Solvent-free and low temperature synthesis of chalcogenide Na superionic conductors for solid-state batteries
Sodium chalcogenide ionic conductors are attractive candidates as solid electrolytes (SEs) in solid-state Na metal batteries. They show the advantages of high ionic conductivity of 10 –4 –10 –2 S cm –1 at room temperature and great chemical stability in air. However, simple, efficient, and scalable approaches for the synthesis of chalcogenide solid electrolytes (SEs) are required. In this work, we report a solvent-free mixing to form dry intermediate products, which are subjected to different treatments (electron-beam assisted method or low temperature heating (≤150 °C)) to produce pure phase of Na 3 SbS 4-y Se y (0 ≤ y < 2) chalcogenides. Heavy Se-doping in Na 3 SbS 4 results in the tetragonal-to-cubic phase transition as well as a significant change of Sb-S bonding in Raman spectra. Among all chalcogenide SEs, Na 3 SbS 3 Se showed the highest ionic conductivity of 3.75 × 10 –4 S cm –1 at room temperature, 47% higher than that of pristine Na 3 SbS 4 . Moreover, the Se-dopant also enhanced the electrochemical stability towards Na metal in solid-state batteries. The solid-state Na||FeS 2 battery with Na 3 SbS 3 Se SE displayed long-term cycling ability up to 1,000 cycles within the voltage window of 1.0–2.7 V and retained a specific capacity of 105 mAh g –1 after 600 cycles. As a result, this technique promotes the practical applications of chalcogenide SEs in solid-state batteries.