Search NASA⌕ Search

Engineering topics

Nemeth, William

Publications and source records attributed to Nemeth, William.

At least 73 records · Page 4

Chemical Passivation of Crystalline Si by Al 2 O 3 Deposited Using Atomic Layer Deposition: Implications for Solar Cells

The atomistic-level mechanism for the chemical passivation of the monocrystalline Si (c-Si) surface with thermally annealed Al 2 O 3 was studied using in situ infrared spectroscopy and photoconductance decay measurements. Al 2 O 3 was deposited on high-lifetime, float-zone c-Si substrates using atomic layer deposition (ALD) from trimethylaluminum (TMA), and H 2 O or O 3 . Surface-sensitive attenuated total reflection Fourier transform infrared spectroscopy was used to monitor the c-Si/Al 2 O 3 interface, as well as the bulk of the Al 2 O 3 film during the entire process. Our results show that some surface Si–H bonds are preserved after the ALD of Al 2 O 3 on H-terminated Si. During the annealing step at 400 °C, restructuring occurs at the c-Si/Al 2 O 3 interface to form interfacial SiO x . Isotope labeling was used to differentiate interfacial SiD bonds on the c-Si surface from H incorporated in Al 2 O 3 . Within the sensitivity of our infrared setup (~10 13 cm –2 ), we did not observe any net migration of atomic H or D from Al 2 O 3 to the c-Si/Al 2 O 3 interface. To isolate the effects of chemical and field-effect passivation of Al 2 O 3 thin films, we carried out surface passivation studies on c-Si/SiO 2 /Al 2 O 3 stacks. We also annealed these stacks in different atmospheres to test the influence of annealing atmospheres on the chemical passivation of c-Si by Al 2 O 3 and observed that O 2 -containing atmosphere led to the best surface chemical passivation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Improving GaAsP/Si Tandem Solar Cells Using Silicon Passivated Contacts

The degradation of photocarrier bulk lifetime in Si wafer substrates during the heteroepitaxial growth of III-V materials has been widely reported and is known to limit the efficiency of III-V/Si tandem solar cells. There have been prior strategies to protect Si lifetime in III-V growth chambers, but most require the use of a protective layer that must be removed in subsequent device processing. It would be advantageous for protective layers to remain an active part of the device. In this work, we demonstrate that a polycrystalline silicon (poly-Si) passivated contact can protect the minority carrier lifetime of the Si base wafer during the organometallic vapor phase epitaxy of III-V materials on silicon substrates.

Exascale Computing Project↗

Pinhole Formation in Poly-Si/SiOx Passivating Contacts on Si(111)-Oriented Textures

Poly-Si/SiOx passivating contacts were grown on inverted pyramid and random pyramid textured wafers to investigate the hypothesis that pinhole formation is most susceptible at the valleys and edges of a textured surface. Tetramethylammonium hydroxide (TMAH) etching and electron beam induced current (EBIC) were used to assess pinhole formation and charge-carrier transport. Scanning electron microscopy revealed that TMAH etching can expose pinhole locations on textured surfaces. We show that pinholes may preferentially form at the vertices of inverted pyramids. Our TMAH and EBIC analyses on random pyramids show no preferential oxide breakup at the pyramid valleys.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Submicron Thickness Characterization of Poly-Si Thin Films on Textured Surfaces by X-Ray Diffraction for Minimizing Parasitic Absorption in Poly-Si/SiO2 Passivating Contact Cells

Poly-Si/SiO2 passivating contacts have shown great potential for industry-relevant next-generation solar cells. Previous work has demonstrated an improved Jsc from dry reactive ion etching in an SF6 environment, using front metal grids as a self-aligned mask. Here, we show an effective method to measure the front poly-Si thickness on an alkaline textured surface using X-ray diffraction. The calculated thicknesses are compared with cross-section SEM analysis and Quokka simulation. We show that by thinning the front poly-Si from 200 nm to 60 nm, Jsc increases by 2.4 mA/cm2, leading to an absolute efficiency gain of 1.73%. Finally, we discuss possible reasons for the premature loss of passivation before the removal of all poly-Si.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Effect of Surface Texture on Pinhole Formation in SiO x -Based Passivated Contacts for High-Performance Silicon Solar Cells

High-efficiency silicon solar cells rely on some form of passivating contact structure to reduce recombination losses at the crystalline silicon surface and losses at the metal/Si contact interface. One such structure is polycrystalline silicon (poly-Si) on oxide, where heavily doped poly-Si is deposited on a SiO x layer grown directly on the crystalline silicon (c-Si) wafer. Depending on the thickness of the SiO x layer, the charge carriers can cross this layer by tunneling (<2 nm SiO x thickness) or by direct conduction through disruptions in the SiOx, often referred to as pinholes, in thicker SiO x layers (>2 nm). In this work, we study structures with tunneling- or pinhole-like SiO x contacts grown on pyramidally textured c-Si wafers and expose variations in the SiOx layer properties related to surface morphology using electron-beam-induced current (EBIC) imaging. Using EBIC, we identify and mark regions with potential pinholes in the SiO x layer. We further perform high-resolution transmission electron microscopy on the same areas, thus allowing us to directly correlate locally enhanced carrier collection with variations in the structure of the SiO x layer. Our results show that the pinholes in the SiO x layer preferentially form in different locations based on the annealing conditions used to form the device. With greater understanding of these processes and by controlling the surface texture geometry, there is potential to control the size and spatial distribution of oxide disruptions in silicon solar cells with poly-Si on oxide-type contacts; usually, this is a random phenomenon on polished or planar surfaces. Such control will enable us to consistently produce high-efficiency devices with low recombination currents and low junction resistances using this contact structure.

14 SOLAR ENERGY↗

Isolating p- and n-Doped Fingers With Intrinsic Poly-Si in Passivated Interdigitated Back Contact Silicon Solar Cells

Polycrystalline silicon on silicon oxide (poly-Si/SiO x ) passivating contacts enable ultra high efficiency interdigitated back contact silicon solar cells. To prevent shunt between n- and p-type doped fingers, an insulating region is required between them. We evaluate the use of intrinsic poly Si for this isolation region. Interdigitated fingers were formed by plasma deposition of doped hydrogenated amorphous silicon through mechanically aligned shadow masks, on top of a full-area intrinsic amorphous silicon layer. High temperature annealing then crystallized the a-Si:H to poly Si and drove in the dopants. Two mechanisms were identified which cause contamination of the intrinsic poly Si gap during processing. During deposition of doped fingers, we show using secondary ion mass spectrometry and conductivity measurements that the intrinsic gap becomes contaminated by doped a-Si:H tails several nanometers thick to concentrations of ~10 20 cm -3 . Another source of contamination occurs during high-temperature annealing, where dopants desorb from doped regions and readsorb onto intrinsic a Si:H. Both pathways reduce the resistivity of the intrinsic gap from ~10 5 Ω·cm to ~10 -1 Ω·cm. We show that plasma etching of the a-Si:H surface before crystallizing with a capping layer can eliminate the contamination of the intrinsic poly-Si, maintaining a resistivity of ~10 5 Ω·cm. Lastly, this demonstrates masked plasma deposition as a dopant patterning method for Si solar cells.

14 SOLAR ENERGY↗

Influence of Tabula Rasa on Process- and Light-Induced Degradation of Solar Cells Fabricated From Czochralski Silicon

Monocrystalline Si solar cells are fabricated from Czochralski (Cz) Si, which contains 10 17 –10 18 cm -3 oxygen atoms. Cz Si undergoes degradation during high-temperature thermal processing steps, such as dopant diffusion to form the p - n junction. This degradation in the bulk minority carrier lifetime can be related to the formation of oxygen precipitates. We found that a high-temperature annealing process known as tabula rasa (TR) not only mitigates process-induced degradation via oxygen precipitate nuclei dissolution, but also modifies subsequent light-induced degradation. We report on the bulk carrier lifetime of n - and p -type Cz Si after TR, which homogenizes the interstitial oxygen in the bulk Si to its monoatomic form in either an N 2 or O 2 environment. A control sample, which was not subjected to a TR processing step, experienced severe process-induced degradation during a boron emitter thermal budget as oxygen precipitates were formed in the Si bulk. These precipitates could be imaged using photoluminescence. Additionally, samples that underwent a TR processing step prior to the boron emitter thermal budget show efficient gettering of metallic impurities compared to the control sample, which showed a decline in the implied open-circuit voltage after the gettering step. Furthermore, modification of the interstitial oxygen bonding by TR had a strong effect on the light-induced degradation kinetics. Instead of a typically observed monotonic decrease, minority carrier lifetime increases first, followed by a nonmonotonic decrease over a ~20 h period. Finally, we conclude that by modifying the interstitial oxygen bonding via TR pretreatment, p -type Cz Si wafers become substantially resistant to harsh solar cell processes and strongly modified light-induced degradation, which would open alternative ways to mitigate this degradation mechanism.

14 SOLAR ENERGY↗

Revealing the Nano-Scale Structure and Properties of Pinholes in SiOx Layers for POLO Contacts

In this contribution, we report on the charge collection characteristics of silicon photovoltaic devices with passivated contacts based on the c-Si/SiOx /poly-Si structure. Using electron-beam induced current (EBIC) imaging in plan-view and cross-section orientations, we find that charge collection in a device with a 1.5-nm-thick SiOx layer is fairly uniform in the p-n junction region and does not appear to be influenced by pyramidal surface texture. In contrast, a device with a 2.2-nm-thick oxide layer shows significant spatial variation in the charge-collection signal. The locations where we observe preferential collection of excess carriers is very sensitive to the processing conditions used to grow and breakup the SiOx passivation layer. In some cases the apexes of the pyramids exhibit reduced EBIC signal as the valleys between adjacent pyramids show the strongest collection. Other conditions yield enhanced charge collection at well defined spots on pyramid faces with no observable collection in the valleys.

EBIC↗

Reactive ion etched, self-aligned, selective area poly-Si/SiO 2 passivated contacts

Front/back poly-Si/SiO 2 contact devices suffer from low short-circuit current density, J sc , due to parasitic optical absorption in the front poly-Si layer. Thin poly-Si (~20 nm) allows for high J sc but is not compatible with screen-printed fire-through contacts. We therefore study the effects of post-deposition etching of a thick poly-Si (200 nm) front layer by reactive ion etching (RIE) using the metal grid lines as a self-aligned mask. We show that passivation is maintained in the device during RIE and that J sc is increased by a gain in the blue quantum efficiency response. However, our specific etching parameters cause non-uniform etching of the poly-Si leading to premature loss of passivation without optimal gain in J sc . Etched, unpassivated layers can be re-passivated with a H-containing dielectric layer leading to a gain in Jsc, open circuit voltage, V oc , Fill-Factor, FF, and efficiency.

14 SOLAR ENERGY↗

Scanning Kelvin Probe Microscopy: A Tool to Investigate Nano-Scale Doping Non-Uniformities in Poly-Si/SiOx Contacts: Preprint

Monocrystalline Si (c-Si) solar cells with passivated contacts based on the ultrathin SiOx and doped polycrystalline Si (poly-Si) layers in a poly-Si/SiOx/c Si structure show high solar cell efficiencies that are ~26%. Excellent surface passivation using these contacts is achieved via the combined effects of chemical passivation of the SiOx/c-Si interface by the SiOx layer and field-effect passivation from the heavily doped poly-Si layer. These contacts give best performance only when annealed to temperatures higher than 850 degrees C. Structural changes in the SiOx layer and dopant diffusion from poly-Si into the underlying c-Si wafer occur during this step which are hard to investigate using conventional characterization techniques. In this work we investigate poly-Si/SiOx contacts with both a 1.5 (tunneling transport) and 2.2 (pinhole transport) nm SiOx layer using atomic force microscopy techniques. Conductive AFM on n+-poly-Si/SiOx/p-Si structures show significant spatial variations for both contact types, likely due to non-uniformities in the poly-Si layer itself. The electrical and structural variations deeper into the contact were revealed by scanning Kelvin probe microscopy after precisely etching away the poly-Si and SiOx layers and few nanometers of c-Si surface. This etching was performed using tetramethylammonium hydroxide and dilute HF solutions. The resulting surface potential maps appear similar for both contacts, and show less than 500 nm size heavily-doped regions. However, further etching of the c-Si surface reveals these heavily-doped regions to be less than 200 nm deep for the 2.2 nm SiOx contact and greater than 200 nm deep for the 1.5 nm SiOx contact.

14 SOLAR ENERGY↗

Understanding the charge transport mechanisms through ultrathin SiO x layers in passivated contacts for high-efficiency silicon solar cells

We report on the microscopic structure of the SiO x layer and the transport mechanism in polycrystalline Si (poly-Si) passivated contacts, which enable high-efficiency crystalline Si (c-Si) solar cells. Using electron beam induced current (EBIC) measurements, we accurately map nanoscale conduction-enabling pinholes in 2.2 nm thick SiOx layers in a poly-Si/SiO x /c-Si stack. These conduction enabling pinholes appear as bright spots in EBIC maps due to carrier transport and collection limitations introduced by the insulating 2.2 nm SiO x layer. Performing high-resolution transmission electron microscopy at a bright spot identified with EBIC reveals that conduction pinholes in SiO x can be regions of thin tunneling SiO x rather than a geometric pinhole. Additionally, selectively etching the underlying poly-Si layer in contacts with 1.5 and 2.2 nm thick SiO x layers using tetramethylammonium hydroxide results in pinhole-like etch features in both contacts. However, EBIC measurements for a contact with a thinner, 1.5 nm SiO x layer do not reveal pinholes, which is consistent with uniform tunneling transport through the 1.5 nm SiO x layer. Finally, we theoretically show that reducing the metal to the c-Si contact size from microns, like in the p-type passivated emitter rear contact, to tens of nanometers, like in poly-Si contacts, allows lowering of the unpassivated contact area by several orders of magnitude, thus resulting in excellent passivation, as has been demonstrated for these contacts.

14 SOLAR ENERGY↗

Three-dimensional electronic resistivity mapping of solid electrolyte interphase on Si anode materials

Silicon is a promising candidate for the lithium ion battery (LIB) anode because of the order-of-magnitude improvement in capacity over current state-of-the-art graphite anodes. In systems featuring both C and Si anodes, electronic resistivity of the solid-electrolyte interphase (SEI) layer is a critical factor for preventing continuous electrolyte-decomposition reactions at the electrode/electrolyte interface. However, the in-situ measurement of SEI electronic resistance has been complicated by ion transport and electronic contributions from other parts of the battery circuit. Ex-situ measurements of SEI resistivity at microscopic scales are also lacking. We report on a nanometer-resolution three-dimensional technique that enables ex-situ mapping of electronic resistivity of SEI formed on a model single-crystalline wafer Si anode. Our novel experimental approach uses scanning spreading-resistance microscopy resistance imaging and mechanical depth profiling. In addition to resistance mapping, this method also provides an alternative technique for locating buried interfaces, where mechanical or electronic properties differ sufficiently between layers. Further validation of this method was obtained by resistance mapping of a reference sample with a designed a-Si:H layer stack of different doping concentrations. The results show relatively uniform lateral resistivity distribution of the SEIs but steep decreases in resistivity in the vertical direction. Resistivity vs. depth profiles are highly dependent on cycling conditions, but they generally show a resistivity decrease from the most superficial levels of SEI and a thickness increase with continued cycling prior to SEI stabilization. The most prominent resistivity increase was observed on SEI formed in Gen2 electrolyte (EC:EMC [3:7 by wt.] + 1.2 M LiPF6) with 10 wt% fluoroethylene carbonate additive; this result may partially explain the significant improvements of sustained electrochemical cycling and coulombic efficiency observed with this electrolyte additive. Our approach provides a novel and unparalleled three-dimensional approach in characterizing electronic resistivity, which contributes significantly to understanding SEI formation and the intrinsic properties critical to battery performance.

25 ENERGY STORAGE↗

Interfaces Between CdTe and ALD Al 2 O 3

In this work, we present a combination of X-ray photoelectron spectroscopy (XPS) and time-resolved photoluminescence (TRPL) to probe the details of interface formation between CdTe and alumina deposited by atomic layer deposition (ALD). Alumina ALD using water as the oxygen source causes the elimination of Te oxides that are initially present on air-exposed CdTe surfaces. TRPL on the resulting CdTe interface indicates some degree of passivation. On the other hand, postgrowth treatment of Al 2 O 3 /CdTe structures with CdCl 2 and oxygen causes regrowth of Te oxides. Some of these structures show improved lifetimes, thereby pointing toward a critical role for Te oxides in interfacial CdTe passivation by Al 2 O 3 . Lastly, direct measurement of band positions with XPS indicates that the passivation is caused primarily by chemical rather than field effect mechanisms.

14 SOLAR ENERGY↗

Tabula Rasa for n -Cz silicon-based photovoltaics

High-temperature annealing, known as Tabula Rasa (TR), proves to be an effective method for dissolving oxygen precipitate nuclei in n-Cz silicon and makes this material resistant to temperature-induced and process-induced lifetime degradation. Tabula Rasa is especially effective in n-Cz wafers with oxygen concentration >15 ppma. Vacancies, self-interstitials, and their aggregates result from TR as a metastable side effect. Temperature-dependent lifetime spectroscopy reveals that these metastable defects have shallow energy levels ~0.12 eV. Their concentrations strongly depend on the ambient gases during TR because of an offset of the thermal equilibrium between vacancies and self-interstitials. However, these metastable defects anneal out at typical cell processing temperatures =850 degrees C and have little effect on the bulk lifetime of the processed cell structures. Without dissolving built-in oxygen precipitate nuclei, high-temperature solar cell processing severely degrades the minority carrier lifetimes to below 0.1 millisecond, while TR-treated n-Cz wafers after the cell processing steps exhibit carrier lifetimes above 2.2 milliseconds.

14 SOLAR ENERGY↗

Effect of silicon oxide thickness on polysilicon based passivated contacts for high-efficiency crystalline silicon solar cells

In this paper, we have investigated the effect of SiO x thickness (1-3 nm) on the performance of polycrystalline (poly) Si/SiO x /monocrystalline Si ( c -Si) passivated contacts. Our results show that for both n- and p-type contacts, there is an optimum SiO x thickness of 1.4-1.6 nm for obtaining the highest implied open-circuit voltage ( i-V oc ) values of ~739 and ~700 mV, respectively. For contacts with SiO x thicker than 1.6 nm, the i-V oc drops due to reduced field-effect passivation. We attribute this to the fact that a thicker SiO x layer hinders the diffusion of both n- and p-type dopants into the c-Si wafer resulting in a junction that is very close to the c -Si/SiO x interface, which increases carrier recombination most likely due to the presence of defects at this interface. The resistivity measured through the metal/poly-Si/SiO x / c -Si stack is independent of SiO x thickness up to 1.6 nm, and increases exponentially by several orders of magnitude with further increase in SiO x thickness due to inefficient tunneling transport. Finally, the extent of metallization-induced degradation of the poly-Si/SiO x / c -Si contacts is worst for the thinnest SiO x investigated (~1 nm), and interestingly it is not completely mitigated even for a ~3 nm thick SiO x .

14 SOLAR ENERGY↗

Passivated contact formation using ion implantation

Methods for forming passivated contacts include implanting compound-forming ions into a substrate to about a first depth below a surface of the substrate, and implanting dopant ions into the substrate to about a second depth below the surface. The second depth may be shallower than the first depth. The methods also include annealing the substrate.

36 MATERIALS SCIENCE↗

Hydrogen passivation of poly-Si/SiO x contacts for Si solar cells using Al 2 O 3 studied with deuterium

Here, the interplay between hydrogenation and passivation of poly-Si/SiO x contacts to n-type Si wafers is studied using atomic layer deposited Al 2 O 3 and anneals in forming gas and nitrogen. The poly-Si/SiO x stacks are prepared by thermal oxidation followed by thermal crystallization of a-Si:H films deposited by plasma-enhanced chemical vapor deposition. Implied open-circuit voltages as high as 710 mV are achieved for p-type poly-Si/SiO x contacts to n-type Si after hydrogenation. Correlating minority carrier lifetime data and secondary ion mass spectrometry profiles reveals that the main benefit of Al 2 O 3 is derived from its role as a hydrogen source for chemically passivating defects at SiO x ; Al 2 O 3 layers are found to hydrogenate poly-Si/SiO x much better than a forming gas anneal. By labelling Al 2 O 3 and the subsequent anneal with different hydrogen isotopes, it is found that Al 2 O 3 exchanges most of its hydrogen with the ambient upon annealing at 400 °C for 1 h even though there is no significant net change in its total hydrogen content.

36 MATERIALS SCIENCE↗