Improved high-temperature-strength nickel-base superalloy

Nickel-base superalloy has a strength of 20,000 psi at 2,200 degrees F, approximately double the strength of the strongest available cast nickel-base alloys. It is not subject to the formation of embrittling phases upon long time exposure at intermediate temperatures.

Freche, J. C.↗

Evaluation of coatings for cobalt- and nickel-base superalloys, volume 2

The final results of an oxidation-reduction rig evaluation of aluminide coatings are presented, as applied to 1N-100 and B1900 nickel-base and X-10 and WI-52 cobalt-base alloys. Burner rigs were used which operated on JP-5 fuel and air, producing a gas velocity of 0.85 (2000 to 2500 ft/sec) at the specimen's leading edge. One-hour heating cycles were used with three minutes of air blast cooling. Results of testing at temperatures ranging from T sub max of 1850 to 2050 F indicate that coated B1900 has the longest oxidation life at all temperatures, followed by IN-100X-40WI-52, based on a weight change criterion. Coatings on nickel-base alloys provided more than twice the life of coating on cobalt-base alloys at comparable temperatures. The coatings with higher aluminum content and comparable thickness had longer lives. Silicon appeared to be a beneficial additive in the nickel-base alloy coatings for long term, low temperature life, but not for short term, high temperature performance. Chromium was identified in all coatings. Extrapolating the life results obtained to 1600 F, all the selected coatings on the four alloys would be protective for at least 10,000 hours.

Moore, V. S.↗

Development of high temperature nickel-base alloys for jet engine turbine bucket applications

A program has been initiated to develop a material with superior properties at elevated temperatures for utilization in turbine blade applications. A nickel-base superalloy can provide the necessary high temperature strength by using the maximum capability of the three available strengthening mechanisms - intermetallic gamma prime precipitation (Ni3Al), solid solution strengthening with refractory and precious metals, and stable carbide formations through the addition of strong carbide forming elements. A stress rupture test at 2000 deg F and 15,000 psi was formulated to approximate the desired properties. By adding varying amounts of refractory metals (Mo, W and Ta) it was possible to statistically analyze the effects of each in a basic superalloy composition containing fixed amounts of Co, Cr, C, B, Sr, and Ni at three separate levels of AL and Ta. Metallographic analysis correlated with the mechanical properties of the alloys; those with few strengthening phases were weak and ductile and those with excessive amounts of intermetallic phases present in undesirable morphologies were brittle.

SUPERALLOY↗

New Trends in Coatings Developments for Turbine Blades: Materials Processing and Repair

Turbine engines for aeronautic applications now have to face strenuous requirements concerning not only operating performances but also reliability and repairability. This evolution of the specifications induces important consequences regarding the choice and the design of turbine blade protective coatings. This paper presents several key features concerning the deposition techniques and the real-life behavior of such coatings: (1) complex aluminides well suited to the protection against high temperature oxidation and hot corrosion of directionally solidified nickel-base superalloy turbine blades; (2) ceramic coatings used as thermal barriers - they have to exhibit both high resistance to thermomechanical fatigue and adequate smoothness; (3) processing techniques for thermal barriers, including plasma spraying, electron beam physical vapor deposition and plasma enhanced chemical vapor deposition; and (4) blades and coatings repair techniques.

S Alpérine↗

A Dispersion-Strengthened Low-Density Niobium Alloy and Its Elevated Temperature Mechanical Performance

In response to the elevated-temperature and weight-reduction demands of modern aerospace applications, a novel oxide-dispersion-strengthened low-density niobium alloy (LDNb-ODS) was fabricated using laser powder bed fusion (L-PBF). To overcome powder procurement barriers, L-PBF feedstock was produced by blending commercial Nb521, Ti64, and Cr powder with Y2O3 nanoparticles via resonant acoustic mixing. Following L-PBF and a 1400°C vacuum heat treatment, the alloy achieved a density of 6.73 g/cc and a fine mean grain size of 4.62 µm stabilized by uniform ~30 nm yttria dispersoids. Microstructural analysis revealed a chemically inhomogeneous build with lack-of-fusion defects and a titanium (Ti) shift from a nominal 31.5 wt% in the starting powder blend to 24.8 wt% in the printed part due to preferential Ti loss during printing. Elevated-temperature tensile testing demonstrated that LDNb-ODS maintained a superior specific yield strength of 60-85 MPa/(g/cc) up to 800°C, outperforming nickel-based alloys Ni625, Ni230, and GRX-810. Between 870°C and 950°C, its specific strength surpassed both Ni718 and Ni625. In rapid stress-rupture testing at 1093°C and 20.7 MPa, uncoated LDNb-ODS survived 21.4 hours (a tenfold increase over legacy C-103) while an R512E silicide coating extended rupture life to 84.8 hours, confirming that oxidation accelerates low-stress failure. These findings demonstrate that additive manufacturing of LDNb-ODS provides a viable, lightweight alternative to nickel-based superalloys for high-temperature (>850°C) aerospace components.

Low Density Niobium Alloy↗

Progress in superalloys

Strength and workability of high temperature nickel-base, cobalt-base, and cobalt-refractory metal superalloys

SUPERALLOY↗

Oxidation resistant iron and nickel alloys for high temperature use

Iron-base and nickel-base alloys exhibit good oxidation resistance and improved ductility with addition of small amounts of yttrium, tantalum /or hafnium/, and thorium. They can be used in applications above the operating temperatures of the superalloys, if high strength materials are not required.