Modulated Structure-Electronic Coupling at Pt/CeOx–TiO2 Interfaces Boosts Low-Temperature Preferential CO Oxidation
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Carbonate formation presents a major challenge to energy storage applications based on low-temperature CO 2 electrolysis and recyclable metal–air batteries. While direct electrochemical oxidation of (bi)carbonate represents a straightforward route for carbonate management, knowledge of the feasibility and mechanisms of direct oxidation is presently lacking. Herein, we report the isolation and characterization of the bis(triphenylphosphine)iminium salts of bicarbonate and peroxybicarbonate, thus enabling the examination of their oxidation chemistry. Infrared spectroelectrochemistry combined with time-resolved infrared spectroscopy reveals that the photoinduced oxidation of HCO 3 – by an Ir(III) photoreagent results in the generation of the short-lived bicarbonate radical in less than 50 ns. The highly acidic bicarbonate radical undergoes proton transfer with HCO 3 – to furnish the carbonate radical anion and H 2 CO 3 , leading to the eventual release of CO 2 and H 2 O, thus accounting for the appearance of H 2 O and CO 2 in both electrochemical and photochemical oxidation experiments. Here, the back reaction of the carbonate radical subsequently oxidizes the Ir(II) photoreagent, leading to carbonate. In the absence of this back reaction, dimerization of the carbonate radical provides entry into peroxybicarbonate, which we show undergoes facile oxidation to O 2 and CO 2 . Together, the results reported identify tangible pathways for the design of catalysts for the management of carbonate in energy storage applications.
Adding small amounts of CO 2 or H 2 O to methane pyrolysis boosts hydrogen and carbon yieldsviacyclic catalyst regeneration, enabling efficient low-carbon hydrogen and crystalline carbon production.
Sodium-ion batteries offer low-cost energy storage solutions for the grid and electric vehicles, leveraging the established "rocking-chair" Li-ion design and the natural abundance of sodium. However, SIBs face challenges such as relatively lower voltage and capacity than lithium-ion batteries, as well as dependence on nickel resources. Here, in this work, a new nickel-free cathode material, Na 0.75 Li 0.08 Cu 0.25 Mn 0.66 O 2 , was designed and synthesized. This material has a capacity of ~125 mAh/g and an average discharge voltage of 3.5 V. Notably, more than one-third of the capacity arises from lithium substitution of Cu (~8 mol.%) and high voltage activation to 4.6 V. Multimodal synchrotron x-ray characterization combining spectroscopy, microscopy, and scattering reveal the capacity is primarily from the redox of copper and oxygen, with a minor contribution from the manganese redox. Lithium substitution alters the phase transition mechanism from a two-phase transition in P3-Na 2/3 Cu 1/3 Mn 2/3 O 2 to a solid-solution in Na 0.75 Li 0.08 Cu 0.25 Mn 0.66 O 2 , enhancing the reversibility of this material.
The redox behavior and speciation of cerium at mesoporous thin films composed of nanoparticles of indium tin-doped oxide (nITO) electrodes were characterized in pH 4.8, 0.1 M acetate buffer and both 0.1 and 1 M HNO 3 using electrochemical techniques and X-ray photoelectron spectroscopy. Anodic deposition of ceria species from Ce(III) to the nITO electrode was achieved under all solvent conditions via spontaneous condensation of electrochemically generated ceric hydroxide species. In 1 M nitric acid, the rate of CeO 2 dissolution is on the same order as CeO 2 deposition, resulting in negligible amounts of CeO 2 electrodeposited at the nITO surface. The cathodic stripping of CeO 2 from the nITO substrate deposited in 0.1 M nitric acid or pH 4.8 acetate buffer follows a 2-step process where Ce(IV)-oxide is initially reduced to an unstable Ce(III)-oxide species that rapidly undergoes acid catalyzed dissolution to yield soluble Ce(III) (aq) . These findings provide a foundation for the pH and anodic potential controlled deposition of CeO 2 thin films to ITO substrates, which can aid in the development of materials composed of ceria. As a result, they can also be used to infer likely analogous actinide redox behavior and speciation at these electrodes.
Hydrogen gas is a promising alternative to fossil fuels due to its high energy output and environmentally safe byproducts. Various morphologies of photocatalytic materials have been explored for high-efficiency H 2 production, for instance, quasi-1D nanoscroll structures that provide a larger surface-to-volume ratio. Recently, we predicted layer-by-layer formation of stable oxide nanoscrolls directly from dichalcogenide precursors, eliminating the need for costly formation of two-dimensional oxides for a roll-up synthesis of nanoscrolls. Here, in this study, we evaluate the suitability of those oxide nanoscroll materials—MoO 3 , WO 3 , PdO 2 , HfO 2 , and GeO 2 —for solar-driven photocatalytic H 2 production and storage. Using excited state theory coupled with Bethe–Salpeter equation simulations, we discern their electronic and optical properties as a function of interlayer scroll spacing and find them to be highly conducive for solar-driven photocatalysis. Additionally, using ab initio molecular dynamics simulations, we show that they are also suitable for H 2 storage as the nanoscrolls exhibit an effective trapping of hydrogen, even in the presence of defects and vacancies in the oxides. This work thus demonstrates the discovery of robust and tunable oxide nanoscrolls as materials for advancing solar-driven hydrogen technologies.
The potential of the H2-NiO battery for terrestrial applications was assessed. A multicell design approach that differs significantly from the aerospace individual pressure vessel was used. A number of experimental 100-Ah cells were built to evaluate the new design concepts and components. The experimental cells provided the input needed for a multicell battery design. It is found that new multicell H2-NiO battery has a number of potential advantages for aerospace applications such as the manned space station. The advantages are discussed, and a design concept is presented for a multikilowatt battery in a lightweight pressure vessel.
Metal oxide semiconductors are of interest as efficient, stable, and low-cost photoanode materials for photoelectrochemical water splitting, but their characteristically poor charge transport properties remain a fundamental challenge to practical use. Nanoporous metal oxide films that feature open bicontinuous networks of nanocrystals and nanopores can overcome such inefficient charge transport to enable high-performance photoanodes. Here, this paper describes a general method to make high-quality nanoporous films of metal oxides by spin coating and calcining molecular inks that contain a porosity-generating block copolymer. Phase-pure nanoporous films of BiFeO 3 , FeWO 4 , WO 3 , Fe 2 O 3 , and TiO 2 serve to demonstrate the versatility of the approach. It is demonstrated that the crystallite size, film porosity, and film thickness can be independently tuned by adjusting the ink composition and film processing conditions. The method is extended to fabricate core–shell nanoporous films consisting of a nanoporous film coated in a thin shell of a second metal oxide, using WO 3 –BiVO 4 and BiFeO 3 –BiVO 4 as examples. Given its simplicity and flexibility, this solution-phase route should prove useful for making nanoporous films of many different materials for a variety of applications, including energy conversion and storage, catalysis, and chemical sensing.
The vast, high-dimensional composition space of high-entropy oxides (HEOs) offers exceptional opportunities for functional materials discovery, yet it also poses a fundamental challenge: the rational and efficient prediction of stable, synthesizable compositions and the corresponding structure–property relationships. Despite growing interest, the field still lacks broadly applicable, physically grounded descriptors capable of navigating various large chemical spaces. Here, we introduce a Mixed Enthalpy–Entropy Descriptor (MEED) that enables rapid, first-principles–based prediction of HEOs synthesizability across diverse chemistries. Using MEED, we perform high-throughput screening of two distinct HEO families: rocksalt oxides and perovskite oxides. The predicted top candidates in each family were experimentally validated. MEED reveals unifying thermodynamic and structural principles governing stability across both chemical compositions and polymorphs, providing mechanistic insight into the formation of high-entropy phases. This work significantly broadens the accessible chemical design space for HEOs and establishes a data-efficient framework for accelerating the discovery of next-generation functional materials.
The oxidation behavior of a Ni–5Cr (at.%) alloy was evaluated at 420 ° C using the Rhines pack method and simultaneous tensile and compressive stress states via a miniature four-point bending fixture. At this moderate temperature, grain boundaries dominate mass transport and the resulting oxidation response. Oxidation produced approximately 1μm-wide protective Cr 2 O 3 films capping some grain boundaries and penetrative, intergranular Cr-rich oxides at other grain boundaries. Externally applied tensile and compressive stress during oxidation increased the prevalence of Cr 2 O 3 cap formation compared to no applied stress, with tensile stress resulting in more Cr 2 O 3 caps than compressive stress. The observed oxide cap morphology was similar across all test conditions. Regions under compressive stress showed an order of magnitude greater Cr depletion depth along the grain boundary. Chromium nitrides (CrN), likely from N contamination of the Rhines pack cell, were observed both at the oxide–metal interface and intergranularly within the alloy. Collectively these results demonstrate that applied stress promotes localized protective oxide cap formation over grain boundaries, with compressive stress additionally promoting deeper Cr depletion. Furthermore the experimental approach helped separate out the effects of stress on local oxide formation and grain boundary passivation.
Additive manufacturing has proven useful for introducing oxide particles into superalloys, to provide oxide dispersion strengthening (ODS) at high temperatures. This study screened how such an approach can influence microstructure and failure modes for superalloy 718. The objective of this study was to compare tensile and creep failure modes for additively manufactured superalloy 718 having introduced oxide particles. Fine yttrium-oxide (yttria) particles were introduced into 718 powder using two different powder mixing methods. Additive manufacturing by laser powder bed fusion was then used to prepare specimen blanks for each case, oriented parallel and transverse to the building direction. These were subsequently given consistent stress relief, hot isostatic pressurization, and final heat treatments, then subjected to tensile and creep tests at varied temperatures. Additively manufactured 718 without ODS (“no-ODS”) had nearly equiaxed grains at 50 μm in width. Roll-mixed ODS material had a bimodal grain size distribution, with fine grains at 9 μm and coarse grains at 66 μm in average width. The fine grains were elongated about 5x in the building direction. Acoustic-mixed ODS materials had grains at 10 μm in width that were elongated about 10x in the build direction. Compared to no-ODS, roll-mixed and acoustic mixed ODS materials did not show improved tensile strengths at room temperature, 760 °C, and 1093 °C. The tensile failure strains parallel to the building direction of roll-mixed ODS material were lowest in these tests. Flattened clumps of yttria had formed transverse to the building direction in roll-mixed material, which were easily cracked. Creep rupture response at 760 °C in the building direction was highest for acoustic-mixed material test. Creep tests at 1093 °C showed varied results, with low rupture lives associated with enhanced cavitation at grain boundaries and surface oxidation. Transverse to the building direction, all three materials had low failure strains in tests at 760 °C. The elongated grain boundaries failed readily in all transverse specimens tested at 760 °C and 1093 °C.
A stable steam supply is required for the operation of solid oxide electrolysis cells. Heated water bubblers are the most common method due to the simplicity and inherent safety of the method, however, several design challenges hinder effective implementation. Here, a stable and validated bubbler design is presented, capable of achieving very high steam concentrations, relatively high flow rates, and continuous operation. A piping and instrumentation diagram and bill of materials are provided to enable easy duplication. Critical design parameters are discussed, including safety considerations and materials requirements, which are applicable to any bubbler design. The practical implementation of bubblers is also presented, including methods to prevent condensation instability and reduce backpressure to achieve a stable steam supply. The 3″ x 6″ (7.6 cm × 15.2 cm) bubbler achieves up to 98% steam balance hydrogen at 200 sccm and up to 1 slpm at 96% steam.
A nonvolatile memory device based on protonic transport in oxides has been proposed. The mobile H+ ions are introduced into the SiO2 layer by annealing Si/SiO2/Si structures in H2 at temperatures greater than 500 deg C. This effect has only been observed for confined oxides that have been annealed at greater than or equal to 1100 C prior to the hydrogenation anneal. This includes buried oxides such as Unibond and SIMOX as well as thermal oxides annealed with a polysilicon cap. An applied field moves the charge within the oxide and the charge stops moving when the field is removed. In a memory device, the hydrogen-annealed oxide is the gate oxide and the position of the mobile charge is sensed by the shift of the I-V curve. Much is still not understood about the motion of the charge across the buried oxide. Previous work has assumed that H+ transport and the time it takes to traverse the oxide is governed by interactions within the bulk of the oxide. Based on parameters that affect the transport time, we conclude that H+ trapping and detrapping at the Si/SiO2 interface are more important than H+ interactions within the oxide bulk. These parameters include the applied field, the H+ concentration and the oxide thickness. One consequence is that projections of device write-time based on the previous assumptions of H+ transport mechanisms may be overly optimistic.
Silicon nitride turbine components are under intensive development by AlliedSignal to enable a new generation of higher power density auxiliary power systems. In order to be viable in the intended applications, silicon nitride turbine airfoils must be designed for survival in aggressive oxidizing combustion gas environments. Erosive and corrosive damage to ceramic airfoils from ingested sand and sea salt must be avoided. Recent engine test experience demonstrated that NT154 silicon nitride turbine vanes have exceptional resistance to sand erosion, relative to superalloys used in production engines. Similarly, NT154 silicon nitride has excellent resistance to oxidation in the temperature range of interest - up to 1400 C. Hot corrosion attack of superalloy gas turbine components is well documented. While hot corrosion from ingested sea salt will attack silicon nitride substantially less than the superalloys being replaced in initial engine applications, this degradation has the potential to limit component lives in advanced engine applications. Hot corrosion adversely affects the strength of silicon nitride in the 850 to 1300 C range. Since unacceptable reductions in strength must be rapidly identified and avoided, AlliedSignal and the NASA Lewis Research Center have pioneered the development of an environmental life prediction model for silicon nitride turbine components. Strength retention in flexure specimens following 1 to 3300 hour exposures to high temperature oxidation and hot corrosion has been measured and used to calibrate the life prediction model. Predicted component life is dependent upon engine design (stress, temperature, pressure, fuel/air ratio, gas velocity, and inlet air filtration), mission usage (fuel sulfur content, location (salt in air), and times at duty cycle power points), and material parameters. Preliminary analyses indicate that the hot corrosion resistance of NT154 silicon nitride is adequate for AlliedSignal's initial engine applications. Protective coatings and/or inlet air filtration may be required to achieve required ceramic component lives in more aggressive environments.
To address the high cost, cobalt dependency, and resource constraints typical of conventional high-entropy oxide (HEO) anodes, this study reports the successful synthesis of two Co-free, six-component spinel-type HEOs(FeNiCrMnZnAl) 3 O 4 (HEO-Al) and (FeNiCrMnZnMg) 3 O 4 (HEO-Mg), via a sol-gel method. The distinct effects of Al 3+ and Mg 2+ incorporation on the electrochemical performance and lithium storage kinetics were systematically investigated. XRD, Raman, and TEM characterizations confirm that both materials possess a pure spinel phase, uniform particle size, and homogeneous elemental distribution. Notably, electrochemical evaluations reveal that HEO-Al delivers a superior reversible capacity of 480.7 mAh g −1 after 100 cycles at 0.1 A g −1 , and maintains 354.5 mAh g −1 after 1000 long-term cycles at 1 A g −1 , significantly outperforming HEO-Mg. Kinetic analysis indicates that HEO-Al exhibits lower charge transfer resistance, a higher Li + diffusion coefficient, and a pseudocapacitive contribution of up to 82%. Furthermore, these findings demonstrate that Al substitution effectively optimizes the structural stability and lithium storage kinetics of Co-free HEOs, providing a viable strategy for designing low-cost, highly stable HEO anode systems.
Abstract not provided.