Search NASA⌕ Search

SEARCH · Search NASA

Results for “Eutectic solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

51 records · Page 3

Beyond the eutectic paradigm: nanolamellar patterns in a rapidly solidified peritectic alloy

Peritectic transformations are central to many structural alloys, yet pattern formation remains poorly understood due to complex growth dynamics and limited three-dimensional data. Here, we report an unusual two-phase microstructure in a Zn–Ag peritectic alloy subjected to rapid solidification by laser surface remelting. Synchrotron X-ray nanotomography reveals a lamellar structure of primary 𝜀-AgZn 3 and peritectic Zn with ∼700 nm spacing. Although resembling a eutectic morphology, this pattern forms without a eutectic reaction through non-steady coupled growth from the liquid. SEM and TEM-EDS confirm interface shapes and phase compositions. These findings expand the design space of peritectics for refined microstructural control.

36 MATERIALS SCIENCE↗

Low-temperature bonding with spaced nanorods and eutectic alloys

Bonded surfaces are formed by adhering first nanorods and second nanorods to respective first and second surfaces. The first shell is formed on the first nanorods and the second shell is formed on the second nanorods, wherein at least one of the first nanorods and second nanorods, and the first shell and the second shell are formed of distinct metals. The surfaces are then exposed to at least one condition that causes the distinct metals to form an alloy, such as eutectic alloy having a melting point below the temperature at which the alloy is formed, thereby bonding the surfaces upon which solidification of the alloy.

36 MATERIALS SCIENCE↗

In-Situ Synchrotron X-Ray Diffraction of Ultrasonic Microstructural Refinement During Solidification in a Commercial Al–Si–Mg Alloy

This study reports the first use of in-situ synchrotron X-ray diffraction (SXRD) to study the effects of ultrasonic melt processing (USMP) on phase and grain size evolution during solidification in a commercial Al–Si–Mg casting alloy. USMP is a technique that, when applied to aluminum as it solidifies, can be used to refine the local microstructure of large-scale castings. Analysis of the in-situ SXRD data to estimate the average grain size of primary α-Al grains during USMP demonstrates that USMP slows the growth rate of α-Al grains and reduces grain size by 36 pct. Furthermore, there is also evidence that USMP causes the primary α-Al grains to move relative to the X-ray beam; such motion increases the probability of primary α-Al grains colliding and fragmenting. This movement becomes constrained at the onset of the Al–Si binary eutectic, suggesting that USMP ceases to effectively refine the microstructure once the Al–Si binary eutectic begins to form. Complementary laboratory-scale X-ray diffraction (XRD) data were used to correlate the lattice parameters of the α-Al and Si (D-A4) phases with temperature to estimate cooling rate during solidification. Thus, this study can guide the design of novel castings with spatially distributed fine-grained regions produced using local ultrasonic processing.

Aluminum Alloys↗

Microstructural refinement in ultrasonically modified A356 aluminum castings

Two A356 aluminum alloys (Al-Si-Mg), one with 0.09 wt.% Fe and one with 0.91 wt.% Fe, were cast in a graphite mold with the simultaneous application of local ultrasonic intensification to refine the as-cast microstructure. Ultrasonication during casting transformed the morphology of primary Al grains from dendritic (~140-290 microns in size) to globular (~33-36 microns in size). The alloy with high Fe exhibited globular grains at distances up to 45 mm away from the ultrasound probe, while the alloy with low Fe exhibited globular grains at distances only up to 6 mm away from the ultrasound probe. Near the location of the ultrasound probe (< 2 mm away), a second non-dendritic microstructural morphology was observed with fine aluminum grains (~9-25 microns in size). This unique fine-grained morphology has not been previously reported, contains a greater concentration of Si relative to the globular microstructure, and may be a large, fully eutectic region. Ultrasonication during casting also transformed the morphology of the ß-Al 5 FeSi phase particles (which are deleterious to the strength and ductility of the alloy) in the high Fe alloy from needle-like to rectangular, which could enable the greater use of secondary Al alloys. Thermodynamic simulations conducted to calculate the solidification paths of the two alloys studied predict that the ß-Al 5 FeSi phase begins to form earlier in the alloy with high Fe. Finally, data suggest that the ß-Al 5 FeSi phase (which is more abundant in alloys with high Fe content) may enhance ultrasonically-induced grain refinement.

36 MATERIALS SCIENCE↗

Multimodal and multiscale strengthening mechanisms in Al-Ni-Zr-Ti-Mn alloy processed by laser powder bed fusion additive manufacturing

The unique thermokinetics of laser-powder bed fusion additive manufacturing (L-PBFAM) has been exploited for development of a novel high-strength Al-Ni-Ti-Zr-Mn alloy. The addition of 0.5 wt% Mn leads to extraordinary improvement in ultimate tensile strength (502 MPa) and work hardening due to the activation of two Mn-induced strengthening mechanisms. First, by a bimodal particle strengthening effect due to Al 31 Mn 6 Ni 12 nano-quasi-crystal particles rejected in inter-dendritic spaces and fibrous Al 3 Ni eutectic dendritic channels, which predominately contributes to the strength improvement, and second by solid solution strengthening from remaining Mn entrapped in Al. These mechanisms supplement the particle strengthening effect imparted by coherent and incoherent Al 3 (Ti,Zr) co-precipitates present at melt pool boundaries, dislocation strengthening due to solidification induced strain, and Hall-Petch and backstress strengthening effect due to heterogenous grain size distribution occurring at various length scales. In conclusion, the solidification dynamics and hierarchical heat distribution that are associated with L-PBFAM resulted in complex spatial variations in these strengthening phenomena and were investigated via a high-throughput multiscale structure–property correlation that involved thermokinetic simulation, X-ray diffraction, high-resolution nanoindentation mapping, and site-specific transmission electron microscopy of the alloy.

36 MATERIALS SCIENCE↗

Towards engineering the growth morphology of anisotropic bicrystals

Eutectic alloys, such as Pb-free Bi-Sn-Ag or Sn-Ag-Cu, are essential for their low melting points in solder joints but suffer from brittle intermetallic phases, reducing reliability. Traditional solder design relies on equilibrium phase diagrams, often neglecting the kinetic influence of crystalline anisotropy during solidification. This study hypothesizes that the energetics at the solid-solid-liquid trijunction dictate crystalline facet selection. Using the Al-Al 3 Ni alloy as a model, this project combines atomistic simulations and experimental methods to understand interfacial energies and develop predictive models. This approach aims to mitigate the negative effects of intermetallics, enhancing component reliability in electronic applications.

36 MATERIALS SCIENCE↗

Heterogeneous phase transformation pathways in additively manufactured Al-Ce-Mn alloys

Heat treatment of additively manufactured Al-Ce based multicomponent alloys leads to complex microstructure evolution. In this research, the ability to extend the phase transformation theories involving nucleation of a product phase from a heterogeneous multi-phase microstructure typical to that of additively manufactured samples is explored. The Al-10Ce-8Mn (wt%) was used as a model alloy system. Under additive manufacturing conditions different solidification microstructures were obtained due to spatial and temporal variations of thermal gradients (G) and liquid-solid interface velocities (R) within a given melt pool. Near the melt pool boundary (high G and low R, referred as MPB region), initially, Al 20 Mn 2 Ce forms from the liquid followed by a eutectic of FCC Al and Al 11 Ce 3 . In the melt pool interiors (low G and high R referred as ES region) a eutectic structure between FCC Al and Al 20 Mn 2 Ce is observed. During subsequent heat treatments, the MPB and ES regions transform into different sets of microstructures. In the MPB region, a fine globular microstructure containing FCC Al, Al 11 Ce 3 , Al 6 Mn, and Al 12 Mn results from the decomposition of Al 20 Mn 2 Ce. In the ES region a faceted Al 51 Mn 7 Ce 4 plate phase results from the decomposition of Al 20 Mn 2 Ce. The formation of the Al 51 Mn 7 Ce 4 phase within the eutectic microstructure at the boundaries of FCC Al and Al 20 Mn 2 Ce has not been reported in the literature. Further, these two distinct phase transformation pathways are rationalized based on the role of driving force on the nucleation of (Al 6 Mn) and/or metastable intermetallic (Al 51 Mn 7 Ce 4 ) phases at the interface of aluminum (FCC) and the non-equilibrium intermetallic (Al 20 Mn 2 Ce) phases.

36 MATERIALS SCIENCE↗

Strontium Effects on the Formation of Iron-Intermetallic Phases in Secondary Al–9Si–0.6Fe Alloys

The presence and morphology of Fe-containing intermetallic phases affect the mechanical properties of aluminum alloys, especially in secondary Al–Si-based cast alloys. Although strontium (Sr) addition of 50 to 500 ppm is known to refine the needle-type eutectic silicon structure, the influence of Sr on the formation of Fe-intermetallic phases remains unclear. The present work investigates the combined additions of Sr and Mn to Al–9Si–0.6Fe–0.35Mg (All compositions are in wt pct except otherwise stated.) alloys on the formation of Fe-intermetallic phases at different solidification rates from ~ 1.5 to ~ 60 °C/s. Long and branched-type AlFeSi phase with size ranging from 50 to 120 µm are more common when solidified at the rate of 1.5 °C/s regardless of Sr and Mn additions. However, at the fast solidification rate of 60 °C/s, a 60 ppm Sr addition significantly reduced the average length of needle-shaped AlFeSi phase to less than 3 to 5 µm. Thermodynamic simulations have been performed using CALculation of PHAse Diagrams (CALPHAD) models to predict the formation of various phases and their possible interactions during solidification. The results indicated that the combination of a high solidification rate and about 60 ppm of Sr is beneficial to refining the δ-Al 3 FeSi 2 phase in Al–Si–Mg alloys containing 0.6 pctFe. As a result, this unexpected finding of Fe-intermetallic refinement by low Sr addition (~60 ppm) provides an important guide in designing secondary alloys for sustainable casting applications.

36 MATERIALS SCIENCE↗

Microstructure and properties of additively manufactured Al–Ce–Mg alloys

Additive manufacturing of aluminum alloys is largely dominated by a near-eutectic Al-Si compositions, which are highly weldable, but have mechanical properties that are not competitive with conventional wrought Al alloys. In addition, there is a need for new Al alloys with improved high temperature properties and thermal stability for applications in the automotive and aerospace fields. In this work, we considered laser powder bed fusion additive manufacturing of two alloys in the Al–Ce–Mg system, designed as near-eutectic (Al–11Ce–7Mg) and hyper-eutectic (Al–15Ce–9Mg) compositions with respect to the binary L → Al + Al 11 Ce eutectic reaction. The addition of magnesium is used to promote solid solution strengthening. A custom laser scan pattern was used to reduce the formation of keyhole porosity, which was caused by excessive vaporization due to the high vapor pressure of magnesium. The microstructure and tensile mechanical properties of the alloys were characterized in the as-fabricated condition and following hot isostatic pressing. The two alloys exhibit significant variations in solidification structure morphology. These variations in non-equilibrium solidification structure were rationalized using a combination of thermodynamic and thermal modeling. Both alloys showed higher yield strength than AM Al-10Si-Mg for temperatures up to 350 °C and better strength retention at elevated temperatures than additively manufactured Scalmaloy.

36 MATERIALS SCIENCE↗

Theory-guided design of duplex-phase multi-principal-element alloys

Density-functional theory (DFT) is used to identify phase-equilibria in multi-principal-element and high-entropy alloys (MPEAs/HEAs), including duplex-phase and eutectic microstructures. Here, a combination of composition-dependent formation energy and electronic-structure-based ordering parameters were used to identify a transition from FCC to BCC favoring mixtures, and these predictions experimentally validated in the Al-Co-Cr-Cu-Fe-Ni system. A sharp crossover in lattice structure and dual-phase stability as a function of composition were predicted via DFT and validated experimentally. The impact of solidification kinetics and thermodynamic stability was explored experimentally using a range of techniques, from slow (castings) to rapid (laser remelting), which showed a decoupling of phase fraction from thermal history, i.e., phase fraction was found to be solidification rate-independent, enabling tuning of a multi-modal cell and grain size ranging from nanoscale through macroscale. Strength and ductility tradeoffs for select processing parameters were investigated via uniaxial tension and small-punch testing on specimens manufactured via powder-based additive manufacturing (directed-energy deposition). This work establishes a pathway for design and optimization of next-generation multiphase superalloys via tailoring of structural and chemical ordering in concentrated solid solutions.

36 MATERIALS SCIENCE↗

Degradation science: Integrating modeling and experiments to predict localized corrosion processes (Annual Progress Report)

Additively manufactured (AM) eutectic high-entropy alloys (EHEAs), such as nano-lamellar AlCoCrFeNi 2.1 , have excellent strength, ductility, and wear resistance even at elevated temperatures, but their corrosion behavior in aggressive acids at different length scales remain poorly understood. This work investigates the corrosion behavior of laser powder bed–fused (L-PBF) AlCoCrFeNi 2.1 as a function of annealing temperatures, probing degradation mechanisms from nanoscopic to macroscopic length scales. The alloy is dual phase consisting of a ductile FCC L1 2 phase and a high-strength BCC B2 phase. Rapid solidification during L-PBF produces a far-from-equilibrium nano-lamellar structure with nearly homogeneous elemental distribution, which tends to evolve upon annealing toward Cr/Co/Fe-enriched FCC and Al/Ni-enriched B2. Three conditions were studied: as-printed, 600 °C/5 h, and 1000 °C/1 h, over which B2 lamellae coarsen, lamellar spacing increases, and elemental segregation becomes more prominent. Microstructure and chemistry were characterized by scanning electron microscopy (SEM) and energy-dispersive spectroscopy (EDS), while in-situ electrochemical atomic force microscopy (EC-AFM) was used to link early (<5 h) local dissolution to microstructure after exposure in sulfuric acid. EC-AFM highlights preferential dissolution of the BCC/B2 phase where the surrounding matrix is Cr-depleted and directly quantifies the dissolution rates within individual phases, tracks the transition from early nano-scale attack to partial repassivation, to correlate height differences with current and impedance responses. To monitor longer-term behavior (up to 96 h), ex-situ AFM, SEM, and confocal imaging were combined with conventional bulk electrochemical tests, bridging nanoscale observations to micro/meso-scale damage morphologies. At the meso-scale, the deepest dissolution channels align with the build-direction lamellae and melt-pool boundaries, indicating that printing directionality guides the propagation of these localized corrosion sites. Annealing modifies corrosion by restructuring BCC/FCC phase fractions, lamellar spacing, and Cr/Al segregation, thereby changing the cathode/anode ratio and passive film stability. The results clarify how as-printed and annealed nano-lamellar architectures differ in their susceptibility to selective dissolution; how elemental segregation competes with residual stresses along the build direction. With these insights, future work will use CALPHAD-guided alloy modification to stabilize higher Cr contents in the B2 phase while retaining a dominant FCC+B2/BCC microstructure, with the goal of designing mechanically robust, corrosion-resistant EHEAs for safety-critical applications to leverage the LLNL’s broader national and global security mission.

36 MATERIALS SCIENCE↗

The Beneficial Effect of Iron in Aluminum-Cerium-Based Cast Alloys

Iron (Fe) has been considered a major impurity since it is detrimental to the mechanical properties of many cast aluminum alloys due to the formation of Fe-containing brittle intermetallic phases. Fe is found naturally as an impurity in bauxite ore, resulting in Fe contamination of aluminum alloys with increasing contamination from current recycling practices. The Al–Ce–Fe system was investigated using CALPHAD (CALculation of PHAse Diagrams) modeling and experimental casting techniques. It was found that additions of Fe to the Al–Ce system are beneficial to the strength (slightly) and ductility (significantly) of the ternary alloys, which is attributed to the formation of fine metastable Al 8 CeFe 2 phase with aggregate morphology and equilibrium Al 10 CeFe 2 phase, suppressing coarse proeutectic Al 11 Ce 3 phase in near-eutectic Al–Ce alloys. Heat treatment study showed that the metastable Al 8 CeFe 2 phase transforms to predicted equilibrium Al 10 CeFe 2 phase at 500 °C, with essentially no intermetallic or grain coarsening; thus, the alloy displayed excellent property retention. The Al–Ce–Fe alloy system offers opportunities for sustainable, recyclable alloy development using low-cost Fe and low-cost cerium (a byproduct of rare-earth extraction).

42 ENGINEERING↗

Effects of composition and growth parameters on phase formation in multicomponent aluminum garnet crystals

The effects of com­position on the phase formation of multicom­ponent garnet crystals grown via directional solidification by the micro-pulling-down method are studied. A relatively wide range of rare-earth (RE) average ionic radii (AIR) is explored by formulating ten com­positions from the system (Lu,Y,Ho,Dy,Tb,Gd) 3 Al 5 O 12 . Crystals were grown at either 0.05 or 0.20 mm min -1 . The hypothesis is that multicom­ponent com­pounds with large AIR will form secondary phases as the single-RE aluminum garnets formed by larger Tb 3+ or Gd 3+ ; this will result in crystals of poor optical quality. Crystals with large AIR have a central opaque region in optical microscopy images, which is responsible for their reduced transparency com­pared to crystals with small AIR. Slow pulling rates suppress the formation of the opaque region in crystals with inter­mediate AIR. Powder and single-crystal X-ray diffraction and electron probe microanalysis results indicate that the opaque region is a perovskite phase. Scanning electron microscopy and energy dispersive spectroscopy measurements reveal eutectic inclusions at the outer surface of the crystals. Finally, the concentration of the eutectic inclusions increases with increasing AIR.

36 MATERIALS SCIENCE↗

A New Recycled Al–Si–Mg Alloy for Sustainable Structural Die Casting Applications

The use of secondary aluminum for structural components in the automotive industry is limited by the high Fe contents in recycled alloys which often result in the formation of brittle β-Al 5 FeSi phase which reduces the ductility of aluminum castings. In this study, a new secondary Al-Si-Mg alloy with high Fe content (about 0.44 wt.%) was developed for die casting applications. Based on thermodynamic modeling, manganese was added to obtain a designed Fe-to-Mn ratio of 2 which successfully suppressed the formation of β-Al 5 FeSi phase, by forming α-Al 15 (Fe,Mn) 3 Si 2 phase with rounded or hexagonal morphology. Additionally, a fine needle-like π-Al 8 FeMg 3 Si 2 phase was also formed within the eutectic regions. The new recycled alloy showed comparable mechanical properties in as-cast and heat treated (T5 and T6) conditions to three major primary die cast alloys (≤ 0.2 wt.% Fe) with similar composition. Ductility up to 7.4% from tensile elongation was achieved in as-cast recycled alloy due to the modification and refinement of α-Al 15 (Fe,Mn) 3 Si 2 by Mn and Sr additions. Tensile elongation was further improved to 9.1% after T6 treatment as a result of dissolution of π-Al 8 FeMg 3 Si 2 phase, defragmentation of α-Al 15 (Fe,Mn) 3 Si 2 and the spheroidization of Si phase. This new alloy provides a promising path for increasing usage of recycled aluminum with high Fe content in structural die castings for automotive and other applications.

36 MATERIALS SCIENCE↗