Heterogeneous doping via nanoscale coating impacts the mechanics of Li intrusion in brittle solid electrolytes

Lithium dendrite intrusion in solid-state batteries limits fast charging and causes short-circuiting, yet the underlying regulating mechanisms are not well-understood. Here, in this work, we discover that heterogeneous Ag + doping dramatically affects lithium intrusion into Li 6.6 La 3 Zr 1.6 Ta 0.4 O 12 (LLZO), a brittle solid electrolyte. Nanoscale Ag + doping is achieved by thermally annealing a 3-nm-thick metallic coating on LLZO, inducing Ag–Li ion exchange and Ag diffusion into grains and grain boundaries. Density functional theory calculations and experimental characterization show negligible impact on the electronic properties and surface wettability from Ag + incorporation. Mechanically, nanoindentation experiments show a fivefold increase in the mechanical force required to fracture the surface Ag + -doped LLZO, indicating substantial doping-induced surface toughening. Operando microprobe scanning electron microscopy experiments show that the Ag + -doped LLZO surface exhibits improved lithium plating at >250 mA cm −2 and an electroplating diameter that is expanded by over fourfold, even under an extreme indentation stress of 3 GPa. This demonstrates enhanced defect tolerance in LLZO, rather than electronic or adhesion effects. Our study reveals a chemo-mechanical mechanism via surface heterogeneous doping, complementing present bulk design rules to minimize mechanical failures in solid-state batteries.

36 MATERIALS SCIENCE↗

Effects of Al concentration on the structure and conductivity of lithium lanthanum zirconium oxide

Cubic Li 7-3x Al x La 3 Zr 2 O 12 (LLZO) is a promising, next-generation solid electrolyte due to its stability with Li-metal and high bulk conductivity (~1 mS cm -1 ). However, the source of the high conductivity is not completely understood. In this work, we address this key knowledge gap through the integration of elemental analysis, neutron diffraction sensitive to Li and O atoms, and impedance spectroscopy to understand the structure–property correlations for LLZO. We show the metal–oxygen framework structure remains constant with variation in Al substitution, resulting in a constant activation energy of ~0.35 eV and little effect on the bulk conductivity. Instead, Li concentration, Al blocking and trapping of mobile defects, and Li–Li nearest neighbor interactions largely control the Al substituted LLZO bulk conductivity, resulting in decreases from 0.73 to 0.22 mS cm -1 as the Al concentration increases from 0.17 to 0.32 mol. These results differ from those of Ta substituted LLZO, where the framework structure and Li–Li site distances play large roles in controlling the conductivity. The increased understanding of the controlling factors of conductivity allows for greater ability to tailor the design of and substitution into the LLZO structure for improved conductivity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electro-Chemo-Mechanical Evolution at the Garnet Solid Electrolyte–Cathode Interface

Solid-state batteries promise higher energy density and improved safety compared with lithium-ion batteries. However, electro-chemomechanical instabilities at the solid electrolyte interface with the cathode and the anode hinder their large scale implementation. Here, in this study, we focus on resolving electro-chemo-mechanical instability mechanisms and their onset conditions between a state-of-the-art cathode, LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622), and the garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte. We used thin-film NMC622 on LLZO pellets to place the interfacial region within the detection depth of the X-ray characterization techniques. The experimental probes of the near-interface region included in operando X-ray absorption spectroscopy and ex situ focused ion beam scanning electron microscopy. Electrochemical degradation was not observable during cycling at room temperature with 4.3 V versus Li/Li + charge voltage cutoff, or with stepwise potentiostatic hold up to 4.1 V versus Li/Li + . In contrast, secondary phases including reduced transition metal species (Ni 2+ , Co 2+ ) were found after cycling up to 4.3 V versus Li/Li + at 80 °C and during potentiostatic hold at 4.3 V versus Li/Li + (Ni 2+ ). Intergranular cracks between NMC622 grains and delamination at the NMC622|LLZO interface occurred readily after the first charge. These interface reaction products and mechanical failure lowered the capacity and cell efficiency due to partial loss of the NMC622 phase, partial loss of contact at the interface, and a higher polarization resistance. Electrochemical instability between delithiated NMC622 and LLZO could be mitigated by using a low charge voltage cutoff or cycling at lower temperature. Ways to engineer the mechanical properties to avoid crack deflection and delamination at the interface are also discussed for enhancing mechanical stability.

36 MATERIALS SCIENCE↗

The Key Role of Grain Boundary Dynamics in Revolutionizing the Potential of Solid Electrolytes

Solid electrolytes (SEs) have the potential to enhance the safety and performance of Li-metal batteries. However, the existence of grain boundaries in polycrystalline SEs presents a significant challenge for both ionic and electronic migration, promoting the propagation of detrimental lithium dendrites. This study compares the roles of grain boundaries in electrical properties of three distinct SEs including garnet-type Li 6.5 La 3 Zr 1.5 Ta 0.5 O 12 (LLZO), argyrodite-type Li 6 PS 5 Cl (LPSC), and NASICON-type Li 1+x+y Al x (Ti,Ge) 2-x Si y P 3-y O 12 (LATP). Results demonstrate that the electronic and ionic conductivities of solid-state electrolytes are affected differently by grain boundaries, depending on the specific type of electrolyte. For instance, LLZO and LATP experience dielectric breakdown at 3.7 and 5.3 V, respectively, while LPSC does not exhibit such behavior. Here, a new chemical modification is proposed that simultaneously alters the composition of both the surface and grain boundaries of SEs, ultimately reducing electronic conductivity for the LLZO SEs. Consequently, the proposed LLZO exhibits unprecedented dendrite-free cycling stability, achieving a remarkable 12 000-h lifetime at room temperature, surpassing conventional strategies such as surface coatings in dendrite mitigation. This study highlights the significance of modifying grain boundaries to design safe and durable Li-metal batteries. It provides new insights for developing SEs that are highly resistant to dendrite formation.

36 MATERIALS SCIENCE↗

Particle‐Size‐Dependent Lithium‐Ion Transport in PEO/LLZO Composite Electrolytes

Lithium-metal batteries with solid electrolytes can deliver higher energy density and improved safety than conventional Li-ion batteries. Among solid electrolyte candidates, polymer/ceramic composite electrolytes are attractive because they combine polymer flexibility with the high ionic conductivity of ceramics. However, whether ceramic fillers synergistically reduce polarization losses in the polymer matrix remains unclear. A central unknown is the critical polymer/ceramic interfacial resistance (Rint,crit), below which adding ceramics lowers electrolyte overpotential. Here, we present the first macroscale model framework to quantify R int,crit for composite electrolytes based on polyethylene oxide (PEO) and Ta-doped Li 7 La 3 Zr 2 O 12 (LLZO). A 1D model for DC-polarization of tri-layer cells (PEO-LiTFSI/LLZO/PEO-LiTFSI) shows that LLZO surface functionalization reduces the PEO/LLZO interfacial resistance, consistent with electrochemical impedance measurements. Extending to a 2D composite model, we show notably that Rint,crit scales linearly with LLZO particle diameter and shifts toward experimentally accessible values (e.g., 28.8 Ωcm 2 ) as particle size increases. At fixed ceramic volume fraction, larger LLZO particles reduce the number of interfacial crossings, driving more current through the ceramic phase and lowering concentration polarization. In contrast, R int,crit is largely independent of ceramic volume fraction. These results demonstrate that ceramic filler-size engineering can enable synergistic, energy-efficient transport in polymer/ceramic composite electrolytes.

25 ENERGY STORAGE↗

Probing degradation at solid-state battery interfaces using machine-learning interatomic potential

Solid-state batteries featuring fast ion-conducting solid electrolytes are promising next-generation energy storage technologies, yet challenges remain for practical deployment due to electro-chemo-mechanical instabilities at solid-solid interfaces. These interfaces, which include homogeneous/internal interfaces such as grain boundaries (GBs) and heterogeneous/external interfaces between solid-electrolyte and electrode materials, can impede Li-ion transport, deteriorate performance, and eventually lead to cell failure. Here, in this study, we leverage large-scale molecular simulations, enabled by validated machine-learning interatomic potentials, to directly probe the onset of interfacial degradation at the garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid-electrolyte/LiCoO 2 (LCO) cathode interface. By surveying different interfacial geometries and compositions, it is found that Li-deficient interfaces can lead to severe interfacial disordering with cation mixing and Co interdiffusion from LCO into LLZO. By contrast, Li-sufficient interfaces are less disordered, although elemental segregation with local ordering is observed. As a consequence of Co interdiffusion, Co-rich regions are formed at the GBs of LLZO due to cation segregation and trapping effects. This behavior is independent of the GB tilting axis, degree of disorder at the GBs, and Co concentration, which implies Co clustering at GBs is a general phenomenon in polycrystalline LLZO and can dictate its overall transport and mechanical properties. Our findings elucidate the underlying fundamental mechanisms that give rise to experimentally observed physicochemical properties and provide guidelines for interface design that can mitigate interfacial degradation and improve cycling performance.

25 ENERGY STORAGE↗

High Sulfur Loading and Capacity Retention in Bilayer Garnet Sulfurized‐Polyacrylonitrile/Lithium‐Metal Batteries with Gel Polymer Electrolytes

The cubic‐garnet (Li 7 La 3 Zr 2 O 12 , LLZO) lithium–sulfur battery shows great promise in the pursuit of achieving high energy densities. The sulfur used in the cathodes is abundant, inexpensive, and possesses high specific capacity. In addition, LLZO displays excellent chemical stability with Li metal; however, the instabilities in the sulfur cathode/LLZO interface can lead to performance degradation that limits the development of these batteries. Therefore, it is critical to resolve these interfacial challenges to achieve stable cycling. Here, an innovative gel polymer buffer layer to stabilize the sulfur cathode/LLZO interface is created. Employing a thin bilayer LLZO (dense/porous) architecture as a solid electrolyte and significantly high sulfur loading of 5.2 mg cm −2 , stable cycling is achieved with a high initial discharge capacity of 1542 mAh g −1 (discharge current density of 0.87 mA cm −2 ) and an average discharge capacity of 1218 mAh g −1 (discharge current density of 1.74 mA cm −2 ) with 80% capacity retention over 265 cycles, at room temperature (22 °C) and without applied pressure. Achieving such stability with high sulfur loading is a major step in the development of potentially commercial garnet lithium–sulfur batteries.

25 ENERGY STORAGE↗

Irreversible Multielement Diffusion and the Resulting Compositional and Processing Flexibility in the Synthesis and Densification of Lithium Aluminum Lanthanum Zirconium Oxide

Despite the broad interest in Al-doped lithium lanthanum zirconium oxide (LLZO), the wide range of reported ionic conductivities suggests that the effect of processing parameters on the resulting phase purity and bulk conductivity is not well-understood. Here, in this work, we synthesized six separate series of LLZO with variations in Al concentration, Li excess, Li addition order, Li source, densification method, and mother powder to determine the effect on the composition, phase purity, density, and bulk conductivity. We found that a wider range of compositions (6.08–7.61 mol of Li and 0.06–0.23 mol of Al) than previously reported can result in cubic phase stability and that nearly all elements (Li, Al, Zr, and La) are lost to the MgO crucible during calcination and sintering. The manner in which different elements are lost is affected by the processing parameters. We observed that Al-doped LLZO shows great compositional flexibility in stabilizing the cubic phase, offering an explanation for the range of electrochemical performance metrics reported in the literature.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mapping of fracture and ionic conductivity changes in ion implanted solid electrolytes: Insights from molecular dynamics

Ion implantation emerges as a promising technique to address the persistent challenge of lithium (Li) filament growth in solid-state electrolytes as it can induce compressive stresses inhibiting crack growth and deflect dendrites, de facto mitigating early electrolyte failure. In this study, we examine the potential paradox of ion implantation: while aiming to enhance electrolyte performance, the radiation damage associated with implantation might inadvertently compromise both the ionic conductivity and the intrinsic fracture toughness of the material, rendering the material unsuitable for battery applications. Specifically, we employed molecular dynamics simulations to examine the scope of the downsides of ion implantation, specifically: (i) reduced ionic conductivity (due to radiation-induced amorphization) and (ii) mechanical stability (due to radiation-induced embrittlement) in ion-implanted Li 7 La 3 Zr 2 O 12 (LLZO) solid-state electrolytes. We explore how radiation damage impacts LLZO’s crystalline structure, Li-ion diffusion, and fracture properties at various temperatures and radiation damage levels. The study aims to provide insights into the competing effects of ion implantation and suggest potential engineering strategies for developing more robust solid-state electrolytes with improved conductivity and dendrite resistance.

Conductivity↗

Radiation Damage Mechanisms in Oxide-Based Solid Electrolytes

Ion implantation is a promising approach to mitigate dendrite formation in metal anode solid-state batteries by modifying the chemical and mechanical properties of oxide-based electrolyte surfaces such as Li 7 La 3 Zr 2 O 12 (LLZO). Yet, the detailed atomistic mechanisms and potentially adverse side effects of ion implantation remain poorly understood. In this study, we used molecular dynamics simulations to elucidate the evolution of radiation-induced damage in LLZO. The results reveal that radiation damage is primarily driven by recoils from heavy ions in the lattice, producing antisite defect clusters whose density decreases as recoil energy increases, a counterintuitive finding that highlights complex cascade fragmentation. Radiation-induced disruption to the crystal sublattice connectivity, especially in the La–O network critical for Li-ion transport, leads to degradation in ionic pathways at low energies, while higher energy cascades can form new conduction pathways via enhanced Zr–O network connectivity. These findings provide a mechanistic foundation for optimizing ion implantation strategies that balance disruption of the lattice for surface modification for dendrite resistance with preservation of essential ionic conductivity.

Defects↗

Digital light processing of porous LLZTO scaffolds for Li-garnet solid-state batteries

Li 7 La 3 Zr 2 O 12 (LLZO)-based solid-state electrolytes (SEs) are promising materials for next-generation solid-state batteries. In this work, digital light processing (DLP), an emerging additive manufacturing technology, is employed to produce porous Ta-doped LLZO (LLZTO) scaffolds. The self-standing scaffolds are 100 μm thick and have 40% porosity. The scaffolds demonstrate symmetric cell cycling stability exceeding 1,500 h at 0.1 mA/cm2 current density, with a capacity of 0.1 mAh/cm 2 (1 h for each half cycle). At higher current densities, reversible soft shorts frequently happen, while immediate hard shorts are prevented due to Li dendrite growth being hindered by the tortuous pore network. In addition to the cycling stability, the phase stability of LLZTO is investigated during the post-printing thermal process for printing resin removal. We discovered that the LLZTO partially decomposes into Li 2 Zr 2 O 7 and other impurity phases from 400°C to 800°C, but the pure LLZTO phase is restored upon the completion of resin removal beyond 800°C.

Li-metal anode↗

Effect of H + Exchange and Surface Impurities on Bulk and Interfacial Electrochemistry of Garnet Solid Electrolytes

Contact loss and current constriction pose significant challenges at the Li metal interface of solid-state batteries. For garnet-structured Li 7 La 3 Zr 2 O 12 (LLZO), these effects are amplified by Li + /H + exchange and surface contamination reactions, which lead to conductivity losses and poor Li wetting. In this study, we utilize a variety of surface treatment processes across 37 cells to selectively induce proton exchange and contamination reactions in LLZO. The resulting bulk and surface chemistry is systematically characterized and correlated to changes in electrochemical properties. Additionally, we combine impedance analysis and finite element method modeling to deconvolute sources of impedance contributions at the Li metal interface. Specifically, we show that constriction impedance at the Li metal interface arises not solely from voids, but also from ionically-resistive surface contaminants. Further, these findings emphasize the connection between ionic conductivity and constriction, demonstrating that micron-scale ionically-resistive components increase constriction even with identical contact geometries. Finally, we leverage our comprehensive dataset to highlight unstable overpotential growth as a failure mechanism, additionally showing that the phase of a cell’s impedance is a sensitive indicator for the onset of interfacial instability. Overall, this study clarifies the impacts of proton exchange and surface contamination on electrochemical properties at the Li|solid electrolyte interface and elucidates insights that are generalizable to other solid-state battery systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Identifying Bounds of Inorganic Content in Solventless Processing of Hybrid Solid Electrolytes

Solid-state lithium batteries require safe, robust electrolytes to enable higher energy densities and improved safety over conventional cells. Hybrid polymer–ceramic electrolytes are a promising solution, combining the processability of polymers with the high ionic conductivity and mechanical strength of inorganic fillers. In this work, we demonstrate a solventless, UV-curing method to produce hybrid solid electrolytes using a poly(ethylene glycol) dimethyl ether (PEGDME)-based photocurable matrix incorporating Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 (LAGP) or Li 7 La 3 Zr 2 O 12 (LLZO) ceramic electrolyte. Inorganic filler loadings up to ∼55 wt.% could be successfully incorporated via this process which was the highest inorganic content at which the slurry remains processable and cured into a uniform film. The resulting UV-cured composite electrolytes remain flexible and exhibit room-temperature ionic conductivities on the order of 10 −4 S·cm −1 , along with notably improved lithium-ion transference numbers compared to conventional polymer electrolytes. Similar performance and processing limits were observed for both LAGP and LLZO, indicating that ceramic filler chemistry does not significantly affect the UV-curing process or the electrolyte's ion transport properties in this regime. Eliminating solvents from fabrication not only simplifies processing and mitigates environmental concerns but also enables higher solid contents that enhance mechanical strength and help suppress lithium dendrite formation. In conclusion, this scalable approach thus paves the way for manufacturing robust composite solid electrolytes for next-generation solid-state batteries (SSBs).

Batteries↗

Lithium Dendrite-Free Li 7 N 2 I-LiOH Solid Electrolytes for High Energy Lithium Batteries

All-solid-state lithium batteries (ASSLBs) hold great potential to improve the safety and energy density of today’s lithium-ion batteries by using non-flammable inorganic solid electrolytes. Solid electrolytes (SEs) are believed to prevent Li dendrite growth because of high mechanical strength and high Li+ transference numbers. Significant advances in SE have been achieved, among which, Li7La3Zr2O12 (LLZO) and Li2S–P2S5 (LPS) are the most promising SEs for bulk-type solid-state lithium batteries because of high ionic conductivities (>10-4 S/cm2). However, in contrast to our expectations, the growth of lithium dendrites is not suppressed but is facilitated in LLZOs and LPSs regardless of dopants, porosity, and crystallinity of the electrolytes. Despite the unity Li transference number and over two-times of shear modulus than that of Li metal, the critical current densities for Li plating and stripping in these SEs are less than 1.0 mA cm-2, which is one-fourth to one-tenth of that in liquid electrolytes at room temperature. The incompatibility between LLZO and LPS with Li metal seriously limits the energy density of all-solid-state batteries. The mechanism for lithium dendrite formation and growth in SEs are still disputable. Lack of understanding of the Li dendrite formation mechanism seriously impeded the development of solid-state lithium batteries. The development of the criterion for Li dendrite suppression is essential for the success of solid electrolyte lithium batteries. In this project, a criterion for Li dendrite suppression will be developed through thermodynamics and kinetics analysis of lithium dendrite nucleation/growth, which will guide the solid-state electrolyte design. Li7N2I-LiOH, Li5NI2-LiOH and Li3YCl6 solid electrolyte with high ionic conductivity and low electronic conductivity were used to validate the criterion for lithium dendrite suppression. Different surface modifications were also explored to enhance the dendrite suppression capability of SSEs.

25 ENERGY STORAGE↗

Li Stripping Behavior of Anode‐Free Solid‐State Batteries Under Intermittent‐Current Discharge Conditions

Anode‐free manufacturing holds promise to enable high energy densities and lower Lithium (Li)‐metal solid‐state batteries (LMSSBs). Nevertheless, in contrast to thick Li foil (>50 µm), the stripping capacity of in situ‐formed Li (10–30 µm) is limited due to diminished creep flow, resulting in reduced accessible capacity. This study explores the correlation between stripping capacity and surface roughness of garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte. The results reveal that stripping capacity can be enhanced through the surface modification of solid electrolytes. Additionally, this study scrutinizes the stripping behavior of in situ Li under intermittent‐current discharge conditions, which are more relevant to the operational conditions of electric vehicles (EVs). It is demonstrated that, when compared to constant‐current stripping, intermittent‐current stripping effectively suppresses void formation and enhances the stripping capacity of in situ Li by 40%. It is considered that the intermittent current inhibits the accumulation of Li vacancies, thereby delaying the void formation. These findings provide valuable insights into the development of high‐performance anode‐free LMSSBs for EVs.

25 ENERGY STORAGE↗

A multiscale model to understand the interface chemistry, contacts, and dynamics during lithium stripping

A reversible Li-metal electrode, paired with a solid electrolyte, is critical for attaining higher energy density and safer batteries beyond the current lithium-ion cells. A stable stripping process may be even harder to attain as the stripping process will remove Li-atoms from the surface, and naturally reduce surface contact area, if not self-corrected by other mechanisms, such as diffusion and plastic deformation under an applied external stack pressure. Here, we capture these mechanisms occurring at multiple length- and time- scales, i.e., interface interactions, vacancy hopping, and plastic deformation, by integrating density functional theory (DFT) simulations, kinetic Monte Carlo (KMC), and continuum finite element method (FEM). By assuming the self-affine nature of multiscale contacts, we predict the steady-state contact area as a function of stripping current density, interface wettability, and stack pressure. We further estimate the exponential increase of overpotential due to contact area loss to maintain the same stripping current density. We demonstrate that a lithiophilic interface requires less stack pressure to reach the same steady-state contact area fraction than a lithiophobic interface. A “tolerable steady-state” contact area loss for maintaining stable stripping is estimated at 20 %, corresponding to a 10 % increase in overpotential. To constrain contact loss within the tolerance, the required stack pressure is 0.1, 0.5, and 2 times the yield strength of lithium metal for three distinct interfaces, lithiophilic Li/lithium oxide(Li2O), Li/lithium lanthanum zirconium oxide(LLZO), and lithiophoblic Li/lithium fluoride(LiF), respectively. The modeling results agree with experiments on the impact of the stack pressure quantitatively, while the discrepancy in stripping rate sensitivity is attributed to the simplifying interface interaction in our simulations. Overall, this multiscale simulation framework demonstrates the importance of electrochemical-mechanical coupling in understanding the dynamics of the Li/SE interface during stripping.

Feng, Min↗

Ion Size Effects on the Thermodynamic, Kinetic, and Mechanical Properties during Ion Exchange in Solid-State Electrolytes

Ion exchange offers a pathway to impose residual compressive stresses to mitigate the electro-chemo-mechanical cracking of solid-state electrolytes such as lithium lanthanum zirconium oxide. This study uses a coupled multiscale framework (integrating density functional theory (DFT), molecular dynamics (MD), and continuum modeling) to examine how exchange ion size influences stress, diffusion, fracture toughness, and electronic properties. Larger isovalent ions (Na + , Ag + , K + ) were exchanged with Li + , with DFT confirming their preference for octahedral 96h sites and a linear relationship between ion size and chemical free expansion coefficient. MD simulations reveal stress and concentration effects on exchange ion diffusivity at elevated temperatures, with Na + and Ag + maintaining favorable mobility while K + showing concentration-dependent clustering. Continuum modeling predicts the range of fracture strength improvements and the required ion exchange concentration profile. It was shown that a 5% surface exchange concentration can induce ∼0.6 GPa of surface compressive stress using Na + and ∼1.0 GPa of surface compressive stress using Ag + . On the other hand, larger ion exchange species may penalize Li + diffusivity by increasing the activation volume and activation energy. Interestingly, Na + has a negligible penalty on Li-ion diffusivity. The room temperature Li + ion diffusivity is reduced by ∼40% with Ag + ion exchange. Electronic band structure analysis shows no size-dependent change in the bandgap, though Ag + introduces localized defect states near the valence band maximum. This study highlights ion size as a key factor in optimizing LLZO properties, offering a framework to improve the solid-state battery performance.

Jagad, Harsh D. [Brown Univ., Providence, RI (Unit↗