Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solid state battery”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Visualizing diverse lithium growth and stripping behaviors in anode-free solid-state batteries with operando X-ray tomography

Anode-free solid-state batteries (SSBs), which eliminate the need for lithium metal use during cell assembly, have the potential to enable high energy densities and simplified manufacturing. However, the factors that control lithium growth/stripping at the anode current collector are not well understood. Here, we use operando X-ray microcomputed tomography to comprehensively image and quantify lithium deposition and stripping under various conditions in three different Li|Li 6 PS 5 Cl|current collector cells, revealing diverse behavior that depends on interface morphology, cell resistance, and solid-state electrolyte (SSE) microstructure. A cell with high resistance exhibits extensive lithium filament growth across the entire current collector interface, with filaments that grow around pre-existing pores in the SSE rather than lithium filling these pores. Lithium filament formation is partially reversible, with the cracks shrinking as lithium metal is stripped. Uniform lithium deposition is achievable at low current densities in low-resistance cells, whereas higher current densities in these cells cause an increase in interfacial roughness, which is correlated with subsequent filamentary growth at the edges of the cell. These results provide insight into filamentary vs. planar lithium growth and highlight that the evolution of lithium is sensitively dependent on SSE microstructure and electrochemical processes.

25 ENERGY STORAGE↗

Impacts of the Conductive Networks on Solid‐State Battery Operation

The micromorphology of composite cathodes is known to play a vital role in determining all-solid-state battery (ASSB) performance. However, much of our current understanding is derived from empirical observations, lacking a deeper mechanistic foundation. The “rocking chair” concept of battery chemistry requires maintaining charge neutrality, emphasizing the necessity of examining electrode micromorphology from the perspective of conductive networks. This study systematically investigates the microscopic electrochemical impacts of conductive network micromorphology by varying the Li + -to-e − channel ratio in cathodes comprising LiNbO 3 -coated LiNi 0.8 Co 0.1 Mn 0.1 O 2 , Li 6 PS 5 Cl, and carbon fibers. Utilizing multiscale synchrotron-based spectro-microscopy, we unravel that unbalanced Li + and e − conducting channels intensify charge polarization within active cathode particles and accelerate their degradation. A further model system with X-ray nano-tomography resolved e − and Li + channels indicates that spatially uniform and well-paired Li + and e − conducting channels are highly desirable as they could promote more uniform lithiation/delithiation, mitigating microscopic electrochemical polarization. Electrode-scale X-ray holotomography analysis reveals that the impact of conductive networks is particle-size-dependent, with smaller cathode particles being more significantly affected. These findings provide mechanistic insights into the interplay between conductive networks and all-solid-state battery operation, laying the groundwork for rational design and optimization of cathode architectures in future solid-state battery technologies.

36 MATERIALS SCIENCE↗

Stable Cycling of Sodium All‐Solid‐State Batteries with High‐Capacity Cathode Presodiation

Sodium all-solid-state batteries (NaSSBs) with an alloy-type anode (e.g., Sn and Sb) offer superior capacity and energy density compared to hard carbon anode. However, the irreversible loss of Na + at the alloy anode during the initial cycle results in diminished capacity and stability, impairing full-cell performance. Here, this study presents an easy-to-implement cathode presodiation strategy by employing a Na-rich material to address these challenges. Leveraging the high theoretical capacity and suitable voltage window, Na 2 S is chosen as the Na donor, which is activated by creating a mixed electron-ion conducting network, delivering a high capacity of 511.7 mAh g −1 . By adding a small amount (i.e., 3 wt.%) of Na 2 S to the cathode composite, a NaCrO 2 || Sn full cell demonstrated capacity improvement from 90.8 to 118.2 mAh g −1 (based on cathode mass). The capacity-balanced full cell can thus cycle to more than 300 times with >90% capacity retention. This work provides a practical solution to enhance the full-cell performance and advance the transformation from half-cell to full-cell applications of NaSSBs.

25 - ENERGY STORAGE↗

Deciphering the Conflict Between Ion and Electron Percolating Networks in Solid-State Battery Cathodes

High-energy- and power-density solid state batteries require an optimal cathode composition and microstructural arrangement of cathode active material, solid-state electrolyte, conductive carbon, and binder to simultaneously support lithium-ion transport, electron conduction, and storage capacity. The ion and electron conducting phases in solid-state cathodes counteract each other's percolating networks as their mass ratios increase or decrease relative to each other. Here, we investigate targeted mass ratio variations of argyrodite solid electrolyte and two different types of conductive carbon (particles and fibers) in composite LiNi0.8Mn0.1Co0.1O2 (NMC811) solid-state cathodes to ascertain the ionic-electronic tradeoffs in cathode performance. Through ionic and electronic conductivity measurements on composite cathodes, as well as rate-testing and cycling performance in full cells, it is shown that the conductive carbon fibers form a percolative electronic network within the composite at a lower mass ratio (3-5 wt%) than particulate carbon (>5 wt%). The threshold to achieve electronic percolation coincides with higher accessible capacity in the cathode as the active material particles become electronically connected. However, carbon loadings beyond this percolation threshold lead to increased ion transport resistance, arising from disruptions to ionic conduction pathways and degraded contact at the interface between the electrolyte and active materials. Imaging, spectroscopy, and physics-based models quantitatively describe the relationship between carbon and electrolyte compositions and the cell's capacity and rate performance through percolation theory. This work demonstrates the importance of quantitatively understanding percolating networks in solid-state cells and that strategic engineering of conductive carbon morphologies can further increase the energy- and power-density of solid-state cells.

25 ENERGY STORAGE↗

Revealing the Roles of CuF 2 /NiF 2 Incorporation in the Electrochemical Performance of FeF 3 Cathodes in Solid‐State Batteries

Mixed metal fluorides have been considered as a promising candidate to lower the voltage hysteresis of conversion-type iron fluoride cathodes, but their cycling stability is limited due to transition metal dissolution and interphase growth in liquid electrolyte batteries. Here, we study the role of incorporating CuF 2 and NiF 2 in the electrochemical performance of FeF 3 cathode in halide-based solid-state batteries to test whether we can transfer the kinetic benefit of low voltage hysteresis to solid-state batteries while using solid electrolyte to eliminate transition metal dissolution and stabilize the interphase. Synchrotron X-ray absorption spectroscopy results indicated the redox reactions are attributed to Cu 0 /Cu + and Fe 0 /Fe 2+ in 25CuF 2 -75FeF 3 and Ni 0 /Ni 2+ and Fe 0 /Fe 3+ in 10NiF 2 -90FeF 3 . While no apparent improvement in electrode kinetics can be observed, the incorporation of CuF 2 and NiF 2 can largely improve the cycling stability of FeF 3 cathodes. In conclusion, the results demonstrate the advantages of using solid-state concept to improve the cycling stability of conversion-type cathodes.

25 ENERGY STORAGE↗

Eliminating chemo-mechanical degradation of lithium solid-state battery cathodes during >4.5 V cycling using amorphous Nb2O5 coatings

Abstract Lithium solid-state batteries offer improved safety and energy density. However, the limited stability of solid electrolytes (SEs), as well as irreversible structural and chemical changes in the cathode active material, can result in inferior electrochemical performance, particularly during high-voltage cycling (>4.3 V vs Li/Li + ). Therefore, new materials and strategies are needed to stabilize the cathode/SE interface and preserve the cathode material structure during high-voltage cycling. Here, we introduce a thin (~5 nm) conformal coating of amorphous Nb 2 O 5 on single-crystal LiNi 0.5 Mn 0.3 Co 0.2 O 2 cathode particles using rotary-bed atomic layer deposition (ALD). Full cells with Li 4 Ti 5 O 12 anodes and Nb 2 O 5 -coated cathodes demonstrate a higher initial Coulombic efficiency of 91.6% ± 0.5% compared to 82.2% ± 0.3% for the uncoated samples, along with improved rate capability (10x higher accessible capacity at 2C rate) and remarkable capacity retention during extended cycling (99.4% after 500 cycles at 4.7 V vs Li/Li + ). These improvements are associated with reduced cell polarization and interfacial impedance for the coated samples. Post-cycling electron microscopy analysis reveals that the Nb 2 O 5 coating remains intact and prevents the formation of spinel and rock-salt phases, which eliminates intra-particle cracking of the single-crystal cathode material. These findings demonstrate a potential pathway towards stable and high-performance solid-state batteries during high-voltage operation.

Science & Technology - Other Topics↗

Control of Two Solid Electrolyte Interphases at the Negative Electrode of an Anode‐Free All Solid‐State Battery based on Argyrodite Electrolyte

Abstract Anode‐free all solid‐state batteries (AF‐ASSBs) employ “empty” current collector with three active interfaces that determine electrochemical stability; lithium metal – Solid electrolyte (SE) interphase (SEI‐1), lithium – current collector interface, and collector – SE interphase (SEI‐2). Argyrodite Li 6 PS 5 Cl (LPSCl) solid electrolyte (SE) displays SEI‐2 containing copper sulfides, formed even at open circuit. Bilayer of 140 nm magnesium/30 nm tungsten (Mg/W‐Cu) controls the three interfaces and allows for state‐of‐the‐art electrochemical performance in half‐cells and fullcells. AF‐ASSB with NMC811 cathode achieves 150 cycles with Coulombic efficiency (CE) above 99.8%. With high mass‐loading cathode (8.6 mAh cm −2 ), AF‐ASSB retains 86.5% capacity after 45 cycles at 0.2C. During electrodeposition of Li, gradient Li‐Mg solid solution is formed, which reverses upon electrodissolution. This promotes conformal wetting/dewetting by Li and stabilizes SEI‐1 by lowering thermodynamic driving force for SE reduction. Inert refractory W underlayer is required to prevent ongoing formation of SEI‐2 that also drives electrochemical degradation. Inert Mo and Nb layers likewise protect Cu from corroding, while Li‐alloying layers (Mg, Sn) are less effective due to ongoing volume changes and associated pulverization. Mechanistic explanation for observed Li segregation within alloying Li x Mg layer is provided through mesoscale modelling, considering opposing roles of diffusivity differences and interfacial stresses.

Wang, Yixian [Materials Science and Engineering Pr↗

Texture Evolution of Plated Lithium in Anode-Free Solid-State Batteries

Here, this study investigates lithium plating texture in anode-free solid-state batteries using synchrotron-based X-ray diffraction. Conventional methods are limited by lithium’s low electron density and softness, which hinders direct interrogation in anode-free solid-state batteries. Results reveal that lithium plating texture is influenced by temperature and current density. Under mild conditions, lithium exhibited a ⟨110⟩ fiber texture. However, higher current densities and elevated temperatures led to a more randomized orientation, suggesting a dependence on plating conditions. The results highlight how the operating and processing conditions for lithium metal can influence the texture of lithium metal and reversible operation.

36 MATERIALS SCIENCE↗

A Dendrite-Resistant Sodium/Porous-Carbon Anode for Solid-State Batteries – Strategies and Challenges for Low-Pressure Operation

Sodium solid-state batteries (Na-SSB) have gained interest recently due to the abundance of Na over Li, but they still tend to fail due to dendrites under practical current densities and cycling capacities. To overcome this, Na-SSBs are frequently tested with impractically high applied pressure. In this work, a porous carbon interfacial layer is utilized in conjunction with Na-ß”-Al2O3 solid electrolytes to enable Na-cycling at milder cell pressures. This sodium/porous carbon layer enables improved solid-state Na cycling in symmetric cells, up to a current density of 10 mA cm-2 at 25 °C. Cycling up to 1 mAh cm-2 is challenging with low pressure, but 1 mAh cm-2 capacity can be reliably cycled at 1 mA cm-2 at an elevated temperature of 60 °C in symmetric cells. Finally, the evolution of the interface and sodium/carbon anode is evaluated with cryogenic ion-milling and cross-sectional imaging revealing that, depending on testing temperature, pressure, current density, and capacity, void formation, Na-extraction from porous carbon, delamination of the porous carbon matrix, or a combination of these occurs at the interface between Na-metal and BASE. Despite this, excellent dendrite resistance is achieved, and a full-cell design utilizing a Na-transition metal oxide cathode is still able to achieve an areal capacity of ~ 2.7 mAh cm-2 at 0.125 mA cm-2. This work demonstrates an alternative pathway toward a Na-metal anode for Na-SSBs without the requirement of excessive stack pressure.

low-cost↗

Pushing the Limits: Maximizing Energy Density in Silicon Sulfide Solid‐State Batteries

Here, for the first time, we demonstrate a silicon solid-state battery (SSB) architecture that achieves >400 Wh kg −1 , approaching the theoretical limit for silicon-based SSBs. This configuration features a 99.9 wt% micro-Si, a thin sulfide solid electrolyte (SSE), and a high-loading NMC811. Key to these results is strategically selecting and evaluating the processing techniques, whether wet or dry, for the negative electrode, positive electrode and thin sheet-type SSE. Excessive lithium incorporation into the silicon host, beyond the Li 3.75 +Si phase to form a LiSi composite, is essential to match the high capacity of the positive electrode. This SSB achieves over 1000 cycles for a 2 mAh cm −2 with ≈80% capacity retention and 94% capacity retention for 3 mAh cm −2 over 500 cycles at 25 °C. Post analysis identifies the primary capacity decay mechanisms as oxidation at the NMC/SSE interface and structural disruptions within NMC. Meanwhile, the Si electrode maintains a robust solid-electrolyte interphase layer, minimizing capacity decay. This study highlights the necessity for improved NMC coatings, lattice oxygen stabilization, and a durable positive electrode-electrolyte interface to improve the long-term stability of SSBs. Strategies leading to a single-layer pouch cell SSB exceeding 400 Wh kg −1 are developed.

25 ENERGY STORAGE↗

Interface diagnostics platform for thin-film solid-state batteries

Understanding the impedances of battery materials and their interfaces remains a major challenge, usually addressed by electrochemical impedance spectroscopy (EIS) where frequency-dependent complex impedance of full battery cells is measured and then modeled by a network of connected electrical elements. As conventionally applied, this approach produces ambiguity in that (1) multiple different network configurations may fit the data convincingly and (2) the method offers no direct association of the electrical elements with physical features of the battery. Here we present a new methodology that resolves both sources of ambiguity, enabled by expanding the experimental scope to directly inform the configuration of elements and their parameters in the network model. We demonstrate this methodology using thin film fabrication of solid state battery devices patterned by shadow masked sputter deposition, so that diagnostic devices corresponding to individual interface and material components can be fabricated simultaneously with full cell batteries. EIS models for the diagnostic devices can then be connected to form full cell networks whose topology matches the well-known physical configuration of the battery. When connected in this way, the full network model – made from connecting the diagnostic device EIS models – fits the full cell EIS data. For the case of a thin film solid state battery composed of amorphous silicon anode, lithium phosphorus oxynitride (LiPON) solid electrolyte, and lithium vanadium oxide (Li x V 2 O 5 ) cathode, we show that the approach allows us to identify ionic impedance/conductivity of the cathode/electrolyte as a limiting impedance and the anode/electrolyte interface cycling instability as a primary degradation factor.

25 ENERGY STORAGE↗

Solid-state batteries enabled by ultra-high-frequency self-heating

Solid-state batteries (SSBs) are promising next-generation batteries due to their high energy density and enhanced thermal stability and safety. However, their sluggish kinetics and transport at room temperature result in high internal impedance and critically reduce the attainable discharge energy density. Taking advantage of their strong temperature-dependent ionic conductivity, here we introduce ultra-high-frequency (greater than 105 Hz) self-heating (UHFSH) of SSBs, which can rapidly warm up the batteries from room temperature to operating temperature (∼65°C) in less than a minute. As proof of concept, UHFSH experiments were conducted on symmetric solid-state cells with lithium aluminum germanium phosphate electrolyte in different configurations. Using an experimentally validated model, pack-level simulations predict fast heating (50 K/min) and minimized heating energy consumption (less than 4%). Without any modification of the materials or structure of the batteries, our non-intrusive self-heating strategy potentially enables SSBs to discharge more than 2-fold energy in 25°C ambient.

pulse heating↗

All‐Solid‐State Batteries With Mechanically Stable Interfaces Consisting of a Zero‐Strain Cation‐Disordered Rocksalt Cathode

Interface stabilization is critical to the development of working all‐solid‐state batteries. Rigid cathode/solid electrolyte interfaces often disintegrate due to anisotropic volume change of cathode‐active materials, resulting in irreversible capacity loss. Herein, we demonstrate that Li 1.211 Mo 0.467 Cr 0.3 O 2 (LMCO), a pioneering cation‐disordered rocksalt oxide (DRX) cathode that has intrinsically small volume change upon lithium intercalation, can be integrated with a thiophosphate‐based solid electrolyte for all‐solid‐state batteries. Interface stability of the all‐solid LMCO cell was investigated by electrochemical impedance spectroscopy, X‐ray micro‐computed tomography, and electron microscopy. Since LMCO was initially synthesized as a layered phase exhibiting a large volume change, interface disintegration can be observable in the early cycles. As layered LMCO phase‐transformed into DRX LMCO in subsequent cycles, reintegration of the interfaces occurs within a pressurized cell as a result of its zero‐stain behavior. Consequently, the DRX LMCO cathode maintains interface integrity, and thus electrical wiring, over an extended number of cycles, leading to improved capacity retention with small internal cell resistance.

DRX↗

Digital light processing of porous LLZTO scaffolds for Li-garnet solid-state batteries

Li 7 La 3 Zr 2 O 12 (LLZO)-based solid-state electrolytes (SEs) are promising materials for next-generation solid-state batteries. In this work, digital light processing (DLP), an emerging additive manufacturing technology, is employed to produce porous Ta-doped LLZO (LLZTO) scaffolds. The self-standing scaffolds are 100 μm thick and have 40% porosity. The scaffolds demonstrate symmetric cell cycling stability exceeding 1,500 h at 0.1 mA/cm2 current density, with a capacity of 0.1 mAh/cm 2 (1 h for each half cycle). At higher current densities, reversible soft shorts frequently happen, while immediate hard shorts are prevented due to Li dendrite growth being hindered by the tortuous pore network. In addition to the cycling stability, the phase stability of LLZTO is investigated during the post-printing thermal process for printing resin removal. We discovered that the LLZTO partially decomposes into Li 2 Zr 2 O 7 and other impurity phases from 400°C to 800°C, but the pure LLZTO phase is restored upon the completion of resin removal beyond 800°C.

Li-metal anode↗

Investigation of MgO additives on microstructure and properties of thin LLZO electrolytes for all-solid-state batteries

To realize high-energy density lithium lanthanum zirconate (LLZO)-based solid-state batteries (SSB), LLZO electrolytes should be fabricated with low thickness and high mechanical strength. An effective strategy for strengthening ceramic materials is to use additives. Here, we employed MgO nanopowders and fibers as additives for the thin LLZO electrolyte in order to improve the mechanical strength. The microstructure, mechanical properties, and electrochemical properties are characterized to investigate the effects of adding MgO and sintering time. The MgO remains at grain boundaries after sintering, making the microstructure of LLZO fine and uniform. The mechanical strength of the MgO-added LLZO was enhanced by more than 60% while maintaining high ionic conductivity (1 × 10 -4 S cm -1 ) at room temperature. Li symmetric cells using the MgO fiber–LLZO and MgO powder–LLZO exhibit 2 and 3 times higher critical current density (CCD) than those of pure LLZO, and a solid-state full cell exhibits stable cycling performance. Further, these results demonstrate that the use of MgO nanopowder or fiber as an additive for thin LLZO is beneficial for high-current density cycling, by improving mechanical properties and microstructure.

25 ENERGY STORAGE↗

Molecular Interlocking Multidimensional Modulations of Cathode‐Electrolyte Interface for Constructing High Energy Density Quasi‐Solid‐State Batteries

Gel polymers are regarded as a promising candidate electrolyte for lithium-metal quasi-solid-state batteries, primarily due to their high ionic conductivity and solid-liquid synergistic properties. However, challenges such as interfacial side reactions, limitations in Li + transport caused by interfacial issues, and leaching of transition metals from the cathode have yet to be effectively solved. Herein, a novel gel electrolyte modulation strategy based on electrostatic filler assembly is proposed to address the issues of ineffective capacity utilization and inadequate cycling stability of high-energy-density cathode materials in solid-state lithium-ion batteries. It constructs a 3D interpenetrating charge-bridge network that effectively tackles the phase-separation challenge between fillers and electrolytes at the molecular level. Meanwhile, the molecular interlocking structure effectively inhibits the electrolyte erosion. More critically, it optimizes and stabilizes the cathode-electrolyte interface film, which facilitates the conduction of Li + -ions through a size-sieving mechanism. Consequently, this strategy enables effective adaptation across diverse high-energy-density cathode materials with satisfactory capacity performance (170.4 mAh g −1 at 4.5 V/1 C for LiNi 0.6 Co 0.2 Mn 0.2 O 2 and 194.0 mAh g −1 at 4.3 V/1 C for LiNi 0.9 Co 0.08 Mn 0.02 O 2 ). In conclusion, this investigation offers a straightforward and effective reference for addressing the critical challenges of ionic transport and interface stabilization in the design of gel electrolytes.

cathode-electrolyte interface↗

Tailoring Binder Molecular Weight to Enhance Slurry-Cast NMC Cathodes for Sulfide Solid-State Batteries

We demonstrate for the first time the critical influence of binder molecular weight on the performance of slurry-cast lithium nickel manganese cobalt oxide (NMC) cathodes in sulfide-based all-solid-state batteries (SSBs). SSBs are increasingly recognized as a safer and potentially more efficient alternative to traditional Li-ion batteries, owing to the superior ionic conductivities and inherent safety features of sulfide solid electrolytes. However, the integration of high-voltage NMC cathodes with sheet-type sulfide solid electrolytes presents significant fabrication challenges. Our findings reveal that higher molecular weight binders not only enhance the discharge capacity and cycle life of these cathodes but also ensure robust adhesion and structural integrity. By optimizing binder molecular weights, we effectively shield the active materials from degradation and mechanical stress, significantly boosting the functionality and longevity of SSBs. These results underscore the paramount importance of binder properties in advancing the practical application of high-performance all-solid-state batteries.

25 ENERGY STORAGE↗

X-ray Micro-Computed Tomography for Structural Analysis of All-Solid-State Battery at Pouch Cell Level

Characterizing the microstructure of all-solid-state batteries (ASSBs) during fabrication and operation is vital for their advancement, particularly as scaling to pouch cell levels introduces challenges in probing large-scale microstructural evolution. This work highlights the potential of synchrotron X-ray micro-computed tomography (sXCT) as a nondestructive, rapid (<30 min), and high-resolution technique for visualizing and quantifying key microstructural features, including overhang, porosity, contact loss, active surface area, and tortuosity, in all-solid-state pouch cells. The large field of view (up to millimeters) of sXCT enables detailed analysis at an industry-relevant scale, bridging the gap between laboratory research and commercial applications. Furthermore, integrating realistic sXCT-derived 3D models into multiphysics simulations could provide insights into chemo-mechanical degradation, particularly at the edges of the pouch cells, offering a pathway for designing robust, high-performance ASSBs. This perspective establishes sXCT as an indispensable tool for advancing both the understanding and the engineering of next-generation energy storage systems.

25 ENERGY STORAGE↗