Optimizing the quality factor of InP nanobeam cavities using atomic layer deposition

Abstract

Photonic crystal nanobeam cavities are valued for their small mode volume, CMOS compatibility, and high coupling efficiency-crucial features for various low-power photonic applications and quantum information processing. However, despite their potential, nanobeam cavities often suffer from low quality factors due to fabrication imperfections that create surface states and optical absorption. In this work, we demonstrate InP nanobeam cavities with up to 140% higher quality factors by applying a coating of Al 2 O 3 via atomic layer deposition to terminate dangling bonds and reduce surface absorption. Additionally, changing the deposition thickness allows precise tuning of the cavity mode wavelength without compromising the quality factor. This Al 2 O 3 atomic layer deposition approach holds great promise for optimizing nanobeam cavities that are well-suited for integration with a wide range of photonic applications.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Rahaman, Mohammad Habibur, Lee, Chang-Min, Buyukkaya, Mustafa Atabey, Harper, Samuel, Islam, Fariba, Addamane, Sadhvikas Jayachandra, Waks, Edo. 2024-05-01. Optimizing the quality factor of InP nanobeam cavities using atomic layer deposition. https://doi.org/10.1063/5.0190964

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Large language models for transportation research: Methodologies, state of the art, and future opportunities

The rapid rise of large language models (LLMs) is transforming transportation research, with significant advancements emerging between 2023 and 2025, a period marked by the inception and swift growth of adopting and adapting LLMs for various transportation applications. Despite these significant advancements, however, a systematic review and synthesis of the existing literature remains lacking. This paper aims to fill this gap by providing a comprehensive review of the methodologies and applications of LLMs in transportation. We explore key applications, including autonomous driving, travel behavior prediction, and general transportation-related queries, alongside LLM methodologies such as zero- or few-shot learning, prompt engineering, and fine-tuning. From the review, critical research gaps are identified. From the methodological perspective, many of the research limitations can be addressed by integrating LLMs with existing tools and refining LLM architectures. From the application perspective, research opportunities for LLMs to address various transportation challenges are also explored. By synthesizing these findings, this review not only presents the state-of-the-art LLM adoption and adaptation in transportation, but also proposes future research directions as well as insights and recommendations for policymakers and practitioners, paving the way for greater LLM-driven research innovations in transportation in the future.

42 ENGINEERING↗