Abstract
There is substantial lag in the development of atomic layer deposition (ALD) processes for nitrides compared to the high-quality, conformal oxides for which ALD has become the standard. A major factor in this disparity is the ready availability of highly reactive oxygen sources (mainly H2O, O2, and H2O2). High-energy nitrogen precursors are similarly required for the efficient incorporation of nitrogen in a film. Ammonia has often been used in conjunction with metal chlorides but requires relatively high temperatures for thermal ALD. Plasma-enhanced ALD can utilize molecular nitrogen as a precursor but can reduce film conformality on complex supports and damage the underlying substrate. Hydrazine (N2H4) is an alternative precursor which has been rarely explored for the fabrication of nitrides in ALD, but which is experiencing a surge in popularity due to its high reactivity, which enables the deposition of nitrides as-yet undemonstrated by ALD.(1) The added reactivity and volatility of liquid hydrazine may enable new reaction mechanisms, lower deposition temperatures, and conformality for high aspect ratio applications. Sn3N4 is a metastable semiconductor which shares a crystal structure with its analog, Si3N4; unlike Si3N4, Sn3N4 has only recently been grown by ALD,(2) being synthesized much more often through reactive sputtering.(3) As a binary, Sn3N4 has applications as a battery anode material, for photoelectrochemistry, and optoelectronic devices. We will report progress on the deposition of SnxNy films from tetrakis(dimethylamido) tin (TDMASn) and N2H4. Growth per cycle of this material (determined by x-ray reflectivity) is 0.4 A at 200 C, similar to the sole report of Sn3N4 from PE-ALD,(2) despite films being substantially Sn-rich. Identification of ALD growth window and self-limiting deposition characteristics are underway; initial testing indicates a competing chemical vapor deposition process which can be eliminated with adequate tuning of pulse/purge characteristics. A comparison of film conductivity and optical absorption at different growth temperatures will be presented. General issues of N2H4 purity and routes to prevent or control oxynitride formation will be discussed. (1) Du, L., et al. The First Atomic Layer Deposition Process for FexN Films. Chem. Comm., 2019, ASAP. DOI: 10.1039/C8CC10175B. (2) Stewart, D. M., et al. Tin Oxynitride Anodes by Atomic Layer Deposition for Solid-State Batteries. Chem. Mater. 2018, 30, 2526-34. (3) Caskey, C. M., et al. Semiconducting Properties of Spinel Tin Nitride and Other IV3N4 Polymorphs. J. Mater. Chem. C 2015, 3, 1389-96.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Greenaway, Ann, Shulda, Sarah, Link, Elisa M, Tamboli, Adele C, Christensen, Steven T. 2019-07-31. Tin Nitride Atomic Layer Deposition Using N2H4. https://searchnasa.com/record/osti%3A1547255/tin-nitride-atomic-layer-deposition-using-n2h4
Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Search NASA by Indiciae: BibTeX · RIS.