Effects of Oxide Dispersion on Failure Modes in an Additively Manufactured Superalloy

Additive manufacturing opens new paths for introducing oxide particles into superalloys, to potentially provide oxide dispersion strengthening (ODS) at high temperatures. This provides opportunities to study how such dispersions can influence failure modes for a given superalloy, after nearly identical material processing paths. The objective of this study was to compare monotonic failure modes for additively manufactured superalloys with versus without an introduced oxide dispersion. The superalloy for each case was produced by laser powder bed fusion additive manufacturing. Specimens were subsequently given consistent thermal treatment paths and then tested in tensile and creep tests at varied temperatures. Failure modes were then compared. Additively manufactured NiCrAl without ODS had randomly oriented equiaxed grains while this alloy with 0.25 wt% Y 2 O 3 ODS additions had elongated [001] oriented grains in the build direction. Material made without ODS (“No-ODS”) was nearly completely single phase gamma, while ODS additions resulted in gamma, chromium carbide, and Y-Al-Cr oxide phases, with carbide and oxide phases contents estimated at no more than 13 and 1 vol%, respectively. Compared to No-ODS, material made with ODS had higher tensile strengths at room, 760 and 1093 °C. The elongation of ODS material was lower than No-ODS at room temperature, but higher at 760 °C. At 1093 °C ODS material had higher elongation than No-ODS when tested in the build direction, however elongation was lower for ODS material in the transverse direction at 1093 °C. Creep rupture strain, life, and area reduction at 760 and 1093 °C were all much higher for ODS material compared to No-ODS; 760 °C rupture life was nearly 100 times longer for ODS material. The presence of Y in the ODS material significantly improved oxidation resistance.

supperalloys↗

Methods for preparing superalloy articles and related articles

A method for preparing an improved article including a nickel-based superalloy is presented. The method includes heat-treating a workpiece including a nickel-based superalloy at a temperature above the gamma-prime solvus temperature of the nickel-based superalloy and cooling the heat-treated workpiece with a cooling rate less than 50 degrees Fahrenheit/minute from the temperature above the gamma-prime solvus temperature of the nickel-based superalloy so as to obtain a cooled workpiece. The cooled workpiece includes a coprecipitate of a gamma-prime phase and a gamma-double-prime phase, wherein the gamma-prime phase of the coprecipitate has an average particle size less than 250 nanometers. An article having a minimum dimension greater than 6 inches is also presented. The article includes a material having a coprecipitate of a gamma-prime phase and a gamma-double-prime phase, wherein the gamma-prime phase of the coprecipitate has an average particle size less than 250 nanometers.

36 MATERIALS SCIENCE↗

Direct measurements of slip irreversibility in a nickel-based superalloy using high resolution digital image correlation

Fatigue crack nucleation in crystalline materials typically develops due to highly localized cyclic slip. During a fatigue cycle, reverse slip differs locally from slip in the forward direction particularly in precipitate-containing materials such as superalloys. In this paper we report the first direct measurements of irreversibility at the scale of individual slip bands by high-resolution digital image correlation (DIC) in a polycrystalline nickel-based superalloy. Quantitative measurements of the slip irreversibility are challenging for regions of material that have a size that captures the microstructure and its variability. High spatial resolution at the nanometer scale during experimental measurements is needed to observe slip localization during deformation. Moreover, large fields are also needed to obtain the material response over statistically representative populations of microstructural configurations. Recently, high resolution scanning electron microscope (SEM) digital image correlation (DIC) has been extended for quantitative analysis of discontinuities induced by slip events using the Heaviside-DIC method. Therefore, this novel method provides quantitative measurements of slip localization at the specimen surface. In this paper, the Heaviside-DIC method is used to measure slip irreversibility and plastic strain accumulation in a nickel-based superalloy. The method detects bands with high levels of irreversibility early in cycling that ultimately form fatigue cracks upon further cycling. The local microstructural configurations that induce large amounts of plasticity and slip irreversibility are correlated to crack nucleation locations.

36 MATERIALS SCIENCE↗

Evolution of carbide precipitates in Haynes® 282 superalloy processed by wire arc additive manufacturing

Precipitation hardening regulated with heat treatments is a critical technique for tuning the mechanical properties of Ni-based superalloys fabricated with additive manufacturing, where mechanical deformation is no longer viable for microstructural refinement. As one of the key precipitates, carbides prevail in the additively manufactured alloys, whose precipitation kinetics remain largely vague. This work studies the influence of heat treatments on the evolution of MC- and M 23 C 6 -type carbides within a Haynes® 282 superalloy prepared by wire arc additive manufacturing (WAAM). SEM-EDS analysis was performed to identify the evolution pathways of the carbides, and TEM and XRD characterizations were carried out to track the crystallographic features. The MC-type carbides are originally present in the as-printed alloy, which distribute uniformly across the whole material and remain largely unchanged in size during the heat treatments. By contrast, the incipiently non-existent M 23 C 6 -type carbides precipitate during an aging treatment at 1010 °C, which majorly extend along the grain boundaries as kinetically feasible sites. Further experimental and computational analysis confirms the enhancing effect of the M 23 C 6 -type carbides on the Vickers hardness. For the first time, this work revealed the evolution pathways of carbides within a Haynes® 282 superalloy prepared by WAAM, providing critical information for tunning the microstructure and mechanical properties. Finally, the carbide evolution kinetics established in this work can be potentially extended to other alloys prepared with WAAM, providing critical information to prevent mechanical failures associated with carbide coarsening.

36 MATERIALS SCIENCE↗

Custom-designed heat treatment simultaneously resolves multiple challenges facing 3D-printed single-crystal superalloys

Single-crystal Ni-based superalloys are currently the material of choice for turbine blade applications, especially with the emerging additive manufacturing (AM) that facilitates the manufacture/repair of these single crystals. This promising AM route, however, comes with a dilemma: in the fusion and heat affected zones after e-beam or laser induced melting, one needs a solutionizing annealing to relieve the residual stresses and homogenize the chemical/microstructure. The super-solvus solutionizing temperature is usually adopted from the protocol for the cast superalloys, which almost always causes recrystallization and stray grain growth, resulting in a polycrystalline microstructure and degrading the high-temperature mechanical performance. Here, in this paper, we demonstrate a custom-designed post-printing heat treatment to replace the conventional super-solvus one. The recovery and relatively low temperature diminish the driving force for recrystallization and the movement of stray grain boundaries, without suffocating the chemical/microstructural homogenization thanks to the narrow dendrite width and short element segregation distance. The optimal duration of the heat treatment is proposed to achieve atomic-diffusion mediated chemical homogenization while limiting γ'-particle coarsening in the interdendritic regions. Our strategy makes it practically feasible to resolve several bottleneck problems with one processing/treatment, removing a seemingly formidable obstacle to effective additive manufacturing of superalloy single crystal products.

36 MATERIALS SCIENCE↗

Fatigue Failures at Defective Grains in a Single Crystal Nickel-Base Superalloy

Single crystal nickel-base superalloys used as turbine engine blades can have much higher creep and fatigue resistance than many polycrystalline superalloys due to the absence of weak grain boundaries as well as the ability to orient the blades in the primary loading direction on to the low elastic modulus [001] orientation, which significantly lowers the stresses imposed on the blades. However, grain defects can occur in these crystals, impairing these advantages. In the present study, fatigue tests of a single crystal superalloy uncovered unexpected defective grains in the test specimens, which initiated premature fatigue failures. The characteristics of these defective grains and the associated failures were evaluated and related to the observed fatigue lives.

superalloy↗

The Application of Differential Scanning Calorimetry to Investigate Precipitation Behavior in Nickel-Base Superalloys Under Continuous Cooling and Heating Conditions

In this study, a suite of experimental tools and fast-acting, numerical-simulation techniques was used to quantify the precipitation behavior of three nickel-base superalloys: IN-100, LSHR, and 718. Experimental methods comprised differential scanning calorimetry (DSC) to establish the specific heat as a function of temperature and selected direct-resistance heating trials (using a Gleeble ® machine) to obtain samples for microstructural analysis. For the DSC experiments, each alloy was cooled at a prescribed constant rate (between 5 and 20 K/min) after an initial soak/equilibration in the high-temperature, single-phase (supersolvus) temperature regime. On-heating DSC trials beginning at ambient temperature were also performed on alloy 718 in three different starting conditions: super- δ -solvus solution treated and water quenched (denoted as ST), solution treated and aged (STA), and solution treated and overaged (STOA). DSC results, revealing the thermal signatures associated with the kinetics of precipitation of γ ' (IN-100, LSHR) or γ ' and γ " (718), were interpreted using a previously-developed fast-acting routine that treats concurrent nucleation, growth, coarsening, and dissolution. For these simulations, special attention was paid to various thermo-kinetic input parameters including equilibrium solvus-approach curves, bulk free energies of transformation, matrix-precipitate interface energies, and effective diffusivities. For the γ - γ ' superalloys (IN-100 and LSHR), estimates of precipitate volume fraction as a function of temperature from the specific-heat data revealed semi-quantitative agreement with simulation predictions. For the γ - γ '- γ " superalloy (718), simulation predictions of precipitate volume fractions were converted to specific heat as a function of temperature and showed semi-quantitative agreement with the direct measurements.

36 MATERIALS SCIENCE↗

Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High $\gamma ^{\prime }$ CoNi-Base Superalloy

Here, the cracking behavior of a high γ' volume fraction CoNi-base superalloy fabricated via laser powder bed fusion (LPBF) is studied in relation to the content of carbon and boron. Severe cracking occurred with the increase in boron content from 0.08 to 0.16 at. pct (0.015 to 0.029 wt pct), while compositions with 0.1 to 0.36 at. pct C (0.02 to 0.076 wt pct) and 0.08 at. pct B exhibited minimal cracking. Assessment of cracks in the high-boron composition shows a variation in crack density with printing parameters, and alignment of the cracks with the build direction. Scanning electron microscopy (SEM) of the crack surfaces shows evidence of a solidification cracking mode. Differential thermal analysis (DTA) reveals a decreased incipient melting temperature for the high-boron composition, and atom probe tomography (APT) is used to measure the enrichment at grain boundaries, revealing distinct boron segregation. Scheil-Gulliver solidification simulations for the different C and B levels are consistent with the incipient melting behavior observed with DTA. Evaluation of the solidification cracking susceptibility from the simulations allow for comparison of the CoNi alloy behavior to Ni-base superalloys studied for LPBF fabrication and displays how such metrics may aid in the design of new precipitation-strengthened superalloys for additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Creep Deformation and Damage Mechanisms in an Advanced High-Temperature Additively Manufactured Nickel-Base Superalloy

Abstract This research investigates the processing–structure–properties–performance relationship in a novel nickel-base superalloy, ABD ® -900AM, designed for extreme environments. Specifically tailored for additive manufacturing (AM), ABD ® -900AM maintains mechanical integrity at high temperatures and is comparable to other nickel-based superalloys with a 30–40% gamma-prime volume fraction. A comprehensive study was conducted using laser-beam powder bed fusion and electron-beam powder bed fusion methods. Factors such as heat treatment, porosity, build orientation, and hot isostatic pressing were evaluated to understand their effects on microstructure and mechanical performance. Microstructural characterization revealed significant differences in grain size and orientation across build processes and heat treatments. High-temperature mechanical testing indicated that grain size, heat treatment, and orientation significantly influence creep behavior. A super-solvus heat treatment led to recrystallization and grain growth, significantly improving creep properties compared to a near-solvus heat treatment. Various creep mechanisms were identified across different conditions, and creep rupture models were developed for each build process. Post-test microstructural analysis showed grain boundary damage, with differences in creep cavitation morphology under varying stress conditions. It was shown that MC carbides grow at the expense of gamma-prime near grain boundaries, leading to precipitate-free zones in specimens tested at higher temperatures. This study fills a significant gap in fundamental research by offering a deeper insight into the high-temperature mechanical behavior of additively manufactured nickel-base superalloys. It also explores critical research questions regarding the role of carbides and the significance of heat treatment. The insights gained enhance confidence in the industry adoption of ABD ® -900AM and similar alloys for high-temperature applications, bridging the knowledge gap and supporting the development of reliable AM processes for extreme environments.

Bridges, Alex (ORCID:000000030338759X)↗

A transport-based framework for solidification cracking in Ni-based superalloys processed by laser powder bed fusion

Solidification cracking remains a persistent barrier to laser powder bed fusion (LPBF) processing of solid-solution-strengthened (SSS) Ni-based superalloys and is commonly attributed to carbide formation, liquation-type failure, or elemental segregation. In this work, the cracking behavior of three SSS Ni-based superalloys—Inconel 625 (625), Inconel 617 (617), and Haynes 230 (230)—is examined under comparable LPBF conditions to evaluate the origins of their cracking susceptibility. Carbides were present in both 625 and 230, yet cracking behavior differed significantly. MC-type carbides in 625 remain discrete and preserve liquid connectivity, whereas Cr-rich M23C6 carbides in 230 form at cellular triple junctions that bottleneck the interdendritic liquid network, influencing cracking through liquid connectivity rather than as an independent cause. Alloy 617 exhibited anomalous segregation without resolvable secondary phases yet cracked mildly, indicating that extensive carbide formation is not a prerequisite for cracking. To rationalize these observations, a transport-limited framework is proposed in which cracking occurs when terminal-liquid feeding cannot accommodate solidification-induced strain; among the mechanisms evaluated, this framework is most consistent with the physical constraints imposed by LPBF solidification. Transport-based crack-susceptibility indexes incorporating permeability, viscosity, and solidification kinetics distinguish the alloy hierarchy; permeability ratios Krat increased from approximately 7 (625) to 11.5 (617) and 14.5 (230), with corresponding increases in the μ-weighted mushy zone risk index (CSIMZRM). These results are consistent with transport-limited liquid feeding as a rate-limiting contributor to solidification cracking in LPBF-processed SSS Ni-based superalloys, providing a physically grounded basis for alloy and process design.

Hyer, Holden [ORNL] (ORCID:0000000343915561)↗

Rapid Alloy Selection and Additive Manufacturing of Nickel Based Superalloys

In this work the rapid alloy selection and subsequent processability via additive manufacturing of nickelbased superalloys was investigated. Rapid alloy selection protocols developed within the project produced two viable nickel-based superalloys. This phase I CRADA demonstrates a viable route for selecting new nickel-based superalloys for additive manufacturing.

36 MATERIALS SCIENCE↗

Physics-based Multiscale Additively Manufactured Superalloy Design for Optimized High Cycle Fatigue Life (Final Report)

The objectives of this project are to: (i) Gain fundamental understandings towards the microscopic damage mechanisms, as impacted by pertinent materials properties (e.g. stacking fault energy (SFE) and microstructure (e.g., grain size), leading to high-cycle fatigue (HCF) damage to AM Ni-based superalloy parts; (ii) Provide scientific insight into the effect of testing frequency on damage mechanisms and fatigue life of AM Ni-based superalloy parts under HCF regime, thereby establishing an appropriate correlation between accelerated testing and materials’ true service life; (iii) Devise an accurate, experimentally validated multiscale model across atomic, micro- and meso-scales, to predict the cyclic stress-strain responses and fatigue damage accumulation for AM Ni-based superalloys under various loading frequencies.

36 MATERIALS SCIENCE↗

Rapid Alloy Selection and Additive Manufacturing of Nickel-Based Superalloys

In this work the rapid alloy selection and subsequent processability via additive manufacturing of nickelbased superalloys was investigated. Rapid alloy selection protocols developed within the project produced two viable nickel-based superalloys. This phase I CRADA demonstrates a viable route for selecting new nickel-based superalloys for additive manufacturing.

36 MATERIALS SCIENCE↗

High strength, superplastic superalloy

High strength superplastic superalloys are produced by extruding a pre-alloyed powder. The cast nickel base superalloy was remelted and converted to pre-alloyed powder by inert gas atomization. The superalloy shows high tensile strength and superplasticity and finds use in hot working and casting.

Ashbrook, R. L.↗

The elastic modulus correction term in creep activation energies Applied to oxide dispersion strengthened superalloy

The effect of elastic modulus and the temperature dependence of elastic modulus on creep activation energies for an oxide dispersion strengthened nickel-base superalloy are investigated. This superalloy is commercially known as Inconel Alloy MA 753, strengthened both by gamma-prime precipitates and by yttria particles. It is shown that at intermediate temperatures, say below 1500 F, where elastic modulus is weakly dependent on temperature, the modulus correction term to creep activation energy is small. Accordingly, modulus corrections are insignificant for the superalloy considered, which shows high apparent creep activation energies at this temperature. On the contrary, at very high temperatures, the elastic modulus correction term can be significant, thus reducing the creep activation energy to that of vacancy self-diffusion. In order to obtain high-temperature creep resistance, a high-value elastic modulus with a weak dependence on temperature is required.

Malu, M.↗

A new diffusion-inhibited oxidation-resistant coating for superalloys

A concept for enhanced protection of superalloys consists of adding an oxidation- and diffusion-resistant cermet layer between the superalloy and the outer oxidation-resistant metallic alloy coating. Such a duplex coating was compared with a physical-vapor-deposited (PVD) NiCrAlY coating in cyclic oxidation at 1150 C. The substrate alloy was MA 754 - an oxide-dispersion-strengthened superalloy that is difficult to coat. The duplex coating, applied by plasma spraying, outperformed the PVD coating on the basis of weight change and both macroscopic and metallographic observations.

Gedwill, M. A.↗

Elevated temperature mechanical properties and residual tensile properties of two cast superalloys and several nickel-base oxide dispersion strengthened alloys

The elevated temperature tensile, stress-rupture and creep properties and residual tensile properties after creep straining have been determined for two cast superalloys and several wrought Ni-16Cr-4Al-yttria oxide dispersion strengthened (ODS) alloys. The creep behavior of the ODS alloys is similar to that of previously studied ODS nickel alloys. In general, the longitudinal direction is stronger than the long transverse direction, and creep is at least partially due to a diffusional creep mechanism as dispersoid-free zones were observed after creep-rupture testing. The tensile properties of the nickel-base superalloy B-1900 and cobalt-base superalloy MAR-M509 are not degraded by prior elevated temperature creep straining (at least up to 1 pct) between 1144 and 1366 K. On the other hand, the room temperature tensile properties of ODS nickel-base alloys can be reduced by prior creep strains of 0.5 pct or less between 1144 and 1477 K, with the long transverse direction being more susceptible to degradation than the longitudinal direction.

Whittenberger, J. D.↗

Iron rich low cost superalloys

An iron-rich low-cost superalloy was developed. The alloy, when processed by conventional chill casting, has physical and mechanical properties that compare favorably with existing nickel and cobalt based superalloys while containing significantly lower amounts of strategic elements. Studies were also made on the properties of Cr(20)-Mn(10)-C(3.4)-Fe(bal.), a eutectic alloy processed by chill casting and directional solidification which produced an aligned microstructure consisting of M7C3 fibers in a gamma-Fe matrix. Thermal expansion of the M7C3 (M = Fe, Cr, Mn) carbide lattice was measured up to 800 C and found to be highly anisotropic, with the a-axis being the predominant mode of expansion. Repetitive impact sliding wear experiments performed with the Fe rich eutectic alloy showed that the directionally solidified microstructure greatly improved the alloy's wear resistance as compared to the chill cast microstructure and conventional nickel base superalloys. Studies on the molybdenum cementite phase prove that the crystal structure of the xi phase is not orthorhombic. The crystal structure of the xi phase is made up of octahedra building elements consisting of four Mo and two Fe atoms and trigonal prisms consisting of four Fe and two Mo atoms. The voids are occupied by carbon atoms. The previous chemical formula for the molybdenum cementite MoFe2C is now clearly seen to be Mo12Fe22C10.

Wayne, S. F.↗