Inhibiting inter-layer gliding in transition metal layered oxides through interphase engineering for sodium-ion batteries
Not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not provided.
Solid-state batteries (SSBs) promise a decisive advance beyond conventional Li-ion systems, yet their development remains constrained by persistent solid–solid interfacial instabilities that degrade performance and durability. Interfaces between solid electrolytes and both cathodes and Li metal often exhibit poor wettability, limited physical contact, and high charge–transfer resistance, leading to chemical decomposition, mechanical failure, and impedance growth. Overcoming these limitations requires interphase engineering with atomic-scale precision—capabilities that conventional coating methods cannot reliably deliver. Atomic layer deposition (ALD) and molecular layer deposition (MLD) uniquely meet this need by enabling ultrathin, conformal, and composition-tunable films that stabilize reactive surfaces, suppress parasitic reactions, and regulate Li-metal morphology. Importantly, this Perspective highlights ALD/MLD systems that have already demonstrated effectiveness in liquid-electrolyte cells and discusses how these validated strategies can be deliberately translated to solid-state architectures. By grounding future directions in experimentally proven concepts rather than speculative hypotheses, we outline how atomic- and molecular-scale design principles can accelerate the development of robust, high-performance SSB technologies.
Formation of robust solid/cathode electrolyte interphases (S/CEI) is vital for long-term stability and high-performance operation of lithium-ion batteries (LIBs), particularly under high voltage regimes. However, engineering electrochemically stable S/CEIs that effectively suppress interfacial side reactions remains a key challenge. Herein, we introduce a liquefied sulfur dioxide (SO 2 )– ionic liquid complex as a fluorine-free multifunctional electrolyte additive for the first time that significantly improves the formation of sulfate/sulfite-rich S/CEI layers at both graphite and NMC811 interfaces. The unique SO 2 -N coordination with a 1,2,4-triazolide-based ionic liquid enables homogeneous SO 2 dissolution, resulting in controlled SO 2 decomposition during the initial electrochemical cycle. This decomposition yields sulfur-rich interphase species that stabilize the electrolyte-electrode interface, reduce impedance growth, and lessen electrolyte decomposition. Electrochemical tests show significantly improved cycle life, reduced polarization, and increased Coulombic efficiency for both anodes and cathodes. XPS confirms the presence of SO 2 -derived surface species that contribute to interfacial stability. In conclusion, this approach highlights a new direction for interphase engineering using liquefied gas additives and opens pathways for sulfur-based S/CEI chemistry in advanced battery systems.
LiMnxFe1−xPO4 (LMFP) is a promising high-voltage, thermally stable, and earth-abundant cathode material, yet its practical application is limited by interphase instability and Mn dissolution. In this work, we systematically evaluate LiMn0.6Fe0.4PO4/graphite pouch cells using three electrolyte formulations including control carbonate electrolyte, control + 2 wt% vinylene carbonate (VC), and control + 2 wt% VC + 1 wt% 1,3,2-dioxathiolane 2,2-dioxide (DTD), to establish how electrolyte composition governs interphase chemistry and long-term degradation. Electrochemical testing shows that both additives are preferentially reduced prior to ethylene carbonate (EC) during cell formation, generating robust cathode-electrolyte interphase (CEI) and solid-electrolyte interphase (SEI) layers that suppress gas evolution and raise the first-cycle coulombic efficiency to 89.3%. Additionally, the dual-additive electrolyte delivers the most stable performance, retaining over 85% capacity after 600 cycles while minimizing impedance growth under long-term cycling at C/3 and 40 °C. Soft X-ray absorption spectroscopy confirms that VC + DTD effectively suppresses electrolyte oxidation at the cathode surface, and micro-X-ray fluorescence shows substantially reduced Mn dissolution and deposition on the graphite anode. Density functional theory simulations further provided insights into the structural and energetic influences of alkoxide species on the cathode surface, proposing a Mn2+ extraction mechanism. The combined experimental and computational findings establish a mechanistic link between electrolyte composition and interphase evolution, highlighting the effectiveness of electrolyte engineering for extending the operational lifetime of LMFP-based lithium-ion batteries.
By employing 3,5-bis(trifluoromethyl) pyrazole (TFMP) as an electrolyte additive in both aqueous and non-aqueous mediums, a versatile interphase strategy is achieved. This facilitates stable Zn anodes with improved efficiency and longer cycling life.
Aqueous zinc-ion batteries (AZIBs) offer a combination of safety and low cost, but they suffer from dynamic pH fluctuations that drive parasitic reactions and capacity fading. In this review, we report the current mechanistic understanding of the dynamic pH evolution across the electrolyte-electrode interface and its role in triggering interphase instability. We summarize advanced strategies to regulate pH, including electrolyte engineering, electrode surface modification, and interphase construction. We further discuss current methods for probing pH dynamics and outline potential future approaches for gaining deeper mechanistic and design insights.
The practical applications of lithium (Li) metal batteries (LMBs) are limited by challenges such as dendrite formation and unstable solid electrolyte interphase (SEI), especially at higher C-rates. Here, this study introduces melamine-coated Li metal anodes (LMAs), forming a Li 3 N-rich SEI layer that improves ionic conductivity and mechanical stability. The optimized melamine-coated LMA demonstrated uniform coverage resulting in denser Li deposition, nearly doubled cycle life (~148 cycles at 0.5 C, 1C = 4.1 mA cm -2 ), compared to Bare-Li. These findings emphasize that coating materials-induced beneficial SEI components could lead to improvement of LMB performance.
Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.
Conventional solid electrolyte interphases (SEIs) strongly adhere to micro-silicon (µ-Si) and crack under volume changes, causing poor cycling performance. Nano-silicon improves cycling performance but remains costly with limited calendar life. Here potentiostatic ageing tests demonstrate that both calendar and cycle ageing are governed by SEI cracking and dissolution with different relative contributions. When the system is not dominated by SEI dissolution, the relative calendar life of Si anodes could correlates positively with their cycle life. LiF-rich SEI that enables long cycle life in µ-Si is therefore expected to enhance calendar life as well. Using this framework, we screened electrolytes, SEIs and electrodes and validated them with full-cell storage. LiF-rich SEI minimizes cracking and dissolution, enabling μ-Si to achieve excellent calendar life, whereas nano-silicon suffers from SEI dissolution and needs reduced electrolyte–electrode contact for better calendar life. This work clarifies calendar-ageing behaviour and accelerates electrolytes and SEI development for long-life Si anodes.
An algorithm has been developed for the forced convective diffusion-reaction problem for convection inside and outside a droplet by a recirculating flow field hydrodynamically coupled at the droplet interface with an external flow field that at infinity becomes a uniform streaming flow. The concentration field inside the droplet is likewise coupled with that outside by boundary conditions at the interface. A chemical reaction can take place either inside or outside the droplet or reactions can take place in both phases. The algorithm has been implemented and results are shown here for the case of no reaction and for the case of an external first order reaction, both for unsteady behavior. For pure interphase mass transfer, concentration isocontours, local and average Sherwood numbers, and average droplet concentrations have been obtained as a function of the physical properties and external flow field. For mass transfer enhanced by an external reaction, in addition to the above forms of results, we present the enhancement factor, with the results now also depending upon the (dimensionless) rate of reaction.
An algorithm has been developed for time-dependent forced convective diffusion-reaction having convection by a recirculating flow field within the drop that is hydrodynamically coupled at the interface with a convective external flow field that at infinity becomes a uniform free-streaming flow. The concentration field inside the droplet is likewise coupled with that outside by boundary conditions at the interface. A chemical reaction can take place either inside or outside the droplet, or reactions can take place in both phases. The algorithm has been implemented, and for comparison results are shown here for the case of no reaction in either phase and for the case of an external first order reaction, both for unsteady behavior. For pure interphase mass transfer, concentration isocontours, local and average Sherwood numbers, and average droplet concentrations have been obtained as a function of the physical properties and external flow field. For mass transfer enhanced by an external reaction, in addition to the above forms of results, we present the enhancement factor, with the results now also depending upon the (dimensionless) rate of reaction.
Formation of a stable solid electrolyte interphase (SEI) between lithium electrodes and electrolyte upon multiple charge/discharge cycles is crucial to a long-term lithium-ion battery performance. Addition of LiNO3 to lithium bis (fluorosulfonyl) imide/poly(ethylene oxide) (LiFSI/PEO) electrolyte leads to a durable SEI that is electrically insulating yet highly conductive to Li ions, chemically and electrochemically stable, physically uniform, and mechanically robust. ToF-SIMS was used here in combination with sputtering by a gaseous cluster ion beam (GCIB) to examine how the addition of a small proportion of LiNO3 to the LiFSI/PEO electrolyte affects the SEI composition. Negative ion ToF-SIMS spectra of the cycled samples display an intense m/z 26 peak associated with the SEI. Exact mass assignments and isotopic ratios indicate that this peak should be assigned as (CN-)-C-12, with little to no negative secondary ion signal arising from (LiF-)-Li-7. This CN- signal appears to arise from an N-rich portion of the SEI adjacent to the Li electrode that is depleted in LiF relative to the bulk electrolyte. The dearth of LiF- (and LiF+ from the positive ion spectra) is unexpected because LiF has been identified in the SEI in similar samples. Finally, GCIB sputtering indicates that the SEI adheres more strongly to the Li electrode than to the LiFSI/PEO electrolyte.
Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.
The Parties are working together to utilize a one-step atmospheric microplasma reaction for the elimination of electrolyte degradation products and the relithiation of end-of-life cathode materials. This project aims to streamline the direct recycling process of battery components by reducing the required steps and time.
As NASA missions extend beyond low Earth orbit, increasing reliance is placed on carbon fiber reinforced polymer (CFRP) composites for spacecraft structures where mass efficiency, durability, and long-term reliability are critical. In service, these materials are subjected to a combination of ultraviolet radiation, vacuum, ionizing radiation, atomic oxygen, and extreme thermal excursions under sustained mechanical loading. Flight systems such as the Boeing Starliner and SpaceX Dragon employ external composite structures that will experience these environments for extended durations. Although prior spaceflight and ground studies have reported limited changes in bulk mechanical properties, the synergistic effects of these environments on composite microstructure, particularly at the fiber matrix interphase, remain insufficiently characterized and represent a potential qualification and reliability risk. This study investigates the effects of short-term cryogenic exposure on a radiation shielding carbon epoxy composite, SC2020, as a ground-based analog for space relevant thermal extremes. The SC2020 material system has previously flown on the International Space Station under the Materials International Space Station Experiment (MISSE) program. Composite specimens were exposed to liquid nitrogen for 6 and 24 hours and evaluated using a multiscale characterization framework that combined ASTM D3039 tensile testing, Atomic Force Microscopy (AFM) based interphase analysis, and helium gas permeability measurements. Tensile testing showed no statistically significant or permanent degradation in global strength or modulus following cryogenic exposure. In contrast, AFM measurements revealed reductions in interphase modulus, weakened adhesion, and increased nanoscale heterogeneity, indicating localized degradation mechanisms not captured by conventional bulk testing. Gas permeability measurements showed a progressive increase in helium diffusion with exposure duration, consistent with micro-void formation or partial interfacial debonding. The results indicate that cryogenic exposure initiates degradation at the fiber matrix interphase while leaving global mechanical properties largely unchanged over short durations. These findings underscore the importance of multiscale diagnostics for identifying early-stage damage mechanisms that may influence long term performance and qualification margins for spaceflight composite structures. The data presented establish a cryogenic baseline for comparison with forthcoming MISSE flight exposure results and support ongoing NASA Established Program to Stimulate Competitive Research (EPSCoR) efforts aimed at improving composite qualification methodologies, risk assessment, and reliability prediction for space environments.
A new optimized LiFSI–LiPF6 dual-salt controlled-solvation electrolyte (E-DS) is demonstrated to enable practical graphite||LiNi0.8Mn0.1Co0.1O2 cells (˜4.0 mAh cm?²) to achieve exceptional performance and safety under extreme conditions. By optimizing anion coordination with the smaller, more dissociating FSI? anion, the E-DS forms ultrathin, dense, and inorganic-rich electrode/electrolyte interphases that dramatically suppress solvent decomposition, transition-metal dissolution, and surface reconstruction compared to the conventional LiPF6/carbonate electrolyte. Consequently, E-DS cells deliver >78% capacity retention after 300 cycles at 60 °C, retain fast discharging capacity at 30 °C, and operate effectively at -20 °C. Most strikingly, fully charged full cells with E-DS, even under overcharging to 4.8 V, show a lower heat evolution in stable formulations — transforming a traditionally unstable high-voltage/high-temperature configuration into an intrinsically safe state. This work establishes a new benchmark for carbonate-containing electrolytes, simultaneously achieving high energy density, fast-discharging capability, wide-temperature operation (-20 to 60 °C), and outstanding thermal safety in nickel-rich lithium-ion batteries.
For anode‐free sodium batteries to achieve practical consideration, highly reversible chemistries require exceptional ≥99.95% coulombic efficiencies that maintain over prolonged cycling periods. To do so, consumption of this severely limited sodium inventory must be restricted while metal nucleation processes that comprise the in situ formed metal anode are improved. Herein, we describe a fluorine‐free carborane electrolyte that satisfies these criteria by emphasizing reductive stability and weakly coordinating anion behavior as design principles. We find this approach promotes the development of a thin, robust SEI chemistry rich in both organic speciation and boron. The electrolyte described herein exhibits ideal metal nucleation behavior on one‐micron thin carbonaceous current collector surfaces and achieves a metal deposition/stripping efficiency near parity for 400 cycles. This novel anode chemistry is introduced to anode‐free full cell configurations where 87% of the initial discharge capacity is retained after 1000 cycles at 2.0 C. In conclusion, post‐test characterization of deep‐cycled anode‐free cells reveals suppressed capacity fade in these systems is attributed to the chemical stability of the carborane anion.
All‐solid‐state batteries suffer from high interface resistance and lithium dendrite growth leading to low Li plating/stripping Coulombic efficiency (CE) of <90% and low critical current density at high capacity. Here, in this work, both challenges are simultaneously addressed and the Li plating/stripping CE is significantly increased to 99.6% at 0.2 mA cm −2 /0.2 mAh cm −2 , and critical current density (CCD) of > 3.0 mA cm −2 /3.0 mAh cm −2 by inserting a mixed ionic‐electronic conductive (MIEC) and lithiophobic LiF‐C‐Li 3 N‐Bi nanocomposite interlayer between Li 6 PS 5 Cl electrolyte and Li anode. The highly lithiophobic LiF‐C‐Li 3 N‐Bi interlayer with high ionic conductivity (10 −5 S cm −1 ) and low electronic conductivity (3.4×10 −7 S cm −1 ) enables Li to plate on the current collector (CC) surface rather than on Li 6 PS 5 Cl surface avoiding Li 6 PS 5 Cl electrolyte reduction. During initial Li plating on CC, Li penetrates into porous LiF‐C‐Li 3 N‐Bi interlayer and lithiates Bi nanoparticles into Li 3 Bi. The lithiophilic Li 3 Bi and Li 3 N nanoparticles in LiF‐C‐Li 3 N‐Li 3 Bi sub‐interlayer will move to CC along with plated Li, forming LiF‐C/Li 3 N‐Li 3 Bi lithiophobic/lithiophilic sublayer during the following Li stripping. This interlayer enables Co 0.1 Fe 0.9 S 2 /Li 6 PS 5 Cl/Li cell with an areal capacity of 1.4 mAh cm −2 to achieve a cycle life of >850 cycles at 150 mA g −1 . The lithiophobic/lithiophilic interlayer enables solid‐state metal batteries to simultaneously achieve high energy and long cycle life.