Particle size effects in metallic microparticle impact-bonding

Abstract

In cold spray processing of metals, the critical velocity for particle bonding is dependent on both intrinsic material properties, such as density and (spall) strength, and extrinsic process parameters, such as the powder particle size. Here, we specifically isolate and investigate particle size effects on the critical velocity for bonding through laser- induced single particle impact experiments and finite element simulations. We also present a predictive framework to correlate particle size and critical velocity. We show that an increase in particle size leads to an increase in the temperature of the jet formed at the interface of the particle and the substrate. This increased temperature locally decreases the spall strength of the material which, in turn, decreases the critical velocity for larger particles.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Dowding, Ian, Hassani, Mostafa, Sun, Yuchen, Veysset, David, Nelson, Keith A., Schuh, Christopher A.. 2020-05-10. Particle size effects in metallic microparticle impact-bonding. https://doi.org/10.1016/j.actamat.2020.04.044

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗