Search NASA⌕ Search

SEARCH · Search NASA

Results for “Grain microstructure evolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

The onset of alloying in Cu-Ni powders under high-shear consolidation

Friction consolidation (FC) is a solid phase processing methodology that densifies a material through high-shear deformation and pressure at elevated temperature. The method has garnered interest in the scientific community because of its ability to produce extremely refined and homogeneous microstructures, off-axis texture development, and improved material properties. This manuscript presents an investigation of Cu and Ni material mixing via evaluation of morphological evolution, grain boundary characterization, and compositional analysis to provide insights on the operational alloying mechanisms occurring under high shear and elevated temperature. Using correlative microscopy techniques, we show alloying progresses via a combination of grain boundary diffusion and interfacial roughening at heterophane boundaries. Evidence supporting Cu infiltration along Ni-Ni grain boundaries along with asymmetric diffusion of Cu into Ni grains is highlighted. The resultant, consolidated microstructure was produced directly from a powder compact in ~30 s and exhibited a submicron, equiaxed grain size.

36 MATERIALS SCIENCE↗

Discontinuous Precipitation in U-10 wt.%Mo Alloy: Reaction Kinetics, Effect of Prior gamma-UMo Microstructure, the Role of Grain-Boundary Misorientation, and the Effect of Ternary Alloying Addition

Eutectoid transformation in U-10 wt.% Mo (U10Mo) alloy initiates through discontinuous precipitation (DP) resulting in the formation of a lamellar microstructure that consists of an a-U and Mo-enriched bcc ?-UMo phase along the prior ?-UMo grain boundaries. DP is the main mode of transformation at 500°C. However, continuous precipitation (CP) of ?’ U2Mo phase together with grain-boundary DP is observed at 400°C. The reaction kinetics are noted to be very sluggish at 400°C compared to 500°C. The degree of eutectoid transformation is related to the prior ?-UMo grain size, and a smaller average grain size leads to a larger amount of transformation at a given reaction temperature. Minor addition (0.2 wt.%) of a third alloying element (Cr, Ni, Co) leads to significant changes in the nature of the DP mechanism in U10Mo alloy. In addition, high-angle grain boundaries with a misorientation of 30–45° are observed to be the major DP initiation sites. The microstructural evolution of U10Mo alloy with regard to DP-based reaction is discussed.

Jana, Saumyadeep↗

Development of Predictive Model for Accurate Rupture Time from Multi-Axial Creep in Alloy 709 with Physics-Based Simulations

A physics-based model is developed to predict multiaxial creep behavior in Alloy 709 (A709), an advanced austenitic stainless steel intended for high-temperature applications such as Sodium Fast Reactors (SFRs). Compared to conventional stainless steels like 316H, A709 offers superior high-temperature performance; however, comprehensive data on its multiaxial creep response remain limited. To address this gap, a crystal plasticity finite element (CPFE) framework is used to simulate the deformation and failure mechanisms of A709 under multiaxial loading conditions. The model incorporates an extended Hu-Cocks dislocation creep formulation that accounts for precipitation effects, along with the Sham–Needleman model to capture grain boundary cavitation-driven failure. These advanced constitutive models enable a detailed understanding of the interplay between microstructural evolution and macroscopic creep response. Furthermore, the study evaluates the predictive accuracy of various effective stress measures in estimating creep rupture life, leveraging simulated multiaxial creep data. The findings provide critical insights into the applicability of different stress measures for engineering design and life prediction of A709 components operating under complex loading conditions. This work contributes to improving the reliability of high-temperature structural components by advancing predictive modeling capabilities for advanced austenitic steels.

Alloy 709↗

Short communication on Kinetics of grain growth and particle pinning in U-10 wt.% Mo

Samples of a U-10Mo alloy was annealed at temperatures ranging from 700 °C to 900°C for periods lasting up to 24 hours. Annealed microstructures were examined using Electron Backscattered Diffraction (EBSD) to obtain average grain sizes and grain size distributions. From the temporal evolution of the average grain size, the activation energy of grain growth was determined to be 172.4 ± 0.961 kJ/mol. Grain growth over the annealing period stagnated after a period of 1 to 4 hours. This stagnation is apparently caused by the pinning effect of second-phase particles in the materials. In conclusion, back-scattered electron imaging (BSE) was used to confirm that these particles do not appreciably coarsen or dissolve during annealing at the aforementioned temperatures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of heterogeneous microstructure on the tensile and creep performances of cast Haynes 282 alloy

Precipitation-strengthened Ni-based superalloys are leading candidate materials for advanced ultra-supercritical (A-USC) plants with steam conditions up to 760 °C (1400 °F) and 35 MPa (5 ksi). This study evaluates representative specimens from a large casting of Haynes 282 to study the effect of microstructural heterogeneity on the mechanical behavior of this alloy. The tensile test results of cast Haynes 282 over the temperature range 20–816 °C exhibited lower tensile strength and ductility in comparison with the reference wrought Haynes 282. However, the creep rupture tests of the cast alloy below 704–788 °C and 190–431 MPa presented a similar stress-Larson-Miller parameter to that of the wrought material. Microstructural and dislocation characterizations using scanning electron microscopy, conventional transmission electron microscopy, and scanning transmission electron microscopy in conjunction with energy dispersive X-ray spectroscopy were performed to understand the microstructural evolution before and after the mechanical tests. The heterogeneous microstructures of the cast Haynes 282 material, including the coarse grains, potential casting defects, and a bimodal size distribution of γ' precipitates, were detrimental to the tensile behavior, whereas the coarse-scale grains had a positive effect on the creep performance because diffusional creep was the dominant creep mechanism.

tensile testing↗

Linking microstructure to creep behavior in vertically and horizontally built LPBF Haynes 282 compared with wrought material via θ -projection

Laser Powder Bed Fusion (LPBF) has emerged as a promising route for fabricating intricate geometries in high-performance alloys. Haynes 282 (H282) is a strong candidate for applications such as heat exchangers or engines due to its excellent creep strength and thermal stability; however, the long-term creep behavior of LPBF-processed H282 remains poorly understood. In this study, the θ -projection method is used to analyze and extrapolate the creep behavior of vertically built LPBF, horizontally built LPBF, compared to wrought H282 tested at 816 °C. Vertically built LPBF H282 exhibits the lowest minimum creep rate (MCR), while the horizontally built condition shows a higher MCR comparable to that of wrought H282. Despite these differences, both LPBF conditions exhibit significantly shorter rupture life and reduced rupture strain than the wrought material, with the most severe degradation observed in the horizontal builds, consistent with an earlier onset of tertiary creep and accelerated strain-rate evolution. Microstructural characterization reveals that both LPBF and wrought H282 exhibit abundant twin-related boundary character; however, their grain boundary topologies differ markedly. The wrought alloy contains a higher fraction of low-angle grain boundaries and continuous twin lamellae, whereas the LPBF microstructure is characterized by a suppressed low-angle boundary population and fragmented twin-related boundaries embedded within irregular high-angle grain boundary networks. Fractographic analysis further reveals predominantly intergranular cracking in LPBF H282, accompanied by grain-boundary-decorated carbides, Al 2 O 3 inclusions, and high-aspect-ratio pores. These results demonstrate that grain boundary topology, rather than minimum creep rate alone, plays a critical role in governing creep damage accumulation and rupture behavior in LPBF and wrought H282.

Creep↗

Exascale-capable cellular automaton for nucleation and grain growth

This model is a cellular automata-based algorithm used to predict grain-scale microstructure development. Nucleation and growth of existing grains are considered in an initially liquid domain, where the temperature field evolution is either driven through heat transport simulation data or a frozen temperature approximation (i.e., a constant cooling rate and a fixed thermal gradient). The growth of grains is based on the decentered octahedron algorithm published by Gandin and Rappaz (https://doi.org/10.1016/S1359-6454(96)00303-5), where the grain envelopes are tracked as approximations of the evolving dendritic growth front. The input heat transport data, which can come from simulation of an arbitrary processing technique, consists of coordinates and times at which said coordinates fall below the liquidus and solidus temperatures for the final time. As a result, only the final solidification of a given region is modeled (no remelting). The code is designed to be compatible with pre-Exascale architectures, and uses MPI and the Kokkos library to decompose the computational domain and offload solidification calculations to GPUs.

Rolchigo, MatthewR.↗

Microstructure stability of ultra-fine grained magnesium alloy AZ31 processed by extrusion and equal-channel angular pressing (EX–ECAP)

Thermal stability of the ultra-fine grained (UFG) microstructure of magnesium AZ31 alloy was investigated. UFG microstructure was achieved by a combined two-step severe plastic deformation process: the extrusion (EX) and subsequent equal-channel angular pressing (ECAP). This combined process leads to refined microstructure and enhanced microhardness. Specimens with UFG microstructure were annealed isochronally at temperatures 150–500 °C for 1 h. The evolution of microstructure, mechanical properties and dislocation density was studied by electron backscatter diffraction (EBSD), microhardness measurements and positron annihilation spectroscopy (PAS). The coarsening of the fine-grained structure at higher temperatures was accompanied by a gradual decrease of the microhardness and decrease of dislocation density. Mechanism of grain growth was studied by general equation for grain growth and Arrhenius equation. Activation energies for grain growth were calculated to be 115, 33 and 164 kJ/mol in temperature ranges of 170–210 °C, 210–400 °C and 400–500 °C (443–483 K, 483–673 K and 673–773 K), respectively. - Highlights: • Microhardness of UFG AZ31 alloy decreases with increasing annealing temperature. • This fact has two reasons: dislocation annihilations and/or grain growth. • The activation energies for grain growth were calculated for all temperature ranges.

36 MATERIALS SCIENCE↗

NSUF Report EBSD analyses on metallic fuel samples: Tips and improvements in sample preparation

EBSD (Electron Backscatter Diffraction) is an analytic technique used to evaluate the microstructure of a specimen. It can be used to evaluate interesting crystallographic data ranging from grains size to grain orientation, from grain boundaries to stresses. Moreover, in the field of nuclear materials EBSD can aid in estimating properties important for reactor performance, such as dislocation and residual strain [1]. EBSD patterns are generated by focusing a stationary electron gun on the specimen and detecting the backscatter electrons that satisfy Bragg conditions, and thus are diffracted by the crystal planes forming the so called Kikuchi bands. These bands correspond to each of the lattice diffracting crystal planes and are detected on a phosphor screen via a low-light CCD camera [2]. The patterns are generated within a small interaction volume located at a depth of less than 50-100 nm. Because of this, the data quality is extremely sensitive to the integrity of the crystallographic lattice order at the surface of the sample and thus to sample preparation and to oxidation [3]. While conventional sample preparation methods are widely used in materials science, they often do not lead to quality electron backscatter patterns needed for the characterization of nuclear materials [4]. This has been related by many authors to the challenges associated with handling radiological specimens, their rapid oxidation, and artifacts in such samples (e.g. high number of defects, precipitates and/or porosities) [4-8]. EBSD, however, can be an invaluable technique to evaluate microstructural evolution during fabrication and after irradiation at the required mesoscale for model and simulation. It also provides important information on grain structure necessary to understand irradiation effect, such as grain subdivision. Thus, it is of paramount importance to further the application of this technique to nuclear materials and especially irradiated fuels.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

4D Observations of the initiation of abnormal grain growth in commercially pure Ni

Abnormal grain growth (AGG), where a small fraction of grains grow faster than others, is critical to predict because it can significantly impact material properties. However, the mechanism behind AGG remains unclear. In this study, laboratory-based x-ray diffraction contrast tomography (LabDCT) is employed to non-destructively track the 3D microstructural evolution of high-purity nickel during the onset of AGG at 800 °C. The initial microstructure state is used to test hypothesized microstructure predictors of the initiation of AGG. The change in grain size was not related to the initial grain size or normalized integral mean curvature. Additionally, the grain boundary energy distributions of abnormal grains were indistinguishable from those of control groups exhibiting normal grain growth. However, the grains that later became abnormal exhibit large areas of asymmetric tilt boundaries that were previously found to be fast. This 3D microstructure dataset is useful to investigate new hypotheses for the initiation of AGG.

36 MATERIALS SCIENCE↗

Effect of Zener–Holloman Parameter on the Prior Austenite Grain size in a 12Cr-10Ni Precipitation-Hardenable Stainless Steel

Hot isothermal plane strain compression (PSC) tests were carried out on a 12Cr-10Ni martensitic precipitation-hardenable (PH) stainless steel, in the temperature range of 750-1050 °C, to study microstructural evolution during large strain deformation. The nature of stress–strain curves varies with Zener–Holloman parameter (Z) with specimens deformed at high Z showing steady-state behavior and those deformed at lower Z showing flow softening. Prior austenite grain size (PAGS), d, exhibited a strong correlation to Z showing a bilinear behavior represented as: d = (1803.9)Z{sup −0.094} for high Z deformation and d = (1456.2)Z{sup −0.058} for low Z deformation. Based on the above study, it is recommended to thermomechanically process 12Cr-10Ni steel at Z ≥ 10{sup 22} for obtaining products with good strength–toughness balance.

36 MATERIALS SCIENCE↗

Polycrystal Plasticity: Comparison Between Grain - Scale Observations of Deformation and Simulations

Here, the response of polycrystals to plastic deformation is studied at the level of variations within individual grains, and comparisons are made to theoretical calculations using crystal plasticity (CP). We provide a brief overview of CP and a review of the literature, which is dominated by surface observations. The motivating question asks how well does CP represent the mesoscale behavior of large populations of dislocations (as carriers of plastic strain). The literature shows consistently that only moderate agreement is found between experiment and calculation. We supplement this with a current example of microstructure evolution in the interior of a copper sample subjected to tensile deformation. Nondestructive measurements of orientation fields were performed using the near-field high-energy X-ray diffraction microscopy (nf-HEDM) technique at the Advanced Photon Source (APS). Starting at highly ordered grains, a single two-dimensional slice of microstructure containing ~150 grains was followed through multiple strain states, where it tracked lattice rotations and defect accumulation of up to 14% elongation. In accord with the literature, at the scale of individual grains, comparison of observations with CP models indicates reasonable qualitative agreement but significant variations between simulation and experiment are apparent. The conclusion is that in order to be able to quantify the effects of microstructure on the distributions of slip, orientation change, and damage accumulation, the empirically derived constitutive relations used in continuum-scale simulations need to be improved. Equally important will be the development of large-scale simulations of polycrystals that directly model dislocations.

36 MATERIALS SCIENCE↗

Deep operator network surrogate for phase-field modeling of metal grain growth during solidification

A deep operator network (DeepONet) has been constructed that generates accurate representations of phase-field model simulations for evolving two dimensional metal grain morphology growing from melt. These representations serve as lower resolution, computationally efficient stand-ins for quick parameter space exploration of solutions to the the Allen-Cahn equations that dictate the phase-field model simulations. The experimental target for the phase-field model is a uranium casting system cooling a 434 g uranium charge from a maximum temperature of 1400° C at an average rate of 30° C / min , traversing the crystallographic phases of the pure metal. Experimental parameters inform the phase-field model, whose higher resolution computational model solutions are used to train the DeepONet in a given parameter space with the aim of developing a faster, more efficient method for predicting the solidifying metal's microstructure at different potential experimental values. The final DeepONet generates high accuracy, lower resolution predictions with cumulative relative approximation error over all timesteps of less than 0.5%, while ensuring solutions remain within physically feasible ranges. Further, these relative error values are comparable with other state-of-the-art DeepONet models for microstructure evolution, while significantly reducing the amount of training data required. Training a convolutional neural network simultaneously with the DeepONet, enforcing realistic values at the complex metal grain boundaries, and mathematically encoding boundary conditions into the structure of the DeepONet improved prediction accuracy and computational efficiency over a standard DeepONet model.

36 MATERIALS SCIENCE↗

Magnetization reversal mechanism of Nd-Fe-B films with perpendicular magnetic anisotropy

The microstructure and magnetic properties of Nd-Fe-B films with thicknesses from 100 nm to 3 nm have been investigated. All the films show excellent perpendicular magnetic anisotropy with a squareness ratio of 1 in the perpendicular direction and almost zero coercivity in the in-plane direction. Of particular interest is that the initial magnetization curves sensitively depended on the film thickness. Films thicker than 15 nm show steep initial magnetization curve. Although the films have coercivities larger than 21 kOe, the films can be fully magnetized from the thermally demagnetized state with a field as small as 5 kOe. With the decrease of film thickness to 5 nm, the initial magnetization curve becomes flat. The evolution of initial magnetization curves with film thickness can be understood by the microstructure of the films. Films with thickness of 15 nm show close-packed grains without any intergranular phases. Such microstructures lead to steep initial magnetization curves. On the other hand, when the film thickness decreased to 3 nm, the film thickness became nonuniform. Such microstructure leads to flat initial magnetization curves.

36 MATERIALS SCIENCE↗

Mechanical Properties of the Mg-Gd-Y-Zn-Zr Alloys with Different Morphologies of Long-Period Stacking Ordered Phases

Long-period stacking ordered (LPSO) phases with different morphologies and distributions were obtained in the direct chill cast Mg-6.9Gd-3.2Y-1.5Zn-0.5Zr (wt.%) alloy by controlling the homogenization time or cooling rate. Microstructural evolution and the effect of various LPSO phases on the mechanical properties were investigated. There is no obvious α-Mg grain growth during homogenization at 510 °C. Intragranular thin-platelet and coagulated LPSO phases hardly improve the strength but help to develop the ductility. Numerous lamellar phases, which contain “ABCA”-type building blocks with RE and Zn segregation, form during the furnace-cooling process. Lamellar phases, which exhibit lower thermostability compared with the thin-platelet LPSO, slightly improve the tensile yield strength and induce numerous cracks which result in the premature fracture.

36 MATERIALS SCIENCE↗

Scaling laws and stability of nano-sized defect clusters in niobium via atomistic simulations and statistical analysis

The predictions of scaling laws for the structure and properties of defect clusters are generally limited to small defect clusters in their ground-state configurations. We investigated the size and geometrical configuration dependence of nano-sized defect clusters in niobium (Nb) using molecular dynamics. We studied the structure and stability of large clusters of size up to fifty defects for vacancies and one hundred defects for interstitials, as well as the role of helium and metastable configurations on the stability of these clusters. We compared three different interatomic potentials in order to determine the relative stability of these clusters as a function of their size and geometrical configurations. Additionally, we conducted a statistical analysis to predict the formation and binding energies of interstitial clusters as a function of both their size and configuration. We find that the size dependence of vacancy and interstitial clusters can be approximated by functional forms that account for bulk and surface effects as well as some considerations of elastic interactions. We also find that helium and metastable configurations can make vacancy and interstitial clusters thermally stable depending on the configuration. Our parameterized functional forms for the formation and binding energies are valid for a very broad range of defect sizes and configurations making it possible to be used directly in a coarse-grained modeling strategy such as Monte Carlo, cluster dynamics or dislocation dynamics which look at defect accumulation and evolution in microstructures.

36 MATERIALS SCIENCE↗

Deformation textures of aluminum in a multilayered Ti/Al/Nb composite severely deformed by accumulative roll bonding

The accumulative roll bonding process was carried out to produce multilayered Ti/Al/Nb composites up to four cycles. Scanning electron microscopy, transmission electron microscopy electron backscattered diffraction and nanoindentation were employed to investigate the microstructural and texture evolution. A homogenous distribution of Ti/Nb necking layers in Al matrix was achieved after four ARB cycles. Grain refinement was observed to increase with increasing number of ARB cycles. The fraction of high-angle grain boundaries as also increased. Strong recrystallization texture appeared for high number of ARB cycles due to the adiabatic heat that occurs during ARB processing. The shear band at the Ti/Al interface reduced the intensity of the cold rolling fiber textures of Al. There was no evidence of shear component from the orientation distribution function results.

36 MATERIALS SCIENCE↗

Time at Temperature Abstract and Intern Poster

Current NRC regulations for BWR operations dictate that any occurrence reaching the point of Departure from Nucleate Boiling (DNB) disqualifies the use of the fuel rod for further reactor operation. That criteria does not account for duration of rate of the power increase, the corresponding effects on material properties or rewetting that may occur. Previous Anticipated Operational Occurrences (AOOs) show short durations power increase that may require limited amounts of heat removal. Industrial experience has shown evidence that fuel can reach dryout yet continue to safely operate in regular reactor conditions. The gap in research into such occurrences is the motivation for a series of experiments, including this current work. Time-at-Temperature experiments aim to identify and characterize the microstructural changes in Zircaloy-2 under oxygen-free high temperatures. This work uses the FlashDSC instrument to rapidly ramp up and down the temperature of a focus ion beam (FIB) prepared large area lift-out (LALO) of Zircaloy-2 at a rate of 10,000 K/s to desired values. The focus is to characterize the microstructure evolution, if any, of Zircaloy-2 that may impact its performance under typical BWR conditions. This characterization includes analyzing grain structure and size, secondary phase particle (SPPs) size, shape, composition, and location using Transmission Electron Microscopy (TEM). Further data collection and analysis is in progress including diffraction pattern indexing and 4D STEM processing. While current results focus on the testing and characterizing unirradiated material, future plans include expansion to irradiated material to explore the effects of rapid transition rates seen in DNB and dryout conditions on irradiationg damage and defect annealing.

36 - MATERIALS SCIENCE↗