Search NASASearch

SEARCH · Search NASA

Results for “epitaxial growth”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

165 records · Page 2

Crystal Growth of Selected II-VI Semiconducting Alloys By Directional Solidification

A Hg 0.84 Zn 0.16 Te alloy crystal was back-melted and partially resolidified during the first United States Microgravity Laboratory (USML-1) mission in the Marshall Space Flight Center's Crystal Growth Furnace. The experiment was inadvertently terminated at about 30% of planned completion. Nonetheless, it was successfully demonstrated that HgZnTe alloy ingots partially grown and quenched on the ground can be back-melted and regrown in space under nearly steady state growth conditions. An identical 'ground-truth' experiment was performed following the mission. Preliminary results are presented for both crystals, as well as for a series of other crystals grown prior to the mission for the purposes of optimizing in-flight growth conditions.

S L Lehoczky

The Study of Dopant Segregation Behavior During the Growth of GaAs in Microgravity

An investigation into the segregation behavior of selenium doped gallium arsenide during directional solidification in the microgravity environment was conducted using the Crystal Growth Furnace (CGF) aboard the first United States Microgravity Laboratory (USML-1). The two crystals grown were 1.5 cm in diameter and 16.5 cm in length with an initial melt length of 14 cm. Two translation periods were executed, the first at 2.5 microns/s and after a specified time, which was different between the two experiments, the translation rate was doubled to 5.0 microns/s. The translation was then stopped and the remaining sample melt was solidified using a gradient freeze technique in the first sample and a rapid solidification in the second experiment. Measurement of the selenium dopant distribution, using quantitative infrared transmission imaging, indicates that the first sample initially achieved diffusion controlled growth as desired. However, after about 1 cm of growth, the segregation behavior was driven from a diffusion controlled growth regime to a complete mixing regime. Measurements in the second flight sample indicated that the growth was always in a complete mixing regime. In both experiments, voids in the center line of the crystal, indicative of bubble entrapment, were found to correlate with the position in the crystal when the translation rates were doubled.

D H Matthiesen

Protein Crystal Growth Results From the United States Microgravity Laboratory-1 Mission

Protein crystal growth experiments have been performed by this laboratory on 18 Space Shuttle missions since April, 1985. In addition, a number of microgravity experiments also have been performed and reported by other investigators. These Space Shuttle missions have been used to grow crystals of a variety of proteins using vapor diffusion, liquid diffusion, and temperature-induced crystallization techniques. The United States Microgravity Laboratory - 1 mission (USML-1, June 25 - July 9, 1992) was a Spacelab mission dedicated to experiments involved in materials processing. New protein crystal growth hardware was developed to allow in orbit examination of initial crystal growth results, the knowledge from which was used on subsequent days to prepare new crystal growth experiments. In addition, new seeding hardware and techniques were tested as well as techniques that would prepare crystals for analysis by x-ray diffraction, a capability projected for the planned Space Station. Hardware that was specifically developed for the USML-1 mission will be discussed along with the experimental results from this mission.

L J Delucas

Virtual Growth of SRF Materials

Niobium's native surface oxide affects SRF cavity and superconducting qubit performance, motivating interest in controlling its crystalline structure. We combine a literature-derived machine-learning analysis with temperature-dependent XRD to study crystalline ordering in Nb2O5. Random Forest models, trained on 74 processing conditions from 17 papers and validated by leave-one-group-out cross-validation, predicted broad crystallinity outcomes well (balanced accuracy 0.809), but struggled with specific polymorph identity (0.577). Annealing temperature was the dominant predictor across all targets; oxygen partial pressure showed negligible importance, reflecting narrow literature coverage rather than physical irrelevance. Temperature-dependent XRD on anodized and H2O2-treated Niobium showed structural evolution consistent with the machine learning predictions. Our model and overall approach provide a data-driven framework for identifying and optimizing conditions that promote crystallization in initially amorphous oxides. This framework can guide the selection of growth and post-annealing conditions for Nb surfaces by narrowing the experimental parameter space, thereby reducing trial-and-error efforts in developing oxide structures relevant to SRF applications.

Tilkin, Anthony [Fermilab]

Crystal Growth Scale-Up and Stability of RbSr 2 X 5 :Eu Scintillators

The discovery and development of new scintillation materials support national security needs. In these applications, large volumes of scintillator crystals are needed to achieve efficient screening for contraband. Therefore, one important step in the discovery of new scintillator compositions is testing their feasibility for scale-up and their stability. In this work, high-quality Ø22 mm crystals of two new scintillators RbSr 2 Br 5 :Eu and RbSr 2 I 5 :Eu were grown via the Vertical Bridgman method, and their scintillation properties were characterized. Here, the Ø22 mm RbSr 2 I 5 :Eu crystals could be grown with fast translation rates up to 3.5 mm/h. Both RbSr 2 Br 5 :Eu and RbSr 2 I 5 :Eu had high scintillation performance, including light yields of 46,000 and 61,000 ph/MeV, respectively, for Ø22 × 35 mm crystals. Additionally, properties related to physical stability were investigated, including the coefficients of thermal expansion via high-temperature X-ray diffraction (HTXRD) as well as moisture sensitivity. HTXRD confirmed the absence of solid–solid phase transitions and showed that RbSr 2 Br 5 had minimal thermal expansion anisotropy compared to RbSr 2 I 5 and some other inorganic metal halide scintillators, which favors the growth of large-sized crystals.

36 MATERIALS SCIENCE

Single‐photon emitters in PECVD‐grown silicon nitride films: from material growth to photophysical properties

Abstract Silicon nitride (SiN) is a key material for quantum photonics due to its wide transparency window, high refractive index, low optical losses, and semiconductor foundry compatibility. We study the formation of single‐photon emitters in SiN films grown by plasma‐enhanced chemical vapor deposition (PECVD), exploring their photophysical properties and dependence on growth conditions. Emitters were observed across the entire range of nitrogen‐to‐silicon precursor ratios, from silicon‐rich to nitrogen‐rich conditions, enabled by the low background fluorescence. We demonstrate single‐photon emitters in SiN films with a higher refractive index (1.8–1.9) compared to our previous reports (∼1.7). Notably, nitrogen‐rich, thinner films yield particularly bright emitters with shorter emission lifetimes, likely due to more efficient annealing. Silicon‐rich SiN films exhibit red‐shifted emission, suggesting that composition may provide a mechanism for wavelength tuning. These findings establish the feasibility of emitters formation in foundry standard PECVD tools, advancing the scalability and lab‐to‐fab transition of SiN‐based quantum photonic technologies.

Materials Science

Netload Range Cost Curves for Coordinated Transmission-Distribution Planning Under DER Growth Uncertainty

The increasing penetration of distributed energy resources (DERs) requires better coordination between transmission and distribution (T&D) planning to ensure system security and cost efficiency. However, misaligned planning horizons, computational burdens, and privacy concerns hinder effective coordination, leading to either underutilized resources caused by overinvestments or reliability risks due to underinvestment. To address this challenge, we introduce netload range cost curves (NRCCs), a novel approach for managing long-term DER growth uncertainty through T&D coordination, while preserving existing data-sharing and regulatory structures. NRCCs provide pairs of (i) peak substation netload guarantees and (ii) corresponding distribution upgrade options and costs, enabling their seamless integration into transmission planning workflows. To compute NRCCs efficiently, we develop a transmission-aware distribution network planning (TADNP), which is subsequently integrated to an iterative computation procedure. These NRCCs are then embedded into an NRCC-informed transmission planning model to enable resource-efficient coordination. We illustrate our proposed approach with a case study based on realistic distribution and transmission systems in the San Francisco Bay Area, California. Our results indicate the possibility of dramatic savings in transmission investments by incorporating the proposed NRCC-integrated T&D coordination framework.

Li, Yujia

Superconducting Material Growth for Radio-Frequency (RF) Cavities

Superconducting radio-frequency (SRF) cavities, usually manufactured from Niobium (Nb), are vital components of modern particle accelerators because of their ability to achieve high acceleration gradients with little power dissipation. Naturally forming Nb surface oxides significantly alter cavity performance by changing surface resistance. A nondestructive characterization of oxide thickness is helpful for relating surface processing treatments to cavity performance. This work develops a protocol to measure Nb oxide thickness using Angle-Resolved X-ray Photoelectron Spectroscopy (ARXPS) while correcting instrumental errors. Using uniform bulk standard samples (Silver, Aluminum oxide, and Germanium), we determined a baseline correction factor to account for analyzer-related intensity evolution as the measurement angle increases. The correction factor was then applied to Nb 3d ARXPS data. Applying the Strohmeier equation to the corrected data yielded a Nb2O5 thickness of 6.04 nm, closely matching the 5.5 (±.05) nm value obtained from cross-sectional transmission electron microscopy. Our approach will bring a method to incorporate inherent errors in the thickness measurements using ARXPS and can be broadly applied to improve the accuracy of thickness measurements in a wide range of heterostructures.

Lambert, Nathan [Fermilab]

Phase-field modeling of stored-energy-driven grain growth with intra-granular variation in dislocation density

Abstract We present a phase-field (PF) model to simulate the microstructure evolution occurring in polycrystalline materials with a variation in the intra-granular dislocation density. The model accounts for two mechanisms that lead to the grain boundary migration: the driving force due to capillarity and that due to the stored energy arising from a spatially varying dislocation density. In addition to the order parameters that distinguish regions occupied by different grains, we introduce dislocation density fields that describe spatial variation of the dislocation density. We assume that the dislocation density decays as a function of the distance the grain boundary has migrated. To demonstrate and parameterize the model, we simulate microstructure evolution in two dimensions, for which the initial microstructure is based on real-time experimental data. Additionally, we applied the model to study the effect of a cyclic heat treatment (CHT) on the microstructure evolution. Specifically, we simulated stored-energy-driven grain growth during three thermal cycles, as well as grain growth without stored energy that serves as a baseline for comparison. We showed that the microstructure evolution proceeded much faster when the stored energy was considered. A non-self-similar evolution was observed in this case, while a nearly self-similar evolution was found when the microstructure evolution is driven solely by capillarity. These results suggest a possible mechanism for the initiation of abnormal grain growth during CHT. Finally, we demonstrate an integrated experimental-computational workflow that utilizes the experimental measurements to inform the PF model and its parameterization, which provides a foundation for the development of future simulation tools capable of quantitative prediction of microstructure evolution during non-isothermal heat treatment.

Materials Science

Three-dimensional nucleation and growth of deformation twins in magnesium

At two-thirds the weight of aluminum, magnesium alloys have the potential to reduce the fuel consumption of transportation vehicles. These advancements depend on our ability to optimize the desirable versus undesirable effects of deformation twins, which are three-dimensional (3D) microstructural domains that form under mechanical stresses. Previously only characterized through surface or thin-film measurements, we here present 3D in situ characterization of deformation twinning inside an embedded grain over mesoscopic fields of view using dark-field x-ray microscopy supported by crystal plasticity finite element analysis. The results revealed the role of triple junctions on twin nucleation and the sequence and irregularity of twin growth and showed that twin-grain junctions, twin-twin junctions, and twin boundaries were the sites of localized dislocation accumulation.

Lee, Sangwon [Univ. of Michigan, Ann Arbor, MI (Un

Stoichiometric effects on grain growth in zirconium carbide coatings for high-temperature nuclear fuel

Interest in coated particle fuel for space nuclear propulsion (SNP) has expanded in recent years due to successful demonstrations of the resiliency of the coatings to extreme environments. For SNP applications, the coating layer for the particle design needs to be able to withstand exposure to high temperature hydrogen during operating conditions. ZrC has been proposed as a protective layer, however, it is important to understand the high temperature behavior to ensure adequate protection to this fuel. In this study, surrogate ZrC coated particles were heat treated at 1900 °C up to 300 min, to examine how the microstructure evolves when exposed to high temperature. Scanning electron microscopy and electron backscatter diffraction (EBSD) were conducted to determine grain size and grain boundary character and orientation to determine the degree of change in the ZrC layer post heat treatment. Raman spectroscopy provided insight to understand how the as-fabricated stoichiometry of each sample contributed to the differences in grain growth behavior. Despite the as-fabricated samples showing a similar initial grain size and grain boundary character, the samples with a higher amount of excess carbon exhibited smaller grain areas and slower growth rates when exposed to 1900 °C. In conclusion, this investigation details the as-fabricated microstructure of the ZrC layer, specifically grain size, evolved under high temperature as this can impact the performance of the fuel under operating conditions.

EBSD

Reduced instability growth and improved radiation trapping with optimized shock timing in double-shell inertial confinement fusion capsules

The double shell is a volume-burn inertial confinement fusion concept consisting of two concentric shells: a low-Z outer shell that collides with and transfers momentum to a high-Z inner shell which compresses and heats the thermonuclear fuel. The increased number of capsule interfaces and severe hydrodynamic instability of the high-density pusher during its acceleration phase provide challenges to the success of the double shell. Two-dimensional radiation-hydrodynamics simulations predict the hydrodynamic instability growth on the outer surface of the pusher can be greatly reduced through appropriate timing of two shocks that cross this interface. One of these shocks, unique to multi-shell designs, arises from radiation-driven ablation of the inner shell ahead of the main shock, the second shock of concern. The shock timing is optimized by increasing the thickness of a low-Z tamper layer exterior to the pusher, resulting in only minimal changes to the implosion timing. Reducing the instability growth on the outer surface of the high-Z pusher can dramatically decrease the modulations that feedthrough to the pusher inner surface, improving the efficacy of radiation trapping in the thermonuclear fuel and increasing the predicted thermonuclear yield by ≳20×.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY

Apollo-Soyuz Test Project: Preliminary Science Report

This document summarizes the experimental concepts and preliminary analyses (as of December 1975) for each of the 28 scientific experiments conducted during the Apollo-Soyuz Test Project from July 15 to 24, 1975. The scientific topics are X- ray and extreme ultraviolet astronomy, solar astronomy, gamma- ray detectors, Earth studies (including the upper atmosphere, meteorological phenomena, hydrology, oceanography, geology, desert studies, and gravity field studies), microbiology, heavy cosmic particle interaction with live cells, vestibular system studies, and materials processing (including high-temperature and ambient-temperature processing of industrial materials and electrophoretic processing of biological materials) .

Microbiology

The Growth of Zeolites A, X and Mordenite in Space

Zeolites are a class of crystalline aluminosilicate materials that form the backbone of the chemical process industry worldwide. They are used primarily as adsorbents and catalysts and support to a significant extent the positive balance of trade realized by the chemical industry in the United States (around $19 billion in 1991). The magnitude of their efforts can be appreciated when one realizes that since their introduction as 'cracking catalysts' in the early 1960's, they have saved the equivalent of 60 percent of the total oil production from Alaska's North Slope. Thus the performance of zeolite catalysts can have a profound effect on the U.S. economy. It is estimated that a 1 percent increase in yield of the gasoline fraction per barrel of oil would represent a savings of 22 million barrels of crude oil per year, representing a reduction of $400 million in the United States' balance of payments. Thus any activity that results in improvement in zeolite catalyst performance is of significant scientific and industrial interest. In addition, due to their 'stability,' uniformity, and, within limits, their 'engineerable' structures, zeolites are being tested as potential adsorbents to purify gases and liquids at the parts-per-billion levels needed in today's electronic, biomedical, and biotechnology industries and for the environment. Other exotic applications, such as host materials for quantum-confined semiconductor atomic arrays, are also being investigated. Because of the importance of this class of material, extensive efforts have been made to characterize their structures and to understand their nucleation and growth mechanisms, so as to be able to custom-make zeolites for a desired application. To date, both the nucleation mechanics and chemistry (such as what are the 'key' nutrients) are, as yet, still unknown for many, if not all, systems. The problem is compounded because there is usually a 'gel' phase present that is assumed to control the degree of supersaturation, and this gel undergoes a continuous 'polymerization' type reaction during nucleation and growth. Generally, for structure characterization and diffusion studies, which are useful in evaluating zeolites for improving yield in petroleum refining as well as for many of the proposed new applications (e.g., catalytic membranes, molecular electronics, chemical sensors) large zeolites (greater than 100 to 1000 times normal size) with minimum lattice defects are desired. Presently, the lack of understanding of zeolite nucleation and growth precludes the custom design of zeolites for these or other uses. It was hypothesized that the microgravity levels achieved in an orbiting spacecraft could help to isolate the possible effects of natural convection (which affects defect formation) and minimize sedimentation, which occurs since zeolites are twice as dense as the solution from which they are formed. This was expected to promote larger crystals by allowing growing crystals a longer residence time in a high-concentration nutrient field. Thus it was hypothesized that the microgravity environment of Earth orbit would allow the growth of large, more defect-free zeolite crystals in high yield.

A Sacco, Jr

Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC Cathodes

Degradation of LiNi x Mn y Co 1-x-y O 2 (NMC)-based lithium-ion batteries depends strongly on cut-off voltage ranges. In addition to the high upper cut-off voltage, a high depth of discharge (i.e., lower cut-off voltage) significantly worsens cathode impedance growth and capacity fade during long-term cycling. However, there is currently no consensus on the mechanism behind the negative role of a deep discharge. Here, this phenomenon was investigated in graphite||NMC cells with single-crystal cathodes (LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC622) or LiNi 0.76 Co 0.14 Mn 0.10 O 2 (NMC76)) using targeted aging protocols (constant high-voltage holds vs. charge–discharge cycling), while monitoring transition-metal (TM) dissolution, cathode-electrolyte interface (CEI) impedance, and NMC surface composition. We demonstrate a correlation between discharge-driven CEI impedance growth and increased TM dissolution. Furthermore, this degradation pathway is more pronounced in lower-Ni NMC622 than in higher-Ni (NMC76) under comparable delithiation states at charge, with both compositions undergoing the H2→H3 phase transition. X-ray photoelectron spectroscopy (XPS) reveals NMC composition-dependent evolution of surface lattice oxygen and restructured surface layer composition between charged and discharged states. These findings add mechanistic depth to the role of discharge as an active driver of interfacial degradation and provide new insights into its composition dependence.

25 ENERGY STORAGE

Growth of deuterium supersaturated surface layer with increasing ion flux and fluence in plasma-exposed tungsten

Deuterium supersaturated surface layer (DSSL) in tungsten, a few nm thick layer exhibiting extremely high deuterium content (> 5%), has been studied as a function of deuterium plasma ion flux and fluence. Tungsten samples were exposed at 400 K and deuterium ion energy of ∼ 60 eV. The deuterium ion flux spanned over an order of magnitude, being 7.3 × 10 20 , 4.2 × 10 21 , and 3.8 × 10 22 D/m 2 . The fluence ranged from 3.4 × 1024 to 3.4 × 1025 D/m2. The samples and their deuterium content were analyzed by nuclear reaction analysis (NRA), scanning transmission electron microscopy (STEM), and thermal desorption spectroscopy (TDS). The largest thickness of DSSL was found to be around 10.5 nm and was observed in the case of the highest exposure flux and fluence, whereas the layer was only about 3.8 nm thick in the case of the lowest value of the two parameters. The thickness of the DSSL was found to monotonically increase with both deuterium flux and fluence. Finally, similar to the thickness, the estimated D concentration seems to follow the same trend, increasing from the lowest value of around 3 at.% to the highest value of around 5 at.%.

Deuterium

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE