Dopant Compensation within the Intrinsic Poly-Si Isolation Region in Poly-Si/SiOx Passivated IBC Si Solar Cells

We report on the effect of dopant compensation within intrinsic poly-Si regions between p- and n-type fingers of poly-Si/SiOx passivated interdigitated back contact (IBC) solar cells using intrinsic poly-Si as the isolation region between the doped poly-Si fingers. First, we show that dopants from the doped fingers contaminate the intrinsic gap, resulting in doping of the entire intrinsic gap and overlap of the dopant tails from each finger. Next, we show that despite this doping across the gap, shunting between the doped fingers does not occur. We show that this is a result of trap-assisted compensation creating a highly resistive intrinsic region, preventing shunt. We simulate shunt resistance across the gap based on local carrier concentration and deep trap density. We show that trap defects within the poly-Si enhance compensation between the dopant tails. We experimentally confirm these predictions by scanning spreading resistance microscopy of the gap showing ~20 um domain with resistivity ~10^7 ..omega.. cm. Additionally, Kelvin probe force microscopy are compared to finite element simulations which result in the same approximate shape for potential profile, indicating diode behavior across the isolation region. These results demonstrate the powerful effect that trap defects have within the poly-Si isolation region and suggest that precision patterning is not as essential as once thought.

dopant compensation↗

Non-Equilibrium Doping of Poly-Si:Ga/SiOx Passivating Contacts Solar Cells

In this contribution, we show that Ga-hyperdoped poly-Si/SiOx contacts are realized by pulsed laser annealing and post-hydrogenation. The motivation behind this work is to improve the inferior performance of boron-doped poly- Si/SiOx contacts when compared to the phosphorus-doped contacts. Here we used Ga as a novel p-type dopant to replace B, as B is known to accumulate at the interface between the oxide and the crystalline silicon and cause recombination. Due to a high diffusivity of Ga in oxide and a much higher segregation coefficient (Si:SiOx), Ga is shown to be immune to the oxide pileup phenomenon. However, Ga has a low solid solubility limit in Si (5x10^19 cm-3), which is not enough to form a low resistivity contact. To overcome this problem, we explored pulsed laser annealing via excimer laser by varying the laser energy densities and pulses. The passivation and electrical properties are studied systematically using photoluminescence (PL), secondary ion mass spectrometry (SIMS), and Van der Pauw-Hall measurements. We show an active Ga doping concentration above 1x10^20 cm^-3, which is above the solid solubility limit of Ga in Si. Good passivation quality is demonstrated with the highest implied Voc (iVoc) of 721 mV on single side polished samples. Furthermore, a low diode contact resistivity of ~22 m..omega.. cm^2 is obtained using Ti/Ag contacts, with minimal metal-to-semiconductor contact resistivity of 0.9 m..omega.. cm^2.

non-equilibrium doping↗

Hydrogen Transport from Dielectrics to poly-Si/SiOx Passivating Contacts Measured by Mass Spectrometry and Vibrational Spectroscopy

We demonstrate the relationship between Si solar cell passivation and hydrogen content of various passivating films, including hydrogenated amorphous silicon (a-Si:H), aluminum oxide (Al2O3), silicon nitride (SiNx) and combinations thereof. Through isotopic studies using quadrupole mass spectrometry (QMS), Fourier transform infrared spectroscopy (FTIR), and Raman spectroscopy, we determine how hydrogen content and stability within each type of film relates to final passivation quality of solar cell test structures. Si solar cells using polycrystalline silicon on silicon oxide (poly-Si/SiOx) passivating contacts are at the forefront of Si solar cell research and emerging as top performers within industrial production. Performance of passivating contact Si solar cells is largely determined by a parameter known as the open-circuit voltage Voc, which directly relates to material quality within the bulk of the device and at surfaces. High Voc is achieved when defects within the bulk crystalline silicon (c-Si) and at interfaces are passivated, preventing them from acting as charge carrier recombination centers. One of the most important means of passivating defects within Si solar cells is via hydrogenation, injecting the cells with large amounts of H to satisfy dangling bonds in the bulk and at interfaces. Hydrogen is especially important in deactivating a prevalent defect in industrial p-type devices which leads to decreased device performance over long-term exposure to light, called light-induced degradation (LID). Some of the most common materials used to supply H to devices are a-Si:H, Al2O3, and SiNx, which can contain very large amounts of H. Upon annealing at elevated temperatures, the hydrogen becomes mobile enough to find and disable defect sites. However, too much hydrogen can also be problematic, sometimes leading to an effect called light and elevated temperature induced degradation (LeTID). It has been shown that these films passivate the interfaces of poly-Si passivating contacts differently, leading to differing performance. Though Al2O3 is a well-defined dielectric material, SiNx can have many different values of x depending on precursor gases and deposition conditions. We observe different FTIR and Raman spectra from different SiNx over a range of x values films to determine the bonding environments within them and further correlate the relative concentrations of Si, N, and H to the stability of H within SiNx and the passivation performance of each film. Because deuterium is chemically identical to hydrogen within these systems, but gives different signals in FTIR and Raman spectroscopy as well as in QMS, isotopic substitution can be used as an excellent tool to probe the H within films. In addition to measuring the H and D bonding within films using FTIR and Raman spectroscopy, we will use such isotopic experiments to observe H and D movement out of these hydrogenating films at elevated temperatures using QMS to determine the stability of H bonding within such systems. With these films characterized based on elemental composition, we will relate such measurements to passivation quality of these films and combinations thereof on poly-Si/SiOx contact structures using quasi-steady state photoconductance decay measurements to obtain implied open-circuit voltage (iVoc) and saturation current density J0 values. Such investigations into the performance of different passivating films and film stacks will lead to greater understanding of dielectrics in semiconductor devices, further improvements in passivated contact design, and eventually, greater proliferation of renewable solar energy worldwide.

Al2O3↗

Controlled Dielectric Breakdown to Form Pinhole Passivated Contacts

This contribution explores a low-temperature route to forming dielectric pinholes to form poly-Si/dielectric/c-Si passivated contacts. The method utilizes controlled dielectric breakdown to form nanoscale pinholes in a thick (non-tunnelling) dielectric which, when annealed, allows dopant atoms to pass from doped poly-Si through the dielectric and into the c-Si wafer forming conductive pathways. We show that the pinholes can be repassivated with dopants and H diffusion which results in increased PL signals after processing. The method can be expanded to optimized dielectric passivation stacks (not just a single layer) and can be formed in parallel over the faces of the wafer in selected areas (only under the grid).

controlled dielectric breakdown↗

Self-Aligned Selective Area Front Contacts on Poly -Si/SiO x Passivating Contact c -Si Solar Cells

We report both polarity poly-Si/SiO x passivating contacts in a front/back device configuration may represent the next solar cell architecture after tunnel oxide passivating contacts (TOPCon) cells, but high parasitic absorption in the front poly -Si layer often limits its performance. This work explores a wet etching technique to remove the front poly -Si in the nonmetallized regions using self-aligned metal grids as an etch mask. We systematically examine various dielectric layers (SiN x ,Al 2 O 3 , and stacks thereof) to study the repassivation of the etched n + surface, and find that an SiN x /Al 2 O 3 passivation stack can effectively repassivate the etched surface, which we attribute to field-effect passivation from the positive fixed charge from the SiN x layer, and excellent chemical passivation property from Al 2 O 3 in the form of atomic H. We demonstrate a front/back poly-Si/SiO x passivating contact device, with an open-circuit voltage (V oc ) of 690 mV, short-circuit current density (J sc ) of 39.8 mA/cm 2 , fill factor of 78%, and power conversion efficiency of 21.4%. Furthermore, simulations using SunSolve and Quokka 3 show good agreement with both the optical and electrical properties of the experimental device. The power loss analysis reveals improvements in the optical loss from the back Ti adhesion and front SiN x layers would lead to a 23.5% device. Lastly, a techno-economic model compares the production cost of this improved cell with the current TOPCon cells. Our results highlight that further cost reductions in single-sided doped poly -Si layers are needed to compete with mainstream passivated emitter and rear cell, and TOPCon technologies.

14 SOLAR ENERGY↗

Measurement of Poly-Si Film Thickness on Textured Surfaces by X-Ray Diffraction in Poly-Si/SiOx Passivating Contacts for Monocrystalline Si Solar Cells

Polycrystalline Silicon on tunneling silicon oxide (poly-Si/SiOx) passivating contacts have shown great potential for the next-generation monocrystalline Si (c-Si) industrial photovoltaic technology. However, these cells typically suffer from strong parasitic absorption in the thick front poly-Si layer, which is designed to reduce metal-induced recombination. In previous work, we demonstrated an improved short-circuit current density, Jsc, by thinning the front poly-Si film in an SF6 plasma using the front metal grids as a self-aligned mask, but the sub - 100 nm thick poly-Si film is difficult to measure on an alkaline textured surface. Conventional optical techniques such as spectroscopic ellipsometry cannot be used due to the high scattering nature of the random pyramids. At poly-Si thicknesses below 50 nm, secondary electron microscopy (SEM) has difficulty distinguishing the poly-Si from the underlying c-Si substrate. Here, we demonstrate X-ray diffraction as an effective method to quantitatively measure the front poly-Si thickness. The thickness calculated from the diffraction peak height of the Si(111) crystallographic plane agrees well with the cross-section SEM analysis and simulations using SunSolve. We show that by thinning the front poly-Si from 200 to 60 nm, Jsc increased by 2.4 mA/cm2, while maintaining the same Voc. This led to an absolute efficiency gain of 1.73%. In addition, we also discuss possible reasons for the premature loss of passivation before the removal of all poly-Si, which prevented an even higher gain in Jsc.

light/electron beam induced current↗

Accelerated reliability tests of n + and p + poly-Si passivated contacts

We report on the stability of encapsulated, low-pressure chemical vapor-deposited phosphorus (n + poly-Si) doped and boron (p + poly-Si) doped poly-Si/SiO x passivated contacts by exposing the samples to three different accelerated tests: damp heat test, thermal cycling and ultraviolet exposure, adhering closely to the IEC 61215 standard. Outdoor testing was also performed by exposing the samples in the outdoor testing field at the National Renewable Energy Laboratory, and preliminary data accumulated for 1000 h from February to April of 2021 is reported. We studied non-metallized, thermally-metallized, and screen-printed n + and p + poly-Si by monitoring the effective minority carrier lifetime at the implied maximum power point using a Sinton lifetime tester, and recorded photoluminescence images before and after the exposure. Furthermore, the samples were found to be stable under all test conditions, which is encouraging for incorporation of these contacts in next-generation industrial silicon solar cells.

14 SOLAR ENERGY↗

Effective Dielectric Passivation Scheme in Area-Selective Front/Back Poly-Si/SiOx Passivating Contact Solar Cells

Explored different dielectric passivation schemes on lifetime samples after removing poly-Si completely. Showed that SiNx/Al2O3 had the best passivation properties on SiOx/n+ c-Si in diffused surface. Applied SiNx/Al2O3 stack on poly-Si/SiOx passivating contact device and showed large improvement in Jsc, with best device efficiency of 21.8%. Future work: CV measurement of dielectric stacks to obtain Qf and Dit.

dielectric↗

Fabrication of Poly-Si on Locally Etched SiOx as Passivating Contacts for c-Si Solar Cells

Proof-of-concept for polysilicon on locally etched oxide (PLEO) contacts. Room temperature approach (via MACE) to engineer pinholes decouples charge-carrier transport across contact from passivation scheme of choice. 19 and 17% PLEO devices fabricated on double-side textured and saw-damage etched n Cz wafers, respectively. Preliminary work on polysilicon on locally etched nitride/oxide (PLENO) contacts. 0.2 fA/cm2 achieved with p PLENO; contact displays Ohmic behavior but still very resistive due to low pinhole density.

c-Si↗

Damp Heat Degradation of Polycrystalline Silicon Passivated Contacts

After 1000 hours of damp heat exposure at 85% humidity and 85 C, LPCVD n-poly and p-poly are stable for both metallized and non-metallized regions whereas for PECVD, only n-poly is stable; PECVD p-poly suffers significant degradation and defects became more pronounced with exposure time; and PECVD p-poly degrades more than LPCVD p-poly with or without additional dielectric layers (i.e., SiNx + Al2O3 stack).

damp heat degradation↗

Effects of Plasma Etching on Dopant Compensation between p- and n-Type Poly-Si Fingers in Passivated Interdigitated Back Contact Solar Cells

Efficiencies surpassing 26% have been achieved for single-junction Si solar cells based on the interdigitated back contact (IBC) architecture. However, the possibility of lateral shunting between the doped fingers has limited industrial adoption thus far. To avoid this possibility of shunt, complicated patterning techniques of the doped rear fingers have been developed, but spreading can still occur through multiple pathways during cell processing. Patterning can be simplified by using masked plasma-enhanced chemical vapor deposition (PECVD), but spreading during deposition will also lead to contamination of the isolation region between doped fingers. We significantly reduce the effect of this spreading through a short, gentle plasma etching step, which enables a trap-assisted compensation mechanism to take effect more easily than without the plasma etch. These two effects combined allow for the use of a simple patterning technique while still maintaining a highly resistive region between the doped fingers, and will reduce the complexity of IBC cell fabrication overall.

atom probe↗

Novel Poly-Si:Ga/SiOx Passivating Contacts through Non-Equilibrium Doping

Poly-Si/SiOx passivating contacts are one of the key enablers for high-efficiency, low-cost c-Si solar cells. In recent years, record devices have reached efficiencies of 26% in the laboratory and 25% in the industry. The current cell structure utilizing a tunneling oxide passivating contact structure with a back phosphorus-doped poly- Si/SiOx passivating contact and a front boron diffused emitter suffers from large emitter recombination. Thus, replacing the front B diffused emitter with a p-type passivating contact is a route to overcome this deficiency. This gives rise to front/back poly-Si based passivating contacts. To address the low passivation performance of the B-doped poly-Si passivating contacts, we replace B with Ga as a novel p-type dopant to avoid dopant accumulation in the tunneling oxide, which is known to lead to large degradation loss in passivation quality. Here, we introduce a non-equilibrium method via pulsed laser melting to thermally melt and recrystallize the poly-Si and redistribute the dopants, achieving doping concentrations above the solid solubility limit (~4E19 cm-3). We demonstrate a good passivation quality with an iVoc of 721 mV with an active Ga doping concentration in poly-Si >1020 cm-3. Furthermore, we show a low contact resistivity of 33.2 +/- 9.3 mO cm2 using a diode model calculation. Finally, cross-section scanning spreading resistance microscopy was performed to determine the resistance profile across the non-homogeneously doped poly-Si layer.

c-Si↗

Trap-Assisted Dopant Compensation Prevents Shunting in Poly-Si Passivating Interdigitated Back Contact Silicon Solar Cells

Using a trap-assisted compensation model, we explain why polycrystalline Si (poly-Si) passivating contacts are able to achieve low leakage current between the doped fingers of interdigitated back contact (IBC) monocrystalline Si solar cells despite mixing of boron and phosphorus dopants in the isolation region. The fill factor of IBC solar cells is strongly affected by the electrical isolation region between n- and p-type fingers, as this region is critical in minimizing shunting losses. During fabrication of monocrystalline Si solar cells with poly-Si passivating contacts, the intrinsic poly-Si isolation region inevitably gets contaminated with both p- and n-type dopants. Using dopant profiles measured with time-of-flight secondary ion mass spectrometry and scanning probe measurements of the isolation region, we demonstrate that despite the dopant spreading during cell processing, a well-compensated region between the doped fingers exists that prevents shunting. The trap-assisted dopant compensation mechanism significantly widens the compensated region to tens of microns, where the residual dopant densities are below the trap density. This enables a high-resistivity region, resulting in low shunt current. Using one-dimensional (1-D) finite element diode simulations, we identify the design parameters and experimental conditions under which a sufficiently resistive region can form. Furthermore, our measurements of 2-D local resistivity and work function maps across the isolation region using scanning spreading resistance microscopy and Kelvin probe force microscopy demonstrate the existence of a highly resistive, wide compensated region and confirm our proposed compensation mechanism. For our structures, this region is ~25 µm in width within a ~150 µm wide finger isolation region with nearly 3 orders of magnitude higher resistivity than the regions dominated by a single type of dopant.

14 SOLAR ENERGY↗

Trap-Assisted Dopant Compensation Prevents Shunting in poly-Si Passivating Interdigitated Back Contact Silicon Solar Cells

Interdigitated back contact (IBC) solar cells achieve the highest efficiencies of single-junction architectures, but complicated patterning of the rear fingers and spreading of dopants during processing inhibit their mainstream adoption due to concerns of shunting between the IBC fingers. One method of simplifying patterning at the rear is by using contact masks combined with plasma-enhanced chemical vapor deposition (PECVD) or ion implantation. However, the intrinsic isolation region becomes contaminated during high-temperature annealing by lateral diffusion of dopants and during masked PECVD by spreading of dopant radicals through region between the mask and the substrate. Despite this contamination, we show through scanning spreading resistance microscopy and Kelvin probe force microscopy that a ~20 µm wide compensating region exists with high enough resistivity to prevent shunting. We model this p-i-n poly-Si system using two simulation models: a simple resistor model considering only the capture of charge carriers by trap defects in poly-Si to reduce the conductivity, and a more refined 1-dimensional finite element model using Poisson’s equation, drift-diffusion equations, and recombination of carriers. Using this model, we show that high defect density significantly decreases the current across the region between the p- and n-type fingers, preventing shunting.

atom probe↗

Fabrication of Poly-Si on Locally Etched SiOx as Passivating Contacts for c-Si Solar Cells

Polysilicon on silicon oxide (poly-Si/SiO x ) passivating contacts with predominant charge-carrier transport via pinholes were prepared with room temperature metal-assisted chemical etching. Pinhole areal densities in the range of 2.8 x 10^4 to 4.5 x 10^7 cm^-2 were imaged by SEM. Contact resistivity of 32 m-ohm-cm^2 and implied open circuit voltage of 729 mV were obtained for symmetric n+ poly-Si/SiOx grown onto randomly textured n-Cz. We also show preliminary data pertaining boron-doped polysilicon on nitride/oxide passivating contacts, with which we achieved implied open circuit voltage above 730 mV and recombination current of 0.2 fA/cm^2.

amorphous Si↗

Effective Dielectric Passivation Scheme in Area-Selective Front/Back Poly-Si/SiOx Passivating Contact Solar Cells

Despite the high efficiencies reached by heavily doped poly-Si/SiO x passivating contact solar cells, challenges like the high front parasitic absorption still limit their performance. Previously, we showed a wet etching technique using self-aligned metal grids to remove the front poly-Si in the non-metallized region. Here, we focus on the effective dielectric passivation on this tunneling oxide/n + in-diffused region. The effect of poly-Si thickness was studied to balance between the passivation quality and the current gain. We then compared various dielectric passivation schemes using SiN x , Al 2 O 3 , and stacks thereof via injection-level dependent lifetime and the transfer length method. We demonstrate a SiN x /Al 2 O 3 stack yielded the best passivation performance within device process limitation and obtained an improved front/back poly-Si/SiO x passivating contact device, with a short circuit current density of 41.8 mA/cm 2 and an efficiency of 21.8%.

anisotropic wet etching↗

Electron Paramagentic Resonance Investigation of Mechanism of Light- and Elevated-Temperature-Induced Degradation in Ga-doped Cz Si

We report on the electron paramagnetic resonance (EPR) spectra recorded at 6 K for Ga-doped Czochralski (Cz) Si in the initial stages of light- and elevated-temperature-induced degradation (LeTID). We show that the narrow-range EPR spectrum depends on the duration of simultaneous heat and light exposure. After prolonged LeTID, the EPR intensity increases at ~334 mT. The EPR signature at ~334 mT is characteristic of Si dangling bonds, and the increase in the dangling bond density can be attributed to the bulk and not the surface. Additionally, we show that the inverse of the minority carrier lifetime in Ga-doped Cz Si samples, measured by quasi-steady-state photoconductance (QSSPC) decay, correlates with the increase in the intensity of the Si dangling bond signal measured by EPR. Based on these observations, we put forth a hypothesis connecting H to LeTID and the corresponding defect structure.

Cz Si↗

Atomic structure of light-induced efficiency-degrading defects in boron-doped Czochralski silicon solar cells

Boron-doped Czochralski (Cz) Si is the most commonly used semiconductor in the fabrication of solar cells. The minority carrier lifetime of boron-doped Cz Si decreases upon exposure to light due to B–O-related defects, which reduce the performance of ~10 9 solar modules worldwide. Using electron paramagnetic resonance (EPR), we have identified the spin-active paramagnetic signatures of this phenomenon and gained insights into its microscopic mechanism. We found a distinct defect signature, which diminished when the degraded sample was annealed. The second signature, a broad magnetic field spectrum, due to the unionized B acceptors, was present in the annealed state but vanished upon light exposure. These observations show that, on degradation, nearly all the ~10 16 cm –3 B atoms in Cz Si complexed with interstitial O atoms, whereas only ~10 12 cm –3 of these complexes created defects that were recombination-active. The formation rate of these recombination-active defects correlated with the decay of the minority carrier lifetime. Furthermore, the line shape parameters linked these defects to both B and O impurities in Cz Si.

14 SOLAR ENERGY↗