At least 73 records · Page 4

Stabilizing Cathode–Electrolyte Interphase of Nickel-Rich Single-Crystal Cathodes for Lithium-Ion Batteries

Nickel-rich single-crystal (SC) layered oxides are promising cathode candidates for next-generation lithium-ion batteries (LIBs) owing to their high energy density and structural robustness against intergranular cracking. However, their intrinsic surface reactivity with liquid electrolytes accelerates parasitic reactions at the cathode–electrolyte interphase (CEI), leading to transition-metal dissolution, gas generation, and impedance buildup. In this work, we synthesized SC-Li x Ni 0.9 Mn 0.05 Co 0.05 O 2 (NMC9055, 1 ≤ x ≤ 1.2) using a eutectic-assisted method and investigated interface stabilization strategies. A nickel-deficient Li x Ni 0.6 Mn 0.2 Co 0.2 O 2 (NMC622, 1 ≤ x ≤ 1.2) coating was applied via evaporation-based deposition to suppress CEI degradation pathways. Structural and compositional analyses confirmed uniform shell formation and preserved particle integrity. Half-cell electrochemical testing against lithium metal revealed ∼10% higher capacity retention and improved reversibility compared with pristine SC NMC9055, particularly under high-voltage operation. In conclusion, these results highlight the critical role of controlled surface chemistry in mitigating CEI instability in nickel-rich SC cathodes, offering a pathway toward enabling durable high-energy LIBs.

Coating processes

Observation of N-rich solid-electrolyte interphase by ToF-SIMS.

Formation of a stable solid electrolyte interphase (SEI) between lithium electrodes and electrolyte upon multiple charge/discharge cycles is crucial to a long-term lithium-ion battery performance. Addition of LiNO3 to lithium bis (fluorosulfonyl) imide/poly(ethylene oxide) (LiFSI/PEO) electrolyte leads to a durable SEI that is electrically insulating yet highly conductive to Li ions, chemically and electrochemically stable, physically uniform, and mechanically robust. ToF-SIMS was used here in combination with sputtering by a gaseous cluster ion beam (GCIB) to examine how the addition of a small proportion of LiNO3 to the LiFSI/PEO electrolyte affects the SEI composition. Negative ion ToF-SIMS spectra of the cycled samples display an intense m/z 26 peak associated with the SEI. Exact mass assignments and isotopic ratios indicate that this peak should be assigned as (CN-)-C-12, with little to no negative secondary ion signal arising from (LiF-)-Li-7. This CN- signal appears to arise from an N-rich portion of the SEI adjacent to the Li electrode that is depleted in LiF relative to the bulk electrolyte. The dearth of LiF- (and LiF+ from the positive ion spectra) is unexpected because LiF has been identified in the SEI in similar samples. Finally, GCIB sputtering indicates that the SEI adheres more strongly to the Li electrode than to the LiFSI/PEO electrolyte.

Shavandi, Seyedeh Reyhaneh

The Solid Electrolyte Interphase Dispersion Can Predict Cycle and Calendar Lifetimes in Silicon Anodes for Lithium-Ion Batteries

The solid electrolyte interphase (SEI) plays a critical role in lithium-ion battery (LIB) anodes. It is responsible for passivating the reactive surface of lithiated anodes against degradation of the electrolyte which enables long cycle and calendar lifetimes for LIBs. This role is especially important in high energy density anodes like silicon, that undergo massive volumetric changes during electrochemical cycling. The mechanism by which the SEI performs this role, however, is not clear which makes designing an SEI to passivate silicon anodes impossible. Through decades of research, dozens of chemical species have been identified within the SEI ranging from inorganic solids to polymeric coatings all of which simultaneously exist in a 'mosaic' composition at the anode surface. This mosaic creates a highly dispersive environment in which electrostatic screening of the anode surface from the electrolyte is not always complete. Here, we present an electrochemical technique to directly test the dispersion at the anode surface. We use this technique to screen more than 20 different electrolytes against silicon anodes and find correlations between both the cycle life and calendar life. The insights from this study offer a new framework to think about the SEI and a rapid screening method to test novel electrode/electrolyte combinations.

battery

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory

Machine-Learning-Guided Insights into Solid-Electrolyte Interphase Conductivity: Are Amorphous Lithium Fluorophosphates the Key?

Despite decades of study, the identity of the dominant Li + -conducting phase within the inorganic SEI of Li-ion batteries remains unresolved. While the mosaic model describes LiF/Li 2 O/Li 2 CO 3 nanocrystallites within a disordered matrix, these crystalline phases inherently offer limited ionic conductivity. Growing evidence suggests that interfaces, grain boundaries, and amorphous phases may instead host the primary fast-ion pathways. Using diffusion-based generative structure prediction and machine-learning interatomic potentials (MLIPs), we investigate lithium difluorophosphate (LiPO 2 F 2 ), a key mixed-anion decomposition product of phosphorus- and fluorine-containing electrolytes. We identify a stable crystalline polymorph and demonstrate that the amorphous counterpart is conductive, with projected room-temperature σ ≈ 0.18 mS cm –1 and E a ≈ 0.40 eV. Here, this enhancement stems from structural disorder flattening the Li site-energy landscape and a low formation energy for Li-interstitial defects, which supplies additional mobile carriers. We propose amorphous mixed-anion Li-P-O-F phases as a promising conducting medium in the SEI, offering a specific target for engineering improved battery interfaces.

Zhong, Peichen [University of California, Berkeley

Solid-state prealkylation of electrode architectures to tune solid electrolyte interphase composition

Efficient electrochemical cycling of certain Si anodes is limited by irreversible Li consumption to form and continually reform the solid electrolyte interface (SEI) due to Si expansion/contraction and fracture. Prelithiation can compensate for these losses; however, the starting open circuit potential (VOC) becomes highly reducing and, therefore, the electrolyte reduction chemistry that influences the SEI composition can change. Herein, we compare SEI formation for electrodes prelithiated using Solid State Prealkylation of Electrode Architectures (SPEAR) versus traditional electrochemically lithiated architectures (ECLAR), focusing on SEI compositional changes as a function of stoichiometry (0.28 ≤ x ≤ 1.38 in LixSi). Increasing SPEAR prelithiation decreased the initial VOC of Si anodes vs. Li/Li+ from ∼3 V (Li0.28Si) to < 0.5 V for Li1.38Si, enabling simultaneous competitive reduction of EC, EMC, and LiPF6 at low potentials. Ex situ7Li and 29Si cross-polarization NMR and XPS reveal that SPEAR drives thicker SEI formation with substantially increased P/F contributions and a predominantly inorganic insoluble SEI (71.4% inorganic for Li1.38Si), consistent with accelerated LiPF6-derived POx/LiPFx/LiF formation relative to ECLAR analogs which exhibit carbonate-rich organic SEI compositions. Symmetric-cell EIS further indicates SPEAR-specific impedance features consistent with pore reduction (filling) during LixSi formation. In full cells, SPEAR prelithiation increases the initial coulombic efficiency (ICE) and accelerates SEI formation and stabilization with Li1.38Si reaching 99.4% coulombic efficiency (CE) by cycle 2.

Musgrove, Amanda [ORNL] (ORCID:0009000220910389)

Atomistic Modeling of the Interphase Structure between Alumina and Al12Fe2Cr Quasicrystal Approximant

Molecular dynamics simulations are performed to study the stability of an fcc metallic interlayer phase between an iron aluminide quasicrystal approximant (QCA) phase (84.2 Al, 5.7 Fe, 5.4 Ni, and 4.7 at.% Cr) and aluminum oxides (α-Al 2 O 3 and γ-Al 2 O 3 ). The presence of the interlayer phase was experimentally observed in some regions of the inner diameter surface of a TPBAR cladding tube. The simulations employed existing many-body (MEAM and EAM) interatomic potentials to describe atomic interactions in the interlayer and QCA phases, and Buckingham+Coulomb pair interactions for the alumina and between the alumina and the QCA (or fcc). Interface systems of QCA/alumina, fec/alumina, and QCA/fcc are modeled and the fracture energy of the interfaces is calculated. Based on the fracture energies, for the γ-Al 2 O 3 , both MEAM and EAM suggest that the fcc interlayer phase would not form. For the α-Al 2 O 3 , the MEAM predicts that the fcc phase would form, however, the EAM predicts that it forms only if the α-Al 2 O 3 is Al-terminated at the interface. For the O-terminated α-Al 2 O 3 , the EAM predicts the fcc phase would not form, consistent with the results for γ-Al 2 O 3 .

36 MATERIALS SCIENCE

Glassy interphases reinforce elastomeric nanocomposites by enhancing percolation-driven volume expansion under strain

For nearly a century, introduction of nanoparticles to elastomers has yielded extraordinarily tough nanocomposites that are critical to technologies from actuators to tires. The mechanisms by which this reinforcement occurs have nevertheless remained a central open question in material science. One widely debated hypothesis posits that strong interactions between polymer and particles induce "glassy bridges" that cement particles into a cohesive percolating network that resists elongation. Here, molecular dynamics simulations show that glassy particle shells do not primarily provide elongational cohesion. Instead, they amplify an underlying mechanism wherein competition between filler and elastomer networks causes the elastomer's volume to increase on deformation. This induces contributions from the elastomer's bulk modulus, which is of order 1000 times larger than its Young's modulus. These findings establish a unified understanding of low-strain reinforcement in filled elastomers as emanating from volumetric competition between coexisting particulate and elastomeric networks. This reframes and unifies our understanding of low-strain reinforcement, provides a clear-cut diagnostic for the presence of glassy bridging, and offers a new design principle for tough elastomeric nanocomposites.

Computational Physics (physics.comp-ph)

Improved interfacial li-ion transport in composite polymer electrolytes via surface modification of LLZO

Composite polymer electrolytes that incorporate ceramic fillers in a polymer matrix offer mechanical strength and flexibility as solid electrolytes for lithium metal batteries. However, fast Li + transport between polymer and Li + -conductive filler phases is not a simple achievement due to high barriers for Li + exchange across the interphase. This study demonstrates how modification of Li 7 La 3 Zr 2 O 12 (LLZO) nanofiller surfaces with silane chemistries influences Li + transport at local and global electrolyte scales. Anhydrous reactions covalently link amine-functionalized silanes [(3-aminopropyl)triethoxysilane (APTES)] to LLZO nanoparticles, which protects LLZO in air. APTES functionalization lowers the poly (ethylene oxide) (PEO)-LLZO interphase resistance to half that of unmodified LLZO and increases effective Li + transference number, while insulating Al 2 O 3 completely blocks ion exchange and lowers transference number and conductivity in PEO-lithium bis(trifluoromethanesulfonyl)imide (LiTFSI)-LLZO composites. Modeling an inner resistive interphase between LLZO and PEO surrounded by an outer conductive interphase explains non-linear conductivity trends. Solid-state 7 Li & 6 Li nuclear magnetic resonance shows Li + only exchanges between PEO-LiTFSI and some LLZO interphase, with no appreciable Li + transport through bulk LLZO. Surface functionalization is a promising path toward lowering the polymer-ceramic interphase resistance. This work demonstrates that local changes in Li + transport affect macroscopic performance, highlighting the intricate relationships between all interfaces in inherently heterogeneous composite polymer electrolytes.

25 ENERGY STORAGE

High-Voltage Sodium–Metal Batteries with Asymmetric Fluoroalkoxylated Organoborate Anion Chemistry

The high reactivity of sodium (Na) metal restricts its compatibility to ether-based electrolytes, while the poor oxidative stability of ethers precludes their coupling to high-voltage cathodes, fundamentally limiting the operating voltage and energy density of sodium–metal batteries (SMBs). We present here a coordination-asymmetry strategy to reconcile this thermodynamic mismatch by generating in situ an asymmetric fluoroalkoxylated organoborate anion, [FB(OCH(CF 3 ) 2 ) 3 ] − (BOF – ), via a Lewis acid–base adduct reaction in ether electrolyte. The asymmetric ligand architecture differentiates oxidative and fluorination pathways: oxidizable B–O moieties mediate controlled interfacial reconstruction, whereas the terminal B–F units supply fluorine for chemical passivation. This self-adaptive chemistry yields nanoscale, conformal, compositionally graded interphases: a boron-oxide/boron-oxycarbide-rich cathode-electrolyte interphase (CEI) that mitigates ether oxidation and a bilayered inorganic–organic solid–electrolyte interphase (SEI) that regulates Na deposition. The nanostructured interphases enable highly reversible Na plating/stripping with an average Coulombic efficiency (CE) of 99.98% and sustain stable 4.3 V operation of anode-free SMBs in oxidation-prone ether electrolytes. Furthermore, this work establishes asymmetric boron coordination as a molecular-level design principle for creating chemically adaptive interphases that overcome the redox asymmetry in energy-dense electrochemical systems.

Anions