Search NASA⌕ Search

SEARCH · Search NASA

Results for “electrode degradation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

A04-0491 - Reduced Electrolyte Reactivity of Pitch-Carbon Coated Si Nanoparticles for Li-Ion Battery Anodes

Silicon-based anodes for Li-ion batteries (LIB) have the potential to increase the energy density over graphite-based LIB anodes. However, silicon anodes exhibit poor cycle and calendar lifetimes due to mechanical instabilities and high chemical reactivity with the carbonate-based electrolytes that are typically used in LIBs. In this work, we synthesize a pitch-carbon coated silicon nanoparticle composite active material for LIB anodes that exhibits reduced chemical reactivity with the carbonate electrolyte compared to an uncoated silicon anode. Silicon primary particle sizes <10 nm minimize micro-scale mechanical degradation of the anode composite, while conformal coatings of pitch-carbon minimized the parasitic reactions between the silicon and the electrolyte. When matched with a high voltage NMC622 cathode, the pitch-carbon coated Si anode retains -75% of its initial capacity over 1000 cycles. Efforts to increase the areal loading of the pitch-carbon coated silicon anodes to realize real energy density improvements over graphite anodes results in severe mechanical degradation on the electrode level. Developing procedures to engineer the architecture of the composite silicon anode may be a solution to this mechanical challenge.

DIRECT ENERGY CONVERSION,ENERGY STORAGE↗

Proton-Conducting Solid Oxide Electrolysis Cells for Large-scale Hydrogen Production at Intermediate Temperatures

Proton-conducting electrolyte based SOECs offer potential for operation at low to intermediate temperatures. Although yttrium-doped barium zirconate (BZY) and ceria-doped barium zirconate (BCY) have conductivity of 0.01 and 0.017 S.cm -1 respectively at 650C in comparison to the conductivity of 0.015 S.cm -1 for 8-YSZ at 850°C, there remains technology gaps and research needs related to understanding of chemical and structural stability in oxidizing and/or reducing atmospheres at intermediate temperatures, material processing and densification techniques, high polarization losses, and electrode poisoning due to intrinsic and extrinsic gas phase contaminants. Synthesis methods have produced proton-conducting materials and cells that met degradation rate targets, showcasing stable hydrogen production. Improved performance was evident in the HSOEC cell, achieving higher hydrogen production at a lower operating temperature compared to standard cells. Collaborations with multiple research facilities ensured scaling up of synthesis processes and milestone achievements for large-scale manufacturing. Assessment of contaminants revealed their adverse effects on electrode performance and structural stability. Contaminants like Cr and Si compounds, in high humidity, degraded electrodes by forming stable silicate and chromates, inhibiting active surface reactions. Getter materials showed promise in capturing contaminants, suggesting potential for mitigation.

08 HYDROGEN↗

Robust highly durable solid oxide fuel cell cathodes – Improved materials compatibility & self-regulating surface chemistry

Solid oxide fuel cells (SOFCs) are electrochemical conversion devices that directly transform hydrogen or hydrocarbon fuels to electricity, with energy efficiencies as high as 90%, coupled with reduced emissions. Several factors, however, remain to be addressed when considering scale-up of SOFC technology, including the need to overcome decreased performance due to sluggish rates of the oxygen reduction reaction (ORR) at the cathode under reduced temperatures and susceptibility to degradation in performance from surface poisoning e.g. from chromia, while limiting the use of critical raw materials (lanthanides and transition metals) present in high performing mixed ionic electronic conducting electrodes like (La,Sr)CoO 3 (LSC). In this project we explored the key descriptors for determining ORR activity in SOFC electrodes and tried to recover performance degradation by applying them to SOFC electrodes. In order to do this, we first selected a model mixed ionic electronic conducting (MIEC) oxide, Pr-doped CeO 2 (Pr 0.1 Ce 0.9 O 2-δ , PCO), which is a chemically stable fluorite and free of inherent poison sources (e.g. Sr segregation in LSC) that potentially react with external impurities such as Cr-species vaporized from the interconnect. The three approaches originally planned in this project are as follows: 1) evaluation of scavenger exsolution characteristics, 2) study of scavengers gettering efficacy following Cr and Si poisoning and 3) integration of new compositions into porous electrodes. Among them, exceptional progress has been made in 2) and 3), especially understanding the role of surface infiltrants in impacting electrode performance and degradation of PCO materials. We found that the Smith acidity scale for binary oxides serves as a powerful descriptor for tuning and predicting the oxygen exchange kinetics on MIEC PCO surfaces. As a result, with infiltration with binary oxides, ranging from strongly basic (Li 2 O) to strongly acidic (SiO 2 ) onto the surface of porous PCO, it was possible to systematically vary the chemical surface exchange coefficient (k chem ) by 6 orders of magnitude! L i2 O increased k chem by nearly 1,000 times over that of pristine PCO, while SiO 2 decreased k chem by nearly the same factor. Strikingly, although the pre-exponential of k chem scales linearly with the acidity of the infiltrated binary oxide, there is nearly no change in the activation energy. With this insight, we attributed the origin of these dramatic changes in k chem values to the systematic increase and decrease in the surface electron density induced by infiltrated binary oxides. More interestingly, although both Cr 2 O 3 and SiO 2 were determined to be acidic by Smith, suggesting that this feature could likely be the primary reason that these compounds serve to poison the ORR on SOFC cathodes, the effect of poisoning could be subsequently tuned by adding multiple infiltrants and controlling their relative surface acidities. We also systematically examined the effect of serial infiltration of basic and acidic oxides. It turned out that serial infiltration of Li not only recovers approximately 20-fold degraded k chem of PCO by acidic Cr 2 O 3 but its k chem is enhanced even beyond that of the non-infiltrated PCO by more than three orders of magnitude. This was further verified with a screen-printing PCO symmetric cell in terms of the electrode performance (area-specific resistance, ASR) related to approach 3). These observations point to acidity as a key descriptor not only in tuning and predicting the ORR activity of SOFC cathodes that largely determines the overall performance of SOFC, but in mitigating and reactivating poisoned electrode performance. This work provides novel guidelines for making the electrode performance much more active and robust in SOFCs, which can further be applied to all applications requiring oxygen exchange reaction, such as electrolyzers, permeation membranes and gas sensors.

30 DIRECT ENERGY CONVERSION↗

Voltage cycling as a dynamic operation mode for high temperature electrolysis solid oxide cells

Solid Oxide Electrolysis Cells (SOECs) have emerged as a promising technology for the efficient production of H2 via high-temperature electrolysis. However, power input from dynamic energy sources remains a significant challenge for their long-term stability. It is important to analyze the tolerance of cells under dynamic operation conditions. This study focuses on evaluating the impact of voltage cycling on the performance and durability of electrode-supported SOECs. We explore the operational limits and degradation mechanisms of SOECs subjected to various voltage conditions and find that the cells have high tolerance for dynamic voltage. Voltage cycling between 1.3 V and 1.5 V for 9000 cycles does not damage the cell. Conversely, cycling to higher voltages (≥1.7 V) results in accelerated degradation. Advanced characterization is used to screen for various degradation modes post operation. Within the oxygen electrode, XRD and STEM EDS find compositional and phase evolution in all voltage cycled samples including increased decomposition of the air electrode resulting in cation migration. Microstructural analysis of the fuel electrode from nano-CT data shows minimal change throughout the sample set and no evidence of Ni migration, indicating the fuel electrode is stable and not impacted by cycling to higher voltages within the timeframe studied.

Zhu, Zhikuan↗

Microstructure Scale Lithium-Ion Battery Modeling: Part III. When and Where Lithium Plating Occurs and its Correlation with the Electrode Microstructure

Li-ion battery performance and degradation are closely related to the cell’s underlying electrode microstructure. Electrode microstructures are typically characterized with volume-averaged properties that neglect the impact of local heterogeneities. However, local heterogeneities create hot spots that can trigger degradation onset. Herein, a microstructure scale electrochemical model is used to investigate the impact of microstructure heterogeneity on lithium plating. The model predicts lithium plating is not uniform, even when considering a relatively small portion of the electrode (a cross-sectional area of 154×144 µm 2 ), preferring to plate on larger particles as compared to smaller particles. While local heterogeneities control where plating occurs, the model predicts that volume-averaged properties control when plating occurs. Additionally, the model predicts that the active material specific surface area has a linear relationship with the plating onset. However, the linear relationship between increased active material surface area and delayed plating response appears to be sensitive to the microstructure feature used to increase the active interface area. Here, a comparative case-study is explored where the specific surface area is increased by either reducing the active material particle diameter, adding open-porosity cracks, or increasing the active material surface roughness. The model predicts that increasing the specific surface area by reducing the active material particle diameter is the most effective strategy for delaying lithium plating. At 6C, reducing particle size is shown to be 3 and 20 times more effective than, respectively, adding open-porosity cracks and increasing surface roughness. A dual-layer electrode architecture combining gradations both for average properties and uniformities is eventually proposed to improve homogeneous material utilization and reduce degradation at high charge rates.

25 ENERGY STORAGE↗

Performance degradation in proton-conducting ceramic fuel cell and electrolyzer stacks

Proton-conducting ceramics are emerging as enabling materials for efficient electrochemical electricity generation, energy storage, and fuels synthesis. In this work, we present longer-term degradation results for protonic-ceramic fuel cells and electrolyzers based on a BaCe 0.4 Zr 0.4 Y 0.1 Yb 0.1 O 3-δ (BCZYYb) electrolyte. The cells are packaged within unit-cell stacks, including metallic interconnects, current collectors, sealing glasses and gaskets. Durability is found to be superior in protonic-ceramic electrolyzers in comparison to fuel cells. Operating conditions have a large impact on degradation rates; better stability is found at fuel-cell operating temperatures above 600 °C, and electrolyzer steam feeds below 20%. Here, we find that both fuel-cell and electrolyzer degradation is greatly reduced via the introduction of a gadolinium-doped ceria interlayer between the electrolyte and the air–steam electrode. Fuel-cell degradation falls to 1.2% khr –1 under methane fuel at 600 °C; electrolyzer degradation is reduced to 1% khr –1 at 550 °C and 50% steam. Further analyses of electrochemical impedance spectroscopy and distribution of relaxation times provide insight to root processes and degradation phenomena in protonic electroceramics.

25 ENERGY STORAGE↗

Microstructure-based modeling of inner oxygen pressure in solid oxide electrolysis cells: Analysis of electrode delamination and mitigation

One major degradation mechanism during long-term operation of solid oxide electrolysis cells (SOECs) is delamination of oxygen electrodes (OEs). The driving force for the electrode delamination could be the generated high inner oxygen pressure near the electrode-electrolyte interface during operation. However, the effects of transport properties and electrode thickness on the inner oxygen partial pressure are not well understood. Here a microstructure-based electrochemical model, which includes the conduction of electrons and oxygen ions coupled with Butler-Volmer-type chemical reactions at triple-phase-boundaries (TPBs), is employed to investigate the oxygen pressure in lanthanum strontium manganate (LSM)-based SOECs. The model is applied to both two-dimensional (2D) prototype microstructures and three-dimensional (3D) realistic microstructures, and the oxygen pressure is analyzed as a function of transport properties and electrode thickness under both potentiostatic and galvanostatic operations. The simulation results suggest strategies to suppress electrode delamination. The simulation results are compared to an analytical solution, and the discrepancies are attributed to the Butler-Volmer-type kinetics included in the microstructure-based model.

25 ENERGY STORAGE↗

Operando Bragg Coherent Diffraction Imaging of LiNi 0.8 Mn 0.1 Co 0.1 O 2 Primary Particles within Commercially Printed NMC811 Electrode Sheets

Due to complex degradation mechanisms, disparities between the theoretical and practical capacities of lithium-ion battery cathode materials persist. Specifically, Ni-rich chemistries such as LiNi 0.8 Mn 0.1 Co 0.1 O 2 (or NMC811) are one of the most promising choices for automotive applications; however, they continue to suffer severe degradation during operation that is poorly understood, thus challenging to mitigate. Here in this paper we use operando Bragg coherent diffraction imaging for 4D analysis of these mechanisms by inspecting the individual crystals within primary particles at various states of charge (SoC). Although some crystals were relatively homogeneous, we consistently observed non-uniform distributions of inter- and intracrystal strain at all measured SoC. Pristine structures may already possess heterogeneities capable of triggering crystal splitting and subsequently particle cracking. During low-voltage charging (2.7–3.5 V), crystal splitting may still occur even during minimal bulk deintercalation activity; and during discharging, rotational effects within parallel domains appear to be the precursor for the nucleation of screw dislocations at the crystal core. Ultimately, this discovery of the central role of crystal grain splitting in the charge/discharge dynamics may have ramifications across length scales that affect macroscopic performance loss during real-world battery operation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Elucidating Cathode Degradation Mechanisms in LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)/Graphite Cells Under Fast Charge Rates Using Operando Synchrotron Characterization

Li-ion batteries capable of extreme fast charging (XFC) are in demand to facilitate widespread electric vehicle (EV) adoption. While the impact of fast charge on the negative electrode has been studied, degradation of state-of-the-art NMC811 under XFC conditions has not been studied in detail. Herein, cathode degradation is probed in NMC811/graphite batteries by analysis of structural and chemical changes for recovered samples previously cycled under XFC conditions and during typical cycling. NMC surface reconstruction, as determined by soft X-ray absorption, was not detected for recovered electrodes. Furthermore, bulk redox activity from X-ray absorption near edge structure measurements showed more change in the oxidation state of Ni and Co under the 1C charge rate compared to the 4C rate consistent with the electrochemistry. Increased unit cell volume contraction under the 1C rate as determined by operando X-ray diffraction suggests that higher charge rates may provide a protective effect on the cathode by reducing structural distortion due to less delithiation.

25 ENERGY STORAGE↗

Chapter 1: Halide Organic Photovoltaics for Energy: Hybrid Perovskites for Solar Cells

The following sections are included: Fundamentals of Photovoltaics, What Limits PV Device Efficiencies?, Traditional Photovoltaics, Perovskite Halide-Based Hybrid Semiconductors for Photovoltaics: Novel Materials in a League of Their Own, Solution Processability, Tunability, Perovskite Solar Cell Architectures, Pairing Perovskite Absorbers, Reduction/Oxidation and Electrochemical Reactivity Considerations for High-Performance Halide Perovskite Solar Cells, Metal Electrode Corrosion, Proton-Mediated Reduction of Ni3+ at NiOx Interfaces, Electrochemistry in Solid-State Perovskite Devices, Overview of Stability Considerations for High Performance Perovskite Solar Cells, Moisture-Induced Degradation, Oxygen-Mediated Degradation, Illumination-Dependent Degradation, Bias-Dependent Degradation, Stability Considerations for Charge Selective Contacts, Electrode-Induced Degradation Modes, Conclusion, and References.

absorbers↗

Coaxial Nanowire Electrodes Enable Exceptional Fuel Cell Durability

Polymer-electrolyte-membrane fuel cells (PEMFCs) hold great promise for applications in clean energy conversion, but cost and durability continue to limit commercialization. This work presents a new class of catalyst/electrode architecture that does not rely on Pt particles or carbon supports, eliminating the primary degradation mechanisms in conventional electrodes, and thereby enabling transformative durability improvements. The coaxial nanowire electrode (CANE) architecture consists of an array of vertically aligned nanowires, each comprising an ionomer core encapsulated by a nanoscale Pt film. This unique design eliminates the triple-phase boundary and replaces it with two double-phase boundaries, increasing Pt utilization. It also eliminates the need for carbon support and ionomer binder, enabling improved durability and faster mass transport. Fuel cell membrane electrode assemblies based on CANEs demonstrate extraordinary durability in accelerated stress tests (ASTs), with only 2% and 5% loss in performance after 5000 support AST cycles and 30000 catalysts AST cycles, respectively. The high-power density and extremely high durability provided by CANEs can enable a paradigm shift from random electrodes based on unstable platinum nanoparticles dispersed on carbon to ordered electrodes based on durable Pt nanofilms, facilitating rapid deployment of fuel cells in transportation and other clean energy applications.

25 ENERGY STORAGE↗

Oxynitrides enabled photoelectrochemical water splitting with over 3,000 hrs stable operation in practical two-electrode configuration

Solar photoelectrochemical reactions have been considered one of the most promising paths for sustainable energy production. To date, however, there has been no demonstration of semiconductor photoelectrodes with long-term stable operation in a two-electrode configuration, which is required for any practical application. Herein, we demonstrate the stable operation of a photocathode comprising Si and GaN, the two most produced semiconductors in the world, for 3,000 hrs without any performance degradation in two-electrode configurations. Measurements in both three- and two-electrode configurations suggest that surfaces of the GaN nanowires on Si photocathode transform in situ into Ga-O-N that drastically enhances hydrogen evolution and remains stable for 3,000 hrs. First principles calculations further revealed that the in-situ Ga-O-N species exhibit atomic-scale surface metallization. This study overcomes the conventional dilemma between efficiency and stability imposed by extrinsic cocatalysts, offering a path for practical application of photoelectrochemical devices and systems for clean energy.

14 SOLAR ENERGY↗

A Review on Lithium Phosphorus Oxynitride

Lithium phosphorus oxynitride (LiPON) has paved the way for thin film solid-state battery technology development and has shown application in a large range of fields since its first reported synthesis in 1993. The term LiPON describes the family of materials with the general formula of LixPOyNz offering a great range of stoichiometries with varying properties. Understanding how the properties of LiPON are affected by different preparation methods is important for tuning this material to fit the required application. It is also useful to understand the LiPON relation between the amorphous structure and ionic conductivity, as well as the electrochemically degradation in contact with electrode materials. This review summarizes various methods of synthesizing LiPON and evaluates them on the basis of multiple properties of the resulting material. Structure–property relationships are identified to categorize the various LiPON stoichiometries that have been synthesized. Possible lithium ion conduction pathways and electrochemical degradation mechanism in LiPON are discussed. Representative applications of LiPON films are also introduced. At the end of this review, insights for future research into LiPON materials are provided.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In Situ Reliability Investigation of All-Vanadium Redox Flow Batteries by a Stable Reference Electrode

Redox flow batteries (RFBs) have been studied over the past several decades as a promising candidate for stationary energy storage applications. It is therefore important to understand the reliability of RFBs and the mechanisms that cause degradation with time. Contributions from individual electrodes (cathode or anode) are difficult to separate especially for long-term cycle testing, due to the lack of a stable reference electrode. In our work, the reliability and degradation mechanisms of an all-vanadium RFB were investigated by a stable reference electrode based on the dynamic hydrogen electrode (DHE). With factor exploration and design optimization, the newly developed DHE reference electrode demonstrated high accuracy and long-term stability that enables in-situ monitoring of individual electrode signals (potentials and impedances) over hundreds of cycles in a vanadium RFB. This approach enables the full cell degradation to be separated and the degradation attributed to contributions from the cathode and anode. The cathode and anode were found to play quite different roles in the increase in overpotential of the vanadium RFB during long-term cycling. The anode reaction limited both the charge and discharge capacity over 100 cycles. In addition, the negative side also appeared to be the rate limiting factor throughout cycling as determined by EIS measurement. The cathode contributed to the performance degradation as cycling exceeded 50 cycles.

Huang, Qian↗

Three-Dimensional Mapping of Resistivity and Microstructure of Composite Electrodes for Lithium-Ion Batteries

Nanoparticle silicon–graphite composite electrodes are a viable way to advance the cycle life and energy density of lithium-ion batteries. However, characterization of composite electrode architectures is complicated by the heterogeneous mixture of electrode components and nanoscale diameter of particles, which falls beneath the lateral and depth resolution of most laboratory-based instruments. In this work, we report an original laboratory-based scanning probe microscopy approach to investigate composite electrode microstructures with nanometer-scale resolution via contrast in the electronic properties of electrode components. Applying this technique to silicon-based composite anodes demonstrates that graphite, SiOx nanoparticles, carbon black, and LiPAA binder are all readily distinguished by their intrinsic electronic properties, with measured electronic resistivity closely matching their known material properties. Resolution is demonstrated by identification of individual nanoparticles as small as ~20 nm. Our technique presents future utility in multiscale characterization to better understand particle dispersion, localized lithiation, and degradation processes in composite electrodes for lithium-ion batteries.

25 ENERGY STORAGE↗

Mapping of Heterogeneous Catalyst Degradation in Polymer Electrolyte Fuel Cells

Pt catalysts in polymer electrolyte fuel cells degrade heterogeneously as the catalyst particles are exposed to local variations throughout the catalyst layer during operation. State-of-the-art analytical techniques for studying degradation of Pt catalysts do not possess fine spatial resolution to elucidate such non-uniform degradation behavior at a large electrode level. A new methodology is developed to spatially resolve and quantify the heterogeneous Pt catalyst degradation over a large area (several cm ) of aged MEAs based on synchrotron X-ray microdiffraction. PEFC single cells are aged using voltage cycling as an accelerated stress test and the degradation heterogeneity at a micrometer length scale is visualized by mapping Pt catalyst particle size after voltage cycling. It is demonstrated in detail that the Pt catalyst particle size growth is non-uniform and follows the flow field geometry. The Pt particle size growth is greater in the area under the flow field land, while it is minimal in the area under the flow field channel. Additional non-uniformity is observed with the Pt particle size increasing more rapidly at the air outlet area than the Pt particle size at the inlet area.

36 MATERIALS SCIENCE↗

Multiscale electro-chemo-mechanical model of high-capacity amorphous silicon anode material in sodium-ion batteries

The growing interest in sodium-ion batteries (SIBs) is fueled by their abundant resources and environmentally friendly nature, with amorphous silicon (a-Si) emerging as a promising anode material for enhancing capacity. However, the key challenge lies in sustaining reversible capacity during cycling. Here, in this work, we developed a multiscale electrochemical model incorporating an a-Si anode to elucidate the performance parameters of SIBs. Additionally, we integrated an electro-chemo-mechanical model at the particle level to capture stress generation, an essential factor in the degradation of high-capacity electrodes. Unlike existing models, our approach accounts for large-deformation chemo-mechanics at the particle scale and includes simulations under varying charge rates to explore multiscale behavior. The results reveal that coupled sodiation significantly prolongs complete cycling times and influences discharge dynamics, indicating that neglecting this coupling leads to an underestimation of actual capacity. Furthermore, we observed pronounced polarization effects at higher charge rates, resulting in heterogeneous stress distributions across the anode. With the identification of critical failure parameters for both active particles and binder materials, offering novel insights for mitigating degradation in high-capacity electrode systems.

Amorphous silicon anode↗