Photovoltage behaviour of p-Sb 2 S 3 photocathodes for hydrogen evolution: effect of n-In 2 S 3 passivation layers

The 1.76 eV band gap of antimony(iii) sulphide (Sb 2 S 3 ) makes this semiconductor material a promising light absorber for photoelectrochemical water splitting, but scalable fabrication approaches to efficient devices are still lacking. Here we show that compact Sb 2 S 3 films on FTO can be obtained by electrochemical growth from aqueous colloidal sulphur and antimony trichloride solutions, followed by mild annealing. These films can be converted into hydrogen evolution photocathodes after coating with In 2 S 3 passivation layers and the addition of Pt proton reduction co-catalysts. For the first time, vibrating Kelvin probe surface photovoltage (VKP-SPV) spectroscopy is used to observe the carrier dynamics in such photoelectrodes. While the bare Sb 2 S 3 films suffer from high surface recombination rates and poor electron extraction, the In 2 S 3 overlayer is found to raise the photovoltage and cathodic photocurrent density, due to passivation of surface defects and formation of a p–n heterojunction. In thick In 2 S 3 films, these benefits are offset by shading and slow electron transfer. Also, we find that O 2 strongly affects the band bending in the Sb 2 S 3 –air and In 2 S 3 –air junctions and their photovoltage. The optimised devices evolve H 2 at 77.5% Faradaic efficiency and with 0.084% applied bias photon-to-current efficiency (ABPE) at 0.12 V vs. RHE. The low ABPE value is attributed to Sb 2 S 3 sub-bandgap defects visible in SPV spectra, the random orientation of Sb 2 S 3 crystallites in the films, which inhibits charge transport, the absence of crystal facets of Sb 2 S 3 , and a detrimental Schottky junction at the FTO|Sb 2 S 3 interface.

de Araújo, Moisés A. [University of California, Da

Bipolar Ag-Zn battery

The silver-zinc (AgZn) battery system has been unique in its ability to safely satisfy high power demand applications with low mass and volume. However, a new generation of defense, aerospace, and commercial applications will impose even higher power demands. These new power demands can be satisfied by the development of a bipolar battery design. In this configuration the power consuming, interelectrode current conductors are eliminated while the current is then conducted via the large cross-section electrode substrate. Negative and positive active materials are applied to opposite sides of a solid silver foil substrate. In addition to reducing the weight and volume required for a specified power level, the output voltage performance is also improved as follows. Reduced weight through: elimination of the plastic cell container; elimination of plate leads and intercell connector; and elimination of internal plate current collector. Increased voltage through: elimination of resistance of current collector; elimination of resistance of plate lead; and elimination of resistance of intercell connector. EPI worked previously on development of a secondary bipolar silver zinc battery. This development demonstrated the electrical capability of the system and manufacturing techniques. One difficulty with this development was mechanical problems with the seals. However, recent improvements in plastics and adhesives should eliminate the major problem of maintaining a seal around the periphery of the bipolar module. The seal problem is not as significant for a primary battery application or for a requirement for only a few discharge cycles. A second difficulty encountered was with activation (introducing electrolyte into the cell) and with venting gas from the cell without loss of electrolyte. During previous work, the following projections for energy density were made from test data for a high power system which demonstrated in excess of 50 discharge/charge cycles. Projected system power = 100 kilowatts; discharge time = 30 seconds; discharge current density = 1.75 amps/sq in.; system weight = 86 lbs (9.7 WH/lb); and system volume = 1071 cu. in. (.78 WH/cu. in.). EPI is currently working on a development program to produce a bipolar silver-zinc battery design for NASA. The potential application would be to power electromechanical actuators for space launch vehicles.

Giltner, L. John

FY26 Progress on Demonstration of a Multiphysics Steady State Capability for Modeling Core Radial Expansion in SFRs

Under the U.S. Department of Energy Office of Nuclear Energy Advanced Modeling and Simulation (NEAMS) Program, an integrated multiphysics approach is being developed to model the core bowing phenomena important to liquid metal-cooled fast reactors. Core bowing is an important passive safety mechanism in liquid metal-cooled fast reactors and involves multiphysics effects including radiation transport, fluid flow, heat transfer, and mechanical response to temperature and flux gradients. This report summarizes recent progress on developing a multiphysics, MOOSE-based workflow to predict core bowing and associated reactivity feedback. Significant new capabilities in the reactor physics code Griffin - sodium backfill and pin power reconstruction for deformed geometries - were applied in this effort. This year’s work included verification, code comparisons, sensitivity studies, and coupled demonstrations that advance the state of MOOSE-based core bowing workflow. Griffin’s sodium backfill capability was verified by demonstrating that its automated treatment of geometry expansion and material-density updates reproduces manual calculations exactly, confirming solid mass conservation and proper coolant backfilling in expanded geometries. Reconstructed pin powers were compared for Griffin’s ductheterogeneous and ring-heterogeneous treatments in single-, seven-, and nineteen-assembly cases, with best agreement observed in lower-leakage configurations and the duct-heterogeneous approach offering substantially lower computational cost. Thermal-hydraulic sensitivity sensitivities showed that MOOSE SCM, SAM, and CFD are expected to produce similar deformation predictions despite variances in their temperature predictions, and that explicit treatment of inter-assembly flow becomes increasingly important as gap flow rate increases. Finally, coupled demonstrations on small multi-assembly configurations using Griffin, MOOSE Solid Mechanics, MOOSE SCM, and Heat Conduction produced physically consistent reactivity feedback from thermal expansion and bowing. The coupled demonstrations simulated grid plate expansion as well as resultant core bowing at full power conditions. Simplifications were made in current workflow, namely the assumption of instantaneous full power conditions following hot zero power, and pre-expanding the Griffin geometry axially due to lack of an axial fuel pin expansion model and temperature feedback to Griffin.

Wozniak, Nicholas

Delamination recycling of multilayer plastic films: Solvent-assisted separation pathways and recovery of solid polyolefins

Multilayer plastic films are excellent packaging materials due to the bound layers of multiple polymers, with each different polymer contributing to the film properties. Desirable properties lead to continuously growing demand for multilayer films. Multilayer plastic films are typically single-use and, as such, their increased production and disposal have led to waste management problems. Multilayer films are not currently recyclable primarily due to the multiple bound polymers. This work advances delamination as a recycling process to separate and sequester valuable polymers from multilayer films, facilitating the incorporation of these polymers into the circular economy. We effect delamination in a physical process that preserves targeted polymers as solid film, hence retaining their embodied energy. This work documents three different pathways of inducing delamination of multilayer films, with appropriate solvents disrupting adhesion between adjacent layers or dissolving a minor component of the film in less than an hour and at temperatures below 90°C, and where all initial polyethylene is maintained in its solid form throughout the process and is recovered at high purity. Solvent-based delamination is exemplified on commercial multilayer films with majority polyethylene (PE), and polyethylene terephthalate (PET) or ethylene vinyl alcohol copolymer (EVOH) or nylon also present. Solvent-based delamination is an energy-efficient and environmentally friendly recycling process that improves upon dissolution-precipitation recycling, since delamination involves very little dissolution and no precipitation, and is superior to pyrolysis which breaks down the polymers, while delamination keeps polymer chains intact. Furthermore, delamination recycling can contribute to the sustainable use of multilayer films as they continue to protect our food and medicine.

Chemical Recycling

NASA Alternative Orion Small Cell Battery Design Support

The NASA Orion Crew Module Reference Design was produced to address large scale thermal runaway (TR) hazard with specific safety controls for the Orion Spacecraft. The design presented provides the description of a full scale battery design reference for implementation as a drop in replacement to meet all spacecraft energy requirements with compatible 120 Vdc electrical and mechanical interface using small cell technology (18650) packaging. The 32V SuperBrick incorporates unique support features and an electrical bus bar arrangement that allows cells negative can insertion into heat sink that is compressively coupled to the battery enclosure to promote good thermal management. The housing design also provides an internal flame suppression "filter tray" and positive venting path internal to the enclosure to allow hot effluent ejecta to escape in the event of single cell TR. Virtual cells (14P Banks) that are supported to provide cell spacing with interstitial materials to prevent side can failures that can produce cell to cell TR propagation. These features were successfully test in four separate TR run with the full scale DTA1 test article in February 2016. Successfully Completed Test Objectives - Four separate TR test runs with Full-Scale DTA1 housing with Two SuperBricks, Two SuperBrick Emulators All Tests resulted in "clean" gas with less than 6 C rise at Battery vent All Tests resulted in less than 2 C temperature rise on cold-plate outlet All Tests resulted in less than 6 psi pressure rise in the battery housing Test Run 1 -One neighbor cell TR, highest remaining neighbor 139 C. Ejecta shorted to bus caused prolonged additional heating, One shorted cell did experience TR after 12 minutes, remaining cells had adequate thermal margin Test Run 2 - No cell to cell propagation, highest neighbor cell 112 C; Test Run 3 - No cell to cell propagation, highest neighbor cell 96 C; Test Run 4 - No cell to cell propagation, highest neighbor cell 101 C; Primary TR testing and analysis were completed and reviewed for endorsement by NASA Engineering and Safety Center team members. All Key Test Objectives were met and the small cell design alternative was demonstrated and selected to be a feasible drop in replacement for the MPCV Orion CM Battery for EM2 mission.

Haynes, Chuck

Tailored Solvent Treatment for Optimized Production of Upcycled Anodes from End-Of-Life Li-Ion Batteries

Recycling processes for lithium-ion batteries typically overlook graphite because of its lower market value relative to that of transition-metal-containing cathode materials. However, graphite recovered from cycled lithium-ion batteries holds additional engineered value associated with the solid-electrolyte interphase (SEI). The SEI contributes critical electronic passivation of the graphite surface but becomes highly resistive with extended cycling, yielding poor cell performance. In this work, we apply tailored solvent treatment to end-of-life (EOL) graphite anodes to selectively remove adverse SEI components while retaining beneficially passivating species. We evaluate a series of polar protic solvents to achieve targeted removal of SEI components and control selectivity through rational variation in solvent properties. The physiochemical properties of treatment solvents correlate with both the retained SEI composition and the corresponding electrochemical performance of solvent-treated “upcycled” graphite anodes. Within the initial set of solvents evaluated, top-performing candidates show capacity and Coulombic efficiency nearly equivalent to those of an analogous pristine anode, as well as promising electrochemical performance enhancement with regard to irreversible capacity-loss metrics. This study establishes critical design principles for an optimized anode upcycling method that enhances the value of recycled graphite by retaining and upgrading the SEI.

25 ENERGY STORAGE

The Origin of Palimpsests

Palimpsests are the most enigmatic impact features observed on icy worlds of the Solar System. Palimpsests are large impact features which are bright, old, mostly flat, and roughly circular. They range from >150 to ~350 km in diameter and sometimes exhibit recognizable associated radial secondary ejecta crater strings beyond their rims. Curiously, among all the Solar System's icy worlds, palimpsests are exclusively seen on the icy Galilean moons. Palimpsests are obviously different than similarly sized impact features seen on other icy satellites. For example, Evander, a 350 km diameter peak-ring impact basin on Saturn’s moon Dione, has a very low depth/diameter ratio of 0.008, indicating significant viscous relaxation. Nevertheless, it still retains short wavelength topography including a prominent central peak, peak ring, and a continuous rim, none of which are seen at palimpsests. Palimpsests display an approximately circular, and dominating, expanse of undulating plains, which is level with surrounding terrain and shows no recognizable rim. At the center of palimpsests are smooth central plains that are enclosed by a low scarp. Central plains material superposes the surrounding undulating plains and is littered with small blocks reminiscent of “small chaos” on Europa. Palimpsests have yet to be explored using modern impact simulation tools. We have begun to investigate two competing hypotheses: (A) Palimpsests form on targets which have a preexisting near-subsurface layer that is liquid or solid but very weak, and is excavated as proximal ejecta; or (B) They form in a solid ice target underlain by a steep thermal gradient that strongly influences the resulting impact feature, including the production of impact-induced melting at depth that is then a major component of proximal ejecta. Our results will have profound implications for the early thermal history of the icy Galilean satellites. We will test our two hypotheses for the formation of palimpsests on Ganymede (where they are both best observed and preserved) by means of 2D iSALE hydrodynamic simulations of impacts into ice targets that will be structured according to the scenarios for each hypothesis, with select runs in 3D. We have already conducted a pilot study using 2D iSALE that has yielded promising results, which we will report out at the meeting.

palimpsests

Understanding Photovoltage Deficits in Electrochemically Grown Tin Sulfide (SnS) Thin-Film Photovoltaic Devices

Tin­(II) sulfide (SnS) is an earth-abundant semiconductor with a direct optical bandgap of ca. 1.1 eV, which makes it a promising absorber material for thin-film photovoltaic (PV) devices. However, existing devices have significant photovoltage deficits, which may be related to the anisotropic structure of the layered Herzenbergite SnS crystal structure. Here, we explore electrochemical deposition as a near room temperature path to oriented SnS crystal films on Mo and FTO substrates and employ vibrating Kelvin probe surface photovoltage (SPV) spectroscopy and J–V measurements to identify conversion losses in them. According to grazing-incidence X-ray diffraction and SEM, the SnS films consist of crystalline microplates with preferred orientation in the [111] and [001] directions. The bare SnS films produce only small and irreversible surface photovoltage signals, due charge trapping and recombination at the SnS surfaces, but addition of a CdS buffer layer lowers the charge recombination rate by 2 orders of magnitude and increases both the photovoltage and its reversibility due to the formation of a p-SnS/n-CdS junction. According to SPV, the FTO/SnS back interface (but not the Mo/SnS interface) forms a detrimental p–n junction that hinders hole transfer. Additional shunting through the relatively open microcrystal SnS layers and a lower conductivity of the FTO substrate explain the low power conversion efficiencies of the final devices (0.18 and 0.10% for the Mo and FTO substrates). Altogether, this work establishes a low-temperature path for the fabrication of crystalline SnS film-based solar cells and identifies the bottlenecks that limit high photoconversion efficiency.

deposition

Calculations of the Moon's Thermal History at Different Concentrations of Radioactive Elements, Taking Into Account Differentiation on Melting

Calculations of the thermal history of the moon were carried out by solving the thermal conductivity equation for the case in which the heat sources are the long-lived radioactive elements Th, U, and K 40 . The concentrations of these elements were adjusted to give four variations of the heat flow: 1.35 x 10 -8 and 0.91 x 10 -6 cal cm -2 s -1 (I and I**), 0.61 x 10 -6 (variant II, the terrestrial mixture of Lyubimova and Starkova), and 0.236 x 10 -6 (variant III, the chondrite model of Urey and MacDonald). In the same calculations, we considered layering of the differentiated material with transport to the surface of the radioactive elements after the temperature of the layer rose to 200 K above the melting temperature, which is considered in five variants that differ in the amount of transported radioactive elements: 100 percent ( n = 1), 80 percent n = 0.8), 40 percent, 20 percent ( n = 0.6, 0.4, 0.2). During fusion the heat capacity and heat conductivity were changed. We considered two variants of an initially cold (273 K) and hot (900 K) Moon. Calculations show that the interior of the Moon was heated to melting during the first 0.7 to 2.3 x 10 9 years. The maximum fusion involved practically the entire Moon to a distance from 15 to 45 km beneath the surface, and started 3.5 to 4.0 x 10 9 years ago (I, I**), or 2.5 to 3.0 x 10 9 years ago (II, III) and continued for 1 to 2 x 10 9 years. Today the Moon is cooling. The current thickness of the solid crust is from 150 to 200 km and the heat flow exceeds the stationary value 1.5 fold. Apparently the most realistic variant is II (terrestrial mixture) for an initially hot Moon, and gives, regardless of the moderate concentration of radioactive elements, a heat flow of 0.9 to 0.95 x 10 -6 cal cm -2 s -1 , which agrees with the radioastronomical measurements of Troitsky and Krotikov and with the Apollo 15 data.

O I Ornatskaya

Distributed Mafic Rock Resources for Carbon Mineralization in Arizona

Ex-situ carbon mineralization is a process by which CO2 is reacted with alkaline silicate minerals and rocks to produce stable carbonate materials, which can be used for other industrial processes. Arizona, U.S.A., hosts abundant surficial mafic rocks in three young volcanic fields, Geronimo-San Bernardino, San Francisco, and Springerville, and other distributed locations throughout the state. We created a Mafic Rock Resource Inventory (MRRI) that categorizes geochemical, physical, and textural characteristics of a diverse suite of surficial mafic rock samples and provide a benchmark reaction dataset parameterizing the temperature, pressure, and pH conditions best suited ex-situ mineralization in different rock types. MRRI data is publicly available online via a map-viewer. We establish two reaction condition sets, varied in temperature, pressure, and pH, where crystal-rich and glassy rocks reach maximum reaction extent and different carbonate phases are formed. Systematic ex-situ mineralization experiments on 21 diverse rock types show trends in geochemical, mineralogical, and reactivity behavior and establish maximum effective capture capacity. From this, scoria cones in three Arizona volcanic fields have a ~62 Gt effective CO₂ storage capacity with one of the fields having a ~42 Gt storage capacity in lava flows. Reactivity results have applications to alkaline mafic rock resources exposed globally, including producing additional effective storage capacity estimates and scaled commercialization of mafic rock ex-situ mineralization, should reaction extents be improved through advances in mineralization techniques. MRRI data were used to create a Direct Air Capture to Mineralization (DACM) systems model, technoeconomic analysis, and life-cycle assessment. These documents are presented as three appendices.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI

Mechanics of Preloaded Bolt Tensile Loading With Focus on Load Introduction Factor

The bolt tensile and joint separation loads are directly influenced by the locations at which the external loads enter the clamped members of a preloaded bolted joint (PBJ) and the associated load-paths through the joint. This physical load introduction mechanism affecting the bolt tensile loading is typically represented in the bolt tensile load equation, in part, by a load introduction factor (LIF), which was shown by H.M. Lee of Marshall Spaceflight Center to be a natural product of the bolt tensile load equation using a linear spring stiffness model. This LIF, being a function of load-path stiffness, has subsequently been denoted as the stiffness-based LIF (SBLIF), providing a framework to calculate the LIF using whatever load-path stiffness approximations are appropriate. Expanding upon the work of Lee, it is shown that the SBLIF and the joint stiffness factor are functions of the stiffnesses of the same load-paths and regions within a PBJ, and thus they should not be treated as independent variables. Mathematical expressions for the SBLIF are presented. Comparisons are shown between the analytically calculated SBLIF, the analytically calculated geometric LIF (GLIF), which is a simple clamped-member thickness ratio, the experimentally derived LIF, and the LIF determined by finite element analysis (FEA). Using experiment and FEA as a benchmark, the SBLIF, using traditional load-path stiffness approximations, enables a more accurate prediction of bolt tensile loading than the GLIF, although it can be unconservative near joint separation. The GLIF generally attributes more of the externally applied tensile load to the bolt than does the SBLIF, potentially resulting in heavier and/or more costly bolted joints. Mathematical relationships between the SBLIF and the GLIF are developed. Supplemental material is provided in the appendixes where the historical practice of using the joint compressive stiffness in place of the joint tensile stiffness is evaluated. The appendixes include step-by-step examples demonstrating the calculation of the SBLIF using traditional stiffness approximations and conclude with the development of the joint diagram in terms of the SBLIF, culminating into formulas for the key features of a joint diagram, which is useful for programming.

Load Path

Block-Type Antiferromagnetism in Single Chain Quasi-One-Dimensional K 3 ⁢Fe 2 ⁢Se 4

One-dimensional (1D) structures provide a unique platform to study the correlated quantum interactions and phase transitions such as unconventional magnetism and superconducting states. Here, we report that iron chalcogenide K 3 ⁢Fe 2 ⁢Se 4 exhibits an unusual block-type canted antiferromagnetic (AFM) order with a clear single chain quasi-1D structure, which is structurally different from the two-leg ladder BaFe 2 ⁢Se 3 , through both experimental measurements and density matrix renormalization group (DMRG) calculations. The narrow bandgap semiconductor K 3 ⁢Fe 2 ⁢Se 4 has a quasi-1D edge-shared FeSe4 tetrahedra chain structure and orders antiferromagnetically below 110 K. The magnetic moments couple antiferromagnetically along the quasi-1D chain direction of the 𝑏 axis and form an up-down-down-up (↑−↓−↓−↑)–like spin structure with a commensurate propagation vector 𝒌=⁢(0,0,0), where block-type spin ↑−↑ or ↓−↓ coupling are between the longer Fe-Fe bonds of the quasi-1D chain. DMRG results show that block antiferromagnetic state is stable in K 3 ⁢Fe 2 ⁢Se 4 and reveal that the block-ordered arrangement of Fe 2.5+ ions spins arise from the competition between ferromagnetic and AFM interaction in the presence of strong electronic correlation. Our research results not only report the discovery of a clear block-type canted antiferromagnetic structure in a real quasi-1D chain material but also provide a theoretical approach to understand the block-type antiferromagnetism in quasi-1D iron chalcogenides.

antiferromagnetism

Introduction to Radiation Issues for International Space Station Extravehicular Activities: Chapter 1

The International Space Station (ISS) provides significant challenges for radiation protection of the crew due to a combination of circumstances including: the extended duration of missions for many crewmembers, the exceptionally dynamic nature of the radiation environment in ISS orbit, and the necessity for numerous planned extravehicular activities (EVA) for station construction and maintenance. Radiation protection requires accurate radiation dose measurements and precise risk modeling of the transmission of high fluxes of energetic electrons and protons through the relatively thin shielding provided by the space suits worn during EVA. Experiments and analyses have been performed due to the necessity to assure complete radiation safety for the EVA crew and thereby ensure mission success. The detailed characterization described of the material and topological properties of the ISS space suits can be used as a basis for design of space suits used in future exploration missions. In radiation protection practices, risk from exposure to ionizing radiation is determined analytically by the level of exposure, the detrimental quality of the radiation field, the inherent radiosensitivity of the tissues or organs irradiated, and the age and gender of the person at the time of exposure. During low Earth orbit (LEO) EVA, the relatively high fluxes of low-energy electrons and protons lead to large variations in exposure of the skin, lens of the eye, and tissues in other shallow anatomical locations. The technical papers in this publication describe a number of ground-based experiments that precisely measure the thickness of the NASA extravehicular mobility unit (EMU) and Russian Zvezda Orlan-M suits using medical computerized tomography (CT) X-ray analysis, and particle accelerator experiments that measure the minimum kinetic energy required by electrons and photons to penetrate major components of the suits. These studies provide information necessary for improving the understanding of the current ISS space suits and provide insights into improved approaches for the design of future suits. This chapter begins with a summary of the dynamic ionizing radiation environment in LEO space and introduces the concepts and quantities used to quantify exposure to space radiation in LEO. The space suits used for EVA and the experimental partial human phantom are described. Subsequent chapters report results from measured charged particle fields before and after incident protons and secondary particles are transported through the space suits and into organs and tissues.

M R Shavers

Probing the role of local tunnel variations in early-stage lithiation of α-MnO₂ nanowires via in situ TEM

Understanding lithium-ion transport in tunnel-structured manganese oxides is essential for designing high-performance lithium-ion battery electrode materials. Here, we elucidate the early-stage lithiation mechanism of potassium-stabilized α-MnO 2 nanowires using in situ transmission electron microscopy (TEM) coupled with electron energy-loss spectroscopy (EELS), high-resolution TEM (HRTEM), and geometric phase analysis (GPA). Real-time TEM imaging reveals clear volume expansion at the reaction front, while EELS analysis uncovers lithium-ion diffusion far beyond this region, where no visible expansion is observed, indicating fast, defect-assisted transport. GPA and HRTEM analyses show that localized tensile and compressive strain fields, originating from pre-existing local tunnel structural variations, persist after lithiation. The tensile-strained regions enable lithium-ion insertion with minimal lattice distortion, offering additional free volume that facilitates rapid lithium-ion accommodation ahead of the structural transformation. Our results demonstrate a local tunnel variation-mediated fast diffusion pathway that precedes bulk reaction, underscoring the critical role of local strain in enabling early-stage lithium transport. Given the structural versatility of MnO 2 and its ability to accommodate diverse atomic arrangements beyond the well-known tunnel phases (β-, γ-, δ-, λ-, R-phases), our findings highlight the importance of understanding and engineering local structural environments. This work provides fundamental insights into the interplay between defects, strain, and ion dynamics, and presents defect engineering as a promising approach to enhance both rate performance and structural stability in manganese-based cathodes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND

Final Report Document: Microgravity Medical Eyewash B

Senior Capstone Design Team 15 has been commissioned by the National Aeronautics and Space Administration (NASA) to redesign the current microgravity eye wash station. The current design exhibits four primary limitations: single-use operation, excessive mass and volume, operational complexity requiring coordination with external systems, and dependence on frequent Earth resupply missions. Our updated eyewash design will be deployed on long-range space missions that could last multiple years. Based on these and other requirements from our customer, we have developed our updated eyewash design. Our compact, single-eye system uses capillary-driven flow and a free-floating water ball. This design allows us to eliminate pumps and bulky tubing, decreasing the mass and volume of the overall system. The containment eyecup is held to the astronaut's face with a strap, and a silicone seal prevents leakage while improving user comfort. Contaminated water is contained within a disposal bag containing wicking material to pull it back out of the eyecup after washing the eye. This system is reusable, efficient, and easy to activate quickly. We evaluated our design through calculations, microfluidic testing, and user try-on testing to verify our requirements. Our work demonstrated that steady-state flow was capable with our capillary framework, achieving 1.31 L/min. The prototype construction confirmed mass and volume reductions, and try-on-testing evaluated the ability to put on the system quickly. Almost all major design requirements were achieved, and water loss could be validated by testing in microgravity. Our design went through a number of iterations to reach the final solution presented in this report. These changes were driven by our testing and collaboration from each member of the team. Updated models optimized tube placement and geometry of the eyecup to better direct flow as it pools across the eye. Changes to our tubing bends improved capillary efficiency and increased the flow rate we were capable of achieving. And improved bracket placements adjusted the fit, comfort, and seal of the eyecup to the astronaut's face. Our capillary-based eyewash system is technically feasible and has been theoretically validated to operate effectively in microgravity conditions. Testing and analysis indicate that it can meet or exceed the required performance metrics, including flow rate and safety constraints. Overall, the design represents a viable alternative to current ISS-dependent eyewash systems for future space missions.

Jeffrey Allen

Generation of 3.3-mJ, 2.45-µm, sub-2-cycle laser pulses via hollow-core fiber pulse compression

We demonstrate nonlinear compression of mid-infrared pulses from a Cr:ZnSe chirped-pulse amplifier using a gas-filled stretched hollow-core fiber followed by bulk-material compression. Starting from 90 fs, 2.45 µm pulses with 5.3 mJ energy, spectral broadening in the gas-filled capillary combined with optimized dispersion management enables compression to 15 fs, less than two optical cycles at 2.45 µm, with 3.3 mJ pulse energy, corresponding to a peak power of approximately 0.12 TW. The simplicity of the approach, based on a single hollow-core fiber stage and bulk dispersion compensation, makes it scalable to higher energies and establishes a robust route to mid-infrared drivers for high harmonic generation and attosecond applications.

Britton, Mathew [SLAC National Accelerator Laborat

Evaluation of Fatigue Damage Accumulation Functions for Delamination Initiation and Propagation

The present report follows on the cohesive fatigue damage model methodology proposed in NASA-TP-2018-219838. In that report, an empirical function describing the incremental damage due to cyclic loading was used to calculate fatigue damage within a cohesive formulation. The form of the function was developed such that, when integrated at a constant stress amplitude from no damage to failure, it produces a life versus load response that is consistent with an S-N diagram. Therefore, the parameters of the damage model could be obtained by fitting the model predictions to an S-N diagram. The finite element analyses performed demonstrate that the cohesive fatigue accumulation function provides a link between the S-N diagram that describes crack initiation, and the Paris law that characterizes the rate of crack propagation. However, when the model was proposed, it was not known whether the form of the damage accumulation function associated with a desired S-N diagram is unique and, if not, if the link between S-N and the Paris law is unique and independent of the fatigue function selected. In the effort described herein, several alternative forms of the damage function that reproduce the desired features of S-N diagrams were found and evaluated. The effects of each of these functions on the predicted parameters of the Paris law and the propagation threshold are discussed. The results indicate that the predicted exponent m of the Paris law is indeed independent of the damage accumulation function. However, different functions predict different values for the pre-factor C of the Paris law. Therefore, the proper damage accumulation function must be selected by comparison with experiments. One of the new damage accumulation functions proposed herein was found to be particularly useful for analysis because of the ease with which the model parameters can be determined with a minimal amount of experimental information. The effectiveness of the proposed methodology and damage function was demonstrated by conducting analyses of a double cantilever beam test, a mixed-mode bending test, and a three-point bending test of a skin/doubler specimen. The results indicate that the same set of model parameters can provide accurate predictions of the rate of fatigue crack propagation for a variety of material interfaces, mode mixities, load levels, and stress ratios.

DKIN/Stiffener Debonding

Laser Forming of Sheet Metal for In-Space Manufacturing Applications

As the in-space economy matures, the migration of typically Earth-bound manufacturing methods, such as metal forming and joining, up to space will be required to meet the increasing demand for refueling and supply depots, habitats, laboratories, lunar surface structures, and sites for deep-space exploration shipbuilding. Only in this way can the magnitude of individual structures begin to exceed what can be launched, deployed, docked, or inflated and allow true economies of scale to be unlocked in space. However, typical terrestrial methods of forming and shaping sheet metal require massive machinery with the ability to deflect reaction forces to a large mass in a fixed reference frame (Earth). To both limit up-mass required for manufacture and to mitigate the issues of reaction forces in the relative reference frames of space, a non-contact, laser-based method of forming metal sheet is proposed. NASA Marshall Space Flight Center (MSFC), in cooperation with DARPA and the University of Florida (UF), have begun investigation of non-contact methods of laser forming sheet metal in thermal vacuum (TVAC) conditions to great success. To date, several grades of aluminum, stainless steel, and titanium coupons have been formed via laser-induced internal stresses in these metals at both ambient atmosphere and vacuum conditions. Temperatures in these tests ranged from -120 to 60 C, and though the total energy required to induce strain does vary with workpiece temperature and environmental pressure, the method remains predictable and controllable for the materials investigated. It is believed that this method will revolutionize manufacturing in-space as it not only continues to build upon the capabilities of the laser (sensing, marking, cutting, drilling, joining, and now forming) as an all-in-one tool, but also reduces the need to counteract forming forces as would be required in mechanical bending. In theory, all required stress to induce bending is generated through thermal gradient and strain within the workpiece, meaning that the need for reaction control and fuel expense on-orbit will be limited. Archimedes once stated, “Give me a lever long enough and a fulcrum on which to place it, and I shall move the world”. With a laser as our lever and our workpiece its own fulcrum, we can move the world’s manufacturing into space.

Laser