MC-type carbides in 625 remain discrete and preserve liquid connectivity, whereas Cr-rich M23C6 carbides in 230 form at cellular triple junctions that bottleneck the interdendritic liquid network, influencing cracking through liquid connectivity rather than as an independent cause. Alloy 617 exhibited anomalous segregation without resolvable secondary phases yet cracked mildly, indicating that extensive carbide formation is not a prerequisite for cracking. To rationalize these observations, a transport-limited framework is proposed in which cracking occurs when terminal-liquid feeding cannot accommodate solidification-induced strain; among the mechanisms evaluated, this framework is most consistent with the physical constraints imposed by LPBF solidification. Transport-based crack-susceptibility indexes incorporating permeability, viscosity, and solidification kinetics distinguish the alloy hierarchy; permeability ratios Krat increased from approximately 7 (625) to 11.5 (617) and 14.5 (230), with corresponding increases in the μ-weighted mushy zone risk index (CSIMZRM). These results are consistent with transport-limited liquid feeding as a rate-limiting contributor to solidification cracking in LPBF-processed SSS Ni-based superalloys, providing a physically grounded basis for alloy and process design.

Hyer, Holden [ORNL] (ORCID:0000000343915561)↗

Predictive design of novel nickel-based superalloys beyond Haynes 282

Nickel-based superalloys are in great demand for harsh-service conditions involving high temperatures and oxidative environments. Haynes 282 stands out due to its excellent high-temperature properties and easy fabricability. However, the upper operation temperature of Haynes 282 is limited due to its relatively low liquidus temperature. Equipped with high-fidelity density-functional theory calculations and high-throughput experimentation methodology, we explored new compositional spaces that exhibit higher liquidus temperature and higher strength. While maintaining the manufacturability, the newly designed alloy shows improved strength and ductility at room temperature and better oxidation resistance up to 800°C. Here, the new compositions showcase a minor change in the refractory and metalloid content can significantly impact the mechanical and oxidation performance of superalloys.

36 MATERIALS SCIENCE↗

Heterogeneous fatigue damage in a nickel-based single-crystal superalloy unraveled using correlative 3D X-ray technology

Nickel-based single-crystal (Ni-SX) superalloys under cyclic stress are susceptible to cracking at stress-concentration sites, eventually leading to low-cycle fatigue (LCF) failure. LCF cracks typically originate from intrinsic defects (e.g., voids and carbides) within solidified dendrites. However, systematic quantitative experimental analyses of defect-mediated local damage remain limited. To thoroughly understand the microscopic origins and evolution of LCF damage, correlated 3D mapping of dendrites across various regions is essential. Here, in this study, macroscale micro-computed tomography (μ-CT) was initially used to capture internal interdendritic secondary cracks within bulk DD413 superalloy after LCF testing at 760 °C. Subsequently, a multimodal methodology combining synchrotron 3D microdiffraction (3D-μXRD), high-resolution μ-CT, and electron microscopy was established. This approach allowed precise localization of internal damage zones near interdendritic secondary cracks and detailed mapping of the 3D correlated distributions of dendrites, defects, and residual stress/strain fields within these zones at submicron spatial resolution. Finally, the same approach was applied to specimens subjected to interrupted loading at approximately 40 % of the fatigue life to uncover the early damage states of dendrites. The dendrite cores (DCs) and interdendritic regions (IDs) exhibit microscale heterogeneous mechanical responses: nearly defect-free DCs accumulate local irreversible slip along specific slip systems to generate slip bands, while the IDs containing various defects accommodate local microplasticity through the activation of multiple slip systems around these defects. The local tensile stress near defects in the IDs exceeds that in the DC slip band regions by more than threefold, leading to the generation of local damage zones within the IDs. Chain-like defect distributions facilitate the interconnection of these local zones into a continuous damage region, further elevating the overall tensile stress in the IDs. Additionally, geometrically necessary dislocations alone are insufficient as indicators of LCF damage; both the internal stress state and its magnitude must be considered. These experimental results provide critical data and insights for the development of multi-physics fatigue models.

Localized deformation↗

Understanding the influence of boron in additively manufactured GammaPrint®-700 CoNi-based superalloy

Boron is commonly added to superalloys in small amounts to enhance creep resistance, but can lead to cracking at high concentrations, especially during the additive manufacturing process. Two variants of CoNi-based GammaPrint®-700 superalloy with different B contents (0.08 at% vs 0.16 at%) were printed via laser powder bed fusion (LPBF) with the same printing parameters, with only the high B alloy exhibiting solidification cracking. Atom probe tomography (APT) revealed stronger segregation behaviors in the high B alloy compared to the low B alloy at both the inter-dendritic regions and grain boundaries (GBs). The segregation behavior at inter-dendritic regions was well captured with Scheil simulation and can correlate with the existing cracking susceptibility index (CSI) on cracking tendencies, although high angle GBs are where cracking occurs according to electron backscatter diffraction (EBSD) measurements. Additionally, the extent of GB segregation was compared between the high B and low B alloy. Higher B additions led to significantly more GB B segregation in the high B alloy compared to the low B alloy. Further, for the high B alloy, the cracked region of one GB exhibited higher levels of B compared to the uncracked region of the same GB. However, much higher B contents were also found in two other uncracked GBs in the high B alloy, which demonstrates that higher GB B concentrations are not fully responsible for the cracking. A much larger variance in GB B segregation content was found in the high B alloy compared to the low B alloy. These phenomena were explained with a solidification model with the GB segregation content expressed explicitly by a modified Langmuir-McLean equation. This model linked the GB segregation content with solidification undercooling, which can be used as quantitative cracking criteria for future builds.

36 MATERIALS SCIENCE↗

High-temperature mechanical properties of a γ′-strengthened Co-based superalloy designed for additive manufacturing

GammaPrint®-700 is a recently developed high γ′ (∼70% volume fraction) CoNi-based superalloy designed to combine high-temperature mechanical performance with laser powder bed fusion processability. Room-temperature yield strength ranged from 610 to 658 MPa and increased to 661 MPa (longitudinal) and 730 MPa (transverse) at 760 °C. The creep behavior compared favorably to high-γ′ Ni-based superalloys manufactured via laser powder bed fusion such as Incoloy® 939 and Inconel® 738LC. In-situ neutron diffraction data measured during creep revealed that plastic deformation was largely localized to the γ phase at 760 °C, allowing the γ’ phase to elastically compensate and maintain creep strain resistance. Furthermore, at 900 °C, this load sharing behavior was weakened, contributing to accelerated creep rate and rupture.

Creep↗

Machine Learning Vacancy Formation Energy in Nickel-Based Superalloys

Creep performance plays a key role in nickel-based superalloys for high temeprature applications. Creep behavior depends on many parameters such as strength, dislocations, diffusivity, and microstructural stability in addition to temeprature, applied stress, and oxidation. This work focuses on predicting vacancy formation energy in nickel-based superalloys using machine learning approach. High-throughput density functional theory (DFT) calculations are performed on Ni-based alloys with the addition of various alloying elements to predict the vacancy formation energy and vacancy concentration. Machine learning is performed using various models including graph neural networks.

creep performance↗

Predicting the High-Temperature Oxidation Response of Nickel Superalloys Using CALPHAD-Enhanced Machine Learning

Structural materials such as Ni-based superalloys used in high-temperature power cycles are routinely exposed to toxic environments including high temperature and pressure, aqueous and gas corrosion, etc. Here, we present a physics-informed machine learning approach to predict the oxidation response of diverse Ni-superalloys. First, a high-fidelity experimental dataset is curated from typical oxidation mass-change experiments in air, covering 25+ elements and different physical behavior such as parabolic growth, non-parabolic growth, and oxide spallation. Second, the dataset is featurized using thermophysical, chemical, and mechanical properties obtained from high-throughput CALPHAD calculations. Third, several machine learning models are developed to identify key features related to mass-change characteristics and model the mass-change curve for various alloys. Finally, the model is deployed to rapidly screen over a new composition space and down-select candidate alloys with high oxidation resistance for experimental validation.

CALPHAD↗

Simulation and analysis of small angle scattering (SAS) patterns of Ni-based superalloy microstructures generated by a phase-field model

This paper investigates the relationship between microstructural features and small-angle scattering (SAS) patterns in Ni-based superalloys using a combined phase-field and SAS simulation approach coupled with microstructure analyses. The simulated SAS patterns accurately capture key experimental observations previously reported in the literature, including the time-dependent transition from circular to square-shaped precipitates and the development of anisotropic SAS patterns. Importantly, our analysis reveals the correlations between characteristic length scales extracted from SAS profiles and microstructural descriptors, such as precipitate size and inter-precipitate distance. These findings provide a comprehensive understanding of the link between SAS profiles and microstructure evolution in Ni-based superalloys, offering valuable insights for materials characterization and design.

Microstructure↗

Gaseous Hydrogen Embrittlement of L-PBF Ni-Based Superalloys for Service in Natural Gas Turbines

Efforts to improve efficiency of industrial gas turbine engines have focused on increasing operating temperatures by use of fuel-flexible gas blends. Ni-based superalloys are susceptible to hydrogen embrittlement (HE), leading to potential risk of premature component failure. Certain turbine components exposed to hydrogen-rich environments are manufactured from additive processes like laser powder bed fusion (L-PBF). The HE susceptibility was evaluated for three Ni-based superalloys: solid solution strengthened Alloy 625, γ’/γ’’-precipitation strengthened Alloy 718, and γ’-precipitation strengthened Haynes® 282®. L-PBF samples were pre-charged under medium and high pressure gaseous hydrogen before tensile testing at temperatures up to 260 °C using a fast strain rate. Selected samples were subjected to a service conditioning heat treatment prior to hydrogen charging to evaluate the change in susceptibility after prolonged service. The susceptibility to HE and HE mechanisms of these three alloys is compared.

additive manufacturing↗

Characterization of γ′/γ″ compact and sandwich type precipitates during long-term high-temperature exposure in Ni-based superalloys

Here, the formation of γ′/γ″ co-precipitates is investigated in Ni-based superalloys with a varying Ti/Al ratio and Ta content and their stability is studied using long-term high-temperature exposure. Transmission electron microscopy and atom probe tomography analyses demonstrate that both higher Ti/Al ratios and increased Ta promote γ″ phase formation, leading to sandwich and compact structures. The compact co-precipitation significantly reduces γ′ precipitate coarsening during 10,000 h exposure at 700°C by restricting elemental diffusion, particularly of aluminum, from the γ matrix to the γ′ phase. For the alloy without a compact structure, and only γʹ precipitates, at the beginning of the exposure, the coarsening rate over 10,000 h was 3.5 times faster than for the alloy with compact γʹ/γʺ precipitates. Evidence of destabilization of the compact morphology was found to occur between 5,000 and 10,000 h exposure and originated from the extensive formation and growth of δ platelets that extended throughout the grains. Thus, the outer layer of the compact, which consists of γʺ, was subjected to the γ″ to δ phase transformation.

gamma double prime↗

Microstructural evolution and hardness changes in ion irradiated nickel-based Haynes 282 superalloy

This study investigated the crucial aspects of thermal and irradiation stability in precipitation hardened Haynes 282 Ni-based superalloy. The Haynes 282 Ni-based alloy was irradiated by 8 MeV Ni 3+ ions to assess its resistance to phase instabilities and mechanical property alterations. The mid-range doses (at a depth of ∼1 µm) were 1 and 10 displacements per atom (dpa) at temperatures of 600°C and 750°C. Nanoindentation tests provided insights into bulk equivalent hardness of the irradiated and pristine regions, while scanning transmission electron microscopy (STEM) and energy dispersive X-ray spectroscopy (EDS) were used to examine the microstructural evolution of irradiation-induced defects and γ′ -Ni 3 (Al, Ti) precipitates and defect structure under irradiation. These precipitates, with an average diameter of 29 nm and a number density of 5 x 10 21 /m 3 , acted as robust dispersion strengthening agents with high radiation point defect sink strength. Remarkably, irradiation did not significantly alter the size or number density of the γ′ precipitates, indicating exceptional thermal stability and radiation resistance of these precipitates at the examined conditions. Radiation-induced dislocation loops were observed at 600°C, albeit without a substantial impact on mechanical properties due to the dominance of γ′ precipitates on the overall alloy strength. The superior stability of γ′ precipitates observed in this study contrasts with several previous research findings on Ni-based alloys that reported poor precipitate stability. Plausible reasons for this difference are discussed. Moreover, this work explicitly outlines a physically grounded approach to ensure accurate microstructure-hardness correlations and clarifies the hardening model by addressing common misapplications of superposition in prior studies.

36 MATERIALS SCIENCE↗

Directed energy deposition of Haynes 282 nickel superalloy

Laser powder directed energy deposition was employed to fabricate Haynes® 282 Ni-based superalloy for high temperature creep testing. Material was heat treated using a single-step aging heat treatment of 800 °C for 4 h. Microstructural analysis was conducted in the as-deposited, solution-annealed, and age-hardened conditions. γ′ precipitates were absent in the as-deposited and annealed condition but formed during aging with an average size of 48.5 ± 12 nm. γ’ denuded zones ranging in thickness from 73 to 469 nm were observed adjacent to an effectively continuous grain boundary carbide film that covered 72.5% of the measured boundary length. The heat-treated material contained a high-volume fraction of TiC carbides ranging in size from 38 to 457 nm. Electron backscatter diffraction showed partial recrystallization, with 77-83% recrystallized area and a heterogeneous grain-size distribution. Creep testing at 750 °C at 300, 320, and 350 MPa revealed significantly inferior performance compared to wrought material, with higher strain rates, earlier tertiary onset, and shorter rupture lives. Fractography shows that failure was dominated by intergranular rupture. Post rupture microstructural analysis results suggest that the creep behavior was primarily governed by the non-equilibrium interface network rather than the bulk γ/γ’ matrix. In conclusion, the findings indicate that achieving wrought-like creep performance necessitates substantial improvements in the additive process, specifically focusing on enhanced homogenization, full recrystallization, and precise control over the morphology and distribution of carbides.

36 - MATERIALS SCIENCE↗

Characterization of Build Parameters and Microstructure in Low Heat Input WAAM of Ni-Based Superalloy Haynes 282

Ni-based superalloy Haynes® 282® is being targeted for various applications in advanced power generation systems for its superior fabricability, weldability, and excellent high temperature creep and corrosion performance. This process optimization study aims to use a low heat-input, high deposition rate, controlled Gas Metal Arc Welding (GMAW) process, Cold Metal Transfer (CMT) by Fronius, attempting to achieve fully dense fabrication and possibly avoid the need for HIP. Twenty-one multilayer blocks (~25x100x40 mm3) were deposited to explore a large set of build parameters variations that focused on varying the travel speed from 14 to 42 inches per minute (ipm) and wire feed speed from 150 to 450 ipm. A strong correlation has been observed between arc energy – controlled primarily by travel and wire feed speed. Initial visual inspection, internal microstructural examination, and computed tomography (CT) have been used to determine the effects of built parameters on evolution of internal porosity and defects. Scanning electron microscopy techniques enabled structural and compositional imaging of heterogeneity and changes in microstructural properties.

additive manufacturing↗

Machine Learning Vacancy Formation Energy in Nickel-Based Superalloys

Thermal vacancies play a critical role in high-temperature Ni-based superalloys and influence various properties such as creep resistance, oxidation, etc. This study systematically investigates the impact of commonly used transition metals (Cr, Co, Fe), refractory metals (Nb, Ta, Mo, W) and other elements (Al, Cu, Ti, Mn) on the thermodynamic stability of 36 binary, 20 ternary, 11 quaternary, 9 quinary, and 3 senary FCC Ni-based alloys covering various elemental combinations. Density functional theory-based studies on Ni-X binary alloys show that higher concentrations of Cr, Nb, Ta, Al, and Ti introduce significant lattice distortions and broaden the distribution of vacancy formation energies (standard deviation up to 0.15 eV). These elements partially donate electrons, reducing their self-consistent chemical potentials relative to single-element reference values and lowering vacancy formation energies, while Co, Fe, Mo, and W show lower charge localization. These trends extend from 3-6 element alloys, where Cr, Nb, and Ta-rich compositions have low-energy states (~0.5 eV) that increase vacancy concentrations. Finally, graph neural network models are developed to screen over 5000 virtual alloys. Eleven leading compositions are identified with mean vacancy formation energy higher than 1.75 eV and vacancy concentration ~2 orders of magnitude lower than pure Ni at 1000 K. These results provide valuable guidelines to achieve controlled defect engineering in structural alloys.

DFT↗

Elucidating the corrosion mechanism of Ni-based superalloys in the presence of uranium-containing chloride molten salt

The United States Department of Energy (DOE) is committed to the advancement of nuclear reactor technology through initiatives such as the Advanced Reactor Development Program (ARDP), in an effort to diversify the United States energy portfolio towards more sustainable energy options. The ARDP includes demonstration by industry partners of molten chloride fast reactors (MCFRs). Construction of MCFRs requires qualified nuclear structural materials. Unfortunately, there are no current materials that are fully qualified by the Nuclear Regulatory Commission for the construction of molten salt reactors, including MCFRs. Adapting current structural material qualifications requires expansion of our current knowledgebase on the property-performance relationships regarding corrosion performance. In this investigation, we assess microstructural changes in a Ni-based superalloy after exposure to a UCl3¬-containing chloride salt eutectic mixture through a correlated multi-modal approach combining several advanced characterization techniques, including scanning electron microscopy/focused ion beam (SEM/FIB) and transmission electron microscopy (TEM). SEM/FIB analysis will illustrate changes in elemental composition, microstructure, and isotopic information acquired from energy x-ray dispersive spectroscopy (EDS), electron backscatter diffraction (EBSD), and secondary ion mass spectroscopy (SIMS), respectively. This information will then aid in identifying localized regions to elucidate the corrosion mechanism with TEM through a combination of electron diffraction, electron energy loss spectroscopy (EELS), and additional EDS. The findings from this investigation will further expand our assessment of the corrosion performance of structural materials in molten salt chloride systems, aiding to developing fully qualified materials for construction of MCFRs.

36 MATERIALS SCIENCE↗

Micromechanical and fatigue in situ synchrotron characterization of an additively manufactured superalloy with porosity

Additive manufacturing (AM) has the potential to transform component production, but its widespread adoption is constrained by defects, such as pores, that compromise structural integrity. Here, this study investigates the influence of porosity on the micromechanical and fatigue response of AM Inconel 718 (IN718), a widely used aerospace superalloy. One baseline specimen with minimal stochastic porosity and another intentionally seeded with lack of fusion (LOF) pores were examined using high-energy X-ray diffraction microscopy (HEDM) and micro-computed tomography during cyclic loading. Fatigue cracks in the LOF specimen initiated more frequently and at lower cycle counts than in the baseline specimen. The number fraction of fatigue cracks that grew was comparatively higher in the LOF specimen. Grain-level metrics, including stress and diffraction spot widths, were quantified using far-field HEDM. Across the thousands of grains detected in both specimens, the pores in the LOF specimen increased the variability of stress and spot width evolution in the azimuthal direction, the latter serving as a surrogate measure of plastic deformation. However, no correlations emerged between these metrics and grain proximity to fatigue crack initiation sites or pores, underscoring the limitations of grain-averaged metrics for predicting fatigue. Nonetheless, the rich dataset reported here provides a foundation for future modeling efforts.

High-energy X-ray diffraction microscopy↗

Directed energy deposition of radially functionally graded nickel based superalloys IN625 and IN738: Microstructure and mechanical properties

This study investigates the microstructure and mechanical properties of radially functionally graded (RFG) materials fabricated from nickel-based superalloys IN625 and IN738 using directed energy deposition (DED). RFG cylindrical deposits with radial gradients of IN625-IN738 and IN738-IN625 were successfully fabricated and confirmed to be crack-free through tailored composition grading, scan strategy and process parameters that minimized thermal gradients and solidification velocities. Microstructural analysis revealed distinct variations across the gradient, characterized by differences in dendrite arm spacing, microsegregation, and the formation of distinct γ' precipitates and carbide/boride phases (MC, M 6 C, M 2 C, and MB 2 ) in as-deposited (AD) conditions, which evolved into M 23 C 6 and M 2 B upon subsequent heat treatment (HT). EBSD showed predominant columnar grains with a [100] texture, while microhardness profiles demonstrated consistent variation across the gradients. Mechanical testing highlighted the synergy of the graded structure, combining IN738's strength with IN625's ductility, resulting in enhanced properties such as a yield strength of 1131 MPa, ultimate tensile strength of 1382 MPa, and elongation of 12 % for HT IN625-IN738 grading. Numerical simulations employing CALPHAD thermodynamic calculations and finite element thermal modeling are used to establish phase evolution and microstructural feature correlation with thermal profiles, aiding in the optimization of process-structure-property relationship.

Additive manufacturing↗